Jay Ghatak
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Jay Ghatak has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Sonnada Math Shivaprasad
Chemistry and Physics of Materials Unit Jawaharlal Nehru Centre for Advanced Scientific Research (JNCASR) Bangalore-560064
2 shared publications - Abhijit Chatterjee
Jawaharlal Nehru Ctr Adv Sci Res, Chem & Phys Mat Unit, Bangalore 560064, Karnataka, India
1 shared publication - Anuja Datta
Materials Systems Engineering Max Planck Institute for Dynamics of Complex Technical Systems Magdeburg‐Alte Neustadt Germany
1 shared publication Arpan De
Jawaharlal Nehru Centre for Advanced Scientific Research Chemistry and Physics of Materials Unit, International Centre for Materials Science Jakkur, Bangalore 560064, India
1 shared publication- Chinthamani Nagesa Ramachandra Rao
New Chemistry Unit JNCASR Bangalore INDIA
1 shared publication - Debendra Prasad Panda
School of Advanced Materials, and Chemistry and Physics of Materials Unit, Jawaharlal Nehru Centre for Advanced Scientific Research, Jakkur, Bangalore 560064, India
1 shared publication
Latest Publications
- Open Access
- 1 September 2023
- Published by AIP Publishing in APL Materials
- Vol. 11 (9)
High crystalline epitaxial thin films of NiO by plasma-enhanced ALD and their properties
NiO is an interesting transition metal oxide due to its fascinating properties. High crystalline thin films of NiO are preferred for use in a variety of device applications but are challenging to deposit at low temperatures. We have prepared epitaxial thin films of NiO with [111] as the preferred growth direction on a c-plane sapphire substrate at relatively low temperatures using plasma-enhanced atomic layer deposition (PEALD) exploiting a simple nickel precursor with oxygen plasma. The evolution of crystallinity and surface morphology of the films were studied as a function of substrate temperature. Ultra-smooth NiO films with excellent crystallinity were prepared at 250 °C without the necessity for post-annealing. Different microscopic and spectroscopic methods revealed film characteristics. The magnetic properties of (111) oriented epitaxial NiO films prepared using PEALD are explored for the first time, and they are antiferromagnetic in nature.
- 1 September 2023
- Published by AIP Publishing in APL Materials
- Vol. 11 (9)
Open AccessHigh crystalline epitaxial thin films of NiO by plasma-enhanced ALD and their properties
NiO is an interesting transition metal oxide due to its fascinating properties. High crystalline thin films of NiO are preferred for use in a variety of device applications but are challenging to deposit at low temperatures. We have prepared epitaxial thin films of NiO with [111] as the preferred growth direction on a c-plane sapphire substrate at relatively low temperatures using plasma-enhanced atomic layer deposition (PEALD) exploiting a simple nickel precursor with oxygen plasma. The evolution of crystallinity and surface morphology of the films were studied as a function of substrate temperature. Ultra-smooth NiO films with excellent crystallinity were prepared at 250 °C without the necessity for post-annealing. Different microscopic and spectroscopic methods revealed film characteristics. The magnetic properties of (111) oriented epitaxial NiO films prepared using PEALD are explored for the first time, and they are antiferromagnetic in nature.
- 13 January 2021
- Published by Wiley in Journal of Microscopy
- Vol. 282 (3) , 250-257
Site‐specific angular dependent determination of inelastic mean free path of 300 keV electrons in GaN nanorods
Inelastic mean free path (IMFP) of the electron is a very important parameter for quantitative analysis of several electron spectroscopies and transport properties. In spite of being a fundamental material property, its experimental determination is not trivial due to complexity of the various electron scattering processes in matter. In this report, we demonstrate a procedure to determine the IMFP of 300 keV electrons in GaN, using the log‐ratio technique where the local specimen thickness needs to be accurately known. The GaN nanorod morphology of the sample used here allows the accurate measurement of thickness by ‘thickness map’ under EFTEM measurements which enable the site specific determination of IMFP. IMFP for different collection semi angles have also been measured to validate the angular dependence. Our experimental results estimates the IMFP of GaN for 300 keV electrons to be 143 ± 11 nm at no‐aperture condition and exhibit a strong inverse angular dependence at smaller collection semi angles (β < 20 mrad) and a near angular independence at larger collection semi angles (β > 30 mrad). We discuss these results in the light of three different theoretical models prevalent in the literature.
