Kornkanok Rotjanasuworapong
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Kornkanok Rotjanasuworapong has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Anuvat Sirivat
The Petroleum and Petrochemical College, Chulalongkorn University, Bangkok 10330, Thailand
2 shared publications - Chatrawee Direksilp
Conductive and Electroactive Polymers Research Unit, The Petroleum and Petrochemical College, Chulalongkorn University, Bangkok 10330, Thailand
1 shared publication - Katesara Phasuksom
Conductive and Electroactive Polymers Research Unit, The Petroleum and Petrochemical, College, Chulalongkorn University, Bangkok 10330, Thailand; The Petroleum and Petrochemical College, Chulalongkorn University, Bangkok 10330, Thailand
1 shared publication - Natlita Thummarungsan
Conductive and Electroactive Polymers Research Unit, The Petroleum and Petrochemical College, Chulalongkorn University, Bangkok 10330, Thailand
1 shared publication - Phimchanok Sakunpongpitiporn
Conductive and Electroactive Polymers Research Unit, The Petroleum and Petrochemical College, Chulalongkorn University, Bangkok 10330, Thailand
1 shared publication - Sanhanut Kesornsit
Conductive and Electroactive Polymers Research Unit, The Petroleum and Petrochemical College, Chulalongkorn University, Bangkok 10330, Thailand
1 shared publication
Latest Publications
- Open Access
Synthesis of Highly Conductive Poly(3-hexylthiophene) by Chemical Oxidative Polymerization Using Surfactant Templates
Poly(3-hexylthiophene) (P3HT) was systematically synthesized by chemical oxidative polymerization in chloroform with ferric chloride (FeCl3) as the oxidizing agent and various surfactants of the shape templates. The effects of 3HT: FeCl3 mole ratios, polymerization times, and surfactant types and concentrations on the electrical conductivity, particle shape and size were systematically investigated. Furthermore, dodecylbenzenesulfonic acid (DBSA), p-toluenesulfonic acid (PTSA), sodium dodecyl sulfate (SDS), and sodium dioctyl sulfosuccinate (AOT) were utilized as the surfactant templates. The P3HT synthesized with DBSA at 6 CMC, where CMC stands for the Critical Micelle Concentration of surfactant, provided a higher electrical conductivity than those with PTSA, SDS and AOT. The highest electrical conductivity of P3HT using DBSA was 16.21 ± 1.55 S cm−1 in which the P3HT particle shape was spherical with an average size of 1530 ± 227 nm. The thermal analysis indicated that the P3HT synthesized with the surfactants yielded higher stability and char yields than that of P3HT without. The P3HT_DBSA electrical conductivity was further enhanced by de-doping and doping with HClO4. At the 10:1 doping mole ratio, the electrical conductivity of dP3HT_DBSA increased by one order of magnitude relative to P3HT_DBSA prior to the de-doping. The highest electrical conductivity of dP3HT_DBSA obtained was 172 ± 5.21 S cm−1 which is the highest value relative to previously reported.
Open AccessSynthesis of Highly Conductive Poly(3-hexylthiophene) by Chemical Oxidative Polymerization Using Surfactant Templates
Poly(3-hexylthiophene) (P3HT) was systematically synthesized by chemical oxidative polymerization in chloroform with ferric chloride (FeCl3) as the oxidizing agent and various surfactants of the shape templates. The effects of 3HT: FeCl3 mole ratios, polymerization times, and surfactant types and concentrations on the electrical conductivity, particle shape and size were systematically investigated. Furthermore, dodecylbenzenesulfonic acid (DBSA), p-toluenesulfonic acid (PTSA), sodium dodecyl sulfate (SDS), and sodium dioctyl sulfosuccinate (AOT) were utilized as the surfactant templates. The P3HT synthesized with DBSA at 6 CMC, where CMC stands for the Critical Micelle Concentration of surfactant, provided a higher electrical conductivity than those with PTSA, SDS and AOT. The highest electrical conductivity of P3HT using DBSA was 16.21 ± 1.55 S cm−1 in which the P3HT particle shape was spherical with an average size of 1530 ± 227 nm. The thermal analysis indicated that the P3HT synthesized with the surfactants yielded higher stability and char yields than that of P3HT without. The P3HT_DBSA electrical conductivity was further enhanced by de-doping and doping with HClO4. At the 10:1 doping mole ratio, the electrical conductivity of dP3HT_DBSA increased by one order of magnitude relative to P3HT_DBSA prior to the de-doping. The highest electrical conductivity of dP3HT_DBSA obtained was 172 ± 5.21 S cm−1 which is the highest value relative to previously reported.
