Ahmed S. Ouda
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Ahmed S. Ouda has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
Mahmoud Gharieb
Raw Building Materials Technology and Processing Research Institute, Housing & Building National Research Center, HBRC, Cairo, Egypt
3 shared publicationsAlaa M. Rashad
Building Materials Research and Quality Control Institute, Housing & Building National Research Center (HBRC), Cairo, Egypt
2 shared publications- Alaa M. Rashad
Building Materials Research and Quality Control Institute, Housing and Building National Research Center (HBRC), Cairo, Egypt
2 shared publications Dina M. Sadek
Associate Professor, Building Materials Research and Quality Control Institute, Housing and Building National Research Center, Cairo 11511, Egypt
1 shared publicationHakim S. Abdelgader
Faculty of Engineering, Department of Civil Engineering, University of Tripoli, Tripoli, Libya
1 shared publication- Hamdy A. Abdel-Gawwad
Raw Building Materials and Processing Technology Research Institute, Housing and Building National Research Center (HBRC), Giza, Cairo, Egypt
1 shared publication
Latest Publications
- 17 January 2026
- Published by Springer Nature in Environmental Science and Pollution Research
- Vol. 33 (3) , 1042-1061
Towards sustainable radiation protection: hydration, gamma-ray, and neutron shielding of OPC–limestone composites from diverse geological origins
This study investigates the influence of partial replacement of ordinary Portland cement with limestone from three distinct geological sources at substitution levels of 5–20 Wt. %. The effects on hydration kinetics and phase composition were systematically evaluated over curing periods of 3, 7, 28, and 90 days. The water demand, setting time, chemically bound water, bulk density, total porosity, free lime, and compressive strength were evaluated. Differential thermal analysis and X-ray diffraction were employed to characterize hydration products and phase identification. Results indicated that both limestone replacement levels and source significantly influenced hydration behavior and mechanical performance. Alexandria limestone, particularly at replacement levels of 5 to 10%, enhanced hydration kinetics in the early ages and compressive strength due to favorable particle properties and nucleation effects, while El-Menia limestone showed a higher long-term chemically bound water content, indicating a greater overall degree of hydration at extended treatment lifetimes. In contrast, Helwan limestone showed reduced performance at higher substitution levels, likely due to its coarser texture and lower reactivity. Furthermore, the gamma ray attenuation and neutron shielding performance were significantly influenced by the mixture composition. Alexandria mixtures (Ax5 and Ax10) exhibited the highest linear attenuation coefficients (LAC), lowest half-value layers (HVL), and highest radiation protection efficiency (RPE), particularly at 0.662, 1.17, and 1.33 MeV. Neutron shielding showed a similar trend, with Alexandria mixtures achieving superior macroscopic neutron cross-section, confirming their suitability for multi-functional structural and shielding purposes.
- 17 January 2026
- Published by Springer Nature in Environmental Science and Pollution Research
- Vol. 33 (3) , 1042-1061
Towards sustainable radiation protection: hydration, gamma-ray, and neutron shielding of OPC–limestone composites from diverse geological origins
This study investigates the influence of partial replacement of ordinary Portland cement with limestone from three distinct geological sources at substitution levels of 5–20 Wt. %. The effects on hydration kinetics and phase composition were systematically evaluated over curing periods of 3, 7, 28, and 90 days. The water demand, setting time, chemically bound water, bulk density, total porosity, free lime, and compressive strength were evaluated. Differential thermal analysis and X-ray diffraction were employed to characterize hydration products and phase identification. Results indicated that both limestone replacement levels and source significantly influenced hydration behavior and mechanical performance. Alexandria limestone, particularly at replacement levels of 5 to 10%, enhanced hydration kinetics in the early ages and compressive strength due to favorable particle properties and nucleation effects, while El-Menia limestone showed a higher long-term chemically bound water content, indicating a greater overall degree of hydration at extended treatment lifetimes. In contrast, Helwan limestone showed reduced performance at higher substitution levels, likely due to its coarser texture and lower reactivity. Furthermore, the gamma ray attenuation and neutron shielding performance were significantly influenced by the mixture composition. Alexandria mixtures (Ax5 and Ax10) exhibited the highest linear attenuation coefficients (LAC), lowest half-value layers (HVL), and highest radiation protection efficiency (RPE), particularly at 0.662, 1.17, and 1.33 MeV. Neutron shielding showed a similar trend, with Alexandria mixtures achieving superior macroscopic neutron cross-section, confirming their suitability for multi-functional structural and shielding purposes.
