Yejie Cao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Yejie Cao has a total of 37 co-authors. Here are the top co-authors by number of shared publications:
- Yongsheng Liu
Science and Technology on Thermostructural Composite Materials Laboratory Northwestern Polytechnical University Xi'an China
7 shared publications Jing Wang
Science and Technology on Thermostructural Composite Materials Laboratory Northwestern Polytechnical University Xi'an China
4 shared publicationsJingxin Li
Science and Technology on Thermostructural Composite Materials Laboratory Northwestern Polytechnical University Xi'an China
4 shared publicationsYunhai Zhang
Science and Technology on Thermostructural Composites Materials Laboratory Northwestern Polytechnical University Xi'an Shaanxi P. R. China
4 shared publicationsLiyang Cao
Science and Technology on Thermostructural Composites Materials Laboratory Northwestern Polytechnical University Xi'an Shaanxi P. R. China
3 shared publicationsXutong Zheng
Science and Technology on Thermostructural Composite Materials Laboratory, Northwestern Polytechnical University, Xi’an, China
3 shared publications
Latest Publications
- 18 September 2024
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (1)
Oxidation behaviors of yttrium silicate modified SiC f /SiC composites in air and water‐oxygen environments
SiC f /SiC composites have emerged as one of the most promising materials for aero‐engine hot‐end structures. However, their performance is limited by their susceptibility to oxidation and corrosion reactions with oxygen and water vapor. To overcome this challenge, antioxidant‐modified phases are introduced into matrices of SiC f /SiC composites which improve their water and oxygen resistance. In this study, the resistance of SiC f /SiC composites modified by yttrium silicate matrix (SiC f /SiC‐YS composites) to air at 1000–1400°C and water‐oxygen environments at 1200°C was investigated. The diffusion paths of oxygen in SiC f /SiC‐YS composites and the antioxidant behavior of the yttrium silicate matrix were discussed. Additionally, the differences in oxygen and water‐oxygen corrosion resistance of SiC f /SiC‐YS composites at the same temperature were compared. The strength retention of SiC f/ SiC‐YS composites after oxidation and water‐oxygen corrosion at 1200°C were 138.6% and 108.8%, respectively. This indicates that the addition of water vapor accelerated the degradation of SiC f /SiC‐YS composites. By comparing with SiC f /SiC composites, it can be concluded that the modification of the yttrium silicate matrix considerably improved the oxidation resistance of SiC f /SiC composites.
- 18 September 2024
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (1)
Oxidation behaviors of yttrium silicate modified SiC f /SiC composites in air and water‐oxygen environments
SiC f /SiC composites have emerged as one of the most promising materials for aero‐engine hot‐end structures. However, their performance is limited by their susceptibility to oxidation and corrosion reactions with oxygen and water vapor. To overcome this challenge, antioxidant‐modified phases are introduced into matrices of SiC f /SiC composites which improve their water and oxygen resistance. In this study, the resistance of SiC f /SiC composites modified by yttrium silicate matrix (SiC f /SiC‐YS composites) to air at 1000–1400°C and water‐oxygen environments at 1200°C was investigated. The diffusion paths of oxygen in SiC f /SiC‐YS composites and the antioxidant behavior of the yttrium silicate matrix were discussed. Additionally, the differences in oxygen and water‐oxygen corrosion resistance of SiC f /SiC‐YS composites at the same temperature were compared. The strength retention of SiC f/ SiC‐YS composites after oxidation and water‐oxygen corrosion at 1200°C were 138.6% and 108.8%, respectively. This indicates that the addition of water vapor accelerated the degradation of SiC f /SiC‐YS composites. By comparing with SiC f /SiC composites, it can be concluded that the modification of the yttrium silicate matrix considerably improved the oxidation resistance of SiC f /SiC composites.
