Oleg Z. Yanchevskii
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Oleg Z. Yanchevskii has a total of 48 co-authors. Here are the top co-authors by number of shared publications:
- Oleg Ivanovich V'Yunov
V. I. Vernadsky Institute of General and Inorganic Chemistry, NAS of Ukraine, Kyiv, Ukraine
15 shared publications - Anatolii Grigorievich Belous
V.I. Vernadsky Institute of General and Inorganic Chemistry of the National Academy of Sciences of Ukraine 2 , Palladina Ave., 32/34, Kyiv 03142
11 shared publications - Tetiana Plutenko
Solid-state chemistry department, V.I. Vernadsky Institute of General and Inorganic Chemistry of the National Academy of Sciences of Ukraine
7 shared publications - Oleksandr Fedorchuk
V.I. Vernadsky Institute of General and Inorganic Chemistry of the National Academy of Sciences of Ukraine 2 , Palladina Ave., 32/34, Kyiv 03142
5 shared publications - Alexander I. Tovstolytkin
V. G. Baryakhtar Institute of Magnetism of the National Academy of Sciences of Ukraine 1 , Kyiv 03142
4 shared publications A.G. Belous
3 shared publications
Latest Publications
- 1 December 2025
- Published by Taylor & Francis in Molecular Crystals and Liquid Crystals
- Vol. 770 (2) , 299-313
Impact of preparation conditions on the microstructure and microwave dielectric properties of NdMg 0.5 Ti 0.5 O 3 ceramics
- 1 December 2025
- Published by Taylor & Francis in Molecular Crystals and Liquid Crystals
- Vol. 770 (2) , 299-313
Impact of preparation conditions on the microstructure and microwave dielectric properties of NdMg 0.5 Ti 0.5 O 3 ceramics
- 15 October 2025
- Published by Elsevier in Journal of Solid State Chemistry
- Vol. 353
Solid-state synthesis and microwave dielectric properties of Ca0.61(Nd1-xYx)0.26TiO3 ceramics
- 15 October 2025
- Published by Elsevier in Journal of Solid State Chemistry
- Vol. 353
Solid-state synthesis and microwave dielectric properties of Ca0.61(Nd1-xYx)0.26TiO3 ceramics
- 13 August 2024
- Published by Taylor & Francis in Molecular Crystals and Liquid Crystals
- Vol. 768 (18) , 1163-1173
Microwave properties of SrY 2 O 4 spinel synthesized for advanced applications
- 13 August 2024
- Published by Taylor & Francis in Molecular Crystals and Liquid Crystals
- Vol. 768 (18) , 1163-1173
Microwave properties of SrY 2 O 4 spinel synthesized for advanced applications
- Open Access
- 28 July 2023
- Published by V.I. Vernadsky Institute of General and Inorganic Chemistry in Ukrainian Chemistry Journal
- Vol. 89 (6) , 71-78
Al-DOPED LANTHANUM-LITHIUM TITANATE WITH HIGH DIELECTRIC CONSTANT
La0.67LixTi1-xAlxO3 ceramics (x = 0.05, 0.10, 0.15, 0.20, 0.25, 0.30) were synthesized with the use of Al2O3 and an aqueous solution of Al(NO3)3 as an aluminium source. In both cases, the ceramics preserve a high dielectric constant ε ~ 105. It was found that the single-phase La0.67LixTi1-xAlxO3 perovskite structure is formed at temperatures above 1200 C. It was shown that the use of Al(NO3)3 allows simplifying the synthesis: reduction in the sintering temperature by 20 C, Li loss and, as a result, an increase in the density of ceramics. Ceramics La0.67Li0.15Ti0.85Al0.15O3 with a maximum density higher than 85 % were sintered at about 1280 and 1300 C of with the use of Al(NO3)3 and Al2O3 respectively. Frequency spectra of imaginary parts of impedance and electrical modulus demonstrate two dispersion regions that refer to processes in the ceramic grains’ boundaries and ceramic grains. Ceramic samples synthesized using Al(NO3)3 solutions tend to exhibit higher dielectric constants than those synthesized using Al2O3. At a frequency of 100 Hz, the dielectric constant for ceramics synthesized using Al(NO3)3 aqueous solution is 70600, whereas that for ceramics synthesized using Al2O3 is 44300. Obtained materials are useful for microelectronics, energy storage and harvesting devices.
