Viera Zatkalíková
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Viera Zatkalíková has a total of 69 co-authors. Here are the top co-authors by number of shared publications:
- Milan Uhríčik
University of Žilina
13 shared publications - Lenka Markovičová
University of Žilina, Faculty of Mechanical Engineering, Department of Material Engineering, Univerzitná 8215/1, 010 26 Žilina, Slovakia
11 shared publications Lenka Markovičová
Univ Zilina, Zilina, Slovakia
10 shared publications- Lenka Kuchariková
Department of Materials Engineering, Faculty of Mechanical Engineering, University of Žilina, Univerzitná 8215/1, 010 26 Žilina, Slovakia
8 shared publications - Alan Vaško
University of Žilina, Faculty of Mechanical Engineering, Department of Materials Engineering, Žilina, Slovakia
5 shared publications L Markovičová
University of Žilina, Faculty of Mechanical Engineering, Department of Materials Engineering, Univerzitná 8215/1, 010 26 Žilina, Slovak Republic
5 shared publications
Latest Publications
- Open Access
The Effect of a CrN Interlayer on the Corrosion-Fatigue Performance of DLC-Coated C55 Steel in Simulated Seawater
The work focused on evaluating the tribological, corrosion, and fatigue properties of a Diamond like Carbon (DLC) coating and a duplex CrN/DLC coating in a 3.5% NaCl solution simulating the aggressive environment of seawater. C55 steel was selected as the substrate material due to its widespread industrial application in the production of highly stressed machine components and its relatively low resistance to corrosion damage. The experimental results demonstrated that the application of DLC and CrN/DLC coatings significantly improved the tribological and corrosion properties of the investigated material in a chloride corrosive environment. At the same time, it was shown that the duplex CrN/DLC coating not only eliminated the negative effect of the corrosive environment on the fatigue properties of C55 steel but even led to their improvement. The fatigue limit of C55 steel with the CrN/DLC coating reached 717 MPa, representing an increase of 3.3% compared with the base material and 29.2% compared with uncoated C55 steel after 72 h of corrosion exposure in a 3.5% NaCl solution. The superior fatigue performance of the CrN/DLC system was associated with its improved adhesion and barrier properties provided by the duplex coating architecture and the CrN interlayer.
Open AccessThe Effect of a CrN Interlayer on the Corrosion-Fatigue Performance of DLC-Coated C55 Steel in Simulated Seawater
The work focused on evaluating the tribological, corrosion, and fatigue properties of a Diamond like Carbon (DLC) coating and a duplex CrN/DLC coating in a 3.5% NaCl solution simulating the aggressive environment of seawater. C55 steel was selected as the substrate material due to its widespread industrial application in the production of highly stressed machine components and its relatively low resistance to corrosion damage. The experimental results demonstrated that the application of DLC and CrN/DLC coatings significantly improved the tribological and corrosion properties of the investigated material in a chloride corrosive environment. At the same time, it was shown that the duplex CrN/DLC coating not only eliminated the negative effect of the corrosive environment on the fatigue properties of C55 steel but even led to their improvement. The fatigue limit of C55 steel with the CrN/DLC coating reached 717 MPa, representing an increase of 3.3% compared with the base material and 29.2% compared with uncoated C55 steel after 72 h of corrosion exposure in a 3.5% NaCl solution. The superior fatigue performance of the CrN/DLC system was associated with its improved adhesion and barrier properties provided by the duplex coating architecture and the CrN interlayer.
