Tiejun Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Tiejun Wang has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Qilu Ge
Central Iron & Steel Research Institute, Graduate School, Beijing 100081, China
3 shared publications - Xuanhui Qu
Beijing Advanced Innovation Center for Materials Genome Engineering, Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing, P.R. China
3 shared publications - Yanbin Pei
Central Iron & Steel Research Institute, Graduate School, Beijing 100081, China
3 shared publications - Hongyan Che
Advanced Technology & Materials Limited Company, China Iron & Steel Research Institute Group, Area C, No. 10 Yongcheng North Road, Haidian District, Beijing 100081, China
2 shared publications - Rui Cao
State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China
2 shared publications - Wei Qin
Advanced Technology & Materials Limited Company, China Iron & Steel Research Institute Group, Area C, No. 10 Yongcheng North Road, Haidian District, Beijing 100081, China
2 shared publications
Latest Publications
- Open Access
Research on Microstructure, Mechanical Properties, and High-Temperature Stability of Hot-Rolled Tungsten Hafnium Alloy
W-(0, 0.1, 0.3, 0.5) wt.% Hf (mass fraction, wt.%) materials were fabricated by the powder metallurgy method and hot rolling. The microstructure, mechanical properties, and high-temperature stability of alloys with varying compositions were systematically studied. The active element Hf can react with the impurity O segregated at the grain boundary to form fine dispersed HfO2 particles, refining the grains and purifies and strengthening the grain boundary. The average size of the sub-grains in the W-0.3 wt.% Hf alloy is 4.32 μm, and the number density of the in situ-formed second phase is 6.4 × 1017 m−3. The W-0.3 wt.% Hf alloy has excellent mechanical properties in all compositions of alloys. The ultimate tensile strength (UTS) is 1048 ± 17.02 MPa at 100 °C, the ductile fracture occurs at 150 °C, and the total elongation (TE) is 5.91 ± 0.41%. The UTS of the tensile test at 500 °C is 614 ± 7.55 MPa, and the elongation is as high as 43.77 ± 1.54%. However, more Hf addition will increase the size of the second-phase particles and reduce the number density of the second-phase particles, resulting in a decrease in the mechanical properties of the tungsten alloy. The isochronal annealing test shows that the recrystallization temperature of W-Hf alloy is 1400 °C, which is 200 °C higher than rolling pure tungsten.
Open AccessResearch on Microstructure, Mechanical Properties, and High-Temperature Stability of Hot-Rolled Tungsten Hafnium Alloy
W-(0, 0.1, 0.3, 0.5) wt.% Hf (mass fraction, wt.%) materials were fabricated by the powder metallurgy method and hot rolling. The microstructure, mechanical properties, and high-temperature stability of alloys with varying compositions were systematically studied. The active element Hf can react with the impurity O segregated at the grain boundary to form fine dispersed HfO2 particles, refining the grains and purifies and strengthening the grain boundary. The average size of the sub-grains in the W-0.3 wt.% Hf alloy is 4.32 μm, and the number density of the in situ-formed second phase is 6.4 × 1017 m−3. The W-0.3 wt.% Hf alloy has excellent mechanical properties in all compositions of alloys. The ultimate tensile strength (UTS) is 1048 ± 17.02 MPa at 100 °C, the ductile fracture occurs at 150 °C, and the total elongation (TE) is 5.91 ± 0.41%. The UTS of the tensile test at 500 °C is 614 ± 7.55 MPa, and the elongation is as high as 43.77 ± 1.54%. However, more Hf addition will increase the size of the second-phase particles and reduce the number density of the second-phase particles, resulting in a decrease in the mechanical properties of the tungsten alloy. The isochronal annealing test shows that the recrystallization temperature of W-Hf alloy is 1400 °C, which is 200 °C higher than rolling pure tungsten.