- 28 July 2023
- Published by V.I. Vernadsky Institute of General and Inorganic Chemistry in Ukrainian Chemistry Journal
- Vol. 89 (6) , 71-78
Open AccessAl-DOPED LANTHANUM-LITHIUM TITANATE WITH HIGH DIELECTRIC CONSTANT
La0.67LixTi1-xAlxO3 ceramics (x = 0.05, 0.10, 0.15, 0.20, 0.25, 0.30) were synthesized with the use of Al2O3 and an aqueous solution of Al(NO3)3 as an aluminium source. In both cases, the ceramics preserve a high dielectric constant ε ~ 105. It was found that the single-phase La0.67LixTi1-xAlxO3 perovskite structure is formed at temperatures above 1200 C. It was shown that the use of Al(NO3)3 allows simplifying the synthesis: reduction in the sintering temperature by 20 C, Li loss and, as a result, an increase in the density of ceramics. Ceramics La0.67Li0.15Ti0.85Al0.15O3 with a maximum density higher than 85 % were sintered at about 1280 and 1300 C of with the use of Al(NO3)3 and Al2O3 respectively. Frequency spectra of imaginary parts of impedance and electrical modulus demonstrate two dispersion regions that refer to processes in the ceramic grains’ boundaries and ceramic grains. Ceramic samples synthesized using Al(NO3)3 solutions tend to exhibit higher dielectric constants than those synthesized using Al2O3. At a frequency of 100 Hz, the dielectric constant for ceramics synthesized using Al(NO3)3 aqueous solution is 70600, whereas that for ceramics synthesized using Al2O3 is 44300. Obtained materials are useful for microelectronics, energy storage and harvesting devices.
- 26 August 2021
- Published by V.I. Vernadsky Institute of General and Inorganic Chemistry in Ukrainian Chemistry Journal
- Vol. 87 (7) , 47-60
CARBONATE PRECURSOR ROUTE FOR PREPARATION OF CaCu3Ti4O12
A simple CaCu3Ti4O12 synthesis method by carbonate precipitation has been developed, which is not inferior to the known methods of precipitation from solutions. The optimum temperatures for the synthesis of powder (850 оС) and sintering of ceramics (1080 оС) have been found. The CCTO ceramic prepared has stable and fine electrical properties. In the frequency range of 1 kHz to 1 MHz, the ε’ value always is higher 104 with the dielectric losses, tan δ ~ 0.05–0.08. Such CCTO ceramic prepared by the сarbonate co-precipitation method with good electric properties should find applications in electric devices.
- 26 August 2021
- Published by V.I. Vernadsky Institute of General and Inorganic Chemistry in Ukrainian Chemistry Journal
- Vol. 87 (7) , 47-60
CARBONATE PRECURSOR ROUTE FOR PREPARATION OF CaCu3Ti4O12
A simple CaCu3Ti4O12 synthesis method by carbonate precipitation has been developed, which is not inferior to the known methods of precipitation from solutions. The optimum temperatures for the synthesis of powder (850 оС) and sintering of ceramics (1080 оС) have been found. The CCTO ceramic prepared has stable and fine electrical properties. In the frequency range of 1 kHz to 1 MHz, the ε’ value always is higher 104 with the dielectric losses, tan δ ~ 0.05–0.08. Such CCTO ceramic prepared by the сarbonate co-precipitation method with good electric properties should find applications in electric devices.