- Open Access
Synergistic Effects of Corrosion and Tribocorrosion Behavior in AISI 316Ti Stainless Steel for Engineering and Biomedical Applications
The corrosion behavior of AISI 316Ti stainless steel was examined in NaCl solutions (0.9%, 3.5%, and 5%), whereas tribocorrosion tests were performed in both chloride-containing solutions and distilled water as a reference environment. Potentiodynamic polarization tests were performed to evaluate passive film stability, while tribocorrosion experiments were conducted under a 10 N normal load using a ball-on-flat configuration with continuous monitoring of open circuit potential (OCP) and coefficient of friction (COF). Surface degradation was quantified using optical 3D profilometry and scanning electron microscopy. Electrochemical results confirmed passive behavior in all environments; however, increasing chloride concentration shifted corrosion and pitting potentials toward more negative values and reduced passive stability. During sliding, a pronounced cathodic OCP shift indicated mechanical depassivation, with the magnitude of the shift increasing in chloride-rich solutions. Repassivation after sliding was progressively hindered as NaCl concentration increased. Wear analysis revealed a clear dependence on chloride content, with the wear area in 5% NaCl (0.0020 mm2) exceeding that in distilled water (0.0009 mm2) by approximately 122%. Abrasive wear was identified as the dominant mechanism, accompanied by delamination wear in highly aggressive environments. The results demonstrate a strong synergistic interaction between wear and corrosion, with chloride concentration significantly intensifying tribocorrosion-induced material degradation.
Open AccessSynergistic Effects of Corrosion and Tribocorrosion Behavior in AISI 316Ti Stainless Steel for Engineering and Biomedical Applications
The corrosion behavior of AISI 316Ti stainless steel was examined in NaCl solutions (0.9%, 3.5%, and 5%), whereas tribocorrosion tests were performed in both chloride-containing solutions and distilled water as a reference environment. Potentiodynamic polarization tests were performed to evaluate passive film stability, while tribocorrosion experiments were conducted under a 10 N normal load using a ball-on-flat configuration with continuous monitoring of open circuit potential (OCP) and coefficient of friction (COF). Surface degradation was quantified using optical 3D profilometry and scanning electron microscopy. Electrochemical results confirmed passive behavior in all environments; however, increasing chloride concentration shifted corrosion and pitting potentials toward more negative values and reduced passive stability. During sliding, a pronounced cathodic OCP shift indicated mechanical depassivation, with the magnitude of the shift increasing in chloride-rich solutions. Repassivation after sliding was progressively hindered as NaCl concentration increased. Wear analysis revealed a clear dependence on chloride content, with the wear area in 5% NaCl (0.0020 mm2) exceeding that in distilled water (0.0009 mm2) by approximately 122%. Abrasive wear was identified as the dominant mechanism, accompanied by delamination wear in highly aggressive environments. The results demonstrate a strong synergistic interaction between wear and corrosion, with chloride concentration significantly intensifying tribocorrosion-induced material degradation.
- Open Access
- 12 March 2026
- Published by Elsevier in SSRN Electronic Journal
Environmental Degradation of Plastics: Analysis of Mechanisms, Influencing Factors and Rheological Insights
This study focuses on the degradation behavior and property changes of polyamide/polyamide-imide (PA/PAI) composites reinforced with short glass fibers, with particular emphasis on aspects relevant to failure analysis after accelerated ultraviolet (UV) aging. Composites containing 10%, 20%, and 30% glass fibers were subjected to artificial weathering for 500 hours under controlled conditions. The influence of UV exposure on surface and subsurface regions was evaluated using Shore D hardness measurements, impact toughness testing, oscillatory rheology, and optical microscopy. The results show that conventional mechanical properties, including hardness and impact toughness, exhibit only minor changes after UV aging, indicating their limited sensitivity to the early stages of degradation and damage initiation from a failure analysis perspective. In contrast, oscillatory rheology revealed significant UV-induced molecular degradation manifested by a decrease in complex viscosity and a shift of the modulus cross-over point toward higher frequencies, indicating chain scission and a reduction in molecular weight. Such rheological changes provide important indicators for failure analysis of polymer composites, as they reflect early structural degradation processes preceding macroscopic failure. The degradation was strongly localized in the near-surface region, with the most severe changes occurring within approximately the first 250 µm from the surface, while deeper layers were progressively less affected. Increasing the glass fiber content reduced the effective depth of degradation due to a partial shielding effect against UV radiation and modified oxygen diffusion, resulting in improved resistance to UV-induced degradation. Microstructural observations confirmed the formation of surface cracks and embrittlement of the matrix after UV exposure, with surface-initiated damage identified as a dominant precursor to long-term failure. From the viewpoint of failure analysis, these findings highlight the critical role of surface degradation processes in initiating structural damage in fiber-reinforced polymer composites. Overall, the study demonstrates that oscillatory rheology represents a highly sensitive technique for detecting the early stages of UV-induced degradation in glass fiber-reinforced PA/PAI composites and provides valuable information for failure analysis and lifetime prediction. The results offer important insights for the assessment of durability and reliability of polymer composites used in outdoor and automotive applications, where surface-dominated damage mechanisms can critically influence long-term structural integrity.
