Stefan Doose
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Stefan Doose has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Arno Kwade
Institute for Particle Technology, Technische Universität Braunschweig, Volkmaroder Straße 5, 38104 Braunschweig, Germany
6 shared publications - Jannes Müller
Institute for Particle Technology, Technische Universität Braunschweig, Volkmaroder Str. 5, 38104 Braunschweig, Germany
2 shared publications - Peter Michalowski
Institute for Particle Technology Technische Universität Braunschweig Braunschweig Germany
2 shared publications Alexander Hahn
Institute for Particle Technology Technische Universität Braunschweig 38104 Braunschweig, Lower Saxony Germany
1 shared publication- Alexander Hahn
Institute for Particle Technology, Technische Universität Braunschweig, Volkmaroder Straße 5, 38104 Braunschweig, Germany
1 shared publication - Christian Höfels
Netzsch Trockenmahltechnik GmbH, Rodenbacher Ch 1, 63457 Hanau, Germany
1 shared publication
Latest Publications
- Open Access
Effect of External Compression on the Thermal Runaway of Lithium-Ion Battery Cells during Crush Tests: Insights for Improved Safety Assessment
To gain better understanding of the safety behavior of lithium-ion batteries under mechanical stress, crush tests are performed and reported in literature and in standards. However, many of these tests are conducted without the use of a cell clamping device, whereas external pressure is applied to the cell in a battery module in applications such as in an electric vehicle. The objective of this manuscript is to determine the effect of differing external compression on the thermal runaway of battery cells. Therefore, in this study, crush tests are performed with a hemispherical punch in a battery cell test chamber on commercially available 5 Ah pouch cells in a clamping device at four different normal stresses. The results are compared to cells that are free to expand with gas evolution. It is shown that applying compression to the cells not only results in a greater reproducibility of the experiments but that it also affects the thermal runaway process itself. With decreasing clamping stresses, the reaction time of the thermal runaway is increased by up to 19%, and the mass ejection is decreased by up to 10%, which, in turn, strongly influences the measurable gas concentrations by up to 80%. Based on this, a defined clamping compression was selected to obtain comparable results for different cell formats.
Open AccessEffect of External Compression on the Thermal Runaway of Lithium-Ion Battery Cells during Crush Tests: Insights for Improved Safety Assessment
To gain better understanding of the safety behavior of lithium-ion batteries under mechanical stress, crush tests are performed and reported in literature and in standards. However, many of these tests are conducted without the use of a cell clamping device, whereas external pressure is applied to the cell in a battery module in applications such as in an electric vehicle. The objective of this manuscript is to determine the effect of differing external compression on the thermal runaway of battery cells. Therefore, in this study, crush tests are performed with a hemispherical punch in a battery cell test chamber on commercially available 5 Ah pouch cells in a clamping device at four different normal stresses. The results are compared to cells that are free to expand with gas evolution. It is shown that applying compression to the cells not only results in a greater reproducibility of the experiments but that it also affects the thermal runaway process itself. With decreasing clamping stresses, the reaction time of the thermal runaway is increased by up to 19%, and the mass ejection is decreased by up to 10%, which, in turn, strongly influences the measurable gas concentrations by up to 80%. Based on this, a defined clamping compression was selected to obtain comparable results for different cell formats.
- Open Access
Impact of Spheroidization of Natural Graphite on Fast-Charging Capability of Anodes for LIB
Despite numerous research on new active materials for anodes, graphite remains the most commonly used material in Li-ion batteries. The spherical shape of the graphite particles has proven to be beneficial for application in electric vehicles, especially for fast charging. So far, the spheroidization of natural flake graphite is conducted by a rigid and inefficient cascade process. In this work, a scalable classifier system was used for spheroidization, and it was demonstrated that a spheroidization time of 15 min is sufficient to improve material properties and enhance electrochemical performance while maintaining high process yields of 55%. Insights into the influence of the morphology on the intrinsic and structural properties of the graphite particles and manufactured electrodes are provided. Spheroidization creates a more efficient pore network in the coating layer while reducing the internal resistance and increasing the surface area of the particles by a factor of 1.8. We demonstrate that the spherical shape improves the discharge rate capability by 1.8, and the specific charge capacity could be enhanced by more than 237% at a C-rate of 3. An additional carbon coating could significantly decrease the specific surface area and increase the specific capacity at high C-rates.
