Anatoliy A. Konovalov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Anatoliy A. Konovalov has a total of 55 co-authors. Here are the top co-authors by number of shared publications:
- Alexander S. Fomin
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, 119334 Moscow, Russia
6 shared publications - Margarita A. Goldberg
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, 119334 Moscow, Russia
6 shared publications - Sergey Mironovich Barinov
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, 119334 Moscow, Russia
6 shared publications - Vladimir Sergeevich Komlev
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, 119334 Moscow, Russia
6 shared publications - Dinara R. Khayrutdinova
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, 119334 Moscow, Russia
4 shared publications - Fadis Fanilovich Murzakhanov
Kazan Federal University
4 shared publications
Latest Publications
- Open Access
- 30 October 2026
- Published by MDPI AG in Preprints.org
New Ti–6Al–7Nb–0.3Y Alloy for Laser Powder Bed Fusion of Patient–Specific Biomedical Implants: Ultrasonic Atomization and Characterization
A Ti–6Al–7Nb–0.3Y spherical powder was produced by ultrasonic atomization (UA), and its < 63 µm (d50 ≈ 53 µm) and 63–125 µm (d50 ≈ 82 µm) fractions were characterized for laser powder-bed fusion (LPBF) of patient–specific biomedical implants. Both fractions show near-ideal sphericity (1.01) with no satellites or internal pores, flow times of 26.8–28.0 s/50 g and bulk densities of 2.35–2.45 g/cm3 (51–53% of true density), matching commercial powder-bed feedstocks. XRD revealed only hexagonal α(α′)-Ti with a microstrain of 0.45–0.55%. Nanoindentation showed a hardness of 4.55–4.90 GPa, exceeding that of laser-powder-bed-fused Ti–6Al–4V (3.66 GPa), and an elastic modulus of 119–148 GPa on rigidly supported particles. Simultaneous thermal analysis showed stability up to 450 °C in all atmospheres, oxidation in air above 720 °C (Ea ≈ 160–170 kJ/mol) and mass gains at 1195 °C of 23.2–25.7% (air), 4.9–6.8% (N2) and 1.7–2.1% (Ar). The Ti–6Al–7Nb–0.3Y powder contains 0.69–0.74 wt.% Oxygen, far beyond the scavenging capacity of the retained 0.11–0.12 wt.% Yttrium, as well as 0.09–0.12 wt.% Nitrogen and 0.013–0.015 wt.% Hydrogen.
- 30 October 2026
- Published by MDPI AG in Preprints.org
Open AccessNew Ti–6Al–7Nb–0.3Y Alloy for Laser Powder Bed Fusion of Patient–Specific Biomedical Implants: Ultrasonic Atomization and Characterization
A Ti–6Al–7Nb–0.3Y spherical powder was produced by ultrasonic atomization (UA), and its < 63 µm (d50 ≈ 53 µm) and 63–125 µm (d50 ≈ 82 µm) fractions were characterized for laser powder-bed fusion (LPBF) of patient–specific biomedical implants. Both fractions show near-ideal sphericity (1.01) with no satellites or internal pores, flow times of 26.8–28.0 s/50 g and bulk densities of 2.35–2.45 g/cm3 (51–53% of true density), matching commercial powder-bed feedstocks. XRD revealed only hexagonal α(α′)-Ti with a microstrain of 0.45–0.55%. Nanoindentation showed a hardness of 4.55–4.90 GPa, exceeding that of laser-powder-bed-fused Ti–6Al–4V (3.66 GPa), and an elastic modulus of 119–148 GPa on rigidly supported particles. Simultaneous thermal analysis showed stability up to 450 °C in all atmospheres, oxidation in air above 720 °C (Ea ≈ 160–170 kJ/mol) and mass gains at 1195 °C of 23.2–25.7% (air), 4.9–6.8% (N2) and 1.7–2.1% (Ar). The Ti–6Al–7Nb–0.3Y powder contains 0.69–0.74 wt.% Oxygen, far beyond the scavenging capacity of the retained 0.11–0.12 wt.% Yttrium, as well as 0.09–0.12 wt.% Nitrogen and 0.013–0.015 wt.% Hydrogen.