- 12 March 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessEnvironmental Degradation of Plastics: Analysis of Mechanisms, Influencing Factors and Rheological Insights
This study focuses on the degradation behavior and property changes of polyamide/polyamide-imide (PA/PAI) composites reinforced with short glass fibers, with particular emphasis on aspects relevant to failure analysis after accelerated ultraviolet (UV) aging. Composites containing 10%, 20%, and 30% glass fibers were subjected to artificial weathering for 500 hours under controlled conditions. The influence of UV exposure on surface and subsurface regions was evaluated using Shore D hardness measurements, impact toughness testing, oscillatory rheology, and optical microscopy. The results show that conventional mechanical properties, including hardness and impact toughness, exhibit only minor changes after UV aging, indicating their limited sensitivity to the early stages of degradation and damage initiation from a failure analysis perspective. In contrast, oscillatory rheology revealed significant UV-induced molecular degradation manifested by a decrease in complex viscosity and a shift of the modulus cross-over point toward higher frequencies, indicating chain scission and a reduction in molecular weight. Such rheological changes provide important indicators for failure analysis of polymer composites, as they reflect early structural degradation processes preceding macroscopic failure. The degradation was strongly localized in the near-surface region, with the most severe changes occurring within approximately the first 250 µm from the surface, while deeper layers were progressively less affected. Increasing the glass fiber content reduced the effective depth of degradation due to a partial shielding effect against UV radiation and modified oxygen diffusion, resulting in improved resistance to UV-induced degradation. Microstructural observations confirmed the formation of surface cracks and embrittlement of the matrix after UV exposure, with surface-initiated damage identified as a dominant precursor to long-term failure. From the viewpoint of failure analysis, these findings highlight the critical role of surface degradation processes in initiating structural damage in fiber-reinforced polymer composites. Overall, the study demonstrates that oscillatory rheology represents a highly sensitive technique for detecting the early stages of UV-induced degradation in glass fiber-reinforced PA/PAI composites and provides valuable information for failure analysis and lifetime prediction. The results offer important insights for the assessment of durability and reliability of polymer composites used in outdoor and automotive applications, where surface-dominated damage mechanisms can critically influence long-term structural integrity.
- Open Access
- 1 December 2025
- Published by Walter de Gruyter GmbH in System Safety: Human - Technical Facility - Environment
- Vol. 7 (1) , 295-304
Influence of Corrosion on the Fatigue Resistance of a Carbon Steel with Ti and Cr Nitrides Based Coatings
The quality of components and structures is directly related to degradation processes such as corrosion and fatigue that are concomitant phenomena during their operation. One of the options for increasing the quality of components and structures is the use of appropriate surface coating. In this paper is presented an experimental investigation of the corrosion influence on the fatigue resistance of the carbon steel with coatings based on Ti and Cr nitrides. The experimental work included determination of the chemical composition of the base material, heat treatment, microstructure evaluation, mechanical properties measurement, coating depositions, corrosion test and the fatigue tests by rotation bending of the deposited layers. The corrosion and fatigue tests have shown that the coating provides improvement of the corrosion resistance and that there was no reduction of the fatigue resistance.
