NKNikolai Kobasko

Nikolai Kobasko

*This is an algorithmically generated author record based on publicly available information.

Nikolai Kobasko has a total of 13 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Heat Transfer Fundamentals Concerning Quenching Materials in Cold Fluids

    by Nikolai Kobasko

    The current chapter discusses three principles of heat transfer related to transient nucleate boiling process when any film boiling during quenching is completely absent. They include the duration of nucleate boiling establishment, surface temperature behavior during self-regulated thermal process, and generalized fundamental equation for evaluation of transient nucleate boiling length. In fact, majority of authors in their analytical and experimental investigations always considered three classical heat transfer modes: film boiling, nucleate boiling, and convection. It is shown in the chapter that the absence of film boiling process simplifies numerical and analytical calculations. It is very important to know that mentioned principles can be used for calculation of temperature fields and stresses and development of new technologies without performing costly experiments. It is stated that universal correlation for heating and cooling time evaluation, modified by proposed principles, can be widely used for recipes development when exploring new intensive quenching technologies. Examples of calculations are provided.


  • Open Access

    Cooling process optimization during hardening steel in water polyalkylene glycol solutions

    by Nikolai Kobasko

    Objects of investigations are water solutions of polyalkylene glycol (PAG) which are used as the quenchants in the heat-treating industry. They are tested by standard cylindrical probe made of Inconel 600 material. The main and not solved yet is the problem of transition from data achieved for standard probe to data suitable for any form and size of real steel part. It opens possibility to make predictable calculations. Taken this into account, it has been investigated water solutions of PAG of different concentration. It is underlined that cooling intensity of quenchant can be evaluated by Kondratiev number Kn. The mentioned number Kn varies within 0≤Kn≤1 when generalized Biot Biv number varies within 0≤Biv≤∞. As a main achievement of investigation is established correlation between standard Kn number and Kn number of real steel part. In many cases, when film boiling is absent, the established correlation is a linear function. It allows optimizing quenching processes: obtain high surface compressive residual stresses, save alloy elements and improve environment condition. All of this is achieved by tolerating chemical composition of steel with size and form of quenched object as it is proposed by UA Patent No. 114174. Also, the number Kn allows interruption of quench process when surface compressive residual stresses are at their maximum value that essentially improves the quality of steel components. Moreover, interrupted cooling prevents quench crack formation, decreases distortion of quenched steel parts. The results of investigations can be used by engineers in the heat-treating industry and scientists for further research.

  • Open Access

    Intensive Quenching Technology Accuracy Analysis Based on Study Physics of Transient Nucleate Boiling Process

    by Nikolai I. Kobasko

    Intensive Quenching Technology Accuracy Analysis Based on Study Physics of Transient Nucleate Boiling Process

  • Open Access

    NEW DIRECTION IN LIQUID QUENCHING MEDIA DEVELOPMENT

    by N.I. Kobasko, A.A. Moskalenko, P.N. Logvinenko, V.V. Dobryvechir

    It is shown that in contrast to well known surface active additives (SAA), affecting physical properties of a liquid, the elimination of film boiling during quenching is achieved by creation of the thin polymeric layer on the surface of hardened metal. It is performed by using special polymers of optimal concentration in water. The obtained insulating polymeric layer decreases initial heat flux density below its critical value and by this way eliminates completely the film boiling without affecting clearly the physical properties of a liquid. Based on this fact and on the principle of decreasing distortion, quench crack formation, and increasing strength of material during intensive quenching, it is proposed to use low concentration of special polymers instead of their high concentration in water. All of this results in significant strengthening of metal, saves costly materials, and increases service life of hardened products.


  • Open Access

    NEW APPROACH IN MODIFYING QUENCHING PROCESSES BASED ON POSSIBILITY OF CONTROLLING STEEL’S SURFACE TEMPERATURE BY INSULATING LAYER

    by Nikolai Kobasko

    In the paper is shown a possibility to govern surface temperature of steel parts during quenching by controlling the thickness of the insulating layer. That results in developing the new quenching technologies like austempering process via cold liquids. The investigations were performed with a low concentration of the polyethylene in cold water using 20 mm cylindrical probe instrumented with two thermocouples. It is established that with the increase concentration of polyoxyethylene in cold water (beginning from 0.001 %) different heat transfer modes are observed resulting in the elimination of film boiling process at 0.001 % concentration, increasing surface temperature of probe during self – regulated thermal process, periodical changing of heat flux densities, slow cooling of surface temperature like in oil when concentration reaches 1 % polyoxyethylene in water, and so on. It is underlined that low concentration of polyoxyethylene in water can serve as an excellent quenchant for accelerated and uniform cooling of steel parts decreasing by this way the cost of a coolant. In this case accelerated cooling should be interrupted at proper time to provide optimal hardened layer afterr quenching. Such approach guarantees increasing service life of steel parts after accelerated cooling with the significant decrease of their cost and eliminates carburization process, The technology can be used for hardening large steel parts like large wind mill gears, large bearing rings, etc.