- 25 June 2021
- Published by V.I. Vernadsky Institute of General and Inorganic Chemistry in Ukrainian Chemistry Journal
- Vol. 87 (5) , 15-24
THE SYNTHESIS IMPACT ON DIELECTRIC PROPERTIES OF La0.5Li0.5-xNaxTiO3
Using X-ray powder, diffraction the sequence of reactions occurring during the synthesis La0.5Li0.5-xNaxTiO3 by solid-state reaction technique has been determined. Using electron microscopy it has been shown that the grain size decreases with increasing x in La0.5Li0.5-xNaxTiO3 system. The influence of the grain size of ceramics on the dielectric characteristics has been indicated. The frequency dependences of permittivity and dielectric loss tangent have been investigated by ac impedance spectroscopy. It has been established that ceramic sample of La0.5Li0.4Na0.1TiO3 solid solution has the largest value of permittivity ɛ > 104 at wide frequency range (1–104 Hz) in La0.5Li0.5-xNaxTiO3 system.
- 25 June 2021
- Published by V.I. Vernadsky Institute of General and Inorganic Chemistry in Ukrainian Chemistry Journal
- Vol. 87 (5) , 15-24
THE SYNTHESIS IMPACT ON DIELECTRIC PROPERTIES OF La0.5Li0.5-xNaxTiO3
Using X-ray powder, diffraction the sequence of reactions occurring during the synthesis La0.5Li0.5-xNaxTiO3 by solid-state reaction technique has been determined. Using electron microscopy it has been shown that the grain size decreases with increasing x in La0.5Li0.5-xNaxTiO3 system. The influence of the grain size of ceramics on the dielectric characteristics has been indicated. The frequency dependences of permittivity and dielectric loss tangent have been investigated by ac impedance spectroscopy. It has been established that ceramic sample of La0.5Li0.4Na0.1TiO3 solid solution has the largest value of permittivity ɛ > 104 at wide frequency range (1–104 Hz) in La0.5Li0.5-xNaxTiO3 system.
- 31 July 2019
- Published by V.I. Vernadsky Institute of General and Inorganic Chemistry in Ukrainian Chemistry Journal
- Vol. 85 (6)
SYNTHESIS, PROPERTIES CaCu3Ti4O12 WITH COLOSSAL VALUE OF THE DIELECTRIC PERMITTIVITY
Ceramic materials CaCu3Ti4O12 were synthesized by solid-phase reactions technique. The sequence of chemical reactions during the synthesis has been determined. Phase CaCu3Ti4O12 appears at 700 °C. At 800 – 900 °C, the intermediate phases CaTiO3, CuTiO3 and Ca3Ti2O7 are formed. Calcium and copper titanates, CaTiO3 and CuTiO3 interact to form CaCu3Ti4O12. Ca3Ti2O7 phase with pyrochlore structure is stable and prevent the formation of final product, CaCu3Ti4O12. A method for the synthesis of CaCu3Ti4O12 by solid-state reactions technique from previously synthesized CaTiO3 (at 1050 °С) and CuTiO3 (at 950 °С), taken in a molar ratio of 1:3, is proposed. This method give the possibility to avoid the appearance of an undesirable Ca3Ti2O7 phase with the pyrochlore structure and to reduce the content of free copper oxide to value less than 0.5 mol.%. In addition, instead of the copper oxide, which is usually used in solid-state reaction technique, the chemically more active form of the copper-containing reagent, CuCO3∙Cu(OН)2 were used. This reduce the synthesis time of the intermediate CuTiO3. The crystal structure, chemical composition, microstructure and electrophysical parameters of ceramics have been analyzed. The synthesized ceramics CaCu3Ti4O12 is cubic body-centered (space group Im-3) with the unit cell parameter a = 7.3932 Å, which agreed with the literature data. The calculated tolerance factor of CaCu3Ti4O12, t = 0.7626 is not sufficient for a stabilization of peroskite ABO3 structure; that is why the crystal structure of this compound contains 3 different cation sites: dodecahedral (Ca2+), octahedral (Ti4+), tetrahedral (Cu2+). At 1150 °C, the density of CaCu3Ti4O12 ceramic sintered has a maximum (90% of the theoretical density). At infra-low frequencies (10-3 Hz), the dielectric constant (e) reaches record values of 107, however, dielectric losses (tg d) up to 10 were observed. In the frequency range 10-3 - 105 Hz the value of ɛ exceeds 104; and at 105 Hz minimum of the dielectric losses (tg δ ~ 0.1) is observed. A comparative analysis of methods for the synthesis of CaCu3Ti4O12 shows that the synthesis conditions of material of the same chemical composition can be crucial in creating high dense ceramic with uniform grains, high dielectric constant and low dielectric losses in a wide frequency range.