- 16 October 2025
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry A
- Vol. 99 (10) , 2404-2410
Xerogels and Nanopowders Al2O3–ZrO2 and Al2O3–[ZrYb]O2 for Sorption of Anions
The results of our study of the sorption of the anionic dye methylene orange (MO) and hexavalent chromium oxy ions from aqueous solutions using mono-, bi-, and three-component systems Al2O3 (A), ZrO2 (Z), xAl2O3−ZrO2 (xAZ), and xAl2O3−[ZrYb]O2 (xAZYb) with different heat treatments after sol-gel synthesis are presented. The influence of the sorbent composition and heat treatment temperature of 180, 500, and 800°C on the extraction of sorbate anions was determined based on the parameters of sorption isotherms and adsorption kinetics at 25°C. The Henry constants of sorption of the methyl orange dye (L/m2) on the samples calcinated at 500°C decrease linearly with the increasing content of A. The xAZYb samples showed better dye and dichromate ion sorption characteristics than xAZ. The studied systems, which are precursors of alumina–zirconia ceramics, can be used in the adsorption removal of pollutant anions from the aquatic environment.
- 16 October 2025
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry A
- Vol. 99 (10) , 2404-2410
Xerogels and Nanopowders Al2O3–ZrO2 and Al2O3–[ZrYb]O2 for Sorption of Anions
The results of our study of the sorption of the anionic dye methylene orange (MO) and hexavalent chromium oxy ions from aqueous solutions using mono-, bi-, and three-component systems Al2O3 (A), ZrO2 (Z), xAl2O3−ZrO2 (xAZ), and xAl2O3−[ZrYb]O2 (xAZYb) with different heat treatments after sol-gel synthesis are presented. The influence of the sorbent composition and heat treatment temperature of 180, 500, and 800°C on the extraction of sorbate anions was determined based on the parameters of sorption isotherms and adsorption kinetics at 25°C. The Henry constants of sorption of the methyl orange dye (L/m2) on the samples calcinated at 500°C decrease linearly with the increasing content of A. The xAZYb samples showed better dye and dichromate ion sorption characteristics than xAZ. The studied systems, which are precursors of alumina–zirconia ceramics, can be used in the adsorption removal of pollutant anions from the aquatic environment.
- Open Access
Novel Catalysts Based on Synthetic Mesoporous Silicates of the MCM-41 Type and Hydroxyapatite for Desulfurization of Model Fuel
Nanopowders of hydroxyapatite (HA) and Fe-substituted hydroxyapatite (HAFe) were synthesized by wet precipitation on either MCM-41 (a synthetic, mesoporous aluminosilicate material) or an aluminum-containing MCM-41 (AlMCM) support. According to X-ray diffraction data, all of the synthesized materials are composite powders consisting of amorphous silicate and an HA phase with low crystallinity. The presence of aluminum and iron in the structure of the powders resulted in further amorphization. The obtained samples showed high specific surface areas (SSAs), ranging from 162.3 to 186.6 m2/g for MCM-41-HA and from 112.6 to 127.2 m2/g for AlMCM-HA. The hysteresis loops were found to be of type H3, indicating the formation of slit-like pores in the intercrystalline space, as confirmed by transmission electron microscopy, which revealed the presence of lamellar and flake-like particles. Catalytic activity tests showed that the conversion of dibenzothiophene depended on the iron concentration in the material and the acidity of the support. To further improve the catalytic activity of the materials, they were impregnated with molybdenum compounds. Active molybdenum peroxo complexes formed under these conditions enabled 100% conversion of dibenzothiophene. To our knowledge, this is the first study on the influence of MCM-41-HA- or AlMCM-HA-based materials on dibenzothiophene conversion via oxidative desulfurization using hydrogen peroxide as an oxidant.
