Stanko O. Aleksic
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Stanko O. Aleksic has a total of 37 co-authors. Here are the top co-authors by number of shared publications:
- Nina Obradovic
Institute of Technical Sciences of SASA, Belgrade, Serbia
7 shared publications - Nebojša Mitrović
University of Kragujevac, Faculty of technical sciences Čačak
6 shared publications - Milica G. Kisic
Faculty of Technical Sciences, University of Novi Sad, Novi Sad, Serbia
5 shared publications - Miloljub D. Lukovic
Information Technology School-ITS, Zemun, Serbia
5 shared publications - Darko Kosanovic
Institute of Technical Sciences of the Serbian Academy of Sciences and Arts, Belgrade, Serbia
4 shared publications - Marko Pavlović
Faculty of Mechanical Engineering, University of Belgrade - Innovation Center, Belgrade, Serbia
3 shared publications
Latest Publications
- 7 March 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Sensors Journal
- Vol. 25 (8) , 12695-12702
Temperature Response, Time Delay, and Hysteresis Loop of Heat Loss Flowmeter Thermistors
A heat loss flowmeter for water was made of two NTC (negative temperature coefficient) thick film thermistors Th1 and Th2 and placed in a metal housing. The first thermistor Th1 is cold and measures input water temperature Tw, and the second thermistor Th2 is self-heated at a constant voltage and measures water flow rate Q. At first temperature responses T(Q), heat loss and time delay td were measured and analyzed. Then a temperature hysteresis loops of self-heating thermistor at switching waterflow regime was measured. The electrical responses I(Q) were measured using the flowmeter and DAC (digital acquisition card). An independent ultrasonic flowmeter was used in series with a novel heat loss flowmeter. The current values of temperature T(Q, t) of the water flow Q(t) were obtained using Stenhart-Hart equation for thermistors. Input water temperature Tw was used as a parameter (in the range of 5 °C to 25 °C). The maximum thermistor power dissipation was less than 1 W. The inaccuracy of the water flow rate measurement was estimated to be less than 3%. The measuring flowmeter range of 0.003 l/s to 0.3 l/s (1/2 inch pipe) is suitable for measuring water consumption in households.
- 7 March 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Sensors Journal
- Vol. 25 (8) , 12695-12702
Temperature Response, Time Delay, and Hysteresis Loop of Heat Loss Flowmeter Thermistors
A heat loss flowmeter for water was made of two NTC (negative temperature coefficient) thick film thermistors Th1 and Th2 and placed in a metal housing. The first thermistor Th1 is cold and measures input water temperature Tw, and the second thermistor Th2 is self-heated at a constant voltage and measures water flow rate Q. At first temperature responses T(Q), heat loss and time delay td were measured and analyzed. Then a temperature hysteresis loops of self-heating thermistor at switching waterflow regime was measured. The electrical responses I(Q) were measured using the flowmeter and DAC (digital acquisition card). An independent ultrasonic flowmeter was used in series with a novel heat loss flowmeter. The current values of temperature T(Q, t) of the water flow Q(t) were obtained using Stenhart-Hart equation for thermistors. Input water temperature Tw was used as a parameter (in the range of 5 °C to 25 °C). The maximum thermistor power dissipation was less than 1 W. The inaccuracy of the water flow rate measurement was estimated to be less than 3%. The measuring flowmeter range of 0.003 l/s to 0.3 l/s (1/2 inch pipe) is suitable for measuring water consumption in households.
- Open Access
Cavitation Erosion of Protective Coating Based on Cordierite Filler and Epoxy Matrix
The goal of this study is to investigate the surface morphology changes induced by the cavitation erosion of a coating based on cordierite with an epoxy matrix for an aluminum substrate. The literature review shows a certain lack of knowledge regarding the coating’s resistance to wearing induced by water flow, which is a highly important property of the material immersed in or in contact with water streams. The main idea behind the investigation is that such a protective coating will also improve the cavitation erosion resistance of metal substrates. The protective coatings were based on cordierite filler (88 wt.%) and epoxy resin (7 wt.%). The filler, made of a mixture of kaolin, alumina, and talc, is obtained by a sintering procedure that took place at 1350 °C. X-ray diffraction analysis and scanning electron microscopy were employed in the characterization of the produced filler. The adherence of the obtained epoxy-based protective coating and resistance to water flow were tested by the ultrasonic vibration method (i.e., cavitation erosion testing). Scanning electron microscopy was used for analysis of the coating’s morphology upon cavitation erosion. Based on the value of the cavitation erosion rate and the analyzed final surface damage, it was assessed that the investigated protective coating is resistant to cavitation erosion.