- Open Access
Evolution of Microstructure and Elements Distribution of Powder Metallurgy Borated Stainless Steel during Hot Isostatic Pressing
Prepared by powder metallurgy process incorporating atomization and hot isostatic pressing (HIP) sintering at six different temperatures from 600 to 1160 °C, borated stainless steel (BSS) containing boron content of 1.86 wt% was studied. The phase of BSS, relative density of different temperature, microstructure, elemental distribution, and mechanical properties were tested and analyzed. The phases of the alloy were calculated by the Thermo-Calc (2021a, Thermo-Calc Software, Solna, Sweden) and studied by quantitative X-ray diffraction phase analysis. The distributions of boron, chromium, and iron in grains of the alloy were analyzed by scanning electron microscopy and transmission electron microscope. The grain size distributions and average grain sizes were calculated for the boron-containing phases at 900, 1000, 1100, and 1160 °C, as well as the average grain size of the austenite phase at 700 and 1160 °C. After undergoing HIP sintering at 900, 1000, 1100, and 1160 °C, respectively, the tensile strength and ductility of the alloy were tested, and the fracture surfaces were analyzed. It was found that the alloy consisted of two phases (austenite and boron-containing phase) when HIP sintering temperature was higher than 900 °C, and the relative density of the prepared alloys was higher than 99% when HIP temperature was higher than 1000 °C. According to the boron-containing phase grain size distribution and microstructure analysis, the boron-containing phase precipitated both inside the austenite matrix and at the grain boundaries and its growth mechanism was divided into four steps. The tensile strength and elongation of alloy were up to 776 MPa and 19% respectively when the HIP sintering was at 1000 °C.
Open AccessEvolution of Microstructure and Elements Distribution of Powder Metallurgy Borated Stainless Steel during Hot Isostatic Pressing
Prepared by powder metallurgy process incorporating atomization and hot isostatic pressing (HIP) sintering at six different temperatures from 600 to 1160 °C, borated stainless steel (BSS) containing boron content of 1.86 wt% was studied. The phase of BSS, relative density of different temperature, microstructure, elemental distribution, and mechanical properties were tested and analyzed. The phases of the alloy were calculated by the Thermo-Calc (2021a, Thermo-Calc Software, Solna, Sweden) and studied by quantitative X-ray diffraction phase analysis. The distributions of boron, chromium, and iron in grains of the alloy were analyzed by scanning electron microscopy and transmission electron microscope. The grain size distributions and average grain sizes were calculated for the boron-containing phases at 900, 1000, 1100, and 1160 °C, as well as the average grain size of the austenite phase at 700 and 1160 °C. After undergoing HIP sintering at 900, 1000, 1100, and 1160 °C, respectively, the tensile strength and ductility of the alloy were tested, and the fracture surfaces were analyzed. It was found that the alloy consisted of two phases (austenite and boron-containing phase) when HIP sintering temperature was higher than 900 °C, and the relative density of the prepared alloys was higher than 99% when HIP temperature was higher than 1000 °C. According to the boron-containing phase grain size distribution and microstructure analysis, the boron-containing phase precipitated both inside the austenite matrix and at the grain boundaries and its growth mechanism was divided into four steps. The tensile strength and elongation of alloy were up to 776 MPa and 19% respectively when the HIP sintering was at 1000 °C.
- Open Access
Study on the Hot Deformation Characterization of Borated Stainless Steel by Hot Isostatic Pressing
Borated stainless steel (BSS) specimens have a boron content of 1.86 wt%, and are prepared by hot isostatic pressing (HIP) conducted at different temperatures, ranging from 1000 to 1100 °C and a constant true strain rate (0.01, 0.1, 1 and 10 s−1). These tests, with observations and microstructural analysis, have achieved the hot deformation characteristics and mechanisms of BSS. In this research, the activation energy (Q) and Zener–Hollomon parameter (Z) were contrasted against the flow curves: Q = 442.35 kJ/mol. The critical conditions associated with the initiation of dynamic recrystallization (DRX) for BSS were precisely calculated based on the function between the strain hardening rate with the flow stress: at different temperatures from 1000 to 1100 °C: the critical stresses were 146.69–254.77 MPa and the critical strains were 0.022–0.044. The facts show that the boron-containing phase of BSS prevented the onset of DRX, despite the saturated boron in the austenite initiated DRX. The microstructural analysis showed that hot deformation promoted the generation of borides, which differed from the initial microstructure of HIP. The inhomogeneous distribution of elements in the boron-containing phase was caused by hot compression.