Open AccessNovel Catalysts Based on Synthetic Mesoporous Silicates of the MCM-41 Type and Hydroxyapatite for Desulfurization of Model Fuel
Nanopowders of hydroxyapatite (HA) and Fe-substituted hydroxyapatite (HAFe) were synthesized by wet precipitation on either MCM-41 (a synthetic, mesoporous aluminosilicate material) or an aluminum-containing MCM-41 (AlMCM) support. According to X-ray diffraction data, all of the synthesized materials are composite powders consisting of amorphous silicate and an HA phase with low crystallinity. The presence of aluminum and iron in the structure of the powders resulted in further amorphization. The obtained samples showed high specific surface areas (SSAs), ranging from 162.3 to 186.6 m2/g for MCM-41-HA and from 112.6 to 127.2 m2/g for AlMCM-HA. The hysteresis loops were found to be of type H3, indicating the formation of slit-like pores in the intercrystalline space, as confirmed by transmission electron microscopy, which revealed the presence of lamellar and flake-like particles. Catalytic activity tests showed that the conversion of dibenzothiophene depended on the iron concentration in the material and the acidity of the support. To further improve the catalytic activity of the materials, they were impregnated with molybdenum compounds. Active molybdenum peroxo complexes formed under these conditions enabled 100% conversion of dibenzothiophene. To our knowledge, this is the first study on the influence of MCM-41-HA- or AlMCM-HA-based materials on dibenzothiophene conversion via oxidative desulfurization using hydrogen peroxide as an oxidant.
- Open Access
- 12 August 2024
- Published by MDPI AG in Nanomaterials
- Vol. 14 (16) , 1338
Meso-Macroporous Hydroxyapatite Powders Synthesized in Polyvinyl Alcohol or Polyvinylpyrrolidone Media
Mesoporous hydroxyapatite (HA) is widely used in various applications, such as the biomedical field, as a catalytic, as a sensor, and many others. The aim of this work was to obtain HA powders by means of chemical precipitation in a medium containing a polymer—polyvinyl alcohol or polyvinylpyrrolidone (PVP)—with concentrations ranging from 0 to 10%. The HA powders were characterized by X-ray diffraction, Fourier transform infrared spectroscopy, atomic emission spectroscopy with inductively coupled plasma, electron paramagnetic resonance, scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The specific surface area (SSA), pore volume, and pore size distributions were determined by low-temperature nitrogen adsorption measurements, and the zeta potential was established. The formation of macropores in powder agglomerates was determined using SEM and TEM. The synthesis in 10% PVP increased the SSA from 101.3 to 158.0 m2/g, while the ripening for 7 days led to an increase from 112.3 to 195.8 m2/g, with the total pore volume rising from 0.37 to 0.71 cm3/g. These materials could be classified as meso-macroporous HA. Such materials can serve as the basis for various applications requiring improved textural properties and may lay the foundation for the creation of bulk 3D materials using a technique that allows for the preservation of their unique pore structure.
- 12 August 2024
- Published by MDPI AG in Nanomaterials
- Vol. 14 (16) , 1338
Open AccessMeso-Macroporous Hydroxyapatite Powders Synthesized in Polyvinyl Alcohol or Polyvinylpyrrolidone Media
Mesoporous hydroxyapatite (HA) is widely used in various applications, such as the biomedical field, as a catalytic, as a sensor, and many others. The aim of this work was to obtain HA powders by means of chemical precipitation in a medium containing a polymer—polyvinyl alcohol or polyvinylpyrrolidone (PVP)—with concentrations ranging from 0 to 10%. The HA powders were characterized by X-ray diffraction, Fourier transform infrared spectroscopy, atomic emission spectroscopy with inductively coupled plasma, electron paramagnetic resonance, scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The specific surface area (SSA), pore volume, and pore size distributions were determined by low-temperature nitrogen adsorption measurements, and the zeta potential was established. The formation of macropores in powder agglomerates was determined using SEM and TEM. The synthesis in 10% PVP increased the SSA from 101.3 to 158.0 m2/g, while the ripening for 7 days led to an increase from 112.3 to 195.8 m2/g, with the total pore volume rising from 0.37 to 0.71 cm3/g. These materials could be classified as meso-macroporous HA. Such materials can serve as the basis for various applications requiring improved textural properties and may lay the foundation for the creation of bulk 3D materials using a technique that allows for the preservation of their unique pore structure.