Open AccessImpact of Spheroidization of Natural Graphite on Fast-Charging Capability of Anodes for LIB
Despite numerous research on new active materials for anodes, graphite remains the most commonly used material in Li-ion batteries. The spherical shape of the graphite particles has proven to be beneficial for application in electric vehicles, especially for fast charging. So far, the spheroidization of natural flake graphite is conducted by a rigid and inefficient cascade process. In this work, a scalable classifier system was used for spheroidization, and it was demonstrated that a spheroidization time of 15 min is sufficient to improve material properties and enhance electrochemical performance while maintaining high process yields of 55%. Insights into the influence of the morphology on the intrinsic and structural properties of the graphite particles and manufactured electrodes are provided. Spheroidization creates a more efficient pore network in the coating layer while reducing the internal resistance and increasing the surface area of the particles by a factor of 1.8. We demonstrate that the spherical shape improves the discharge rate capability by 1.8, and the specific charge capacity could be enhanced by more than 237% at a C-rate of 3. An additional carbon coating could significantly decrease the specific surface area and increase the specific capacity at high C-rates.
- 6 September 2022
- Published by Elsevier in Journal of Power Sources
- Vol. 548
Effects of carbon coating on calendered nano-silicon graphite composite anodes of LiB
- 6 September 2022
- Published by Elsevier in Journal of Power Sources
- Vol. 548
Effects of carbon coating on calendered nano-silicon graphite composite anodes of LiB
- Open Access
- 1 April 2022
- Published by Wiley in Batteries & Supercaps
- Vol. 5 (7)
Scaling Methodology to Describe the Capacity Dependent Responses During Thermal Runaway of Lithium‐Ion Batteries
In this work, internal short‐circuit tests on prototypically battery cells of different cell capacities were performed to determine scalable dependencies of the thermal runaway. It shows that this pouch cells with NMC111/graphite electrodes must have a minimum capacity of 1.5 A h to develop a thermal runaway. In addition, it could be determined that with increasing battery capacity the strength of the reaction also increases, which is visible, among other things, in the linear temperature increase on the cell surface from 1.5 A h to 3.0 A h of overall 66.77 °C and the increasing weight loss, of up to 37.5 % compared to the starting weight. It could also be shown that the processes of the thermal runaway can be described within certain limits by simple linear (cell surface temperatures, penetration depth, time until cell voltage reaches 0 V) and nonlinear fits (cell weight loss, setoff voltage at TR). This allows the determination of scalable parameters and test results with a minimum of test effort. Furthermore, increasing concentrations of the determined substances could be measured for the infrared‐active gaseous reaction products. In particular, the decomposition products CO and CO 2 , as well as the linear hydrocarbons, increase significantly with increasing capacity. On the whole, parameters for the description of the thermal runaway could be determined, which describe the effects and reactions of the thermal runaway well and could minimize test efforts with known materials.
- 1 April 2022
- Published by Wiley in Batteries & Supercaps
- Vol. 5 (7)
Open AccessScaling Methodology to Describe the Capacity Dependent Responses During Thermal Runaway of Lithium‐Ion Batteries
In this work, internal short‐circuit tests on prototypically battery cells of different cell capacities were performed to determine scalable dependencies of the thermal runaway. It shows that this pouch cells with NMC111/graphite electrodes must have a minimum capacity of 1.5 A h to develop a thermal runaway. In addition, it could be determined that with increasing battery capacity the strength of the reaction also increases, which is visible, among other things, in the linear temperature increase on the cell surface from 1.5 A h to 3.0 A h of overall 66.77 °C and the increasing weight loss, of up to 37.5 % compared to the starting weight. It could also be shown that the processes of the thermal runaway can be described within certain limits by simple linear (cell surface temperatures, penetration depth, time until cell voltage reaches 0 V) and nonlinear fits (cell weight loss, setoff voltage at TR). This allows the determination of scalable parameters and test results with a minimum of test effort. Furthermore, increasing concentrations of the determined substances could be measured for the infrared‐active gaseous reaction products. In particular, the decomposition products CO and CO 2 , as well as the linear hydrocarbons, increase significantly with increasing capacity. On the whole, parameters for the description of the thermal runaway could be determined, which describe the effects and reactions of the thermal runaway well and could minimize test efforts with known materials.
- Open Access
Challenges in Ecofriendly Battery Recycling and Closed Material Cycles: A Perspective on Future Lithium Battery Generations
The global use of lithium-ion batteries of all types has been increasing at a rapid pace for many years. In order to achieve the goal of an economical and sustainable battery industry, the recycling and recirculation of materials is a central element on this path. As the achievement of high 95% recovery rates demanded by the European Union for some metals from today’s lithium ion batteries is already very challenging, the question arises of how the process chains and safety of battery recycling as well as the achievement of closed material cycles are affected by the new lithium battery generations, which are supposed to enter the market in the next 5 to 10 years. Based on a survey of the potential development of battery technology in the next years, where a diversification between high-performance and cost-efficient batteries is expected, and today’s knowledge on recycling, the challenges and chances of the new battery generations regarding the development of recycling processes, hazards in battery dismantling and recycling, as well as establishing a circular economy are discussed. It becomes clear that the diversification and new developments demand a proper separation of battery types before recycling, for example by a transnational network of dismantling and sorting locations, and flexible and high sophisticated recycling processes with case-wise higher safety standards than today. Moreover, for the low-cost batteries, recycling of the batteries becomes economically unattractive, so legal stipulations become important. However, in general, it must be still secured that closing the material cycle for all battery types with suitable processes is achieved to secure the supply of raw materials and also to further advance new developments.
