Meijie Sun
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Meijie Sun has a total of 21 co-authors. Here are the top co-authors by number of shared publications:
Zhiqiang Xu
School of Chemical and Environmental Engineering, China University of Mining and Technology-Beijing, Beijing 100083, PR China; Inner Mongolia Research Institute, China University of Mining and Technology-Beijing, Ordos 017001, PR China
3 shared publicationsYanan Tu
School of Chemical and Environmental Engineering, China University of Mining & Technology (Beijing), Beijing 100083, China
2 shared publications- Dinghua Liu
Suzhou Sinoma Design and Research Institute of Non-Metallic Minerals Industry Co., Ltd., Suzhou 215151, China
1 shared publication Haiyan Liu
School of Chemical and Environmental Engineering, China University of Mining & Technology (Beijing), Beijing100083, China
1 shared publicationJianping Zheng
School of Chemical and Environmental Engineering, China University of Mining & Technology (Beijing), Beijing 100083, China
1 shared publication- Jiapeng Li
School of Chemical and Environmental Engineering, China University of Mining & Technology (Beijing), Beijing 100083, China
1 shared publication
Latest Publications
- 9 May 2024
- Published by Elsevier in Waste Management
- Vol. 183, 74-86
Qualitative classification of waste garments for textile recycling based on machine vision and attention mechanisms
- 9 May 2024
- Published by Elsevier in Waste Management
- Vol. 183, 74-86
Qualitative classification of waste garments for textile recycling based on machine vision and attention mechanisms
- 20 July 2023
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 11 (30) , 11199-11206
Separation and Regeneration of LiNi1/3Co1/3Mn1/3O2 Materials from Spent Lithium-Ion Batteries: A Facile Process
- 20 July 2023
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 11 (30) , 11199-11206
Separation and Regeneration of LiNi1/3Co1/3Mn1/3O2 Materials from Spent Lithium-Ion Batteries: A Facile Process
- Open Access
- 20 December 2022
- Published by MDPI AG in Sustainability
- Vol. 15 (1) , 30
Separation of Graphites and Cathode Materials from Spent Lithium-Ion Batteries Using Roasting–Froth Flotation
The separation of graphites and cathode materials from spent lithium-ion batteries (LIBs) is essential to close the loop of material used in LIBs. In this study, the roasting characteristics of the spent LIB materials are carefully analyzed, and the effects of roasting on the surface morphology and elemental chemical states of electrode materials are fully investigated by thermogravimetric analysis, SEM-EDS, and XPS to explore the roasting–flotation enhancement mechanism. Then, froth flotation is utilized to separate the graphites and cathode materials from the spent LIB materials. The optimal roasting temperature is determined by thermogravimetric analysis and the SEM-EDS analysis of the spent LIB materials. The results suggest that the organic binder can be effectively removed from the spent LIB materials at the roasting temperature of 500 °C, and there is almost no loss of graphite. The XPS results indicate that, in the process of roasting, the decomposition products of the organic binder can easily react with valuable metals (Ni, Co, and Mn) to produce corresponding metal fluoride. The flotation results of the spent LIB materials after roasting at the optimal conditions indicate that graphites and cathode materials can be efficiently recovered through roasting–froth flotation. When the dosage of kerosene is 200 g/t and the dosage of methyl isobutyl carbinol (MIBC) is 150 g/t, the cathode materials grade is 91.6% with a recovery of 92.6%, while the graphite grade is 84.6% with a recovery of 82.7%. The roasting–froth flotation method lays the foundation for the subsequent metallurgical process.
