LBL. I. Bohun

L. I. Bohun

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


L. I. Bohun has a total of 18 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Formation of periodic structures on the surface of 12Cr18Ni10Ti steel with ultrashort laser pulses

    by T. L. Tepla, Z. A. Duriagina, D. Mierzhwiński, M. Nykiel, K. Korniejenko, A. Kostryzhev, L. I. Bohun, A. V. Andreikiv


  • Tribological properties of PLA-based composites produced by 3D printing

    by L. Bohun, D. Mierzwiński, T. Tepla, S. Gądek, M. Nykiel, A.-M. Vasylieva

    The current trends in the development of additive technologies, which are actively used in various industries, have been analysed. Special attention was found to be paid to polylactic acid (PLA), an environmentally friendly and biodegradable polymer widely used in 3D printing due to its low melting point and cost-effectiveness. The tribological properties of PLA were improved by adding clay in different concentrations and changing the filling type during printing. The highest indicators of wear resistance and the minimum coefficient of friction were found in the PLA/0.1Clay composite with Grid 90/85 filling. Such a type of filling provided optimal tribological properties for all composites due to the implementation of an abrasive wear mechanism accompanied by plastic deformation. It was revealed that the introduction of clay plasticized the material, which resulted in the widening of the sliding tracks.Pure PLA and PLA/Clay composites with different clay concentrations (0.1, 0.2, 0.3 g per 50 g PLA) were used for the study. The samples were printed with Sphere/100, Grid 90/100 and Grid 90/85 infill to study the effect of structure and density on tribological properties. Density, clay distribution (SEM), tribological tests, as well as wear track structure and friction mechanisms were investigated. The nature of clay distribution in the obtained filaments was evaluated by scanning electron microscopy (SEM) on a JSM-IT200 scanning electron microscope (Tokyo, Japan). To establish the elemental composition of the clay used to create the filaments, X-ray fluorescence analysis was performed on a CEP-01 Elvax Light X-ray spectrometer. The hardness of the samples was measured by indentation according to the Shore method on the Shore hardness tester HT-6510D. Tribological studies of the obtained samples were carried out according to the ball-on-disk scheme on the Tester T-01M computerized friction machine. The microstructure of the surfaces of the studied samples was analysed using an MBS-9 microscope.The influence of the chemical composition of PLA/Clay and the type of filler on the tribological characteristics, including wear resistance, wear intensity and friction mechanisms, was evaluated. The optimal composite composition (PLA/0.1Clay) and the type of filler (Grid 90/85) were determined to ensure the best performance properties.The work focuses on PLA/Clay composites and dry friction conditions, which require further research for other fillers and operating environments. The results provide a basis for developing environmentally friendly wear-resistant materials with improved tribotechnical properties.The study demonstrates the potential of PLA composites for parts operating in friction pairs without lubrication, particularly in the automotive, medical and textile industries. The results contribute to the development of additive manufacturing for manufacturing wear-resistant parts with complex geometries.The article comprehensively analyses the influence of the composition of PLA composites with the addition of clay and the type of filling during 3D printing on tribological properties. The proposed combination of materials science and tribological methods for optimizing polymer properties significantly contributes to the development of environmentally friendly materials and 3D printing technologies.


  • Differences in structure and properties of the metal of the beam of bridge construction

    by H. V. Krechkovska, А. А. Voitovich, А. R. Dzyubyk, B. І. Kindratskyi, О. S. Lampitskyi, L. I. Bohun

    Mechanical properties of the 15KhSND steel of the beam of the bridge structure were analyzed. It was established that the characteristics of strength and plasticity, as well as the resistance to brittle fracture of the steel of its wall correspond to the regulated values. The values of strength and plasticity of the steel shelf do not exceed the normalized limits, but the low values of its impact strength and brittle cleavages on the macrofractures of the samples indicate a tendency to brittle failure. It was found that the resistance to brittle fracture of the metal from the beam shelf decreased in three times on the longitudinal samples, and in two times on the transverse ones to compare to the inherent brittle fracture resistance of steel from the beam wall.

  • Failure analysis of a motor vehicle suspension helical spring

    by Lviv Polytechnic National University, Lidia Bohun, Eduard Pleshakov, Sergiy Shvachko

    The purpose of this work is to reveal the cause of the failure of the motor vehicle rear suspension barrel-shaped spring with the progressive elasticity characteristic and predict measures to increase the lifetime of springs of this type. The fracture of the spring occurred on the middle coil, which operates under conditions of more severe stress in comparison with other coils. The chemical composition of the spring material, determined by X-ray fluorescence spectral and microstructural analyzes, corresponded to chromium-silicon steel 54SiCr6. In terms of structure and mechanical properties, the spring material met the standards. No traces of decarburization were detected, and no crack initiation, caused by non-metallic inclusions, was found in the material of the fractured spring. Macroscopic examination of the spring surface did not reveal any cracks, scratches, dents, traces of blows with stones and marks of spring coiling tool. Instead, extensive areas of exfoliation of the protective coating were found. The metallographic analysis revealed selective corrosion in the form of pitting damage in places of exfoliation of the protective coating. The fatigue crack propagates from the certain deep pit with the reorientation of the crack plane along the spiral surface to the central axis of the coil wire. After depletion of the safety margin, the spring broke down quickly. The fast fracture zone contains steps of the river pattern formed due to the spiral reorientation of the fracture surface. The research can be used to understand the importance of adhesive strength and wear resistance of protective coatings on the spring surface. Their local exfoliation causes subsequent corrosion damage to the spring, which stimulates its fatigue fracture.