Open AccessCavitation Erosion of Protective Coating Based on Cordierite Filler and Epoxy Matrix
The goal of this study is to investigate the surface morphology changes induced by the cavitation erosion of a coating based on cordierite with an epoxy matrix for an aluminum substrate. The literature review shows a certain lack of knowledge regarding the coating’s resistance to wearing induced by water flow, which is a highly important property of the material immersed in or in contact with water streams. The main idea behind the investigation is that such a protective coating will also improve the cavitation erosion resistance of metal substrates. The protective coatings were based on cordierite filler (88 wt.%) and epoxy resin (7 wt.%). The filler, made of a mixture of kaolin, alumina, and talc, is obtained by a sintering procedure that took place at 1350 °C. X-ray diffraction analysis and scanning electron microscopy were employed in the characterization of the produced filler. The adherence of the obtained epoxy-based protective coating and resistance to water flow were tested by the ultrasonic vibration method (i.e., cavitation erosion testing). Scanning electron microscopy was used for analysis of the coating’s morphology upon cavitation erosion. Based on the value of the cavitation erosion rate and the analyzed final surface damage, it was assessed that the investigated protective coating is resistant to cavitation erosion.
- Open Access
- 1 January 2025
- Published by National Library of Serbia in Science of Sintering
- No. 00,p. 43
Colossal permittivity of sintered BaFe12O19 doped with SiO2 in the very low frequency region
Barium hexaferrite BaFe12O19 composition was prepared using the respective powder mixture of metal oxides BaCO3 : 6?Fe2O3 and by performing a solid-state reaction at 1000?C/4h in air. The obtained barium hexaferrite was milled for a prolonged time in the planetary ball mill and agate mill to achieve a fine powder of submicron particle size. The prepared powder was characterized using XRD and SEM techniques.The BaFe12O19 submicron powder was mixed with 2.5 % wt. SiO2 nanopowder as a dopant. After that, the doped barium hexaferrite powder mixture was pressed into small and thin disk samples at 0.2 GPa. The prepared disk samples were sintered at different sintering profiles from 1050?C to 1275?C/2h in air. The sintered samples were also characterized using XRD and SEM. The main electrical properties such as disk capacitance C and resistance R at 1Hz to 100 Hz were measured using a low frequency impedance analyzer. The dielectric permittivity ?r and dissipation factor tg? were calculated from the equivalent disk capacitor electrical schemes. The obtained results were used for observing space charge relaxation effects and colossal permittivity.
- 1 January 2025
- Published by National Library of Serbia in Science of Sintering
- No. 00,p. 43
Open AccessColossal permittivity of sintered BaFe12O19 doped with SiO2 in the very low frequency region
Barium hexaferrite BaFe12O19 composition was prepared using the respective powder mixture of metal oxides BaCO3 : 6?Fe2O3 and by performing a solid-state reaction at 1000?C/4h in air. The obtained barium hexaferrite was milled for a prolonged time in the planetary ball mill and agate mill to achieve a fine powder of submicron particle size. The prepared powder was characterized using XRD and SEM techniques.The BaFe12O19 submicron powder was mixed with 2.5 % wt. SiO2 nanopowder as a dopant. After that, the doped barium hexaferrite powder mixture was pressed into small and thin disk samples at 0.2 GPa. The prepared disk samples were sintered at different sintering profiles from 1050?C to 1275?C/2h in air. The sintered samples were also characterized using XRD and SEM. The main electrical properties such as disk capacitance C and resistance R at 1Hz to 100 Hz were measured using a low frequency impedance analyzer. The dielectric permittivity ?r and dissipation factor tg? were calculated from the equivalent disk capacitor electrical schemes. The obtained results were used for observing space charge relaxation effects and colossal permittivity.