- 22 August 2024
- Published by Elsevier in Ceramics International
- Vol. 50 (21) , 44103-44118
Significant impact of carbon source on microstructure and water–oxygen corrosion behavior of Si–Y alloy modified SiC/SiC composite
- 22 August 2024
- Published by Elsevier in Ceramics International
- Vol. 50 (21) , 44103-44118
Significant impact of carbon source on microstructure and water–oxygen corrosion behavior of Si–Y alloy modified SiC/SiC composite
- 6 November 2023
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (2) , 1094-1103
Water and oxygen corrosion resistance of SiCf/SiC–SiYBC composites prepared by reactive melt infiltration at 1300°C –1500°C
In this work, the static water and oxygen corrosion behavior of SiCf/SiC–SiYBC composites was systematically studied at 1 300°C to 1 500°C. With the increase in corrosion temperature from 1 300°C to 1 500°C, both the residual strength and strength retention rate of SiCf/SiC–SiYBC composites initially increased and then decreased. The highest strength retention rate achieved was 132%, which was 35% higher than that of SiCf/SiC composites. During water and oxygen corrosion of composites, self‐healing boron silicate glass and the Y2Si2O7 phase with excellent resistance to water and oxygen were generated in situ. The oxidation products are fluid at high temperatures and can fill internal pores and microcracks, thus improving the residual strength of the SiCf/SiC–SiYBC composite. The water corrosion resistance of SiCf/SiC–SiYBC materials has been confirmed to be superior to that of SiCf/SiC composites.
- 6 November 2023
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (2) , 1094-1103
Water and oxygen corrosion resistance of SiCf/SiC–SiYBC composites prepared by reactive melt infiltration at 1300°C –1500°C
In this work, the static water and oxygen corrosion behavior of SiCf/SiC–SiYBC composites was systematically studied at 1 300°C to 1 500°C. With the increase in corrosion temperature from 1 300°C to 1 500°C, both the residual strength and strength retention rate of SiCf/SiC–SiYBC composites initially increased and then decreased. The highest strength retention rate achieved was 132%, which was 35% higher than that of SiCf/SiC composites. During water and oxygen corrosion of composites, self‐healing boron silicate glass and the Y2Si2O7 phase with excellent resistance to water and oxygen were generated in situ. The oxidation products are fluid at high temperatures and can fill internal pores and microcracks, thus improving the residual strength of the SiCf/SiC–SiYBC composite. The water corrosion resistance of SiCf/SiC–SiYBC materials has been confirmed to be superior to that of SiCf/SiC composites.
- 26 June 2023
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 106 (11) , 6937-6950
Optimized ablation resistance behavior and mechanism of C/SiC composites with high thermal conductive channels
Aimed to enhance the high‐temperature service performance of C/SiC composites in high‐speed aircraft thermal protection system, in this article, pitch‐based carbon fibers were used to construct high thermal conductive channels to improve the heat transfer capability of C/SiC composites. The results revealed that the as‐prepared composites equipped with 4.7 times higher thermal conductivity than that of conventional C/SiC composites. The oxyacetylene flame ablation test confirmed that the constructed high thermal conductive channels, which quickly conducted the heat flow from the ablation center area to other areas is the main reason of as‐prepared composites exhibiting a very impressive ablation resistance property. Briefly, the ablation temperature of the as‐prepared composite surfaces considerably dropped by about 300°C compared with conventional C/SiC composites, while the linear ablation rate and mass ablation rate of the composites are 1.27 μm/s and 0.61 mg/s respectively, which is superior to many recent reports, demonstrating that this article provides a simple but highly effective measure to improve the ablation resistance property of C/SiC composites.
- 26 June 2023
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 106 (11) , 6937-6950
Optimized ablation resistance behavior and mechanism of C/SiC composites with high thermal conductive channels
Aimed to enhance the high‐temperature service performance of C/SiC composites in high‐speed aircraft thermal protection system, in this article, pitch‐based carbon fibers were used to construct high thermal conductive channels to improve the heat transfer capability of C/SiC composites. The results revealed that the as‐prepared composites equipped with 4.7 times higher thermal conductivity than that of conventional C/SiC composites. The oxyacetylene flame ablation test confirmed that the constructed high thermal conductive channels, which quickly conducted the heat flow from the ablation center area to other areas is the main reason of as‐prepared composites exhibiting a very impressive ablation resistance property. Briefly, the ablation temperature of the as‐prepared composite surfaces considerably dropped by about 300°C compared with conventional C/SiC composites, while the linear ablation rate and mass ablation rate of the composites are 1.27 μm/s and 0.61 mg/s respectively, which is superior to many recent reports, demonstrating that this article provides a simple but highly effective measure to improve the ablation resistance property of C/SiC composites.
