Akira Kiyoi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Akira Kiyoi has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
- Katsumi Nakamura
Power Device Works, Mitsubishi Electric Corporation 3 , 1-1-1 Imajuku-Higashi, Nishi-ku, Fukuoka, Fukuoka 819-0192, Japan
3 shared publications Naoyuki Kawabata
Advanced Technology R&D Center, Mitsubishi Electric Corporation 1 , 8-1-1 Tukaguchi-Honmachi, Amagasaki, Hyogo 661-8661, Japan
3 shared publicationsYasufumi Fujiwara
Division of Materials and Manufacturing Science, Graduate School of Engineering, Osaka University 2 , 2-1 Yamadaoka, Suita, Osaka 565-0871, Japan
3 shared publicationsTakahide Umeda
Graduate School of Pure and Applied Sciences, University of Tsukuba, Tsukuba, Japan
2 shared publications- Daiki Soda
Mitsubishi Electric Corporation
1 shared publication - Kazuya Ishibashi
Mitsubishi Electric Corporation
1 shared publication
Latest Publications
- Open Access
- 19 May 2026
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 1191, 61-67
Carbon Vacancy Engineering on High-Temperature Annealing as a Cost-Effective Approach for Reverse Recovery Suppression in SiC-MOSFETs
A body diode is commonly employed as a free-wheeling diode to reduce costs of SiC components instead of an external Schottky barrier diode. However, one of the key issues is higher reverse recovery loss due to bipolar charge contribution to reverse recovery charge. In this study, we investigated the impact of high-temperature annealing on the characteristics of MOSFETs as a cost-effective approach to introduce minority carrier lifetime killers. The trap densities of Z 1/2 center and EH 6/7 center can be controlled by activation annealing temperature. Q rr of 1900°C measured at 150°C was significantly decrease by 67% compared to that of 1750°C attributed to the 89% suppression of Q BIP . However, reverse leakage current increased adversely with the activation annealing temperature. R on and V th increased with the activation annealing temperature. The trade-off of the annealing temperature worsened slightly compared to that of the doping concentration. It is still possible that high-temperature annealing represents a cost-effective approach to improve the reverse recovery characteristics of the body diode.
- 19 May 2026
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 1191, 61-67
Open AccessCarbon Vacancy Engineering on High-Temperature Annealing as a Cost-Effective Approach for Reverse Recovery Suppression in SiC-MOSFETs
A body diode is commonly employed as a free-wheeling diode to reduce costs of SiC components instead of an external Schottky barrier diode. However, one of the key issues is higher reverse recovery loss due to bipolar charge contribution to reverse recovery charge. In this study, we investigated the impact of high-temperature annealing on the characteristics of MOSFETs as a cost-effective approach to introduce minority carrier lifetime killers. The trap densities of Z 1/2 center and EH 6/7 center can be controlled by activation annealing temperature. Q rr of 1900°C measured at 150°C was significantly decrease by 67% compared to that of 1750°C attributed to the 89% suppression of Q BIP . However, reverse leakage current increased adversely with the activation annealing temperature. R on and V th increased with the activation annealing temperature. The trade-off of the annealing temperature worsened slightly compared to that of the doping concentration. It is still possible that high-temperature annealing represents a cost-effective approach to improve the reverse recovery characteristics of the body diode.
- Open Access
- 13 January 2026
- Published by Springer Nature in Communications Materials
- Vol. 7 (1) , 8
Advancing N-type doping in semiconductors through hydrogen-defect interactions
- 13 January 2026
- Published by Springer Nature in Communications Materials
- Vol. 7 (1) , 8
Open AccessAdvancing N-type doping in semiconductors through hydrogen-defect interactions
- 22 December 2025
- Published by AIP Publishing in Applied Physics Letters
- Vol. 127 (25)
Controlling two-dimensional electron gas density through surface states in ultra-thin-barrier AlGaN/GaN heterostructures
A method to control the two-dimensional electron gas (2DEG) density in AlGaN/GaN heterostructures through post-epitaxial device processing is investigated. This control was achieved by dielectric film deposition and subsequent annealing on an ultra-thin 5-nm Al0.22Ga0.78N barrier layer. The 2DEG density, estimated from sheet resistance assuming constant mobility, was found to be tunable from 8.3 × 107 cm−2 before dielectric film deposition to 4.5 × 1012 cm−2 after SiO2 film deposition and annealing. Hard x-ray photoelectron spectroscopy analysis confirmed a maximum shift of 0.8 eV in the surface pinning level, attributed to the dielectric film deposition and annealing. Numerical calculations indicate that for an AlGaN barrier layer thickness of approximately 5 nm, a surface pinning energy change of ∼0.8 eV can induce a 2DEG density variation of 6–8 orders of magnitude, supporting the validity of the experimental results.