- 7 November 2025
- Published by Elsevier in Progress in Nuclear Energy
- Vol. 192
Examination of thermal loads in M-60 grade high-performance heavy-density concrete for potential use in nuclear facility designs
- 7 November 2025
- Published by Elsevier in Progress in Nuclear Energy
- Vol. 192
Examination of thermal loads in M-60 grade high-performance heavy-density concrete for potential use in nuclear facility designs
- Open Access
- 6 January 2025
- Published by Springer Nature in Scientific Reports
- Vol. 15 (1) , 1-21
Novel approach to enhance the efficiency of mortar against radiations by co-incorporation of lead and boron compounds with calcium chloride
Fabrication of heavy density mortar using aggregates reinforced with available solid inorganic chemical additives is of a great importance as a protective layer to mitigate radiations in nuclear facilities. The effect of lead oxide and borax decahydrate on the hydration kinetics was evaluated by determining setting time, leachability and compressive strength. To speed up the reaction, 0.5% calcium chloride was added to all formulations, and then the results were compared to their blank counterparts. Once, the optimal compositions were explored, another batch of mortar were designed to increase efficiency against radioactive sources with different photon energies. After 28 days, bulk density, linear attenuation coefficient, half-value layer, tenth-value layer, and mean-free path in the field of 137Cs and51Co were considered. Similarly, macroscopic effective removal cross-section was evaluated using radioactive source-239Pu-α-9Be. According to the previous literature, adding 0.2% PbO to cement is the optimal ratio without affecting hydration kinetics and phase composition. The study explored that, co-incorporation of PbO with 0.5% CaCl2 increases the ratio to 2.5%, while enhancing physico-mechanical and radiological characteristics against radioactive sources. Also, formulation incorporating 0.5% borax with 0.5% CaCl2 had superior attenuation against neutrons compared to other competitors.
- 6 January 2025
- Published by Springer Nature in Scientific Reports
- Vol. 15 (1) , 1-21
Open AccessNovel approach to enhance the efficiency of mortar against radiations by co-incorporation of lead and boron compounds with calcium chloride
Fabrication of heavy density mortar using aggregates reinforced with available solid inorganic chemical additives is of a great importance as a protective layer to mitigate radiations in nuclear facilities. The effect of lead oxide and borax decahydrate on the hydration kinetics was evaluated by determining setting time, leachability and compressive strength. To speed up the reaction, 0.5% calcium chloride was added to all formulations, and then the results were compared to their blank counterparts. Once, the optimal compositions were explored, another batch of mortar were designed to increase efficiency against radioactive sources with different photon energies. After 28 days, bulk density, linear attenuation coefficient, half-value layer, tenth-value layer, and mean-free path in the field of 137Cs and51Co were considered. Similarly, macroscopic effective removal cross-section was evaluated using radioactive source-239Pu-α-9Be. According to the previous literature, adding 0.2% PbO to cement is the optimal ratio without affecting hydration kinetics and phase composition. The study explored that, co-incorporation of PbO with 0.5% CaCl2 increases the ratio to 2.5%, while enhancing physico-mechanical and radiological characteristics against radioactive sources. Also, formulation incorporating 0.5% borax with 0.5% CaCl2 had superior attenuation against neutrons compared to other competitors.
- 27 July 2022
- Published by Springer Nature in Environmental Science and Pollution Research
- Vol. 30 (1) , 127-144
Evaluating the role of feldspar on the resistivity of alkali-activated slag towards seawater attack
In this study, the effect of K-feldspar on the behavior of alkali-activated slag pastes (AAS) before and after exposure to seawater was evaluated by measuring the compressive strength and the microstructure. To achieve this objective, the mixtures were prepared upon partial replacement of ground granulated-blast furnace slag (GGBFS) with calcined and un-calcined feldspar fine particles (termed as FS and CFS) at levels ranging from 5 to 20%, by mass. Under processing conditions, the solidified specimens were immersed for 1, 7, 14, and 28 days in 100% RH at 40 ± 2 °C. After 28 days, a group of samples having the same composition were soaked in seawater solution for 1, 3, and 6 months. The new phases were evaluated using X-ray diffraction (XRD), thermogravimetric analysis (TGA/DTG), and scanning electron microscopy (SEM). The inclusion of FS and/or CFS in AAS enhances the performance of the pastes in normal and harsh conditions in relation to their reference counterparts. Among all the mixtures that were tested, alkali-activated composite comprising 15% CFS indicated more durable properties in terms of increased compressive strength and dense morphological structure after exposure to an aggressive environment.
