Sang-Won Cho
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Sang-Won Cho has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Jin-Seok Yoo
Department of Materials Science and Engineering, Sungkyunkwan University, 2066, Seobu-Ro, Jangan-Gu, Suwon-Si 16419, Republic of Korea
2 shared publications - Jung-Gu Kim
Sungkyunkwan University
2 shared publications - Sang-Jin Ko
School of Advanced Materials Science and Engineering, Sungkyunkwan University (SKKU), Suwon 16419, Korea
2 shared publications - Eun-Ha Park
School of Advanced Materials Science and Engineering, Sungkyunkwan University, Suwon-si, Gyeonggi-do 16419, Republic of Korea
1 shared publication - Geon-Il Kim
School of Advanced Materials Science and Engineering, Sungkyunkwan University College of Engineering, Suwon-si, Republic of Korea, 16419
1 shared publication - Ha-Yeong Jo1 shared publication
Latest Publications
- Open Access
Comparison of Hydrogen Embrittlement Susceptibility of Different Types of Advanced High-Strength Steels
This study investigated the hydrogen embrittlement (HE) characteristics of advanced high-strength steels (AHSSs). Two different types of AHSSs with a tensile strength of 1.2 GPa were investigated. Slow strain rate tests (SSRTs) were performed under various applied potentials (Eapp) to identify the mechanism with the greatest effect on the embrittlement of the specimens. The SSRT results revealed that, as the Eapp increased, the elongation tended to increase, even when a potential exceeding the corrosion potential was applied. Both types of AHSSs exhibited embrittled fracture behavior that was dominated by HE. The fractured SSRT specimens were subjected to a thermal desorption spectroscopy analysis, revealing that diffusible hydrogen was trapped mainly at the grain boundaries and dislocations (i.e., reversible hydrogen-trapping sites). The micro-analysis results revealed that the poor HE resistance of the specimens was attributed to the more reversible hydrogen-trapping sites.
Open AccessComparison of Hydrogen Embrittlement Susceptibility of Different Types of Advanced High-Strength Steels
This study investigated the hydrogen embrittlement (HE) characteristics of advanced high-strength steels (AHSSs). Two different types of AHSSs with a tensile strength of 1.2 GPa were investigated. Slow strain rate tests (SSRTs) were performed under various applied potentials (Eapp) to identify the mechanism with the greatest effect on the embrittlement of the specimens. The SSRT results revealed that, as the Eapp increased, the elongation tended to increase, even when a potential exceeding the corrosion potential was applied. Both types of AHSSs exhibited embrittled fracture behavior that was dominated by HE. The fractured SSRT specimens were subjected to a thermal desorption spectroscopy analysis, revealing that diffusible hydrogen was trapped mainly at the grain boundaries and dislocations (i.e., reversible hydrogen-trapping sites). The micro-analysis results revealed that the poor HE resistance of the specimens was attributed to the more reversible hydrogen-trapping sites.
- Open Access
Effect of Cr on Aqueous and Atmospheric Corrosion of Automotive Carbon Steel
This study investigated the effect of Cr alloying element on the corrosion properties of automotive carbon steel (0.1C, 0.5Si, 2.5Mn, Fe Bal., composition given in wt.%) in aqueous and atmospheric conditions using electrochemical measurement and cyclic corrosion tests. Three steels with 0, 0.3, and 0.5 wt.% Cr were studied by electrochemical impedance spectroscopy. Polarization resistance (Rp) of 0.3 Cr and 0.5 Cr steels was higher than that of 0 Cr steel, and the Rp also increased as the Cr content increased. Therefore, Cr increases the corrosion resistance of automotive carbon steel immersed in a chloride ion (Cl−)-containing aqueous solution. In the cyclic corrosion test results, Cl− was concentrated at the metal/rust interface in all of the steels regardless of Cr content. The Cl− was uniformly concentrated and distributed on the 0 Cr steel, but locally and non-uniformly concentrated on the Cr-added steels. The inner rust layer consisted of β-FeOOH containing Cl− and Cr-goethite, while the outer rust layer was composed of amorphous iron oxyhydroxide mixed with various types of rust. FeCl2 and CrCl3 are formed from the Cl− nest developed in the early stage, and the pitting at CrCl3-formed regions are locally accelerated because Cr is strongly hydrolyzed to a very low pH.
Open AccessEffect of Cr on Aqueous and Atmospheric Corrosion of Automotive Carbon Steel
This study investigated the effect of Cr alloying element on the corrosion properties of automotive carbon steel (0.1C, 0.5Si, 2.5Mn, Fe Bal., composition given in wt.%) in aqueous and atmospheric conditions using electrochemical measurement and cyclic corrosion tests. Three steels with 0, 0.3, and 0.5 wt.% Cr were studied by electrochemical impedance spectroscopy. Polarization resistance (Rp) of 0.3 Cr and 0.5 Cr steels was higher than that of 0 Cr steel, and the Rp also increased as the Cr content increased. Therefore, Cr increases the corrosion resistance of automotive carbon steel immersed in a chloride ion (Cl−)-containing aqueous solution. In the cyclic corrosion test results, Cl− was concentrated at the metal/rust interface in all of the steels regardless of Cr content. The Cl− was uniformly concentrated and distributed on the 0 Cr steel, but locally and non-uniformly concentrated on the Cr-added steels. The inner rust layer consisted of β-FeOOH containing Cl− and Cr-goethite, while the outer rust layer was composed of amorphous iron oxyhydroxide mixed with various types of rust. FeCl2 and CrCl3 are formed from the Cl− nest developed in the early stage, and the pitting at CrCl3-formed regions are locally accelerated because Cr is strongly hydrolyzed to a very low pH.