- Open Access
- 1 January 2025
- Published by National Library of Serbia in Science of Sintering
- Vol. 57 (4) , 503-512
Intergranular capacitance of sintered $ \mathrm{BaFe_{12}}\mathrm{O_{19}} $ doped with $ \mathrm{TiO_2} $ in the very low frequency regionA powder of \mathrm{BaFe_{12}}\mathrm{O_{19}} composition (barium hexaferrite) was prepared by using the respective mixture of metal oxides and performing a solid-state reaction at 1000?C/4h in air. The obtained barium hexaferrite powder was milled for a prolonged time in the planetary ball mill and agate mill to achieve submicron powder. The \mathrm{BaFe_{12}}\mathrm{O_{19}} submicron powder was mixed with \mathrm{TiO_2} nanopowder as a dopant. The prepared powder mixture was characterized by using XRD and SEM techniques. After that, the barium hexaferrite powder mixture was pressed into thin and small diameter size disk-shaped samples and sintered at different sintering profiles from 1050?C to 1275?C/2h to 6h. The sintered samples were also characterized by using XRD and SEM. The main electrical properties such as capacitance (intergranular) and bulk resistance R at 1 Hz to 100 Hz were measured at room temperature. The dielectric permittivity was calculated from the equivalent scheme of disk capacitor. The obtained results were used for observing space charge relaxation effects and development of multilayer capacitor forenergy storage device.
- 1 January 2025
- Published by National Library of Serbia in Science of Sintering
- Vol. 57 (4) , 503-512
Open AccessIntergranular capacitance of sintered $ \mathrm{BaFe_{12}}\mathrm{O_{19}} $ doped with $ \mathrm{TiO_2} $ in the very low frequency regionA powder of \mathrm{BaFe_{12}}\mathrm{O_{19}} composition (barium hexaferrite) was prepared by using the respective mixture of metal oxides and performing a solid-state reaction at 1000?C/4h in air. The obtained barium hexaferrite powder was milled for a prolonged time in the planetary ball mill and agate mill to achieve submicron powder. The \mathrm{BaFe_{12}}\mathrm{O_{19}} submicron powder was mixed with \mathrm{TiO_2} nanopowder as a dopant. The prepared powder mixture was characterized by using XRD and SEM techniques. After that, the barium hexaferrite powder mixture was pressed into thin and small diameter size disk-shaped samples and sintered at different sintering profiles from 1050?C to 1275?C/2h to 6h. The sintered samples were also characterized by using XRD and SEM. The main electrical properties such as capacitance (intergranular) and bulk resistance R at 1 Hz to 100 Hz were measured at room temperature. The dielectric permittivity was calculated from the equivalent scheme of disk capacitor. The obtained results were used for observing space charge relaxation effects and development of multilayer capacitor forenergy storage device.
- Open Access
- 25 December 2024
- Published by MDPI AG in Preprints.org
Cavitation Erosion of the Surface of Protective Coating Based on Cordierite Filler and Epoxy Matrix
The goal of this study was to investigate the surface morphology changes induced by cavitation erosion of a coating based on cordierite with epoxy matrix for aluminium substrate. The literature review shows a certain gap in knowledge regarding coating's resistance to wearing induced by water flow, which is a highly important property of the material immersed in or in contact with water streams. The main idea behind the investigation is that such protective coating will also improve the cavitation erosion resistance of metal substrates. The protective coatings were based on cordierite filler (88 wt.%) and epoxy resin (7 wt.%). The filler made of mixture of kaolin, alumina, and talc is obtained by a sintering procedure that took place at 1350°C. X-ray diffraction analysis and scanning electron microscopy were employed in the characterization of the produced filler. Adherence of the obtained epoxy-based protective coating and resistance to water flow were tested by the ultrasonic vibration method (i.e., cavitation erosion testing). Scanning electron microscopy was used for analysis of the coating's morphology upon cavitation erosion. Based on the value of the cavitation erosion rate and the analyzed final surface damage, it was assessed that the investigated protective coating is resistant to cavitation erosion.
- 25 December 2024
- Published by MDPI AG in Preprints.org
Open AccessCavitation Erosion of the Surface of Protective Coating Based on Cordierite Filler and Epoxy Matrix
The goal of this study was to investigate the surface morphology changes induced by cavitation erosion of a coating based on cordierite with epoxy matrix for aluminium substrate. The literature review shows a certain gap in knowledge regarding coating's resistance to wearing induced by water flow, which is a highly important property of the material immersed in or in contact with water streams. The main idea behind the investigation is that such protective coating will also improve the cavitation erosion resistance of metal substrates. The protective coatings were based on cordierite filler (88 wt.%) and epoxy resin (7 wt.%). The filler made of mixture of kaolin, alumina, and talc is obtained by a sintering procedure that took place at 1350°C. X-ray diffraction analysis and scanning electron microscopy were employed in the characterization of the produced filler. Adherence of the obtained epoxy-based protective coating and resistance to water flow were tested by the ultrasonic vibration method (i.e., cavitation erosion testing). Scanning electron microscopy was used for analysis of the coating's morphology upon cavitation erosion. Based on the value of the cavitation erosion rate and the analyzed final surface damage, it was assessed that the investigated protective coating is resistant to cavitation erosion.