- Open Access
- 19 October 2023
- Published by MDPI AG in Preprints.org
Effects of Tb3+ on Properties of Luminescent Calcium Sulfate Cement
Calcium sulfate (CS) materials containing terbium ions at 0, 1.0, or 2.0 mol.% were obtained by mechanochemical synthesis. According to X-ray diffraction data, the powder materials are characterized by the presence of a CaSO4×0.5H2O phase, while Tb3+ is incorporated into the lattice at ≤1.0 mol.%. Specific surface area enlarged from 2.1 to 22.5 m2/g as crystallite size decreased from 68 to 31 nm and the Tb3+ concentration increased up to 1.0 mol.%. Thermal analysis showed that terbium slightly raises the temperature of CaSO4×2H2O-to-CaSO4 transition. The presence of Tb3+ did not affect the solubility of the CS cements. Furthermore, after 7 days of soaking of the materials in a simulated body fluid, a calcium phosphate layer formed corresponding to a hydroxyapatite phase, in contrast to the pure cements. Luminescent properties were studied by excitation at 276 nm. The recorded emission peaks of the CS materials indicated that the luminescence of the samples is green and blue, with the most intense luminescence observed for samples containing 1.0 mol.% Tb3+. The developed materials can find applications in medicine as bioimplants for the regeneration and restoration of bone tissue with a possibility of noninvasive monitoring of the bone restoration process.
- 19 October 2023
- Published by MDPI AG in Preprints.org
Open AccessEffects of Tb3+ on Properties of Luminescent Calcium Sulfate Cement
Calcium sulfate (CS) materials containing terbium ions at 0, 1.0, or 2.0 mol.% were obtained by mechanochemical synthesis. According to X-ray diffraction data, the powder materials are characterized by the presence of a CaSO4×0.5H2O phase, while Tb3+ is incorporated into the lattice at ≤1.0 mol.%. Specific surface area enlarged from 2.1 to 22.5 m2/g as crystallite size decreased from 68 to 31 nm and the Tb3+ concentration increased up to 1.0 mol.%. Thermal analysis showed that terbium slightly raises the temperature of CaSO4×2H2O-to-CaSO4 transition. The presence of Tb3+ did not affect the solubility of the CS cements. Furthermore, after 7 days of soaking of the materials in a simulated body fluid, a calcium phosphate layer formed corresponding to a hydroxyapatite phase, in contrast to the pure cements. Luminescent properties were studied by excitation at 276 nm. The recorded emission peaks of the CS materials indicated that the luminescence of the samples is green and blue, with the most intense luminescence observed for samples containing 1.0 mol.% Tb3+. The developed materials can find applications in medicine as bioimplants for the regeneration and restoration of bone tissue with a possibility of noninvasive monitoring of the bone restoration process.
- 1 October 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (5-6) , 1422-1428
Investigation of the Amount of Polyvinylpyrrolidone as Gelling Agent to Lanthanum Cobaltite Micropowders Synthesized by Sol-Gel Method
The paper focuses on lanthanum cobaltite micropowders LaCoO3 – δ (LCO) synthesized by the sol-gel method using polyvinylpyrrolidone (PVP) as a gelling agent. The PVP content was varied from 0.5 to 5.0 wt % when ionic solutions of the soluble raw components were prepared. The gels were dried in a microwave oven at a microwave power of 90 W for 2 h to evaporate water. Xerogels were thermally treated in a muffle furnace at temperatures 800 and 900°C; the maximum holding time was 10 and 30 h. After heat treatment of xerogels at 800°C for 10 h, the LCO micropowders were slightly aggregated, the particle size was in the range from 0.24 to 0.38 μm, and the specific surface area was in the range from 2.60 to 4.10 m2/g. After heat treatment at 900°C for 10 h, the range of the specific surface area of LCO micropowders decreased from 1.00 to 3.20 m2/g, but particle size range slightly increased from 0.31 to 1.0 μm. The heat treatment of xerogels at a temperature 900°C for 30 h resulted in the particles size range growing from 0.50 to 1.25 μm, and the specific surface area was 2.00 m2/g for all LCO micropowders. There was no effect of PVP content in the ionic solution on the phase composition for all heat-treated LCO micropowders.