- 22 December 2025
- Published by AIP Publishing in Applied Physics Letters
- Vol. 127 (25)
Controlling two-dimensional electron gas density through surface states in ultra-thin-barrier AlGaN/GaN heterostructures
A method to control the two-dimensional electron gas (2DEG) density in AlGaN/GaN heterostructures through post-epitaxial device processing is investigated. This control was achieved by dielectric film deposition and subsequent annealing on an ultra-thin 5-nm Al0.22Ga0.78N barrier layer. The 2DEG density, estimated from sheet resistance assuming constant mobility, was found to be tunable from 8.3 × 107 cm−2 before dielectric film deposition to 4.5 × 1012 cm−2 after SiO2 film deposition and annealing. Hard x-ray photoelectron spectroscopy analysis confirmed a maximum shift of 0.8 eV in the surface pinning level, attributed to the dielectric film deposition and annealing. Numerical calculations indicate that for an AlGaN barrier layer thickness of approximately 5 nm, a surface pinning energy change of ∼0.8 eV can induce a 2DEG density variation of 6–8 orders of magnitude, supporting the validity of the experimental results.
- 5 December 2023
- Published by American Physical Society (APS) in Physical Review B
- Vol. 108 (23) , 235201
How does hydrogen transform into shallow donors in silicon?
We conducted electron paramagnetic resonance (EPR) and cyclotron resonance studies on hydrogen-related donors (HDs) in silicon, whose origins have remained unclear for 50 years. In floating-zone silicon substrates irradiated with 2-MeV protons, followed by optimized annealing at and , we identified three original EPR spectral signals originating from HDs, labeled the MT1, MT2, and MT3 centers. The three centers exhibited a tetragonal symmetry around the axis and were classified into two types of HDs: a HD with a lower thermal stability and a normal single-donor nature/positive- nature (MT1), and a HD with a higher thermal stability and a double-donor nature/negative- nature (MT2 and MT3). Most importantly, the MT2 center revealed hyperfine interactions closely resembling the B3 EPR center with a tetragonal symmetry, which has been identified as a tetrainterstitial cluster, . Contrarily, we could not resolve any hyperfine interactions for the three MT centers. According to the experimental results, an atomistic model was proposed for the HDs based on the center weakly coupled with hydrogen atom(s). We deduce that different numbers of incorporated hydrogen atoms and/or different types of hydrogen bonding to generated the two types of HDs. These findings are the first step in understanding how hydrogen works as a donor in Si and offer important insights into the use of proton-irradiation doping processes in device applications.- 5 December 2023
- Published by American Physical Society (APS) in Physical Review B
- Vol. 108 (23) , 235201
How does hydrogen transform into shallow donors in silicon?
We conducted electron paramagnetic resonance (EPR) and cyclotron resonance studies on hydrogen-related donors (HDs) in silicon, whose origins have remained unclear for 50 years. In floating-zone silicon substrates irradiated with 2-MeV protons, followed by optimized annealing at and , we identified three original EPR spectral signals originating from HDs, labeled the MT1, MT2, and MT3 centers. The three centers exhibited a tetragonal symmetry around the axis and were classified into two types of HDs: a HD with a lower thermal stability and a normal single-donor nature/positive- nature (MT1), and a HD with a higher thermal stability and a double-donor nature/negative- nature (MT2 and MT3). Most importantly, the MT2 center revealed hyperfine interactions closely resembling the B3 EPR center with a tetragonal symmetry, which has been identified as a tetrainterstitial cluster, . Contrarily, we could not resolve any hyperfine interactions for the three MT centers. According to the experimental results, an atomistic model was proposed for the HDs based on the center weakly coupled with hydrogen atom(s). We deduce that different numbers of incorporated hydrogen atoms and/or different types of hydrogen bonding to generated the two types of HDs. These findings are the first step in understanding how hydrogen works as a donor in Si and offer important insights into the use of proton-irradiation doping processes in device applications.- 22 March 2022
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 131 (12) , 125702
Annealing-temperature-dependent evolution of hydrogen-related donor and its strong correlation with X-photoluminescence center in proton-irradiated silicon
We have investigated the formation and decay of hydrogen-related donors (HDs) and irradiation-induced intrinsic defects. N-type m:Cz and FZ silicon wafers, which were irradiated with 2 MeV protons and subsequently annealed at 100–600 °C, were analyzed using spreading resistance profiling and photoluminescence (PL). HDs formed at 260 °C and then disappeared in two stages at 400–440 and 500–540 °C. This decay behavior indicates the existence of two types of HDs with different thermal stabilities. PL measurements showed interstitial silicon clusters (W and X center), a carbon–oxygen complex (C center), and exciton lines bound to unknown shallow centers. The origin of the HDs was investigated based on the correlation of the formation and decay temperatures between HDs and irradiation-induced defects. The predominant defects at the early stage of annealing, such as the C and W centers, are ruled out as candidates for the core defects of HDs because annealing above 260 °C is indispensable for the HD formation. In contrast, the X center was found to be thermally generated above 200 °C and disappeared at 580 °C. The similarity of the formation and decay temperatures between the X and HD centers suggests that HDs are associated with the formation of the interstitial silicon-related defects attached to hydrogen. Our results suggest that controlling the formation of interstitial silicon-related defects is important for realizing desirable doping profiles with high accuracy and reproducibility for power devices. Annealing above 400 °C exclusively provides thermally more stable HDs, leading to the realization of more rugged power devices.
