VGVitaliy P. Guro

Vitaliy P. Guro

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Vitaliy P. Guro has a total of 37 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    High-field narrow-gap electrochemical treatment of chloride-containing industrial wastewater: Organic contaminant transformation and foam-mediated phase separation

    by Vitaliy Guro, Sitorabonu Rasulova, Yodgorjon Safarov, Khabiba Talipova, Shuxrat Buxorov, Navruza Ubaydullayeva, Kutligul Kudiyarova, Adalat Sadikova, Zulfiya Usmonova, Gulnoza Nurjonova

  • Open Access

    Silica–Chitosan Composite Aerogels for Thermal Insulation and Adsorption

    by Xueli Mei, Shihao Li, Yaoyao Chen, Xueli Huang, Yali Cao, Vitaliy P. Guro, Yizhao Li

    The dissipation of energy in the form of heat causes a huge energy loss across the globe. Thermal insulation materials which reduce heat loss can alleviate the energy crisis. Among many thermal insulation materials, silica aerogels (SAs) have attracted extensive attention due to their high surface area, low density and low thermal conductivity. However, the applications of SAs are restricted by their mechanical fragility. In this paper, a series of different ratios of silica–chitosan composite aerogels (SCAs) were prepared by mixing sodium silicate aqueous solution and chitosan solution followed by freeze drying. The surface morphology of SAs, CAs and SCAs was studied by scanning electron microscopy (SEM). The specific surface area, pore volume and pore size of the composite aerogels were studied by N2 adsorption–desorption isotherms. The thermal conductivities, chemical structures, thermal stabilities and hydrophobicities of SAs, CAs and SCAs were tested and analyzed. In addition, the adsorption properties of SCAs were measured using different organic solvents. The results reveal that when the proportion of sodium silicate aqueous solution and chitosan solution is 1:1, the obtained SCA−1/1 has the best performance, with a low thermal conductivity of 0.0369 W/m·K, a large specific surface area of 374.7 m2/g, and good thermal stability. In addition, the prepared SCAs also have good hydrophobicity and absorption properties, with adsorption capacities of 6.7–9.4 g/g, which show great application potential in the fields of insulation and adsorption.


  • Open Access

    KINETICS OF THE REAGENT OXIDATION OF MOLYBDENUM DISULFIDE BY NITRIC ACID

    by Sitorabonu Rasulova, Vitaliy Guro, Matluba Ibragimova, Firuza Rakhmatkariyeva, Khayitali Adinaev, Umid Ernazarov, Gayrat Parmonov, Zokhidjon Rakhimjonov

  • RAW MATERIALS FOR MODIFIED HARD ALLOYS BASED ON TUNGSTEN CARBIDE

    by Chirchik City Jsc Almalyk Mmc, U.N. Ruziev, Uzbekistan, V.P. Guro, Tashkent Igic Asc Ruz, Kh.T. Sharipov, B.B. Kayumov, A.A. Niyazmatov, Chirchik City Llc Vocar

    JSC "Almalyk MMC" produces products from hard alloys, using as a raw material tungsten concentrate from its own industrial waste - leaching cakes. Another potential resource is tungsten ore from the Ingichki deposit. Objective. It was known that the purity of the raw material and the presence of grain growth inhibitors in the carbide components affected the structure. It was of interest to evaluate the effect of impurities and alloying components of hard alloys on their hardness, wear resistance, and structure. The objects of study were samples of tungsten-containing raw materials, alloying components of hard alloys - compounds of vanadium, rhenium, samples modified by them - hard alloys of the "tungsten carbide - cobalt" type. Methodology. Their physical and mechanical parameters (Rockwell hardness, relative wear resistance), structure (EMPYREAN XDR, SEM-EDS EVO-MA Carl Zeiss Oxford Instrum), elemental composition (ICP-Aligent 7500 IСP MS) were controlled. Results and discussion. Installed. that the hard alloys modified with vanadium and rhenium turned out to be ≈ 3% harder and up to 90-100% more resistant to wear, compared to the serial original unmodified sample. Conclusion. Additional cleaning of tungsten anhydride led to an increase in wear resistance: from 38.5% (alloy “modified with 5% rhenium”, to 57.0% (with a single cleaning) and 65.3% (with three cleanings) of the alloy “modified with 5% rhenium with additional cleaning”, relative to unmodified carbide.