- 1 October 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (5-6) , 1422-1428
Investigation of the Amount of Polyvinylpyrrolidone as Gelling Agent to Lanthanum Cobaltite Micropowders Synthesized by Sol-Gel Method
The paper focuses on lanthanum cobaltite micropowders LaCoO3 – δ (LCO) synthesized by the sol-gel method using polyvinylpyrrolidone (PVP) as a gelling agent. The PVP content was varied from 0.5 to 5.0 wt % when ionic solutions of the soluble raw components were prepared. The gels were dried in a microwave oven at a microwave power of 90 W for 2 h to evaporate water. Xerogels were thermally treated in a muffle furnace at temperatures 800 and 900°C; the maximum holding time was 10 and 30 h. After heat treatment of xerogels at 800°C for 10 h, the LCO micropowders were slightly aggregated, the particle size was in the range from 0.24 to 0.38 μm, and the specific surface area was in the range from 2.60 to 4.10 m2/g. After heat treatment at 900°C for 10 h, the range of the specific surface area of LCO micropowders decreased from 1.00 to 3.20 m2/g, but particle size range slightly increased from 0.31 to 1.0 μm. The heat treatment of xerogels at a temperature 900°C for 30 h resulted in the particles size range growing from 0.50 to 1.25 μm, and the specific surface area was 2.00 m2/g for all LCO micropowders. There was no effect of PVP content in the ionic solution on the phase composition for all heat-treated LCO micropowders.
- 1 April 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (2) , 526-535
Obtaining Hybrid Nanostructures Based on Graphene and Nano-ZrO2
A technologically promising method for obtaining nanostructured graphene-ZrO2 has been proposed. Its main idea is to use the suspensions of graphene and nano-ZrO2 and create conditions for the interaction of graphene sheets and ZrO2 crystallites to form a hybrid nanostructured powder without the formation of new chemical bonds. The oxygen-free graphene sheets with thickness of several nanometers were obtained by sonochemical method in N,N-dimethyloctylamine-aqua emulsion. Nano-ZrO2 powder with average crystallite size of 8.1 nm was synthesized by sol-gel method. The morphology and phase composition of all synthesized objects (nano-ZrO2, graphene, composite) were studied by using a set of instrumental methods (transmission electron microscopy (TEM) and electron diffraction, X-ray diffraction (XRD), electron energy loss spectroscopy (EELS), nitrogen adsorption-desorption, diffusion aerosol spectrometry (DAS) and elemental analysis). It was shown that the proposed method allows obtain chemically homogeneous mesoporous hybrid powders consisting of graphene sheets and ZrO2 crystallites with the sizes of 8‒13 nm fixed on them. We investigated an effect of duration of ultrasonic impact to graphite on the morphology of the hybrid and the mechanism of its formation. According to the results of a comprehensive analysis of the obtained data, the mechanisms for the formation of graphene suspension in emulsion and a nanostructured hybrid during the interaction of crystalline ZrO2 and oxygen-free graphene sheets in an aqua-organic medium were proposed. The developed hybrid nanostructures are highly demanded innovative raw-products in the production of (photo)catalysts for a wide range of processes, sensor, ceramic and electrical materials, and materials for medical and biological purposes.
- 1 April 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (2) , 526-535
Obtaining Hybrid Nanostructures Based on Graphene and Nano-ZrO2
A technologically promising method for obtaining nanostructured graphene-ZrO2 has been proposed. Its main idea is to use the suspensions of graphene and nano-ZrO2 and create conditions for the interaction of graphene sheets and ZrO2 crystallites to form a hybrid nanostructured powder without the formation of new chemical bonds. The oxygen-free graphene sheets with thickness of several nanometers were obtained by sonochemical method in N,N-dimethyloctylamine-aqua emulsion. Nano-ZrO2 powder with average crystallite size of 8.1 nm was synthesized by sol-gel method. The morphology and phase composition of all synthesized objects (nano-ZrO2, graphene, composite) were studied by using a set of instrumental methods (transmission electron microscopy (TEM) and electron diffraction, X-ray diffraction (XRD), electron energy loss spectroscopy (EELS), nitrogen adsorption-desorption, diffusion aerosol spectrometry (DAS) and elemental analysis). It was shown that the proposed method allows obtain chemically homogeneous mesoporous hybrid powders consisting of graphene sheets and ZrO2 crystallites with the sizes of 8‒13 nm fixed on them. We investigated an effect of duration of ultrasonic impact to graphite on the morphology of the hybrid and the mechanism of its formation. According to the results of a comprehensive analysis of the obtained data, the mechanisms for the formation of graphene suspension in emulsion and a nanostructured hybrid during the interaction of crystalline ZrO2 and oxygen-free graphene sheets in an aqua-organic medium were proposed. The developed hybrid nanostructures are highly demanded innovative raw-products in the production of (photo)catalysts for a wide range of processes, sensor, ceramic and electrical materials, and materials for medical and biological purposes.
