Jingang Tang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Jingang Tang has a total of 33 co-authors. Here are the top co-authors by number of shared publications:
- Daoxin Liu
Institute of Corrosion and Protection, School of Aeronautics, Northwestern Polytechnical University, Xi’an 710072, China
2 shared publications - Jie Chen
Institute of Machinery Manufacturing Technology, China Academy of Engineering Physics, Mianyang 621000, China
2 shared publications - Shuke Huang
Institute of Machinery Manufacturing Technology, China Academy of Engineering Physics, Mianyang 621000, China
2 shared publications - Xiaohua Zhang
Institute of Corrosion and Protection, School of Aeronautics, Northwestern Polytechnical University, Xi’an 710072, China
2 shared publications - Xiaohui Ge
Institute of Machinery Manufacturing Technology, China Academy of Engineering Physics, Mianyang 621000, China
2 shared publications - Yong Xu
School of Materials Science and Engineering, Tsinghua University, Beijing 100084, China
2 shared publications
Latest Publications
- Open Access
Effects of Cross-Sectional Gradient on Damping Performance and Energy Dissipation of LPBF Self-Sealing Powder Dampers
This study addresses the fabrication difficulty of variable-cross-section structures and the unclear energy dissipation mechanism of micron-scale self-sealing powder dampers. A novel gradient self-sealing powder damper monolithically fabricated via laser powder bed fusion (LPBF) is proposed. Three equal-volume Ti-6Al-4V specimens, including zero-gradient cylindrical, moderate-gradient circular frustum and strong-gradient conical configurations, are tested via sinusoidal swept-sine vibration experiments on a simply supported beam. Experimental results verify the pronounced orientation dependence of the gradient regulation effect. Under axial excitation, the cylindrical cavity delivers stable and robust performance with no failure risk across the full gradient range. Under transverse excitation, the moderate-gradient frustum achieves the maximum equivalent damping ratio of 0.0819, i.e., 3.7 times that of the same specimen under axial excitation, while the regulation intensity of the gradient effect—defined as the spread in the vibration reduction rate across the gradient range—is 4.8 times that under axial excitation. A critical gradient threshold of α* ≈ 0.30, defined as the gradient at which the vibration reduction rate vanishes, is identified (95% confidence interval 0.27–0.32); beyond it, vibration amplification occurs under high-amplitude excitation. The established three-parameter coupled design framework provides quantitative theoretical guidance for the engineering application of LPBF-integrated vibration damping structures.
Open AccessEffects of Cross-Sectional Gradient on Damping Performance and Energy Dissipation of LPBF Self-Sealing Powder Dampers
This study addresses the fabrication difficulty of variable-cross-section structures and the unclear energy dissipation mechanism of micron-scale self-sealing powder dampers. A novel gradient self-sealing powder damper monolithically fabricated via laser powder bed fusion (LPBF) is proposed. Three equal-volume Ti-6Al-4V specimens, including zero-gradient cylindrical, moderate-gradient circular frustum and strong-gradient conical configurations, are tested via sinusoidal swept-sine vibration experiments on a simply supported beam. Experimental results verify the pronounced orientation dependence of the gradient regulation effect. Under axial excitation, the cylindrical cavity delivers stable and robust performance with no failure risk across the full gradient range. Under transverse excitation, the moderate-gradient frustum achieves the maximum equivalent damping ratio of 0.0819, i.e., 3.7 times that of the same specimen under axial excitation, while the regulation intensity of the gradient effect—defined as the spread in the vibration reduction rate across the gradient range—is 4.8 times that under axial excitation. A critical gradient threshold of α* ≈ 0.30, defined as the gradient at which the vibration reduction rate vanishes, is identified (95% confidence interval 0.27–0.32); beyond it, vibration amplification occurs under high-amplitude excitation. The established three-parameter coupled design framework provides quantitative theoretical guidance for the engineering application of LPBF-integrated vibration damping structures.
- Open Access
Stiffness and Damping Properties of LPBF-Fabricated TC4 Alloy Beams Incorporating Self-Sealing Powder and Lattice Structures
Laser powder bed fusion (LPBF) provides an effective method for the preparation of self-sealing powder damping components, but the introduction of cavities simultaneously leads to a decrease in the mechanical properties of the components. In order to achieve a synergistic improvement in the stiffness and damping performance of LPBFed self-sealing powder damping components, this paper designed and prepared TC4 alloy beams incorporating both self-sealing powder and lattice structures, characterized by their manufacturing quality, mechanical properties, and damping performance and established corresponding static and dynamic models. The results show that, as the diameter of the lattice struts increases, the stiffness of the self-sealing powder beams incorporating lattice structures increases, while the amplification factor and structural damping ratio decrease, eventually tending toward that of the solid beam. The changes in damping performance are related to the powder volume and the internal surface area. Compared to self-sealing powder beams containing only cavities, self-sealing powder beams incorporating lattice structures with strut diameters of 0.6 mm and 0.9 mm not only exhibit a significant improvement in stiffness but also demonstrate smaller amplification factors and larger structural damping ratios under 1 g and 2 g vibration inputs, achieving a synergistic enhancement of stiffness and damping. This study provides an effective reference for the regulation and optimization of the mechanical properties and damping performance of LPBFed self-sealing powder structures.
