Wei Deng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Wei Deng has a total of 80 co-authors. Here are the top co-authors by number of shared publications:
- Xufeng Zhou
Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo, PR China
22 shared publications - Zhaoping Liu
Ningbo Institute of Materials Technology & Engineering (NIMTE), Chinese Academy of Sciences (CAS), Ningbo 315201, China
19 shared publications Zhaoping Liu
11 shared publicationsQile Fang
Key Laboratory of Graphene Technologies and Applications of Zhejiang Province Advanced Li‐ion Battery Engineering Laboratory Ningbo Institute of Materials Technology and Engineering Chinese Academy of Sciences Zhejiang 315201 P. R. China
10 shared publicationsXufeng Zhou
8 shared publications- Bao Qiu
Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo, People’s Republic of China
5 shared publications
Latest Publications
- 5 November 2026
- Published by Wiley in Angewandte Chemie
Quantifying the Dissolution of Organic and Inorganic Components in Solid Electrolyte Interphase for Sodium‐Ion Batteries
Anode interphase dissolution is a major cause of instability in sodium‐ion batteries (SIBs) because Na‐based solid electrolyte interphase (SEI) compounds are more soluble than their Li analogues. Here, glyme electrolytes with varied chain lengths are used to regulate Na + solvation structure and clarify its effect on SEI dissolution. A component‐resolved framework combining ion chromatography, mass spectrometry, electrochemical quartz crystal microbalance, and X‐ray photoelectron spectroscopy is developed to quantify the dissolution and retention of organic and inorganic SEI species. This approach determines absolute SEI retention rather than relying on aggregate interphase loss. Compared with the glyme, tetraglyme reduces total SEI dissolution from 75% to 53% and increases the retention of inorganic F‐containing species from 18% to 30%. This improvement arises from an anion‐enriched Na + solvation shell, which promotes the formation of a thinner, denser, and more inorganic‐rich SEI. Consequently, 1.25 Ah NaNi 1/3 Fe 1/3 Mn 1/3 O 2 ||hard carbon pouch cells using the tetraglyme‐based electrolyte retain 91.2% capacity after 500 cycles and exhibit stable voltage retention during 21‐day aging at 60°C. These results establish a quantitative methodology for distinguishing the dissolution behavior of organic and inorganic SEI components, reveal the role of ether chain length in interphase stability, and provide practical guidance for designing durable SIBs.
- 5 November 2026
- Published by Wiley in Angewandte Chemie
Quantifying the Dissolution of Organic and Inorganic Components in Solid Electrolyte Interphase for Sodium‐Ion Batteries
Anode interphase dissolution is a major cause of instability in sodium‐ion batteries (SIBs) because Na‐based solid electrolyte interphase (SEI) compounds are more soluble than their Li analogues. Here, glyme electrolytes with varied chain lengths are used to regulate Na + solvation structure and clarify its effect on SEI dissolution. A component‐resolved framework combining ion chromatography, mass spectrometry, electrochemical quartz crystal microbalance, and X‐ray photoelectron spectroscopy is developed to quantify the dissolution and retention of organic and inorganic SEI species. This approach determines absolute SEI retention rather than relying on aggregate interphase loss. Compared with the glyme, tetraglyme reduces total SEI dissolution from 75% to 53% and increases the retention of inorganic F‐containing species from 18% to 30%. This improvement arises from an anion‐enriched Na + solvation shell, which promotes the formation of a thinner, denser, and more inorganic‐rich SEI. Consequently, 1.25 Ah NaNi 1/3 Fe 1/3 Mn 1/3 O 2 ||hard carbon pouch cells using the tetraglyme‐based electrolyte retain 91.2% capacity after 500 cycles and exhibit stable voltage retention during 21‐day aging at 60°C. These results establish a quantitative methodology for distinguishing the dissolution behavior of organic and inorganic SEI components, reveal the role of ether chain length in interphase stability, and provide practical guidance for designing durable SIBs.