- Open Access
Thermally Coupled NTC Chip Thermistors: Their Properties and Applications
Negative temperature coefficient (NTC) chip thermistors were thermally coupled to form a novel device (TCCT) aimed for application in microelectronics. It consists of two NTC chip thermistors Th1 and Th2, which are small in size (0603) and power (1/10 W). They are in thermal junction, but concurrently they are electrically isolated. The first thermistor Th1 generates heat as a self-heating component at a constant supply voltage U (input thermistor), while the second thermistor Th2 receives heat as a passive component (output thermistor). The temperature dependence R(T) of NTC chip thermistors was measured in the climatic test chamber, and the exponential factor B10/30 of thermistor resistance was determined. After that, a self–heating current I1 of the input thermistor was measured vs. supply voltage U and ambient temperature Ta as a parameter. Input resistance R1 was determined as a ratio of U and I1 while output thermistor resistance R2 was measured by a multimeter concurrently with the current I1. Temperatures T1 and T2 of both thermistors were determined using the Steinhart–Hart equation. Heat transfer, thermal response, stability, and inaccuracy were analyzed. The application of thermally coupled NTC chip thermistors is expected in microelectronics for the input to output electrical decoupling/thermal coupling of slow changeable signals.
Open AccessThermally Coupled NTC Chip Thermistors: Their Properties and Applications
Negative temperature coefficient (NTC) chip thermistors were thermally coupled to form a novel device (TCCT) aimed for application in microelectronics. It consists of two NTC chip thermistors Th1 and Th2, which are small in size (0603) and power (1/10 W). They are in thermal junction, but concurrently they are electrically isolated. The first thermistor Th1 generates heat as a self-heating component at a constant supply voltage U (input thermistor), while the second thermistor Th2 receives heat as a passive component (output thermistor). The temperature dependence R(T) of NTC chip thermistors was measured in the climatic test chamber, and the exponential factor B10/30 of thermistor resistance was determined. After that, a self–heating current I1 of the input thermistor was measured vs. supply voltage U and ambient temperature Ta as a parameter. Input resistance R1 was determined as a ratio of U and I1 while output thermistor resistance R2 was measured by a multimeter concurrently with the current I1. Temperatures T1 and T2 of both thermistors were determined using the Steinhart–Hart equation. Heat transfer, thermal response, stability, and inaccuracy were analyzed. The application of thermally coupled NTC chip thermistors is expected in microelectronics for the input to output electrical decoupling/thermal coupling of slow changeable signals.
- 14 March 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Sensors Journal
- Vol. 24 (8) , 12058-12065
Thermally Coupled NTC Disk Thermistors for Power Applications
A pair of small disc NTC thermistors were joined together laterally using a thin layer of silicon resin between them to form a novel thermally coupled device (TCT). The epoxy coating on disc thermistors enables concurrent galvanic isolation and thermal coupling. Input thermistor Th 1 in the coupled pair was self-heated at constant voltages and acts as heat transmitter while the output thermistor Th 2 acted as a heat receiver through the epoxy layer and silicon resin. Small NTC disc thermistors with different nominal resistances were produced out of nickel manganese and modified nickel manganese powder. The disc thermistor resistances and the thermistor exponential temperature factor B were measured in the climatic test chamber. The input power, resistance and temperature of both disc thermistors were measured at different ambient temperatures as a function of input voltage and time. The temperature of thermistors Th 1 and Th 2 (input and output) was determined using the Steinhart - Hart equation. The TCT device sensitivity, stability and inaccuracy were also analyzed. The applications of disc TCT device are based on the measuring of output temperature vs. input power in automotive electronics, home appliances and power convertors.