- 1 December 2025
- Published by Walter de Gruyter GmbH in System Safety: Human - Technical Facility - Environment
- Vol. 7 (1) , 295-304
Open AccessInfluence of Corrosion on the Fatigue Resistance of a Carbon Steel with Ti and Cr Nitrides Based Coatings
The quality of components and structures is directly related to degradation processes such as corrosion and fatigue that are concomitant phenomena during their operation. One of the options for increasing the quality of components and structures is the use of appropriate surface coating. In this paper is presented an experimental investigation of the corrosion influence on the fatigue resistance of the carbon steel with coatings based on Ti and Cr nitrides. The experimental work included determination of the chemical composition of the base material, heat treatment, microstructure evaluation, mechanical properties measurement, coating depositions, corrosion test and the fatigue tests by rotation bending of the deposited layers. The corrosion and fatigue tests have shown that the coating provides improvement of the corrosion resistance and that there was no reduction of the fatigue resistance.
- Open Access
- 1 December 2025
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 3157 (1)
Effect of long-term exposure to chloride-containing solution on degradation of plasma-nitrided layer on AISI 316L stainless steel
Austenitic stainless steels are highly corrosion resistant and have appropriate mechanical properties but they are not suitable for applications where high wear resistance is required. Conventional plasma nitriding (PN) is one of the possibilities to increase their hardness and tribological properties. This paper deals with an assessment of a plasma-nitrided surface layer degradation during 2-month exposure of AISI 316L specimens to 0.5 M NaCl solution at room temperature (conditions of PN process: 530 °C, 24 hours). Evaluation is based on corrosion rates calculated from the mass losses of the specimens during exposure and on the characterization of the plasma-nitrided layer before and after exposure (SEM, roughness, microhardness and potentiodynamic polarization performed in 0.5 NaCl solution at room temperature). The experiment results point to an intensive corrosion degradation of the plasma-nitrided layer during exposure, proved by its lower thickness, decreased microhardness and by the changed roughness parameters. According to the potentiodynamic polarization parameters measured after exposure, degradation of the plasma-nitrided layer led to an improvement of corrosion behaviour compared to the state before it.
- 1 December 2025
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 3157 (1)
Open AccessEffect of long-term exposure to chloride-containing solution on degradation of plasma-nitrided layer on AISI 316L stainless steel
Austenitic stainless steels are highly corrosion resistant and have appropriate mechanical properties but they are not suitable for applications where high wear resistance is required. Conventional plasma nitriding (PN) is one of the possibilities to increase their hardness and tribological properties. This paper deals with an assessment of a plasma-nitrided surface layer degradation during 2-month exposure of AISI 316L specimens to 0.5 M NaCl solution at room temperature (conditions of PN process: 530 °C, 24 hours). Evaluation is based on corrosion rates calculated from the mass losses of the specimens during exposure and on the characterization of the plasma-nitrided layer before and after exposure (SEM, roughness, microhardness and potentiodynamic polarization performed in 0.5 NaCl solution at room temperature). The experiment results point to an intensive corrosion degradation of the plasma-nitrided layer during exposure, proved by its lower thickness, decreased microhardness and by the changed roughness parameters. According to the potentiodynamic polarization parameters measured after exposure, degradation of the plasma-nitrided layer led to an improvement of corrosion behaviour compared to the state before it.