- 5 November 2026
- Published by Wiley in Angewandte Chemie International Edition
- p. e5211841
Quantifying the Dissolution of Organic and Inorganic Components in Solid Electrolyte Interphase for Sodium‐Ion Batteries
Anode interphase dissolution is a major cause of instability in sodium‐ion batteries (SIBs) because Na‐based solid electrolyte interphase (SEI) compounds are more soluble than their Li analogues. Here, glyme electrolytes with varied chain lengths are used to regulate Na + solvation structure and clarify its effect on SEI dissolution. A component‐resolved framework combining ion chromatography, mass spectrometry, electrochemical quartz crystal microbalance, and X‐ray photoelectron spectroscopy is developed to quantify the dissolution and retention of organic and inorganic SEI species. This approach determines absolute SEI retention rather than relying on aggregate interphase loss. Compared with the glyme, tetraglyme reduces total SEI dissolution from 75% to 53% and increases the retention of inorganic F‐containing species from 18% to 30%. This improvement arises from an anion‐enriched Na + solvation shell, which promotes the formation of a thinner, denser, and more inorganic‐rich SEI. Consequently, 1.25 Ah NaNi 1/3 Fe 1/3 Mn 1/3 O 2 ||hard carbon pouch cells using the tetraglyme‐based electrolyte retain 91.2% capacity after 500 cycles and exhibit stable voltage retention during 21‐day aging at 60°C. These results establish a quantitative methodology for distinguishing the dissolution behavior of organic and inorganic SEI components, reveal the role of ether chain length in interphase stability, and provide practical guidance for designing durable SIBs.
- 5 November 2026
- Published by Wiley in Angewandte Chemie International Edition
- p. e5211841
Quantifying the Dissolution of Organic and Inorganic Components in Solid Electrolyte Interphase for Sodium‐Ion Batteries
Anode interphase dissolution is a major cause of instability in sodium‐ion batteries (SIBs) because Na‐based solid electrolyte interphase (SEI) compounds are more soluble than their Li analogues. Here, glyme electrolytes with varied chain lengths are used to regulate Na + solvation structure and clarify its effect on SEI dissolution. A component‐resolved framework combining ion chromatography, mass spectrometry, electrochemical quartz crystal microbalance, and X‐ray photoelectron spectroscopy is developed to quantify the dissolution and retention of organic and inorganic SEI species. This approach determines absolute SEI retention rather than relying on aggregate interphase loss. Compared with the glyme, tetraglyme reduces total SEI dissolution from 75% to 53% and increases the retention of inorganic F‐containing species from 18% to 30%. This improvement arises from an anion‐enriched Na + solvation shell, which promotes the formation of a thinner, denser, and more inorganic‐rich SEI. Consequently, 1.25 Ah NaNi 1/3 Fe 1/3 Mn 1/3 O 2 ||hard carbon pouch cells using the tetraglyme‐based electrolyte retain 91.2% capacity after 500 cycles and exhibit stable voltage retention during 21‐day aging at 60°C. These results establish a quantitative methodology for distinguishing the dissolution behavior of organic and inorganic SEI components, reveal the role of ether chain length in interphase stability, and provide practical guidance for designing durable SIBs.
- Open Access
- 4 May 2026
- Published by Springer Nature in Research Square
Chemically localized solvent-anion interactions enable ultra-high-loading practical lithium metal batteries operating at −70 ℃
Deploying high-energy practical lithium-based batteries at extreme low temperatures hinges on efficient ion transport within high-loading porous electrodes, yet it remains constrained by the long-range continuity of solvent-solvent interactions. Such interactions typically form percolating solvent networks that undergo substantial rigidification in freezing environments, drastically impeding ion transport. Herein, we reveal that introducing a co-solvent into the weak solvation electrolyte constructs localized solvent-anion motifs, effectively breaking the continuity of these extended interactions and fragmenting the global solvent network. These chemically localized solvent-anion interactions preserve the electrolyte's structural flexibility required for low-temperature operation while simultaneously ensuring an inorganic-rich interphase. Consequently, we demonstrate battery operation down to −70 ℃. Large-format 10.2 Ah lithium metal pouch cells with an ultra-high electrode loading (26.0 mg/cm2 and 96% active material) maintain stable cycling at −50 ℃. This work establishes a new paradigm, highlighting the decisive role of disrupting the long-range connectivity of the solvent network in designing electrolytes for low-temperature batteries.
- 4 May 2026
- Published by Springer Nature in Research Square
Open AccessChemically localized solvent-anion interactions enable ultra-high-loading practical lithium metal batteries operating at −70 ℃
Deploying high-energy practical lithium-based batteries at extreme low temperatures hinges on efficient ion transport within high-loading porous electrodes, yet it remains constrained by the long-range continuity of solvent-solvent interactions. Such interactions typically form percolating solvent networks that undergo substantial rigidification in freezing environments, drastically impeding ion transport. Herein, we reveal that introducing a co-solvent into the weak solvation electrolyte constructs localized solvent-anion motifs, effectively breaking the continuity of these extended interactions and fragmenting the global solvent network. These chemically localized solvent-anion interactions preserve the electrolyte's structural flexibility required for low-temperature operation while simultaneously ensuring an inorganic-rich interphase. Consequently, we demonstrate battery operation down to −70 ℃. Large-format 10.2 Ah lithium metal pouch cells with an ultra-high electrode loading (26.0 mg/cm2 and 96% active material) maintain stable cycling at −50 ℃. This work establishes a new paradigm, highlighting the decisive role of disrupting the long-range connectivity of the solvent network in designing electrolytes for low-temperature batteries.