  • Method of Extraction of Cadmium from Waste Cadmium Calcium Phosphate Catalyst

    by A. Jumanazarov, Institute of General and Inorganic Chemistry of the Academy of Sciences of the Republic of Uzbekistan, V. P. Guro

    JSC "NAVOIYAZOT" in the process of producing acetaldehyde uses the catalyst "Catalyst cadmium-calcium-phosphate (CCP-N)" TU 113-03-00209510-108-2006, at a temperature of 340-350 ° C and a pressure of 0.2- 5-0.7 atm. Its service life is 6 months, after which it must be replaced and stored. Meanwhile, it is a potential raw material for the synthesis of a new catalyst. Due to the toxicity of the component, there are practically no publications on the topic of its recycling, processing and production of CCP-N are highly specialized. However, the authors had previously managed to independently solve this problem, a necessary stage of their research was the testing of their own development in production - in JSC "NAVOIYAZOT". Purpose of the work: testing the developed method for extracting cadmium from spent cadmium-calcium-phosphate catalyst. The cadmium recovered from the spent CCP-N catalyst was sorbed on the C-100 Purolite resin. Control of the content of components: СdO, CaO, and Р2О5 was carried out on an ICP spectrometer Aligent 7500 IСP MS. Information was obtained on the yield of the product of processing the solubility of CCP-N, the efficiency of the selected precipitant of cadmium ions, and their sorption on the C-100 Purolite resin. The test result is positive. The effectiveness of the developed method for extracting cadmium was confirmed, with the registration of an application for a patent for it.

  • Kinetics of Molybdenum Disulfide Oxidation in Sodium Hypochlorite Solutions

    by S. Rasulova, Institute of General and Inorganic Chemistry of the Academy of Sciences of the Republic of Uzbekistan, V.P. Guro

    . The sulfide phase of ore minerals is passivated in the oxidizing conditions of hydrometallurgy. Overcoming passivation is an important stage and condition for their efficient processing. The aim of the work was to describe the kinetics of its oxidative leaching using the example of a Mo concentrate in a hypochlorite electrolyte. Samples of Mo concentrate (38% Mo in the MoS2 phase) were used. The concentration of Cu (II), Fe (III), Mo (VI), Re (VII) ions was determined photocolorimetrically and spectrometrically (AAS Perkin-Elmer 3030B, ICP-Agilent 7500 ICP MS); kinetic measurements were performed with compact discs made of molybdenum disulfide. The kinetics of the reagent oxidation of a sulfide mineral in a hypochlorite electrolyte, in the temperature range of 22-45 ° C, at atmospheric pressure, has been studied by the rotating disk method. The parameters of the kinetic equation of the leaching process were obtained: the order of the reaction in terms of the oxidant concentration and the activation energy of the process of solid-phase diffusion of molybdenum (VI) ions from the crystal lattice of the mineral in the composition of the molybdenite concentrate into the liquid phase of the solution.