- Open Access
The Effect of Surface Corrosion Damage and Fe Content on the Fatigue Life of an AlSi7Mg0.6 Cast Alloy Used in the Electric Automotive Industry
The aluminum casting alloy AlSi7Mg0.6 (A357) is extensively used in the automotive industry due to its favorable balance of mechanical properties, castability, lightweight characteristics, and corrosion resistance. Castings made from this alloy are often subjected to harsh service environments, where surface degradation and microstructural variability can significantly impact fatigue performance. This study investigates the combined effects of surface corrosion damage and higher Fe content on the fatigue life of the AlSi7Mg0.6 alloy, using a rotating bending fatigue test under simultaneous corrosion exposure in a 3.5 wt. % NaCl solution. The effect of corrosion and Fe content on fatigue life was then investigated and analyzed using Wöhler curves and scanning electron microscopy (SEM). The results demonstrate that the corrosion-fatigue interaction accelerated the kinetics of the fatigue process, while the fracture mechanism and crack initiation places are not fundamentally altered compared to alloys in the state without corrosion damage. A comparison of the fatigue lifetime of samples in an air environment and a corrosive environment shows that the corrosive environment (3.5% NaCl) reduces the fatigue lifetime of alloys without T6 by an average of 7.5 MPa and alloys after T6 by 6 MPa. The results are probably due to the penetration of chloride ions into casting defects located on the surface of the samples. Surface pits formed during corrosion act as stress concentrators, increasing the likelihood of stress-induced failure. Microstructural feature morphology, especially Fe-rich intermetallic phases, influences crack propagation mechanisms.
Open AccessThe Effect of Surface Corrosion Damage and Fe Content on the Fatigue Life of an AlSi7Mg0.6 Cast Alloy Used in the Electric Automotive Industry
The aluminum casting alloy AlSi7Mg0.6 (A357) is extensively used in the automotive industry due to its favorable balance of mechanical properties, castability, lightweight characteristics, and corrosion resistance. Castings made from this alloy are often subjected to harsh service environments, where surface degradation and microstructural variability can significantly impact fatigue performance. This study investigates the combined effects of surface corrosion damage and higher Fe content on the fatigue life of the AlSi7Mg0.6 alloy, using a rotating bending fatigue test under simultaneous corrosion exposure in a 3.5 wt. % NaCl solution. The effect of corrosion and Fe content on fatigue life was then investigated and analyzed using Wöhler curves and scanning electron microscopy (SEM). The results demonstrate that the corrosion-fatigue interaction accelerated the kinetics of the fatigue process, while the fracture mechanism and crack initiation places are not fundamentally altered compared to alloys in the state without corrosion damage. A comparison of the fatigue lifetime of samples in an air environment and a corrosive environment shows that the corrosive environment (3.5% NaCl) reduces the fatigue lifetime of alloys without T6 by an average of 7.5 MPa and alloys after T6 by 6 MPa. The results are probably due to the penetration of chloride ions into casting defects located on the surface of the samples. Surface pits formed during corrosion act as stress concentrators, increasing the likelihood of stress-induced failure. Microstructural feature morphology, especially Fe-rich intermetallic phases, influences crack propagation mechanisms.
- Open Access
Wear and Corrosion Behavior of Diamond-like Carbon Coatings in Artificial Saliva
This study investigates the properties of diamond-like carbon (DLC) coatings deposited onto a Ti6Al4V titanium alloy using plasma-assisted chemical vapor deposition (PACVD). The research encompasses adhesion tests, hardness, surface characterization, as well as corrosion and tribological evaluations. Artificial saliva was employed as both the lubricating and corrosive medium. Microscopic examination revealed a uniform coating with a thickness of about 3.2 µm. Scratch test results indicated that the deposited DLC coating exhibited superior adhesion, lower frictional resistance, and reduced wear compared to the titanium alloy. The coating deposition increased the hardness of the Ti6Al4V alloy by about 75%. Friction coefficients, measured under dry and lubricated conditions, were approximately 80% lower for the DLC-coated samples. Corrosion studies revealed that both the coated and uncoated surfaces demonstrated typical passive behavior and high corrosion resistance in artificial saliva. For DLC coatings, the corrosion current density and the corrosion rate were reduced by 85%. Microscopic observations of wear tracks following tribological and scratch tests confirmed the inferior wear and scratch resistance of the titanium alloy relative to the DLC coating. Under both dry and lubricated conditions (with artificial saliva), the volumetric wear rate of the titanium alloy was over 90% higher than for the DLC coating.