- Open Access
- 1 May 2026
- Published by Springer Nature in Nature Communications
- Vol. 17 (1)
Interfacial excess charge dynamics as a quantitative descriptor to understand lithium dendrite growth
Unraveling the origins of Li dendrite growth remains a critical challenge for lithium metal batteries. Existing studies often treat diffusion-reaction mismatches or electrode surface excess charge in isolation, overlooking the coupled interfacial processes at the nanoscale solid-liquid interface that govern Li dendrite growth. Herein, we introduce the interfacial excess charge distribution factor, a quantitative descriptor that captures the dynamic equilibrium by integrating the contributions of electrode surface excess charge, charge depletion rate and solvation chemistry. We further propose an electrochemical method to monitor Li dendrite growth rates, confirming that electrolytes with rapid excess charge redistribution ability favor planar Li plating. Our findings reveal that the depletion rate of interfacial excess charge governed by Li⁺-dipole-anion interactions, and the degree of electrode excess charge modulated by solvation structures and cation screening, competitively determine the interfacial excess charge dynamics. Guided by these insights, we designed an electrolyte with optimized excess charge redistribution capability, which suppresses dendrite formation and enables stable cycling in ~6.4 Ah lithium metal batteries. This work provides mechanistic insight into how competitive interfacial processes dictate Li dendrite growth.
- 1 May 2026
- Published by Springer Nature in Nature Communications
- Vol. 17 (1)
Open AccessInterfacial excess charge dynamics as a quantitative descriptor to understand lithium dendrite growth
Unraveling the origins of Li dendrite growth remains a critical challenge for lithium metal batteries. Existing studies often treat diffusion-reaction mismatches or electrode surface excess charge in isolation, overlooking the coupled interfacial processes at the nanoscale solid-liquid interface that govern Li dendrite growth. Herein, we introduce the interfacial excess charge distribution factor, a quantitative descriptor that captures the dynamic equilibrium by integrating the contributions of electrode surface excess charge, charge depletion rate and solvation chemistry. We further propose an electrochemical method to monitor Li dendrite growth rates, confirming that electrolytes with rapid excess charge redistribution ability favor planar Li plating. Our findings reveal that the depletion rate of interfacial excess charge governed by Li⁺-dipole-anion interactions, and the degree of electrode excess charge modulated by solvation structures and cation screening, competitively determine the interfacial excess charge dynamics. Guided by these insights, we designed an electrolyte with optimized excess charge redistribution capability, which suppresses dendrite formation and enables stable cycling in ~6.4 Ah lithium metal batteries. This work provides mechanistic insight into how competitive interfacial processes dictate Li dendrite growth.
- Top Cited Papers
- 20 February 2026
- Published by Springer Nature in Nature Reviews Chemistry
- Vol. 10 (5) , 315-331
Understanding the degradation complexity of ultrahigh-energy lithium metal batteries
The combination of Li-rich layered oxide cathodes and lithium metal anodes enables lithium metal batteries (LMBs) to achieve specific energies exceeding 600 Wh kg−1, which is a crucial threshold requiring the activation of anionic oxygen-redox of cathode. The specific energy is attained owing to oxygen-redox reactions at the cathode and reversible Li plating–stripping at the anode, but these processes also induce distinct failure mechanisms. Structural destabilization at the cathode and anodic dendrite growth cause cell-level failures that impact the lifespan of LMBs more profoundly than material degradation alone. Moreover, the presence of lithium metal anodes obscures the detection of active Li loss, often leading to misinterpretations related to capacity fading and cycle life. This Review examines the progress in realizing 600 Wh kg−1 LMBs and understanding their lifespan failure mechanisms. We discuss the challenges in accurately assessing the lifespan and Li loss pathways of LMBs, and we elucidate the fundamental chemistry mechanisms driving both material-level and cell-level failures. In particular, the electrochemical implications of cell parameters, cell assembly and operating conditions on the lifespan are highlighted. We also outline the gaps in knowledge and advanced techniques required to decipher detailed failure modes for LMBs with oxygen-redox reactions and Li plating–stripping.