- Open Access
- 19 January 2023
- Published by MDPI AG in Nanomaterials
- Vol. 13 (3) , 418
Effects of Various Ripening Media on the Mesoporous Structure and Morphology of Hydroxyapatite Powders
Mesoporous hydroxyapatite (HA) materials demonstrate advantages as catalysts and as support systems for catalysis, as adsorbent materials for removing contamination from soil and water, and as nanocarriers of functional agents for bone-related therapies. The present research demonstrates the possibility of the enlargement of the Brunauer–Emmett–Teller specific surface area (SSA), pore volume, and average pore diameter via changing the synthesis medium and ripening the material in the mother solution after the precipitation processes have been completed. HA powders were investigated via chemical analysis, X-ray diffraction analysis, Fourier-transform IR spectroscopy, transmission electron microscopy (TEM), and scanning (SEM) electron microscopy. Their SSA, pore volume, and pore-size distributions were determined via low-temperature nitrogen adsorption measurements, the zeta potential was established, and electron paramagnetic resonance (EPR) spectroscopy was performed. When the materials were synthesized in water–ethanol and water–acetone media, the SSA and total pore volume were 52.1 m2g−1 and 116.4 m2g−1, and 0.231 and 0.286 cm3g−1, respectively. After ripening for 21 days, the particle morphology changed, the length/width aspect ratio decreased, and looser and smaller powder agglomerates were obtained. These changes in their characteristics led to an increase in SSA for the water and water–ethanol samples, while pore volume demonstrated a multiplied increase for all samples, reaching 0.593 cm3g−1 for the water–acetone sample.
- 19 January 2023
- Published by MDPI AG in Nanomaterials
- Vol. 13 (3) , 418
Open AccessEffects of Various Ripening Media on the Mesoporous Structure and Morphology of Hydroxyapatite Powders
Mesoporous hydroxyapatite (HA) materials demonstrate advantages as catalysts and as support systems for catalysis, as adsorbent materials for removing contamination from soil and water, and as nanocarriers of functional agents for bone-related therapies. The present research demonstrates the possibility of the enlargement of the Brunauer–Emmett–Teller specific surface area (SSA), pore volume, and average pore diameter via changing the synthesis medium and ripening the material in the mother solution after the precipitation processes have been completed. HA powders were investigated via chemical analysis, X-ray diffraction analysis, Fourier-transform IR spectroscopy, transmission electron microscopy (TEM), and scanning (SEM) electron microscopy. Their SSA, pore volume, and pore-size distributions were determined via low-temperature nitrogen adsorption measurements, the zeta potential was established, and electron paramagnetic resonance (EPR) spectroscopy was performed. When the materials were synthesized in water–ethanol and water–acetone media, the SSA and total pore volume were 52.1 m2g−1 and 116.4 m2g−1, and 0.231 and 0.286 cm3g−1, respectively. After ripening for 21 days, the particle morphology changed, the length/width aspect ratio decreased, and looser and smaller powder agglomerates were obtained. These changes in their characteristics led to an increase in SSA for the water and water–ethanol samples, while pore volume demonstrated a multiplied increase for all samples, reaching 0.593 cm3g−1 for the water–acetone sample.
- Open Access
Effects of Heat Treatment on Phase Formation in Cytocompatible Sulphate-Containing Tricalcium Phosphate Materials
Powders based on β-tricalcium phosphate (β-TCP) containing sulphate groups at up to 12.0 mol.% were synthesised by chemical precipitation from aqueous solutions. The obtained materials were characterised by X-ray phase analysis, Fourier transform infrared spectroscopy, measurement of specific surface area, scanning electron microscopy, energy dispersive analysis, synchronous thermal analysis, mass spectra investigations and biological assays. It was established that during the synthesis, the obtained materials lose the sulphate groups in the course of heat treatment at 900 or 1200 °C. These groups stabilise low-temperature β-TCP, but when introduced at a high concentration, the sulphate groups contribute to the formation of hydroxyapatite during the heat treatment. Specific surface area of the powders proved to be in the range 81.7–96.5 m2/g. Results of biological assays showed cytocompatibility of both pure β-TCP and samples of sulphate-containing β-TCP. Additionally, matrix properties in the culture of MG-63 cells were revealed in all samples. Thus, the obtained materials are promising for biomedical applications.