- 22 March 2022
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 131 (12) , 125702
Annealing-temperature-dependent evolution of hydrogen-related donor and its strong correlation with X-photoluminescence center in proton-irradiated silicon
We have investigated the formation and decay of hydrogen-related donors (HDs) and irradiation-induced intrinsic defects. N-type m:Cz and FZ silicon wafers, which were irradiated with 2 MeV protons and subsequently annealed at 100–600 °C, were analyzed using spreading resistance profiling and photoluminescence (PL). HDs formed at 260 °C and then disappeared in two stages at 400–440 and 500–540 °C. This decay behavior indicates the existence of two types of HDs with different thermal stabilities. PL measurements showed interstitial silicon clusters (W and X center), a carbon–oxygen complex (C center), and exciton lines bound to unknown shallow centers. The origin of the HDs was investigated based on the correlation of the formation and decay temperatures between HDs and irradiation-induced defects. The predominant defects at the early stage of annealing, such as the C and W centers, are ruled out as candidates for the core defects of HDs because annealing above 260 °C is indispensable for the HD formation. In contrast, the X center was found to be thermally generated above 200 °C and disappeared at 580 °C. The similarity of the formation and decay temperatures between the X and HD centers suggests that HDs are associated with the formation of the interstitial silicon-related defects attached to hydrogen. Our results suggest that controlling the formation of interstitial silicon-related defects is important for realizing desirable doping profiles with high accuracy and reproducibility for power devices. Annealing above 400 °C exclusively provides thermally more stable HDs, leading to the realization of more rugged power devices.
- 16 September 2021
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 130 (11) , 115704
Effect of carbon, oxygen, and intrinsic defects on hydrogen-related donor concentration in proton irradiated n-type silicon
We investigated the effect of the concentration of carbon, oxygen, and irradiation-induced intrinsic defects on hydrogen-related donor (HD) concentration. Several n-type silicon wafers having different carbon and oxygen concentrations were irradiated with 2 MeV protons, subsequently annealed at 300–400 °C, and analyzed by spreading resistance profiling. The HD concentration had no correlation with carbon and oxygen concentration. Additionally, the HD concentration showed a strong increasing linear dependence with proton-irradiation dose at 350 and 400 °C and a square root dependence at 300 °C. In the decay process of HD concentration at 400 °C, fast- and slow-decay components were observed regardless of wafer type. Our results show that the HD formation is based on the interactive process of irradiation-induced intrinsic defects and hydrogen, rather than hydrogen-catalyzed thermal double donor formation. Magnetic-field-applied Czochralski (m:Cz) wafers with 300 mm diameter, which are critical for the production scaling of power devices, have a relatively higher oxygen concentration than conventional floating-zone wafers. Our results further suggest that controlling the intrinsic defect formation, rather than oxygen impurity concentration, is more important in realizing designed doping profiles with high accuracy and reproducibility for next-generation power devices using large-diameter m:Cz wafers as a standard starting material.