Open AccessStudy on the Hot Deformation Characterization of Borated Stainless Steel by Hot Isostatic Pressing
Borated stainless steel (BSS) specimens have a boron content of 1.86 wt%, and are prepared by hot isostatic pressing (HIP) conducted at different temperatures, ranging from 1000 to 1100 °C and a constant true strain rate (0.01, 0.1, 1 and 10 s−1). These tests, with observations and microstructural analysis, have achieved the hot deformation characteristics and mechanisms of BSS. In this research, the activation energy (Q) and Zener–Hollomon parameter (Z) were contrasted against the flow curves: Q = 442.35 kJ/mol. The critical conditions associated with the initiation of dynamic recrystallization (DRX) for BSS were precisely calculated based on the function between the strain hardening rate with the flow stress: at different temperatures from 1000 to 1100 °C: the critical stresses were 146.69–254.77 MPa and the critical strains were 0.022–0.044. The facts show that the boron-containing phase of BSS prevented the onset of DRX, despite the saturated boron in the austenite initiated DRX. The microstructural analysis showed that hot deformation promoted the generation of borides, which differed from the initial microstructure of HIP. The inhomogeneous distribution of elements in the boron-containing phase was caused by hot compression.
- Open Access
Effect of Thermo-Mechanical Treatment on the Microstructure and Tensile Properties of the Fe-22Cr-5Al-0.1Y Alloy
Oxide dispersion strengthened ferritic steel is considered an important structural material in fusion reactors due to its excellent resistance to radiation and oxidation. Fine and dispersed oxides can be introduced into the matrix via the powder metallurgy process. In the present study, large grain sizes and prior particle boundaries (PPBs) formed in the FeCrAlY alloy prepared via powder metallurgy. Thermo-mechanical treatment was conducted on the FeCrAlY alloy. Results showed that microstructure was optimized: the average grain diameter decreased, the PPBs disappeared, and the distribution of oxides dispersed. Both ultimate tensile strength and elongation improved, especially the average elongation increased from 0.5% to 23%.
Open AccessEffect of Thermo-Mechanical Treatment on the Microstructure and Tensile Properties of the Fe-22Cr-5Al-0.1Y Alloy
Oxide dispersion strengthened ferritic steel is considered an important structural material in fusion reactors due to its excellent resistance to radiation and oxidation. Fine and dispersed oxides can be introduced into the matrix via the powder metallurgy process. In the present study, large grain sizes and prior particle boundaries (PPBs) formed in the FeCrAlY alloy prepared via powder metallurgy. Thermo-mechanical treatment was conducted on the FeCrAlY alloy. Results showed that microstructure was optimized: the average grain diameter decreased, the PPBs disappeared, and the distribution of oxides dispersed. Both ultimate tensile strength and elongation improved, especially the average elongation increased from 0.5% to 23%.
- Open Access
Effect of Heat Treatment Temperature on Microstructure and Properties of PM Borated Stainless Steel Prepared by Hot Isostatic Pressing
Borated stainless steel (BSS) with a boron content of 1.86% was prepared by a powder metallurgy process incorporating atomization and hot isostatic pressing. After solution quenching at 900–1200 °C, the phase composition of the alloy was studied by quantitative X-ray diffraction phase analysis. The microstructure, fracture morphology, and distributions of boron, chromium, and iron in grains of the alloy were analyzed by field-emission scanning electron microscopy with secondary electron and energy-dispersive spectroscopy. After the coupons were heat treated at different temperatures ranging from 900 to 1200 °C, the strength and plasticity were tested, and the fracture surfaces were analyzed. Undergoing heat treatment at different temperatures, the phases of the alloy were austenite and Fe1.1Cr0.9B0.9 phase. Since the diffusion coefficients of Cr, Fe, and B varied at different temperatures, the distribution of elements in the alloy was not uniform. The alloy with good strength and plasticity can be obtained when the heat treatment temperature of alloy ranged from 1000 to 1150 °C while the tensile strength was about 800 MPa, with the elongation standing about 20%.