Open AccessStiffness and Damping Properties of LPBF-Fabricated TC4 Alloy Beams Incorporating Self-Sealing Powder and Lattice Structures
Laser powder bed fusion (LPBF) provides an effective method for the preparation of self-sealing powder damping components, but the introduction of cavities simultaneously leads to a decrease in the mechanical properties of the components. In order to achieve a synergistic improvement in the stiffness and damping performance of LPBFed self-sealing powder damping components, this paper designed and prepared TC4 alloy beams incorporating both self-sealing powder and lattice structures, characterized by their manufacturing quality, mechanical properties, and damping performance and established corresponding static and dynamic models. The results show that, as the diameter of the lattice struts increases, the stiffness of the self-sealing powder beams incorporating lattice structures increases, while the amplification factor and structural damping ratio decrease, eventually tending toward that of the solid beam. The changes in damping performance are related to the powder volume and the internal surface area. Compared to self-sealing powder beams containing only cavities, self-sealing powder beams incorporating lattice structures with strut diameters of 0.6 mm and 0.9 mm not only exhibit a significant improvement in stiffness but also demonstrate smaller amplification factors and larger structural damping ratios under 1 g and 2 g vibration inputs, achieving a synergistic enhancement of stiffness and damping. This study provides an effective reference for the regulation and optimization of the mechanical properties and damping performance of LPBFed self-sealing powder structures.
- Open Access
Selective Laser Melting Additive Manufactured Tantalum: Effect of Microstructure and Impurities on the Strengthening-Toughing Mechanism
The balance between the strength and the toughness of pure tantalum (Ta) fabricated with selective laser melting (SLM) additive manufacturing is a major challenge due to the defect generation and affinity for oxygen and nitrogen. This study investigated the effects of energy density and post-vacuum annealing on the relative density and microstructure of SLMed tantalum. The influences of microstructure and impurities on strength and toughness were mainly analyzed. The results indicated that the toughness of SLMed tantalum significantly increased due to a reduction in pore defects and oxygen-nitrogen impurities, with energy density decreasing from 342 J/mm3 to 190 J/mm3. The oxygen impurities mainly stemmed from the gas inclusions of tantalum powders, while nitrogen impurities were mainly from the chemical reaction between the molten liquid tantalum and nitrogen in the atmosphere. The proportion of texture decreased after vacuum-annealing at 1200 °C, while that of the texture increased. Concurrently, the density of dislocations and small-angle grain boundaries significantly decreased while the resistance of the deformation dislocation slip was significantly reduced, enhancing the fractured elongation up to 28% at the expense of 14% tensile strength.
Open AccessSelective Laser Melting Additive Manufactured Tantalum: Effect of Microstructure and Impurities on the Strengthening-Toughing Mechanism
The balance between the strength and the toughness of pure tantalum (Ta) fabricated with selective laser melting (SLM) additive manufacturing is a major challenge due to the defect generation and affinity for oxygen and nitrogen. This study investigated the effects of energy density and post-vacuum annealing on the relative density and microstructure of SLMed tantalum. The influences of microstructure and impurities on strength and toughness were mainly analyzed. The results indicated that the toughness of SLMed tantalum significantly increased due to a reduction in pore defects and oxygen-nitrogen impurities, with energy density decreasing from 342 J/mm3 to 190 J/mm3. The oxygen impurities mainly stemmed from the gas inclusions of tantalum powders, while nitrogen impurities were mainly from the chemical reaction between the molten liquid tantalum and nitrogen in the atmosphere. The proportion of texture decreased after vacuum-annealing at 1200 °C, while that of the texture increased. Concurrently, the density of dislocations and small-angle grain boundaries significantly decreased while the resistance of the deformation dislocation slip was significantly reduced, enhancing the fractured elongation up to 28% at the expense of 14% tensile strength.