Open AccessWear and Corrosion Behavior of Diamond-like Carbon Coatings in Artificial Saliva
This study investigates the properties of diamond-like carbon (DLC) coatings deposited onto a Ti6Al4V titanium alloy using plasma-assisted chemical vapor deposition (PACVD). The research encompasses adhesion tests, hardness, surface characterization, as well as corrosion and tribological evaluations. Artificial saliva was employed as both the lubricating and corrosive medium. Microscopic examination revealed a uniform coating with a thickness of about 3.2 µm. Scratch test results indicated that the deposited DLC coating exhibited superior adhesion, lower frictional resistance, and reduced wear compared to the titanium alloy. The coating deposition increased the hardness of the Ti6Al4V alloy by about 75%. Friction coefficients, measured under dry and lubricated conditions, were approximately 80% lower for the DLC-coated samples. Corrosion studies revealed that both the coated and uncoated surfaces demonstrated typical passive behavior and high corrosion resistance in artificial saliva. For DLC coatings, the corrosion current density and the corrosion rate were reduced by 85%. Microscopic observations of wear tracks following tribological and scratch tests confirmed the inferior wear and scratch resistance of the titanium alloy relative to the DLC coating. Under both dry and lubricated conditions (with artificial saliva), the volumetric wear rate of the titanium alloy was over 90% higher than for the DLC coating.
- Open Access
- 1 December 2024
- Published by Walter de Gruyter GmbH in System Safety: Human - Technical Facility - Environment
- Vol. 6 (1) , 421-429
Effect of Solution Annealing on Corrosion Resistance of Austenitic Stainless Steels in Chloride-Containing Environment
Austenitic stainless steels are highly corrosion-resistant in common oxidation environments. However, aggressive chloride-containing solutions can evoke local corrosion, which performs an important risk in the safe use of these materials. This research deals with the effect of the solution annealing (1050 °C, 15 min) on the electrochemical parameters of AISI 304 and AISI 316L stainless steels. Corrosion resistance of the solution-annealed specimens is evaluated and compared to the as received specimens by the potentiodynamic polarization test performed in 1M pH neutral NaCl solution at the 20 ± 3 °C temperature. The obtained results did not clearly confirm the positive effect of solution annealing on corrosion resistance in the given aggressive solution. Although the pitting potentials indicating higher pitting corrosion resistance increased, the kinetics of the corrosion process intensified.
- 1 December 2024
- Published by Walter de Gruyter GmbH in System Safety: Human - Technical Facility - Environment
- Vol. 6 (1) , 421-429
Open AccessEffect of Solution Annealing on Corrosion Resistance of Austenitic Stainless Steels in Chloride-Containing Environment
Austenitic stainless steels are highly corrosion-resistant in common oxidation environments. However, aggressive chloride-containing solutions can evoke local corrosion, which performs an important risk in the safe use of these materials. This research deals with the effect of the solution annealing (1050 °C, 15 min) on the electrochemical parameters of AISI 304 and AISI 316L stainless steels. Corrosion resistance of the solution-annealed specimens is evaluated and compared to the as received specimens by the potentiodynamic polarization test performed in 1M pH neutral NaCl solution at the 20 ± 3 °C temperature. The obtained results did not clearly confirm the positive effect of solution annealing on corrosion resistance in the given aggressive solution. Although the pitting potentials indicating higher pitting corrosion resistance increased, the kinetics of the corrosion process intensified.