- 20 February 2026
- Published by Springer Nature in Nature Reviews Chemistry
- Vol. 10 (5) , 315-331
Top Cited PapersUnderstanding the degradation complexity of ultrahigh-energy lithium metal batteries
The combination of Li-rich layered oxide cathodes and lithium metal anodes enables lithium metal batteries (LMBs) to achieve specific energies exceeding 600 Wh kg−1, which is a crucial threshold requiring the activation of anionic oxygen-redox of cathode. The specific energy is attained owing to oxygen-redox reactions at the cathode and reversible Li plating–stripping at the anode, but these processes also induce distinct failure mechanisms. Structural destabilization at the cathode and anodic dendrite growth cause cell-level failures that impact the lifespan of LMBs more profoundly than material degradation alone. Moreover, the presence of lithium metal anodes obscures the detection of active Li loss, often leading to misinterpretations related to capacity fading and cycle life. This Review examines the progress in realizing 600 Wh kg−1 LMBs and understanding their lifespan failure mechanisms. We discuss the challenges in accurately assessing the lifespan and Li loss pathways of LMBs, and we elucidate the fundamental chemistry mechanisms driving both material-level and cell-level failures. In particular, the electrochemical implications of cell parameters, cell assembly and operating conditions on the lifespan are highlighted. We also outline the gaps in knowledge and advanced techniques required to decipher detailed failure modes for LMBs with oxygen-redox reactions and Li plating–stripping.
- Open Access
- 9 October 2025
- Published by Springer Nature in Research Square
Interfacial excess charge dynamics as a quantitative descriptor for deciphering lithium dendrite growth
Tracing the origins of Li dendrite growth remains a critical challenge for lithium metal batteries. Existing studies have focused on the mismatch between diffusion and reaction kinetics or on isolated electrode excess charge, overlooking the coupled interfacial processes at nanoscale solid-liquid interface that collectively govern dendrite growth. Herein, we introduce a unified descriptor, the interfacial excess charge distribution factor, to capture the dynamic equilibrium at electrode/electrolyte interface by quantitatively integrating the contributions of electrode excess charge, charge depletion rate and solvation chemistries. We further propose an electrochemical method to monitor Li dendrite growth rates, confirming that electrolytes with rapid excess charge redistribution ability favor planar Li plating. Our findings reveal that, the depletion rate of interfacial excess charge determined by Li⁺-dipole-anion interactions, and the degree of electrode excess charge modulated by solvation structures and cation screening, competitively determine the interfacial excess charge dynamics and Li dendrite growth. Leveraging these insights, we designed an electrolyte with rapid excess charge redistribution ability, which markedly suppressed dendrite formation and achieved superior cycling performance in ~ 6.4 Ah lithium metal batteries. This quantitative framework offers the way for deciphering complex interfacial electroplating and holds promise for other metal-based batteries (e.g., Na, K, Zn, Mg).
- 9 October 2025
- Published by Springer Nature in Research Square
Open AccessInterfacial excess charge dynamics as a quantitative descriptor for deciphering lithium dendrite growth
Tracing the origins of Li dendrite growth remains a critical challenge for lithium metal batteries. Existing studies have focused on the mismatch between diffusion and reaction kinetics or on isolated electrode excess charge, overlooking the coupled interfacial processes at nanoscale solid-liquid interface that collectively govern dendrite growth. Herein, we introduce a unified descriptor, the interfacial excess charge distribution factor, to capture the dynamic equilibrium at electrode/electrolyte interface by quantitatively integrating the contributions of electrode excess charge, charge depletion rate and solvation chemistries. We further propose an electrochemical method to monitor Li dendrite growth rates, confirming that electrolytes with rapid excess charge redistribution ability favor planar Li plating. Our findings reveal that, the depletion rate of interfacial excess charge determined by Li⁺-dipole-anion interactions, and the degree of electrode excess charge modulated by solvation structures and cation screening, competitively determine the interfacial excess charge dynamics and Li dendrite growth. Leveraging these insights, we designed an electrolyte with rapid excess charge redistribution ability, which markedly suppressed dendrite formation and achieved superior cycling performance in ~ 6.4 Ah lithium metal batteries. This quantitative framework offers the way for deciphering complex interfacial electroplating and holds promise for other metal-based batteries (e.g., Na, K, Zn, Mg).
