V. Balakumaran
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
V. Balakumaran has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
- Dinesh Kalyanasundaram
Centre for Biomedical Engineering, Indian Institute of Technology Delhi, New Delhi, 110016, India
2 shared publications Ramasamy Alagirusamy
Department of Textile and Fiber Engineering Indian Institute of Technology New Delhi India
1 shared publication- Ramasamy Alagirusamy
Indian Institute of Technology Delhi
1 shared publication
Latest Publications
- 14 June 2024
- Published by Wiley in Polymer Composites
- Vol. 45 (14) , 12995-13016
The synergistic effect and origin of strength in carbon fiber reinforced PAEK, PEEK, and PEKK high‐performance thermoplastic composites manufactured by multi‐scale aqueous dispersion coating
High‐performance thermoplastic composites of polyketones [poly‐aryl‐ether‐ketone (PAEK), poly‐ether‐ether‐ketone (PEEK), poly‐ether‐ketone‐ketone (PEKK)] reinforced with continuous carbon fiber (CF) were consolidated using towpreg produced by multi‐scale aqueous dispersion coating technique. An intra‐matrix trend of composite strength and void fraction was studied to identify the composite with maximum strength free of voids for each polyketone matrix. The CF/PAEK composite with a flexural strength of ~2047 MPa and ILSS of ~99 MPa with a fiber volume fraction of ~67% had the maximum strength free of voids among CF/PAEK composite and all polyketone composites studied. The highest crystallinity (34.5%), and the highest amount of hydrogen bonding and bonds formed between CF, PI nanoparticle, and PAEK explained the origin of strength in CF/PAEK composite. The maximum strength among CF/PEEK and CF/PEKK composite free of voids had a flexural strength of ~1861 MPa, ~1981 MPa; ILSS of ~74 MPa, ~60 MPa; fiber volume fraction of ~61% and ~ 65%, respectively. The polyimide (PI) nanoparticles layer on CF formed the fiber matrix interface, supported hydrogen bonding in all polyketone composites, and formed bonds with CF and matrices of PAEK and PEEK establishing a synergistic effect.Highlights: Intra‐matrix trend of strength and voids in polyketone composites studied. Void‐free, high‐performance, high fiber volume fraction composites developed. CF/PAEK composite had maximum strength among polyketone composites studied. PI nanoparticles formed bonds with CF and matrices of PAEK and PEEK. CF/PAEK composite strength originates from crystallinity, H bond, and bonding.
- 14 June 2024
- Published by Wiley in Polymer Composites
- Vol. 45 (14) , 12995-13016
The synergistic effect and origin of strength in carbon fiber reinforced PAEK, PEEK, and PEKK high‐performance thermoplastic composites manufactured by multi‐scale aqueous dispersion coating
High‐performance thermoplastic composites of polyketones [poly‐aryl‐ether‐ketone (PAEK), poly‐ether‐ether‐ketone (PEEK), poly‐ether‐ketone‐ketone (PEKK)] reinforced with continuous carbon fiber (CF) were consolidated using towpreg produced by multi‐scale aqueous dispersion coating technique. An intra‐matrix trend of composite strength and void fraction was studied to identify the composite with maximum strength free of voids for each polyketone matrix. The CF/PAEK composite with a flexural strength of ~2047 MPa and ILSS of ~99 MPa with a fiber volume fraction of ~67% had the maximum strength free of voids among CF/PAEK composite and all polyketone composites studied. The highest crystallinity (34.5%), and the highest amount of hydrogen bonding and bonds formed between CF, PI nanoparticle, and PAEK explained the origin of strength in CF/PAEK composite. The maximum strength among CF/PEEK and CF/PEKK composite free of voids had a flexural strength of ~1861 MPa, ~1981 MPa; ILSS of ~74 MPa, ~60 MPa; fiber volume fraction of ~61% and ~ 65%, respectively. The polyimide (PI) nanoparticles layer on CF formed the fiber matrix interface, supported hydrogen bonding in all polyketone composites, and formed bonds with CF and matrices of PAEK and PEEK establishing a synergistic effect.Highlights: Intra‐matrix trend of strength and voids in polyketone composites studied. Void‐free, high‐performance, high fiber volume fraction composites developed. CF/PAEK composite had maximum strength among polyketone composites studied. PI nanoparticles formed bonds with CF and matrices of PAEK and PEEK. CF/PAEK composite strength originates from crystallinity, H bond, and bonding.