- 31 July 2019
- Published by V.I. Vernadsky Institute of General and Inorganic Chemistry in Ukrainian Chemistry Journal
- Vol. 85 (6)
SYNTHESIS, PROPERTIES CaCu3Ti4O12 WITH COLOSSAL VALUE OF THE DIELECTRIC PERMITTIVITY
Ceramic materials CaCu3Ti4O12 were synthesized by solid-phase reactions technique. The sequence of chemical reactions during the synthesis has been determined. Phase CaCu3Ti4O12 appears at 700 °C. At 800 – 900 °C, the intermediate phases CaTiO3, CuTiO3 and Ca3Ti2O7 are formed. Calcium and copper titanates, CaTiO3 and CuTiO3 interact to form CaCu3Ti4O12. Ca3Ti2O7 phase with pyrochlore structure is stable and prevent the formation of final product, CaCu3Ti4O12. A method for the synthesis of CaCu3Ti4O12 by solid-state reactions technique from previously synthesized CaTiO3 (at 1050 °С) and CuTiO3 (at 950 °С), taken in a molar ratio of 1:3, is proposed. This method give the possibility to avoid the appearance of an undesirable Ca3Ti2O7 phase with the pyrochlore structure and to reduce the content of free copper oxide to value less than 0.5 mol.%. In addition, instead of the copper oxide, which is usually used in solid-state reaction technique, the chemically more active form of the copper-containing reagent, CuCO3∙Cu(OН)2 were used. This reduce the synthesis time of the intermediate CuTiO3. The crystal structure, chemical composition, microstructure and electrophysical parameters of ceramics have been analyzed. The synthesized ceramics CaCu3Ti4O12 is cubic body-centered (space group Im-3) with the unit cell parameter a = 7.3932 Å, which agreed with the literature data. The calculated tolerance factor of CaCu3Ti4O12, t = 0.7626 is not sufficient for a stabilization of peroskite ABO3 structure; that is why the crystal structure of this compound contains 3 different cation sites: dodecahedral (Ca2+), octahedral (Ti4+), tetrahedral (Cu2+). At 1150 °C, the density of CaCu3Ti4O12 ceramic sintered has a maximum (90% of the theoretical density). At infra-low frequencies (10-3 Hz), the dielectric constant (e) reaches record values of 107, however, dielectric losses (tg d) up to 10 were observed. In the frequency range 10-3 - 105 Hz the value of ɛ exceeds 104; and at 105 Hz minimum of the dielectric losses (tg δ ~ 0.1) is observed. A comparative analysis of methods for the synthesis of CaCu3Ti4O12 shows that the synthesis conditions of material of the same chemical composition can be crucial in creating high dense ceramic with uniform grains, high dielectric constant and low dielectric losses in a wide frequency range.
- Open Access
- 1 January 2018
- Published by Taras Shevchenko National University of Kyiv in French-Ukrainian Journal of Chemistry
- Vol. 6 (1) , 16-20
Zirconium Oxide Stabilized By Scandium (III) And Cerium (IV) Complex Oxides As The Basis For Preparation Of Thick Films And Multilayers Structures For Low Temperature (600 °C) Fuel Cell
Weakly agglomerated zirconium dioxide nanopowders stabilized by complex oxides of scandium (III) and cerium (IV) were synthesized by precipitation from aqueous solutions. Using weakly agglomerated nanopowders, thick films were prepared by tape casting on a-Al2O3 substrates. These thick films have high oxygen conductivity; and their electron conductivity is lower than oxygen conductivity by 4 orders of magnitude. A multilayer system consisting of films of polycrystalline porous anode and solid electrolyte was prepared. The diffusion of cations in the anode boundary layer and change in the chemical composition of the electrolyte film are not observed at optimum synthesis conditions.