- 5 October 2024
- Published by Royal Society of Chemistry (RSC) in Energy & Environmental Science
- Vol. 17 (23) , 9051-9092
Quantitatively detecting and characterizing metallic lithium in lithium-based batteries
Quantitative detection and characterization methods for analysis of metallic Li and related inactive components of Li batteries and their related characteristics are discussed.
- 5 October 2024
- Published by Royal Society of Chemistry (RSC) in Energy & Environmental Science
- Vol. 17 (23) , 9051-9092
Quantitatively detecting and characterizing metallic lithium in lithium-based batteries
Quantitative detection and characterization methods for analysis of metallic Li and related inactive components of Li batteries and their related characteristics are discussed.
- 29 September 2022
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 14 (40) , 46043-46055
CNT/PVDF Composite Coating Layer on Cu with a Synergy of Uniform Current Distribution and Stress Releasing for Improving Reversible Li Plating/Stripping
The uncontrollable formation of polymorphous Li deposits, e.g., whiskers, mosses, or dendrites resulting from nonuniform interfacial current distribution and internal stress release in the upward direction on the conventional current collector (e.g., Cu foil) of Li metal rechargeable batteries with a lithium-metal-free negatrode (LMFRBs), leads to rapid performance degradation or serious safety problems. The 3D carbon nanotubes (CNTs) skeleton has been proven to effectively reduce the current density and eliminate the internal accumulated stress. However, remarkable electrolyte decomposition, inherent Li source consumption due to repeated SEI formation, and Li+ intercalation in CNTs limit the application of 3D CNTs skeleton. Thus, it is necessary to avoid the side effects of the 3D CNTs skeleton and retain uniform interfacial current distribution and stress mitigation. In this work, we integrate the CNTs network with a soft functional polymer polyvinylidene fluoride (PVDF) to form a relatively dense coating layer on Cu foil, which can shield the contact between the internal surface of the 3D CNTs framework and the electrolyte. Simultaneously, the Li-F-rich SEI resulting from the partial reduction of PVDF with deposited Li and the soft nature of the coating layer release the accumulation of internal stress in the horizontal direction, resulting in mosses/whisker-free Li deposition. Thus, improved Li deposition/dissolution and stable cycling performance of the LMFRBs can be achieved.
- 29 September 2022
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 14 (40) , 46043-46055
CNT/PVDF Composite Coating Layer on Cu with a Synergy of Uniform Current Distribution and Stress Releasing for Improving Reversible Li Plating/Stripping
The uncontrollable formation of polymorphous Li deposits, e.g., whiskers, mosses, or dendrites resulting from nonuniform interfacial current distribution and internal stress release in the upward direction on the conventional current collector (e.g., Cu foil) of Li metal rechargeable batteries with a lithium-metal-free negatrode (LMFRBs), leads to rapid performance degradation or serious safety problems. The 3D carbon nanotubes (CNTs) skeleton has been proven to effectively reduce the current density and eliminate the internal accumulated stress. However, remarkable electrolyte decomposition, inherent Li source consumption due to repeated SEI formation, and Li+ intercalation in CNTs limit the application of 3D CNTs skeleton. Thus, it is necessary to avoid the side effects of the 3D CNTs skeleton and retain uniform interfacial current distribution and stress mitigation. In this work, we integrate the CNTs network with a soft functional polymer polyvinylidene fluoride (PVDF) to form a relatively dense coating layer on Cu foil, which can shield the contact between the internal surface of the 3D CNTs framework and the electrolyte. Simultaneously, the Li-F-rich SEI resulting from the partial reduction of PVDF with deposited Li and the soft nature of the coating layer release the accumulation of internal stress in the horizontal direction, resulting in mosses/whisker-free Li deposition. Thus, improved Li deposition/dissolution and stable cycling performance of the LMFRBs can be achieved.
- 29 September 2022
- Published by Springer Nature in Nature Energy
- Vol. 7 (11) , 1031-1041
Quantification of reversible and irreversible lithium in practical lithium-metal batteries
- 29 September 2022
- Published by Springer Nature in Nature Energy
- Vol. 7 (11) , 1031-1041
Quantification of reversible and irreversible lithium in practical lithium-metal batteries
- 1 April 2022
- Published by Elsevier in Materials Today Energy
- Vol. 26
Seamlessly integrated alloy-polymer interphase for high-rate and long-life lithium metal anodes
- 1 April 2022
- Published by Elsevier in Materials Today Energy
- Vol. 26
Seamlessly integrated alloy-polymer interphase for high-rate and long-life lithium metal anodes