Open AccessEffects of Heat Treatment on Phase Formation in Cytocompatible Sulphate-Containing Tricalcium Phosphate Materials
Powders based on β-tricalcium phosphate (β-TCP) containing sulphate groups at up to 12.0 mol.% were synthesised by chemical precipitation from aqueous solutions. The obtained materials were characterised by X-ray phase analysis, Fourier transform infrared spectroscopy, measurement of specific surface area, scanning electron microscopy, energy dispersive analysis, synchronous thermal analysis, mass spectra investigations and biological assays. It was established that during the synthesis, the obtained materials lose the sulphate groups in the course of heat treatment at 900 or 1200 °C. These groups stabilise low-temperature β-TCP, but when introduced at a high concentration, the sulphate groups contribute to the formation of hydroxyapatite during the heat treatment. Specific surface area of the powders proved to be in the range 81.7–96.5 m2/g. Results of biological assays showed cytocompatibility of both pure β-TCP and samples of sulphate-containing β-TCP. Additionally, matrix properties in the culture of MG-63 cells were revealed in all samples. Thus, the obtained materials are promising for biomedical applications.
- Open Access
- 22 March 2021
- Published by MDPI AG in Nanomaterials
- Vol. 11 (3) , 811
Mesoporous Iron(III)-Doped Hydroxyapatite Nanopowders Obtained via Iron Oxalate
Mesoporous hydroxyapatite (HA) and iron(III)-doped HA (Fe-HA) are attractive materials for biomedical, catalytic, and environmental applications. In the present study, the nanopowders of HA and Fe-HA with a specific surface area up to 194.5 m2/g were synthesized by a simple precipitation route using iron oxalate as a source of Fe3+ cations. The influence of Fe3+ amount on the phase composition, powders morphology, Brunauer–Emmett–Teller (BET) specific surface area (S), and pore size distribution were investigated, as well as electron paramagnetic resonance and Mössbauer spectroscopy analysis were performed. According to obtained data, the Fe3+ ions were incorporated in the HA lattice, and also amorphous Fe oxides were formed contributed to the gradual increase in the S and pore volume of the powders. The Density Functional Theory calculations supported these findings and revealed Fe3+ inclusion in the crystalline region with the hybridization among Fe-3d and O-2p orbitals and a partly covalent bond formation, whilst the inclusion of Fe oxides assumed crystallinity damage and rather occurred in amorphous regions of HA nanomaterial. In vitro tests based on the MG-63 cell line demonstrated that the introduction of Fe3+ does not cause cytotoxicity and led to the enhanced cytocompatibility of HA.
- 22 March 2021
- Published by MDPI AG in Nanomaterials
- Vol. 11 (3) , 811
Open AccessMesoporous Iron(III)-Doped Hydroxyapatite Nanopowders Obtained via Iron Oxalate
Mesoporous hydroxyapatite (HA) and iron(III)-doped HA (Fe-HA) are attractive materials for biomedical, catalytic, and environmental applications. In the present study, the nanopowders of HA and Fe-HA with a specific surface area up to 194.5 m2/g were synthesized by a simple precipitation route using iron oxalate as a source of Fe3+ cations. The influence of Fe3+ amount on the phase composition, powders morphology, Brunauer–Emmett–Teller (BET) specific surface area (S), and pore size distribution were investigated, as well as electron paramagnetic resonance and Mössbauer spectroscopy analysis were performed. According to obtained data, the Fe3+ ions were incorporated in the HA lattice, and also amorphous Fe oxides were formed contributed to the gradual increase in the S and pore volume of the powders. The Density Functional Theory calculations supported these findings and revealed Fe3+ inclusion in the crystalline region with the hybridization among Fe-3d and O-2p orbitals and a partly covalent bond formation, whilst the inclusion of Fe oxides assumed crystallinity damage and rather occurred in amorphous regions of HA nanomaterial. In vitro tests based on the MG-63 cell line demonstrated that the introduction of Fe3+ does not cause cytotoxicity and led to the enhanced cytocompatibility of HA.