- Open Access
- 30 March 2021
- Published by MDPI AG in Nanomaterials
- Vol. 11 (4) , 876
Synthesis and Characterization of Fe0.8Mn0.2Fe2O4 Ferrite Nanoparticle with High Saturation Magnetization via the Surfactant Assisted Co-Precipitation
Manganese ferrite nanoparticles (MnFe2O4) were synthesized via surfactant-assisted co-precipitation, where sodium dodecyl sulfate (SDS) was used as the template to control particle size at various SDS concentrations. The substitutions of iron (II) (Fe2+) into the MnFe2O4 ferrite nanoparticles were carried out to obtain Fe(1–x)MnxFe2O4, with various Mn2+: Fe2+ molar ratios. The synthesized ferrite nanoparticles were characterized by the Fourier-transform infrared spectroscopy (FT-IR), thermogravimetric analyzer (TGA), X-ray diffractometer (XRD), energy dispersive X-ray (EDX), X-ray photoelectron spectroscopy (XPS), scanning electron microscope (SEM), transmission electron microscope (TEM), two-point probe, and vibrating sample magnetometer (VSM) techniques. The experimental Mn:Fe mole ratios of the Fe(1−x)MnxFe2O4 ferrite nanoparticles were verified to be in agreement with the theoretical values. The synthesized MnFe2O4 and Fe(1−x)MnxFe2O4 ferrite nanoparticles were of mixed spinel structures, with average spherical particle sizes between 17–22 nm, whereas the magnetite ferrite nanoparticles (Fe3O4) were of the inverse spinel structure. They showed soft ferromagnetic behavior. The synthesized Fe0.8Mn0.2Fe2O4 ferrite nanoparticle possessed the highest saturation magnetization of 88 emu/g relative to previously reported work to date.
- 30 March 2021
- Published by MDPI AG in Nanomaterials
- Vol. 11 (4) , 876
Open AccessSynthesis and Characterization of Fe0.8Mn0.2Fe2O4 Ferrite Nanoparticle with High Saturation Magnetization via the Surfactant Assisted Co-Precipitation
Manganese ferrite nanoparticles (MnFe2O4) were synthesized via surfactant-assisted co-precipitation, where sodium dodecyl sulfate (SDS) was used as the template to control particle size at various SDS concentrations. The substitutions of iron (II) (Fe2+) into the MnFe2O4 ferrite nanoparticles were carried out to obtain Fe(1–x)MnxFe2O4, with various Mn2+: Fe2+ molar ratios. The synthesized ferrite nanoparticles were characterized by the Fourier-transform infrared spectroscopy (FT-IR), thermogravimetric analyzer (TGA), X-ray diffractometer (XRD), energy dispersive X-ray (EDX), X-ray photoelectron spectroscopy (XPS), scanning electron microscope (SEM), transmission electron microscope (TEM), two-point probe, and vibrating sample magnetometer (VSM) techniques. The experimental Mn:Fe mole ratios of the Fe(1−x)MnxFe2O4 ferrite nanoparticles were verified to be in agreement with the theoretical values. The synthesized MnFe2O4 and Fe(1−x)MnxFe2O4 ferrite nanoparticles were of mixed spinel structures, with average spherical particle sizes between 17–22 nm, whereas the magnetite ferrite nanoparticles (Fe3O4) were of the inverse spinel structure. They showed soft ferromagnetic behavior. The synthesized Fe0.8Mn0.2Fe2O4 ferrite nanoparticle possessed the highest saturation magnetization of 88 emu/g relative to previously reported work to date.