  • Phenomena of Physics Taking Place During Hardening of Steel Parts in Liquid Media That Can Be Investigated by Liščić/Petrofer Probe

    by Nikolai I. Kobasko

    This article discusses some phenomena of physics taking place during the quenching of steel parts in liquid media, such as the formation of a double surface electrical layer, poker effect, the existence of the second spike of the cooling rate during the quenching of the standard probe in salt water and alkali water solutions, and the self-regulation of the part surface temperature during the transient nucleate boiling process. A double electrical layer is conceived around the steel part surface during quenching in salt water or alkali water solutions. This layer prevents the film boiling during quenching because of electrical forces arising in it. This is a reason for maximizing critical heat flux densities. When immersing the quench probe into a salt (alkali) water solution, the probe surface temperature drops almost instantly (within 1–2 s) to the liquid boiling point and remains at this level for a relatively long time. A so-called self-regulated thermal process takes place; such a process is possible because of a significant difference between boiling and convection Biot numbers. A new quenching technology that allows for the austempering process to be performed in cold liquids is discussed in the article. It is shown that a Liščić/Petrofer probe can be successfully used for investigations of the discovered phenomena and for controlling austempering processes in cold liquids.

  • A Universal Correlation for the Calculation of Heating and Cooling Time of Any Steel

    by Nikolai I. Kobasko

    In this paper, a universal correlation is proposed for calculating heating and cooling times of any steel part during its hardening. The equation contains Kondratjev form factor K, Kondratjev number Kn, average thermal diffusivity of a material, and a function depending on how N times core temperature of a steel part differs from its initial temperature. It is shown that these parameters are enough to calculate recipes when heating and cooling the steel parts of any configuration. A tendency of thermal equilibrium establishment is considered, which depends on size and configuration of objects, thermal diffusivity of a material, and the condition of cooling (heating) characterized by Kondratjev number Kn. The proposed generalized equation provides engineers with extremely simple and understandable parameters for calculating heating (cooling) soak time of any objects. According to the proposed equation, the time of thermal equilibrium establishment is directly proportional to Kondrtajev form factor K, inversely proportional to thermal diffusivity of material and Kondratjev number Kn, and depends on accuracy of the thermal equilibrium measurement.


  • Open Access

    NEW WAYS OF DESIGNING SUPER STRONG MATERIALS BASED ON USE OF ALLOYED LOW HARDENABILITY STEELS

    by Nikolai Kobasko

    Currently, metallurgists are trying to improve mechanical properties of steel by increasing alloy elements in it that require slow cooling in oils or high concentration of water polymers solutions. The paper discusses opposite way in increasing service life of machine components by cardinal decrease alloy elements in steel and providing intensive cooling in locally agitated plain water performed by moving sprayers. The proposed new approach is based on two fundamental phenomena which include creation of high surface compressive residual stresses after quenching and obtaining super - strengthened material in surface layers after intensive cooling. These two factors compensate decrease alloy elements in steel. The paper provides methodology of calculation for achieving maximal effect in residual surface compressive stress formation and super- strengthening of material depending on martensite finish temperature of steel. Effectiveness and benefits are considerable due to saving alloy elements, energy and increasing service life of products. A team of Ukrainian leading specialists is organized to design appropriate software for governing and optimizing hardening processes with the aim of achieving above benefits and make environment clean. New steel and technology of hardening is based on UA Patents No. 109577 and No. 114174

  • Open Access

    INVESTIGATION OF TRANSIENT NUCLEATE BOILING PROCESSES AND THEIR PRACTICAL USE IN HEAT TREATING INDUSTRY

    by Nikolai Kobasko

    In the paper transient nucleate boiling process is widely discussed. It’s unknown previously and investigated by author characteristics create a basis for designing of new technologies which allow receiving super strengthened materials. Obtained results are also used for appropriate software development to be widely applied for control of technological processes and cooling recipes design. A possibility of transition from real heat transfer coefficients (HTCs) to effective HTCs is discussed in the paper too. It is shown that core temperature of steel parts at the end of transient nucleate boiling (self-regulated thermal process (SRTP)) is a linear function of a part dimension when convective heat transfer coefficient during quenching in liquid media is fixed. Also, it is shown that effective Kondrtajev number Kn is a function of part size and convection intensity and is almost linear function for large sizes of steel parts. Surface temperature at the beginning of self-regulated thermal process and at its end is calculated depending on size and intensity of cooling. Based on obtained new results, it is possible to design DATABASE for liquid quenchants using standard Inconel 600 probe combined with the Liscic/Petrofer probe. Obtained results can be useful for engineers and software designers.


  • Open Access

    RESEARCH ON MAXIMIZING CRITICAL AND REDUCING INITIAL HEAT FLUX DENSITIES TO ELIMINATE ANY FILM BOILING AND MINIMIZE DISTORTION DURING QUENCHING

    by Nikolai Kobasko, Anatolii Moskalenko, Petro Lohvynenko, Volodymyr Dobryvechir

    In the paper the results of testing three types of FUCHS oils: Thermisol QH 120, Thermisol QH 10 and Thermisol QB 46 are discussed. The main attention is paid to critical heat flux densities evaluation because they create a basis for optimizing cooling intensity of any liquid quenchant. In the paper is underlined that any film boiling during quenching is undesirable since it is a reason for big distortion and non-uniform surface harness. It is shown that intensive quenching decreases distortion of steel parts during quenching. To eliminate film boiling during quenching in mineral oils, optimal temperature of oil should be chosen which maximize the first critical heat flux density and special additives should be used to decrease initial heat flux by creating surface micro-coating. Along with the evaluation of heat transfer coefficients, critical heat flux densities inherent to liquid quenchant must be measured first to optimize quenching processes. International DATABASE on cooling characteristics of liquid quenchants must include critical heat flux densities, initial heat flux densities, and heat transfer coefficients allowing optimizing and governing quenching processes.