- 14 March 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Sensors Journal
- Vol. 24 (8) , 12058-12065
Thermally Coupled NTC Disk Thermistors for Power Applications
A pair of small disc NTC thermistors were joined together laterally using a thin layer of silicon resin between them to form a novel thermally coupled device (TCT). The epoxy coating on disc thermistors enables concurrent galvanic isolation and thermal coupling. Input thermistor Th 1 in the coupled pair was self-heated at constant voltages and acts as heat transmitter while the output thermistor Th 2 acted as a heat receiver through the epoxy layer and silicon resin. Small NTC disc thermistors with different nominal resistances were produced out of nickel manganese and modified nickel manganese powder. The disc thermistor resistances and the thermistor exponential temperature factor B were measured in the climatic test chamber. The input power, resistance and temperature of both disc thermistors were measured at different ambient temperatures as a function of input voltage and time. The temperature of thermistors Th 1 and Th 2 (input and output) was determined using the Steinhart - Hart equation. The TCT device sensitivity, stability and inaccuracy were also analyzed. The applications of disc TCT device are based on the measuring of output temperature vs. input power in automotive electronics, home appliances and power convertors.
- Open Access
- 1 January 2024
- Published by National Library of Serbia in Science of Sintering
- Vol. 56 (3) , 299-308
Characterization of NTC thick film thermistor paste Cu0.2Ni0.5Zn1.0Mn1.3O4
A powder of Cu0.2Ni0.5Zn1.0 Mn1.3O4 composition for custom thermistor was prepared by using the respective mixture of metal oxides and solid state reaction at 1000 ?C/4h in air. The obtained thermistor powder was milled in the planetary ball mill and agate mill for a prolonged time to achieve submicron powder. The prepared thermistor powder was further characterized by using XRD and SEM techniques. After that, the thermistor powder was pressed into small disc-shaped samples and sintered at 1150?C/2h. The sintered samples were also characterized by using XRD and SEM. The main electrical properties such as nominal resistance R and thermistor exponential factor B were measured in the climatic test chamber. After that, the thick film paste was prepared using the same powder, an organic vehicle and a glass frit. The paste was printed on alumina substrate, dried at 150 =?C /30 min and sintered in air at 850?C /10 min in a hybrid conveyor furnace. Planar electrodes were printed on the sintered NTC thermistor layer using PdAg thick film paste. The electric properties of the sintered thick film thermistor were also measured in the climatic test chamber. The obtained results were used for development of novel self-heating thermistor applications.
- 1 January 2024
- Published by National Library of Serbia in Science of Sintering
- Vol. 56 (3) , 299-308
Open AccessCharacterization of NTC thick film thermistor paste Cu0.2Ni0.5Zn1.0Mn1.3O4
A powder of Cu0.2Ni0.5Zn1.0 Mn1.3O4 composition for custom thermistor was prepared by using the respective mixture of metal oxides and solid state reaction at 1000 ?C/4h in air. The obtained thermistor powder was milled in the planetary ball mill and agate mill for a prolonged time to achieve submicron powder. The prepared thermistor powder was further characterized by using XRD and SEM techniques. After that, the thermistor powder was pressed into small disc-shaped samples and sintered at 1150?C/2h. The sintered samples were also characterized by using XRD and SEM. The main electrical properties such as nominal resistance R and thermistor exponential factor B were measured in the climatic test chamber. After that, the thick film paste was prepared using the same powder, an organic vehicle and a glass frit. The paste was printed on alumina substrate, dried at 150 =?C /30 min and sintered in air at 850?C /10 min in a hybrid conveyor furnace. Planar electrodes were printed on the sintered NTC thermistor layer using PdAg thick film paste. The electric properties of the sintered thick film thermistor were also measured in the climatic test chamber. The obtained results were used for development of novel self-heating thermistor applications.
- 27 July 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Sensors Journal
- Vol. 23 (18) , 21010-21017
Thermally Coupled Thick-Film Thermistors: Main Properties and Applications
A pair of thick film segmented themistors with negative temperature coefficient (NTC) were joined together (back-to-back) to form thermally coupled device (TCT). The alumina substrate enables a very high galvanic insulation of thermistors and thermal coupling at the same time. The input thermistor R 1 in the coupled pair was self-heated at constant voltages and the output thermistor R 2 was a heat receiver through the alumina substrate. Custom designed NTC thick film thermistor pastes were made out of nickel manganese and modified nickel manganese. Thermistor electrical resistances were measured in a climatic test chamber and the themistor exponential temperature factor B was determined for both pastes. The TCT device was electrically characterized at different ambient temperatures. The input power, heat transfer, resistance and temperature of both thermistors were measured as a function of input voltage and time. The input and output thermistor temperatures T 1 and T 2 were obtained using thermistor resistance and Steinhart - Hart equation.The device sensitivity and measuring inaccuracy were analyzed. The main advantage of TCT is thermal coupling / electrical decoupling. The applications of TCT device are seen in automotive electronics, home appliances and power convertors to measure output temperature vs. input power.