Open AccessChallenges in Ecofriendly Battery Recycling and Closed Material Cycles: A Perspective on Future Lithium Battery Generations
The global use of lithium-ion batteries of all types has been increasing at a rapid pace for many years. In order to achieve the goal of an economical and sustainable battery industry, the recycling and recirculation of materials is a central element on this path. As the achievement of high 95% recovery rates demanded by the European Union for some metals from today’s lithium ion batteries is already very challenging, the question arises of how the process chains and safety of battery recycling as well as the achievement of closed material cycles are affected by the new lithium battery generations, which are supposed to enter the market in the next 5 to 10 years. Based on a survey of the potential development of battery technology in the next years, where a diversification between high-performance and cost-efficient batteries is expected, and today’s knowledge on recycling, the challenges and chances of the new battery generations regarding the development of recycling processes, hazards in battery dismantling and recycling, as well as establishing a circular economy are discussed. It becomes clear that the diversification and new developments demand a proper separation of battery types before recycling, for example by a transnational network of dismantling and sorting locations, and flexible and high sophisticated recycling processes with case-wise higher safety standards than today. Moreover, for the low-cost batteries, recycling of the batteries becomes economically unattractive, so legal stipulations become important. However, in general, it must be still secured that closing the material cycle for all battery types with suitable processes is achieved to secure the supply of raw materials and also to further advance new developments.
- Open Access
Effects of the Nail Geometry and Humidity on the Nail Penetration of High-Energy Density Lithium Ion Batteries
Internal short-circuit tests were carried out in a battery safety investigation chamber to determine the behavior of batteries during the nail penetration test. So far, systematic investigations regarding the test setup and its influence are rarely found in the literature. Especially, to improve the comparability of the multitude of available results, it is essential to understand the effects of the geometric, operating and ambient parameters. In this study commercial lithium ion batteries with a capacity of 5.3 and 3.3 Ah were used to study the influence of the varied parameters on the voltage drop, the development of surface temperatures and of infrared active gas species. We studied both the influence of the geometry of the penetrating nail and concentration of water in the inert atmosphere especially on the quantities of the reaction products under variation of cell capacity. It could be shown that the geometry of the nail, within certain limits, has no influence on the processes of the thermal runaway of high energy density lithium ion batteries (LIBs). However, a change in capacity from 5.3 to 3.3 Ah shows that in particular the gaseous reaction products differ: The standardized gas concentrations show a higher measurable concentration of all gases except CO for the 3.3 Ah LIBs. This circumstance can be explained by the intensity of the reactions due to the different battery capacities: In the 5.3 Ah cells a larger amount of unreacted material is immediately discharged from the reaction center, and by the different available amounts of oxidizing reaction partners. An increase of the water content in the surrounding atmosphere during the thermal runaway leads to a reduction of the measurable gas concentrations of up to 36.01%. In general, all measured concentrations decrease. With increased water content more reaction products from the atmosphere can be directly bound or settle as condensate on surfaces.
Open AccessEffects of the Nail Geometry and Humidity on the Nail Penetration of High-Energy Density Lithium Ion Batteries
Internal short-circuit tests were carried out in a battery safety investigation chamber to determine the behavior of batteries during the nail penetration test. So far, systematic investigations regarding the test setup and its influence are rarely found in the literature. Especially, to improve the comparability of the multitude of available results, it is essential to understand the effects of the geometric, operating and ambient parameters. In this study commercial lithium ion batteries with a capacity of 5.3 and 3.3 Ah were used to study the influence of the varied parameters on the voltage drop, the development of surface temperatures and of infrared active gas species. We studied both the influence of the geometry of the penetrating nail and concentration of water in the inert atmosphere especially on the quantities of the reaction products under variation of cell capacity. It could be shown that the geometry of the nail, within certain limits, has no influence on the processes of the thermal runaway of high energy density lithium ion batteries (LIBs). However, a change in capacity from 5.3 to 3.3 Ah shows that in particular the gaseous reaction products differ: The standardized gas concentrations show a higher measurable concentration of all gases except CO for the 3.3 Ah LIBs. This circumstance can be explained by the intensity of the reactions due to the different battery capacities: In the 5.3 Ah cells a larger amount of unreacted material is immediately discharged from the reaction center, and by the different available amounts of oxidizing reaction partners. An increase of the water content in the surrounding atmosphere during the thermal runaway leads to a reduction of the measurable gas concentrations of up to 36.01%. In general, all measured concentrations decrease. With increased water content more reaction products from the atmosphere can be directly bound or settle as condensate on surfaces.