- 13 January 2021
- Published by Wiley in Journal of Microscopy
- Vol. 282 (3) , 250-257
Site‐specific angular dependent determination of inelastic mean free path of 300 keV electrons in GaN nanorods
Inelastic mean free path (IMFP) of the electron is a very important parameter for quantitative analysis of several electron spectroscopies and transport properties. In spite of being a fundamental material property, its experimental determination is not trivial due to complexity of the various electron scattering processes in matter. In this report, we demonstrate a procedure to determine the IMFP of 300 keV electrons in GaN, using the log‐ratio technique where the local specimen thickness needs to be accurately known. The GaN nanorod morphology of the sample used here allows the accurate measurement of thickness by ‘thickness map’ under EFTEM measurements which enable the site specific determination of IMFP. IMFP for different collection semi angles have also been measured to validate the angular dependence. Our experimental results estimates the IMFP of GaN for 300 keV electrons to be 143 ± 11 nm at no‐aperture condition and exhibit a strong inverse angular dependence at smaller collection semi angles (β < 20 mrad) and a near angular independence at larger collection semi angles (β > 30 mrad). We discuss these results in the light of three different theoretical models prevalent in the literature.
- 23 May 2016
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 119 (20) , 205701
Electron mobility of self-assembled and dislocation free InN nanorods grown on GaN nano wall network template
A kinetically controlled two-step growth process for the formation of an array of dislocation free high mobility InN nanorods (NRs) on GaN nanowall network (NWN) by Molecular Beam Epitaxy is demonstrated here. The epitaxial GaN NWN is formed on c-sapphire under nitrogen rich conditions, and then changing the source from Ga to In at appropriate substrate temperature yields the nucleation of a self assembled spontaneous m-plane side faceted-InN NR. By HRTEM, the NRs are shown to be dislocation-free and have a low band gap value of 0.65 eV. Hall measurements are carried out on a single InN NR along with J-V measurements that yield mobility values as high as ≈4453 cm2/V s and the carrier concentration of ≈1.1 × 1017 cm−3, which are unprecedented in the literature for comparable InN NR diameters.
- 23 May 2016
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 119 (20) , 205701
Electron mobility of self-assembled and dislocation free InN nanorods grown on GaN nano wall network template
A kinetically controlled two-step growth process for the formation of an array of dislocation free high mobility InN nanorods (NRs) on GaN nanowall network (NWN) by Molecular Beam Epitaxy is demonstrated here. The epitaxial GaN NWN is formed on c-sapphire under nitrogen rich conditions, and then changing the source from Ga to In at appropriate substrate temperature yields the nucleation of a self assembled spontaneous m-plane side faceted-InN NR. By HRTEM, the NRs are shown to be dislocation-free and have a low band gap value of 0.65 eV. Hall measurements are carried out on a single InN NR along with J-V measurements that yield mobility values as high as ≈4453 cm2/V s and the carrier concentration of ≈1.1 × 1017 cm−3, which are unprecedented in the literature for comparable InN NR diameters.
- 26 April 2013
- Published by American Chemical Society (ACS) in Crystal Growth & Design
- Vol. 13 (6) , 2407-2412
The Origin of Shape, Orientation, and Structure of Spontaneously Formed Wurtzite GaN Nanorods on Cubic Si(001) Surface
- 26 April 2013
- Published by American Chemical Society (ACS) in Crystal Growth & Design
- Vol. 13 (6) , 2407-2412
The Origin of Shape, Orientation, and Structure of Spontaneously Formed Wurtzite GaN Nanorods on Cubic Si(001) Surface
- 1 February 2007
- Published by American Scientific Publishers in Journal of Nanoscience and Nanotechnology
- Vol. 7 (2) , 677-688
Solvothermal Synthesis of CdS Nanorods: Role of Basic Experimental Parameters
CdS nanorods with varying dimensions were synthesized by solvothermal process. It was observed that the anions present with the Cd-salts play an important role in determining the dimensions of the CdS nanorods. The crystalline nature of the sources was found to play a crucial role in determining the phase of the products. The nature of the sulfur source, molar ratio of the precursors, filling fraction of the solvent, and the synthesis temperature play important role in defining the size and shape of the products. By controlling the experimental parameters it was possible to control the dimension of the CdS nanorods within a certain range (diameter of the nanorods could be varied within a wide range from ∼7 to 100 nm by varying the temperature within 100–250 °C). Optical absorption, photoluminescence, and Raman studies of these samples were carried out to characterize the CdS nanorods.
- 1 February 2007
- Published by American Scientific Publishers in Journal of Nanoscience and Nanotechnology
- Vol. 7 (2) , 677-688
Solvothermal Synthesis of CdS Nanorods: Role of Basic Experimental Parameters
CdS nanorods with varying dimensions were synthesized by solvothermal process. It was observed that the anions present with the Cd-salts play an important role in determining the dimensions of the CdS nanorods. The crystalline nature of the sources was found to play a crucial role in determining the phase of the products. The nature of the sulfur source, molar ratio of the precursors, filling fraction of the solvent, and the synthesis temperature play important role in defining the size and shape of the products. By controlling the experimental parameters it was possible to control the dimension of the CdS nanorods within a certain range (diameter of the nanorods could be varied within a wide range from ∼7 to 100 nm by varying the temperature within 100–250 °C). Optical absorption, photoluminescence, and Raman studies of these samples were carried out to characterize the CdS nanorods.