- 1 January 2018
- Published by Taras Shevchenko National University of Kyiv in French-Ukrainian Journal of Chemistry
- Vol. 6 (1) , 16-20
Open AccessZirconium Oxide Stabilized By Scandium (III) And Cerium (IV) Complex Oxides As The Basis For Preparation Of Thick Films And Multilayers Structures For Low Temperature (600 °C) Fuel Cell
Weakly agglomerated zirconium dioxide nanopowders stabilized by complex oxides of scandium (III) and cerium (IV) were synthesized by precipitation from aqueous solutions. Using weakly agglomerated nanopowders, thick films were prepared by tape casting on a-Al2O3 substrates. These thick films have high oxygen conductivity; and their electron conductivity is lower than oxygen conductivity by 4 orders of magnitude. A multilayer system consisting of films of polycrystalline porous anode and solid electrolyte was prepared. The diffusion of cations in the anode boundary layer and change in the chemical composition of the electrolyte film are not observed at optimum synthesis conditions.
- Open Access
- 4 May 2016
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 5 (2) , 117-125
Semi-oxalate synthesis of (1−x)BaTiO3−xM0.5Bi0.5TiO3 (M = Li, Na, K) PTCR materials
(1−x)BaTiO3–xM0.5Bi0.5TiO3 (M = Li, Na, K) solid solutions were prepared using BaTiO3 pre-synthesized by oxalate method. The stability limits of (1−x)BaTiO3–xLi0.5Bi0.5TiO3 solid solutions have been established. It was shown that increase in M0.5Bi0.5TiO3 concentration results in reduction of ceramic grain size in the (1−x)BaTiO3−xM0.5Bi0.5TiO3 (M = Li, Na, K) system. It was found that the positive temperature coefficient of resistance (PTCR) effect in lead-free materials is due to the presence of a semiconductor core, which is formed by sintering under reducing atmosphere, and dielectric grain boundaries, formed on additional oxidation in air. The use of barium titanate, pre-synthesized by oxalate method, in the synthesis of solid solutions reduced the sintering temperature of ceramics compared with solid state reaction technique. By comparing the electrical properties of the synthesized lead-containing and lead-free materials, it has been shown that lead-free materials exhibit better electrical properties for practical use compared with lead-containing materials.
- 4 May 2016
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 5 (2) , 117-125
Open AccessSemi-oxalate synthesis of (1−x)BaTiO3−xM0.5Bi0.5TiO3 (M = Li, Na, K) PTCR materials
(1−x)BaTiO3–xM0.5Bi0.5TiO3 (M = Li, Na, K) solid solutions were prepared using BaTiO3 pre-synthesized by oxalate method. The stability limits of (1−x)BaTiO3–xLi0.5Bi0.5TiO3 solid solutions have been established. It was shown that increase in M0.5Bi0.5TiO3 concentration results in reduction of ceramic grain size in the (1−x)BaTiO3−xM0.5Bi0.5TiO3 (M = Li, Na, K) system. It was found that the positive temperature coefficient of resistance (PTCR) effect in lead-free materials is due to the presence of a semiconductor core, which is formed by sintering under reducing atmosphere, and dielectric grain boundaries, formed on additional oxidation in air. The use of barium titanate, pre-synthesized by oxalate method, in the synthesis of solid solutions reduced the sintering temperature of ceramics compared with solid state reaction technique. By comparing the electrical properties of the synthesized lead-containing and lead-free materials, it has been shown that lead-free materials exhibit better electrical properties for practical use compared with lead-containing materials.