Open AccessEffect of Heat Treatment Temperature on Microstructure and Properties of PM Borated Stainless Steel Prepared by Hot Isostatic Pressing
Borated stainless steel (BSS) with a boron content of 1.86% was prepared by a powder metallurgy process incorporating atomization and hot isostatic pressing. After solution quenching at 900–1200 °C, the phase composition of the alloy was studied by quantitative X-ray diffraction phase analysis. The microstructure, fracture morphology, and distributions of boron, chromium, and iron in grains of the alloy were analyzed by field-emission scanning electron microscopy with secondary electron and energy-dispersive spectroscopy. After the coupons were heat treated at different temperatures ranging from 900 to 1200 °C, the strength and plasticity were tested, and the fracture surfaces were analyzed. Undergoing heat treatment at different temperatures, the phases of the alloy were austenite and Fe1.1Cr0.9B0.9 phase. Since the diffusion coefficients of Cr, Fe, and B varied at different temperatures, the distribution of elements in the alloy was not uniform. The alloy with good strength and plasticity can be obtained when the heat treatment temperature of alloy ranged from 1000 to 1150 °C while the tensile strength was about 800 MPa, with the elongation standing about 20%.
- Open Access
Effect of Oxygen Content on Microstructure and Tensile Properties of a 22Cr-5Al ODS Steel
The high tensile strength and irradiation resistance of oxide dispersion strengthened (ODS) ferritic steels is attributed to the ultrafine and dispersed oxides within the matrix. The high content of oxygen and yttrium is critical for the formation of dense Y-rich oxides. However, only few studies have reported the effect of oxygen content on the microstructure and mechanical properties of ODS steels. Herein, we employed gas atomization reactive synthesis to prepare pre-alloy powders and then hot isostatic pressing (HIP) to consolidate two 22Cr-5Al ODS steels with different oxygen content. Our results showed Y-rich precipitates at and near grain boundaries of the as-HIPed alloys. Moreover, with the oxygen content increasing from 0.04 to 0.16 wt%, more precipitates precipitated in the as-HIPed alloy, and the ultimate tensile strength of the alloy was improved. However, increasing the oxygen content to 0.16 wt% led to formation of stripe and chain precipitates at and near grain boundaries, which caused a partial intergranular fracture of the as-HIPed alloy.
Open AccessEffect of Oxygen Content on Microstructure and Tensile Properties of a 22Cr-5Al ODS Steel
The high tensile strength and irradiation resistance of oxide dispersion strengthened (ODS) ferritic steels is attributed to the ultrafine and dispersed oxides within the matrix. The high content of oxygen and yttrium is critical for the formation of dense Y-rich oxides. However, only few studies have reported the effect of oxygen content on the microstructure and mechanical properties of ODS steels. Herein, we employed gas atomization reactive synthesis to prepare pre-alloy powders and then hot isostatic pressing (HIP) to consolidate two 22Cr-5Al ODS steels with different oxygen content. Our results showed Y-rich precipitates at and near grain boundaries of the as-HIPed alloys. Moreover, with the oxygen content increasing from 0.04 to 0.16 wt%, more precipitates precipitated in the as-HIPed alloy, and the ultimate tensile strength of the alloy was improved. However, increasing the oxygen content to 0.16 wt% led to formation of stripe and chain precipitates at and near grain boundaries, which caused a partial intergranular fracture of the as-HIPed alloy.