- 1 June 2021
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 865
Microstructure and fracture behavior of 90W-7Ni-3Fe alloy fabricated by laser directed energy deposition
- 1 June 2021
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 865
Microstructure and fracture behavior of 90W-7Ni-3Fe alloy fabricated by laser directed energy deposition
- Open Access
Effects of WC-17Co Coating Combined with Shot Peening Treatment on Fatigue Behaviors of TC21 Titanium Alloy
The improvement and mechanism of the fatigue resistance of TC21 high-strength titanium alloy with a high velocity oxygen fuel (HVOF) sprayed WC-17Co coating was investigated. X-ray diffraction (XRD) and the corresponding stress measurement instrument, a surface roughness tester, a micro-hardness tester, and a scanning electron microscope (SEM) were used to determine the properties of the HVOF WC-17Co coating with or without shot peening. The fatigue behavior of the TC21 titanium alloy with or without the WC-17Co coating was determined by using a rotating bending fatigue testing machine. The results revealed that the polished HVOF sprayed WC-17Co coating had almost the same fatigue resistance as the TC21 titanium alloy substrate. This resulted from the polishing-induced residual surface compressive stress and a decrease in the stress concentration on the surface of the coating. Moderate-intensity shot peening of the polished WC-17Co coatings resulted in significant improvement of the fatigue resistance of the alloy. Furthermore, the fatigue life was substantially higher than that of the substrate, owing to the deep distribution of residual stress and high compressive stress induced by shot peening. The improved surface toughness of the coating can effectively delay the initiation of fatigue crack propagation.
Open AccessEffects of WC-17Co Coating Combined with Shot Peening Treatment on Fatigue Behaviors of TC21 Titanium Alloy
The improvement and mechanism of the fatigue resistance of TC21 high-strength titanium alloy with a high velocity oxygen fuel (HVOF) sprayed WC-17Co coating was investigated. X-ray diffraction (XRD) and the corresponding stress measurement instrument, a surface roughness tester, a micro-hardness tester, and a scanning electron microscope (SEM) were used to determine the properties of the HVOF WC-17Co coating with or without shot peening. The fatigue behavior of the TC21 titanium alloy with or without the WC-17Co coating was determined by using a rotating bending fatigue testing machine. The results revealed that the polished HVOF sprayed WC-17Co coating had almost the same fatigue resistance as the TC21 titanium alloy substrate. This resulted from the polishing-induced residual surface compressive stress and a decrease in the stress concentration on the surface of the coating. Moderate-intensity shot peening of the polished WC-17Co coatings resulted in significant improvement of the fatigue resistance of the alloy. Furthermore, the fatigue life was substantially higher than that of the substrate, owing to the deep distribution of residual stress and high compressive stress induced by shot peening. The improved surface toughness of the coating can effectively delay the initiation of fatigue crack propagation.
- Open Access
Effects of Plasma ZrN Metallurgy and Shot Peening Duplex Treatment on Fretting Wear and Fretting Fatigue Behavior of Ti6Al4V Alloy
A metallurgical zirconium nitride (ZrN) layer was fabricated using glow metallurgy using nitriding with zirconiuming prior treatment of the Ti6Al4V alloy. The microstructure, composition and microhardness of the corresponding layer were studied. The influence of this treatment on fretting wear (FW) and fretting fatigue (FF) behavior of the Ti6Al4V alloy was studied. The composite layer consisted of an 8-μm-thick ZrN compound layer and a 50-μm-thick nitrogen-rich Zr–Ti solid solution layer. The surface microhardness of the composite layer is 1775 HK0.1. A gradient in cross-sectional microhardness distribution exists in the layer. The plasma ZrN metallurgical layer improves the FW resistance of the Ti6Al4V alloy, but reduces the base FF resistance. This occurs because the improvement in surface hardness results in lowering of the toughness and increasing in the notch sensitivity. Compared with shot peening treatment, plasma ZrN metallurgy and shot peening composite treatment improves the FW resistance and enhances the FF resistance of the Ti6Al4V alloy. This is attributed to the introduction of a compressive stress field. The combination of toughness, strength, FW resistance and fatigue resistance enhance the FF resistance for titanium alloy.
Open AccessEffects of Plasma ZrN Metallurgy and Shot Peening Duplex Treatment on Fretting Wear and Fretting Fatigue Behavior of Ti6Al4V Alloy
A metallurgical zirconium nitride (ZrN) layer was fabricated using glow metallurgy using nitriding with zirconiuming prior treatment of the Ti6Al4V alloy. The microstructure, composition and microhardness of the corresponding layer were studied. The influence of this treatment on fretting wear (FW) and fretting fatigue (FF) behavior of the Ti6Al4V alloy was studied. The composite layer consisted of an 8-μm-thick ZrN compound layer and a 50-μm-thick nitrogen-rich Zr–Ti solid solution layer. The surface microhardness of the composite layer is 1775 HK0.1. A gradient in cross-sectional microhardness distribution exists in the layer. The plasma ZrN metallurgical layer improves the FW resistance of the Ti6Al4V alloy, but reduces the base FF resistance. This occurs because the improvement in surface hardness results in lowering of the toughness and increasing in the notch sensitivity. Compared with shot peening treatment, plasma ZrN metallurgy and shot peening composite treatment improves the FW resistance and enhances the FF resistance of the Ti6Al4V alloy. This is attributed to the introduction of a compressive stress field. The combination of toughness, strength, FW resistance and fatigue resistance enhance the FF resistance for titanium alloy.