  • Development of Solutions for Chemical Phosphating of Carbon Steel

    by F. Fuzaylova, Institute of General and Inorganic Chemistry of the Academy of Sciences of the Republic of Uzbekistan, V.P. Guro

    A consumer in Uzbekistan imports concentrates phosphating the surface of carbon steels, such as, for example, Foscon 35 and Foscon 35K. (Russia). Work has been done to create analogs from local raw materials. Having studied the physicochemical properties of the concentrates, a mechanism for the formation of protective phosphate coatings was suggested, and the components of a new phosphating composition were selected. The aim of the work was to develop a composition of a solution for chemical phosphating of the surface of carbon steel at the local resource base. Methods used: elemental chemical analysis, electrochemical and corrosion measurements, conditionally total acidity of solutions was measured according to TU 2149-205-10964029-2004 (Russia). The effect of temperature, pH of the medium, and the exposure time of the sample in the phosphating solution on the quality of the phosphate film was studied. As a result, a phosphating composition FK-1 was developed, functionally similar to imported concentrates Foscon 35 and Foscon 35K, based on local raw materials.

  • Fluidized Bed Pilot Furnace for Modibdenite Concentrate

    by Institute of General and Inorganic Chemistry of the Academy of Sciences of the Republic of Uzbekistan, X. Adinayev, Y. Safarov, V.P. Guro

    In the Rare Metals Processing Shop (CPRM) at the Almalyk MMC JSC, the technology for processing molybdenite concentrate (MOC) provides for the use of kaolin in the granulation charge for oxidative roasting in a drum furnace. Its composition: 8-10% kaolin, the rest is molybdenite concentrate (MOC). Kaolin reduces the Mo content in the cinder. Replacing it with an organic binder eliminates this disadvantage (dilution in Mo), but leads to sticking of the granules in the drum furnace. To avoid sticking, it is proposed to replace it with a furnace of a different design. In addition to kaolin as a binder for MOK, ashless, water-soluble polymers are known. Replacing kaolin with them leads to an enrichment in molybdenum of an industrial product - cinder, by 4-5%. However, for the implementation of such a project, a based selection of the appropriate binder on the local raw material base, modes of its use and replacement of the roasting furnace: drum - with a fluidized (fluidized) bed furnace is required. A binder SK, an alternative to kaolin, and modes of firing granules from a new charge composition with MOC in a fluidized bed furnace have been developed. The design of the fluidized bed furnace has been developed. The introduction of these developments will provide a higher content of Mo in the cinder, better recovery of Mo and Re from it, as well as a lower sulfur content in the cinder, and less time spent on roasting: 1 hour instead of 7 hours in the existing rotary kiln.

  • Alloying Hard Metals of Tungsten Carbide-Cobalt System with Vanadium and Rhenium to Improve Wear Resistance

    by Institute of General and Inorganic Chemistry of the Academy of Sciences of the Republic of Uzbekistan, U. Ruziev, U. Ernazarov, V.P. Guro

    Vanadium and rhenium modified samples of hard alloy systems WC-VC-Co, WC-ReC-Co (grade VK-6) are considered when testing their wear resistance and hardness, in comparison with the serial alloy VK-6. The samples of the groups differed in the content of vanadium and rhenium, and additional purification of the raw material. The reason for the reduced wear resistance of the VK-6 alloy, caused by the structural features and the presence of impurities, is revealed. Sample test results: WC-VC-Co alloys in the VC concentration range of 1.0-16.0% by weight, turned out to be ≈ 3% harder and 30-90% more resistant to wear; WC-ReC-Co alloys, at a ReC concentration of 1-5% by weight, turned out to be ≈3% harder and 38.5% more resistant to wear; additional purification of the W-raw material of the WC-ReC-Co alloy with a ReC concentration of 5% by weight, in comparison with the alloys: VK-6 and VK-6 modified with 5% rhenium without additional purification, increased wear resistance from 38.5% (alloy "VK-6 modified with 5% rhenium"), up to 57.0% (single) and 65.3% (three times purification) alloy "VK-6 modified with 5% rhenium with additional purification". Experimental-industrial tests of products - surfacing on turning tools made of VK-6 alloy with VC 3% wt., Revealed that they were 30-35% more resistant to wear than samples from the serial VK-6 alloy, with an equal content cobalt; this means an increase in the resource of the tool by 30-35%. It was recommended to introduce alloying and additional purification of tungsten raw materials.