- 12 June 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (24) , 9923-9937
Unveiling the formation of Mo2C coating on diamond particles along with anisotropic etching by Mo powder
- 12 June 2023
- Published by Springer Nature in Journal of Materials Science
- Vol. 58 (24) , 9923-9937
Unveiling the formation of Mo2C coating on diamond particles along with anisotropic etching by Mo powder
- Open Access
- 11 January 2022
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 11 (2) , 247-262
Thermal conductivity and bending strength of SiC composites reinforced by pitch-based carbon fibers
In this work, pitch-based carbon fibers were utilized to reinforce silicon carbide (SiC) composites via reaction melting infiltration (RMI) method by controlling the reaction temperature and resin carbon content. Thermal conductivities and bending strengths of composites obtained under different preparation conditions were characterized by various analytical methods. Results showed the formation of SiC whiskers (SiCw) during RMI process according to vapor—solid (VS) mechanism. SiCw played an important role in toughening the Cpf/SiC composites due to crack bridging, crack deflection, and SiCw pull-out. Increase in reaction temperature during RMI process led to an initial increase in thermal conductivity along in-plane and thickness directions of composites, followed by a decline. At reaction temperature of 1600 °C, thermal conductivities along the in-plane and thickness directions were estimated to be 203.00 and 39.59 W/(m·K), respectively. Under these conditions, bending strength was recorded as 186.15±3.95 MPa. Increase in resin carbon content before RMI process led to the generation of more SiC matrix. Thermal conductivities along in-plane and thickness directions remained stable with desirable values of 175.79 and 38.86 W/(m·K), respectively. By comparison, optimal bending strength improved to 244.62±3.07 MPa. In sum, these findings look promising for future application of pitch-based carbon fibers for reinforcement of SiC ceramic composites.
- 11 January 2022
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 11 (2) , 247-262
Open AccessThermal conductivity and bending strength of SiC composites reinforced by pitch-based carbon fibers
In this work, pitch-based carbon fibers were utilized to reinforce silicon carbide (SiC) composites via reaction melting infiltration (RMI) method by controlling the reaction temperature and resin carbon content. Thermal conductivities and bending strengths of composites obtained under different preparation conditions were characterized by various analytical methods. Results showed the formation of SiC whiskers (SiCw) during RMI process according to vapor—solid (VS) mechanism. SiCw played an important role in toughening the Cpf/SiC composites due to crack bridging, crack deflection, and SiCw pull-out. Increase in reaction temperature during RMI process led to an initial increase in thermal conductivity along in-plane and thickness directions of composites, followed by a decline. At reaction temperature of 1600 °C, thermal conductivities along the in-plane and thickness directions were estimated to be 203.00 and 39.59 W/(m·K), respectively. Under these conditions, bending strength was recorded as 186.15±3.95 MPa. Increase in resin carbon content before RMI process led to the generation of more SiC matrix. Thermal conductivities along in-plane and thickness directions remained stable with desirable values of 175.79 and 38.86 W/(m·K), respectively. By comparison, optimal bending strength improved to 244.62±3.07 MPa. In sum, these findings look promising for future application of pitch-based carbon fibers for reinforcement of SiC ceramic composites.
- 1 June 2021
- Published by Elsevier in Surfaces and Interfaces
- Vol. 24
Effect of deposition temperature and time on microstructure of CVD SiC coating on diamond particles
- 1 June 2021
- Published by Elsevier in Surfaces and Interfaces
- Vol. 24
Effect of deposition temperature and time on microstructure of CVD SiC coating on diamond particles
- 1 February 2018
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 38 (2) , 469-478
Design of polymer-derived SiC for nuclear applications from the perspective of heterogeneous interfaces
- 1 February 2018
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 38 (2) , 469-478
Design of polymer-derived SiC for nuclear applications from the perspective of heterogeneous interfaces