- 24 September 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (3) , 1115-1122
Corrosion Resistance of Austenitic NiMn-Nodular Cast Iron in NaCl Solution
Austenitic nodular cast iron is a versatile material that offers a unique combination of properties, making it suitable for use in a wide range of applications where high strength, ductility, toughness, corrosion resistance and wear resistance are required. This material is commonly used in a variety of applications in the chemical and petrochemical industries, in the automotive and aerospace industries, as well as in marine and offshore applications. For the experiments, one of the most common austenitic nodular cast irons (alloyed with nickel and manganese) was chosen. The aim of this paper is to evaluate the corrosion resistance of this austenitic nodular cast iron and compare it with other (non-austenitic) types of nodular cast iron (SiMo- and SiCu-type). Corrosion resistance was determined by an exposure immersion test and an electrochemical potentiodynamic polarization test. Both tests were performed in a 3.5% NaCl solution (to simulate seawater) at ambient temperature. Experimental results prove that austenitic NiMn-nodular cast iron has a higher corrosion resistance than SiMo- and SiCu-nodular cast iron. Moreover, austenitic nodular cast iron has better plastic properties (higher elongation and absorbed energy) but worse strength and fatigue properties (lower tensile strength, hardness and fatigue limit) than the other types of nodular cast iron.
- 24 September 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (3) , 1115-1122
Corrosion Resistance of Austenitic NiMn-Nodular Cast Iron in NaCl Solution
Austenitic nodular cast iron is a versatile material that offers a unique combination of properties, making it suitable for use in a wide range of applications where high strength, ductility, toughness, corrosion resistance and wear resistance are required. This material is commonly used in a variety of applications in the chemical and petrochemical industries, in the automotive and aerospace industries, as well as in marine and offshore applications. For the experiments, one of the most common austenitic nodular cast irons (alloyed with nickel and manganese) was chosen. The aim of this paper is to evaluate the corrosion resistance of this austenitic nodular cast iron and compare it with other (non-austenitic) types of nodular cast iron (SiMo- and SiCu-type). Corrosion resistance was determined by an exposure immersion test and an electrochemical potentiodynamic polarization test. Both tests were performed in a 3.5% NaCl solution (to simulate seawater) at ambient temperature. Experimental results prove that austenitic NiMn-nodular cast iron has a higher corrosion resistance than SiMo- and SiCu-nodular cast iron. Moreover, austenitic nodular cast iron has better plastic properties (higher elongation and absorbed energy) but worse strength and fatigue properties (lower tensile strength, hardness and fatigue limit) than the other types of nodular cast iron.
- Open Access
- 24 September 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (3) , 1123-1130
Effect of Mn Addition on the Corrosion and Fatigue Properties of a Progressive Secondary A357 Alloy
As the modern automotive industry is looking for lightweight alternatives to minimize car emissions and fuel consumption, recycled Al-Si alloys play a key role in achieving this due to their lightweight, high specific strength, good castability, and corrosion resistance. In contrast to many other benefits, these alloys have reduced metallurgical micropurity as a result of recycling. The most significant complication of alloys is iron contamination. Higher Fe contents cause β-Fe-intermetallic phases in the form of long and brittle platelets that negatively affect corrosion resistance and fatigue. Neutralizing elements lead to the formation of less harmful α-Fe-rich phases, therefore a positive effect on properties is also expected. For this reason, the study investigates the effect of Mn addition on the corrosion properties achieved by immersion test and potentiodynamic polarization test and fatigue of secondary AlSi7Mg0.6 secondary alloy.
- 24 September 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (3) , 1123-1130
Open AccessEffect of Mn Addition on the Corrosion and Fatigue Properties of a Progressive Secondary A357 Alloy
As the modern automotive industry is looking for lightweight alternatives to minimize car emissions and fuel consumption, recycled Al-Si alloys play a key role in achieving this due to their lightweight, high specific strength, good castability, and corrosion resistance. In contrast to many other benefits, these alloys have reduced metallurgical micropurity as a result of recycling. The most significant complication of alloys is iron contamination. Higher Fe contents cause β-Fe-intermetallic phases in the form of long and brittle platelets that negatively affect corrosion resistance and fatigue. Neutralizing elements lead to the formation of less harmful α-Fe-rich phases, therefore a positive effect on properties is also expected. For this reason, the study investigates the effect of Mn addition on the corrosion properties achieved by immersion test and potentiodynamic polarization test and fatigue of secondary AlSi7Mg0.6 secondary alloy.