- 20 December 2022
- Published by MDPI AG in Sustainability
- Vol. 15 (1) , 30
Open AccessSeparation of Graphites and Cathode Materials from Spent Lithium-Ion Batteries Using Roasting–Froth Flotation
The separation of graphites and cathode materials from spent lithium-ion batteries (LIBs) is essential to close the loop of material used in LIBs. In this study, the roasting characteristics of the spent LIB materials are carefully analyzed, and the effects of roasting on the surface morphology and elemental chemical states of electrode materials are fully investigated by thermogravimetric analysis, SEM-EDS, and XPS to explore the roasting–flotation enhancement mechanism. Then, froth flotation is utilized to separate the graphites and cathode materials from the spent LIB materials. The optimal roasting temperature is determined by thermogravimetric analysis and the SEM-EDS analysis of the spent LIB materials. The results suggest that the organic binder can be effectively removed from the spent LIB materials at the roasting temperature of 500 °C, and there is almost no loss of graphite. The XPS results indicate that, in the process of roasting, the decomposition products of the organic binder can easily react with valuable metals (Ni, Co, and Mn) to produce corresponding metal fluoride. The flotation results of the spent LIB materials after roasting at the optimal conditions indicate that graphites and cathode materials can be efficiently recovered through roasting–froth flotation. When the dosage of kerosene is 200 g/t and the dosage of methyl isobutyl carbinol (MIBC) is 150 g/t, the cathode materials grade is 91.6% with a recovery of 92.6%, while the graphite grade is 84.6% with a recovery of 82.7%. The roasting–froth flotation method lays the foundation for the subsequent metallurgical process.
- Open Access
- 25 October 2022
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 7 (44) , 40306-40315
Enrichment of Residual Carbon in Coal Gasification Fine Slag via Wet Sieving Separation with Ultrasonic Pretreatment
To overcome the environmental and economic challenges posed by the increasing amounts of the coal gasification slag, here, a simple and efficient method for enriching the residual carbon from the coal gasification fine slag was proposed. The residual carbon enrichment pattern in the particle size distribution of coal gasification fine slags after the ultrasonic pretreatment was mainly enriched toward the 500-250 μm and 250-125 μm particle size classes by analyzing the changes in the particle size distribution and apparent morphology. The pulp pretreatment at the ultrasonic output power of 270 W for 4 min was determined as the optimal experimental condition with respect to the yield, ash content, and ash rejection of the concentrates. Compared to the conventional wet sieving separation, the yield and ash content of the final concentrates were reduced by 7.99 and 14.96%, respectively. Moreover, the ash rejection of the final concentrates was as high as 88.51%, indicating an increment of 11.63% than the conventional wet sieving separation. Furthermore, thermogravimetric analysis confirmed that the final concentrates exhibited the lowest reactivity; however, these demonstrated had the highest carbon content (nearly 70%) with 27.27% ash content. The combustion characteristics analysis showed that the wet screening concentrate after ultrasonic pretreatment had the highest composite combustion characteristic index (S) of 3.17 × 10-8, as compared to the raw and conventional sieving concentrates.
- 25 October 2022
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 7 (44) , 40306-40315
Open AccessEnrichment of Residual Carbon in Coal Gasification Fine Slag via Wet Sieving Separation with Ultrasonic Pretreatment
To overcome the environmental and economic challenges posed by the increasing amounts of the coal gasification slag, here, a simple and efficient method for enriching the residual carbon from the coal gasification fine slag was proposed. The residual carbon enrichment pattern in the particle size distribution of coal gasification fine slags after the ultrasonic pretreatment was mainly enriched toward the 500-250 μm and 250-125 μm particle size classes by analyzing the changes in the particle size distribution and apparent morphology. The pulp pretreatment at the ultrasonic output power of 270 W for 4 min was determined as the optimal experimental condition with respect to the yield, ash content, and ash rejection of the concentrates. Compared to the conventional wet sieving separation, the yield and ash content of the final concentrates were reduced by 7.99 and 14.96%, respectively. Moreover, the ash rejection of the final concentrates was as high as 88.51%, indicating an increment of 11.63% than the conventional wet sieving separation. Furthermore, thermogravimetric analysis confirmed that the final concentrates exhibited the lowest reactivity; however, these demonstrated had the highest carbon content (nearly 70%) with 27.27% ash content. The combustion characteristics analysis showed that the wet screening concentrate after ultrasonic pretreatment had the highest composite combustion characteristic index (S) of 3.17 × 10-8, as compared to the raw and conventional sieving concentrates.
- Open Access
- 30 April 2021
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 6 (18) , 12027-12035
Effect of Hydrothermal Dehydration on the Slurry Ability of Lignite
- 30 April 2021
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 6 (18) , 12027-12035
Open AccessEffect of Hydrothermal Dehydration on the Slurry Ability of Lignite