- 16 September 2021
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 130 (11) , 115704
Effect of carbon, oxygen, and intrinsic defects on hydrogen-related donor concentration in proton irradiated n-type silicon
We investigated the effect of the concentration of carbon, oxygen, and irradiation-induced intrinsic defects on hydrogen-related donor (HD) concentration. Several n-type silicon wafers having different carbon and oxygen concentrations were irradiated with 2 MeV protons, subsequently annealed at 300–400 °C, and analyzed by spreading resistance profiling. The HD concentration had no correlation with carbon and oxygen concentration. Additionally, the HD concentration showed a strong increasing linear dependence with proton-irradiation dose at 350 and 400 °C and a square root dependence at 300 °C. In the decay process of HD concentration at 400 °C, fast- and slow-decay components were observed regardless of wafer type. Our results show that the HD formation is based on the interactive process of irradiation-induced intrinsic defects and hydrogen, rather than hydrogen-catalyzed thermal double donor formation. Magnetic-field-applied Czochralski (m:Cz) wafers with 300 mm diameter, which are critical for the production scaling of power devices, have a relatively higher oxygen concentration than conventional floating-zone wafers. Our results further suggest that controlling the intrinsic defect formation, rather than oxygen impurity concentration, is more important in realizing designed doping profiles with high accuracy and reproducibility for next-generation power devices using large-diameter m:Cz wafers as a standard starting material.
- 8 January 2021
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 129 (2) , 025701
Influence of oxygen on trap-limited diffusion of hydrogen in proton-irradiated n-type silicon for power devices
The growing demand for power devices has led to the use of magnetic field-applied Czochralski (m:Cz) wafers owing to the limited production capacity and available diameters of the traditionally used floating zone (FZ) wafers. Consequently, the influence of oxygen impurities in the wafers on the electrical properties of devices, regardless of the growth method, needs to be investigated to achieve a stable fabrication process for power devices. Using the proton irradiation doping process and spreading resistance profiling technique, we evaluated the effective diffusion coefficient (Deff) related to trap-limited diffusion of hydrogen and the effects of impurities on diffusivity. We irradiated n-type silicon wafers, which have different carbon, oxygen, and phosphorus concentrations, with 2 MeV protons and annealed them at 300–400 °C. By analyzing the width of the n-type region, where hydrogen-related shallow donors (HDs) are induced, we estimated Deff to be five to six orders of magnitude lower than the intrinsic diffusion coefficient, indicating that hydrogen motion is highly trap-limited. Deff was significantly dependent on the oxygen concentration, and the activation energy of hydrogen diffusion varied from 0.57 ± 0.15 eV (pure epitaxial wafer) to 2.19 ± 0.15 eV (m:Cz wafer). This trend suggests that oxygen-related defects preferentially trap the mobile hydrogen released from thermally dissociated HDs. This study also reveals that the diffusion coefficients of different materials when annealed at 400 °C are comparable. This information is essential to realize the cost-effective production of power devices because we can treat m:Cz and FZ wafers equivalently during the doping process.
- 8 January 2021
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 129 (2) , 025701
Influence of oxygen on trap-limited diffusion of hydrogen in proton-irradiated n-type silicon for power devices
The growing demand for power devices has led to the use of magnetic field-applied Czochralski (m:Cz) wafers owing to the limited production capacity and available diameters of the traditionally used floating zone (FZ) wafers. Consequently, the influence of oxygen impurities in the wafers on the electrical properties of devices, regardless of the growth method, needs to be investigated to achieve a stable fabrication process for power devices. Using the proton irradiation doping process and spreading resistance profiling technique, we evaluated the effective diffusion coefficient (Deff) related to trap-limited diffusion of hydrogen and the effects of impurities on diffusivity. We irradiated n-type silicon wafers, which have different carbon, oxygen, and phosphorus concentrations, with 2 MeV protons and annealed them at 300–400 °C. By analyzing the width of the n-type region, where hydrogen-related shallow donors (HDs) are induced, we estimated Deff to be five to six orders of magnitude lower than the intrinsic diffusion coefficient, indicating that hydrogen motion is highly trap-limited. Deff was significantly dependent on the oxygen concentration, and the activation energy of hydrogen diffusion varied from 0.57 ± 0.15 eV (pure epitaxial wafer) to 2.19 ± 0.15 eV (m:Cz wafer). This trend suggests that oxygen-related defects preferentially trap the mobile hydrogen released from thermally dissociated HDs. This study also reveals that the diffusion coefficients of different materials when annealed at 400 °C are comparable. This information is essential to realize the cost-effective production of power devices because we can treat m:Cz and FZ wafers equivalently during the doping process.