- 27 July 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Sensors Journal
- Vol. 23 (18) , 21010-21017
Thermally Coupled Thick-Film Thermistors: Main Properties and Applications
A pair of thick film segmented themistors with negative temperature coefficient (NTC) were joined together (back-to-back) to form thermally coupled device (TCT). The alumina substrate enables a very high galvanic insulation of thermistors and thermal coupling at the same time. The input thermistor R 1 in the coupled pair was self-heated at constant voltages and the output thermistor R 2 was a heat receiver through the alumina substrate. Custom designed NTC thick film thermistor pastes were made out of nickel manganese and modified nickel manganese. Thermistor electrical resistances were measured in a climatic test chamber and the themistor exponential temperature factor B was determined for both pastes. The TCT device was electrically characterized at different ambient temperatures. The input power, heat transfer, resistance and temperature of both thermistors were measured as a function of input voltage and time. The input and output thermistor temperatures T 1 and T 2 were obtained using thermistor resistance and Steinhart - Hart equation.The device sensitivity and measuring inaccuracy were analyzed. The main advantage of TCT is thermal coupling / electrical decoupling. The applications of TCT device are seen in automotive electronics, home appliances and power convertors to measure output temperature vs. input power.
- Open Access
- 1 January 2023
- Published by National Library of Serbia in Science of Sintering
- Vol. 55 (3) , 413-423
Electronic properties of BZT nano-ceramic grades at low frequency region
BZT ceramics was prepared by using fine powder mixture of BaCO3, TiO2 and ZrO2 in the respective molar ratio to form Ba(Zr0.10Ti0.90)O3 via solid state reaction at elevated temperature. The prepared BZT was milled in the planetary ball mill from 0-120 min to achieve different powder grades from micron to nano-sized particles. After the powder characterization by XRD and SEM the samples were pressed in disc shape and sintered at different temperatures from 1100-1350?C in the air. The sintered samples were characterized by SEM and their density and average grain size was determined and presented vs. sintering temperature and powder grades (milling time). After that the silver epoxy electrodes were deposited on sintered disc samples. The disc samples capacity and resistivity were measured at low frequency region from 1 Hz to 200 kHz using low frequency impedance analyzer. The sintering temperatures and powder grades were used as parameters. Finally the specific resistance ?, dielectric constant (?' + j?") and tg? where determined from the impedance measurements. The behavior of electronic properties where analyzed e.g. the relaxation effect of the space charge (inter-granular electric charges) vs. sintering temperature and ceramic grades. The results obtained were compared with best literature data for the losses in BZT ceramics at low frequencies.
- 1 January 2023
- Published by National Library of Serbia in Science of Sintering
- Vol. 55 (3) , 413-423
Open AccessElectronic properties of BZT nano-ceramic grades at low frequency region
BZT ceramics was prepared by using fine powder mixture of BaCO3, TiO2 and ZrO2 in the respective molar ratio to form Ba(Zr0.10Ti0.90)O3 via solid state reaction at elevated temperature. The prepared BZT was milled in the planetary ball mill from 0-120 min to achieve different powder grades from micron to nano-sized particles. After the powder characterization by XRD and SEM the samples were pressed in disc shape and sintered at different temperatures from 1100-1350?C in the air. The sintered samples were characterized by SEM and their density and average grain size was determined and presented vs. sintering temperature and powder grades (milling time). After that the silver epoxy electrodes were deposited on sintered disc samples. The disc samples capacity and resistivity were measured at low frequency region from 1 Hz to 200 kHz using low frequency impedance analyzer. The sintering temperatures and powder grades were used as parameters. Finally the specific resistance ?, dielectric constant (?' + j?") and tg? where determined from the impedance measurements. The behavior of electronic properties where analyzed e.g. the relaxation effect of the space charge (inter-granular electric charges) vs. sintering temperature and ceramic grades. The results obtained were compared with best literature data for the losses in BZT ceramics at low frequencies.