- 27 July 2022
- Published by Springer Nature in Environmental Science and Pollution Research
- Vol. 30 (1) , 127-144
Evaluating the role of feldspar on the resistivity of alkali-activated slag towards seawater attack
In this study, the effect of K-feldspar on the behavior of alkali-activated slag pastes (AAS) before and after exposure to seawater was evaluated by measuring the compressive strength and the microstructure. To achieve this objective, the mixtures were prepared upon partial replacement of ground granulated-blast furnace slag (GGBFS) with calcined and un-calcined feldspar fine particles (termed as FS and CFS) at levels ranging from 5 to 20%, by mass. Under processing conditions, the solidified specimens were immersed for 1, 7, 14, and 28 days in 100% RH at 40 ± 2 °C. After 28 days, a group of samples having the same composition were soaked in seawater solution for 1, 3, and 6 months. The new phases were evaluated using X-ray diffraction (XRD), thermogravimetric analysis (TGA/DTG), and scanning electron microscopy (SEM). The inclusion of FS and/or CFS in AAS enhances the performance of the pastes in normal and harsh conditions in relation to their reference counterparts. Among all the mixtures that were tested, alkali-activated composite comprising 15% CFS indicated more durable properties in terms of increased compressive strength and dense morphological structure after exposure to an aggressive environment.
- 2 December 2021
- Published by Springer Nature in Environmental Science and Pollution Research
- Vol. 29 (18) , 26631-26647
An investigation on the performance of lightweight mortar-based geopolymer containing high-volume LECA aggregate against high temperatures
The influence of lightweight expanded clay aggregate (LECA) on the physico-mechanical properties and microstructure of geopolymer mortar containing slag binder alkali-activated with sodium silicate solution before and after exposure to thermal loads was investigated. In the current procedure, siliceous sand was partially substituted with LECA fine aggregate at levels of 0%, 25%, 50%, 75%, and 100%, by volume. The effect of LECA on the performance before exposure was evaluated by measuring flowability, water absorption, bulk density, thermal conductivity, and compressive strength. To monitor the behavior after exposure, a batch of specimens having the same composition was subjected to high temperatures in the range of 400–1000 °C for 2 h with a heating rate of 5 °C/min. In a similar fashion, mass loss and residual compressive strength were determined. New phase-based geopolymers were examined using Fourier transform infrared spectroscopy (FTIR) and scanning electron microscopy (SEM). The findings indicated that the incorporation of LECA up to 100% as an alternative to siliceous sand aggregate in geopolymer mortar has an adverse effect on compressive strength and water absorption, but has a positive effect on workability, thermal conductivity, and relative strength after exposure to elevated temperatures.
- 2 December 2021
- Published by Springer Nature in Environmental Science and Pollution Research
- Vol. 29 (18) , 26631-26647
An investigation on the performance of lightweight mortar-based geopolymer containing high-volume LECA aggregate against high temperatures
The influence of lightweight expanded clay aggregate (LECA) on the physico-mechanical properties and microstructure of geopolymer mortar containing slag binder alkali-activated with sodium silicate solution before and after exposure to thermal loads was investigated. In the current procedure, siliceous sand was partially substituted with LECA fine aggregate at levels of 0%, 25%, 50%, 75%, and 100%, by volume. The effect of LECA on the performance before exposure was evaluated by measuring flowability, water absorption, bulk density, thermal conductivity, and compressive strength. To monitor the behavior after exposure, a batch of specimens having the same composition was subjected to high temperatures in the range of 400–1000 °C for 2 h with a heating rate of 5 °C/min. In a similar fashion, mass loss and residual compressive strength were determined. New phase-based geopolymers were examined using Fourier transform infrared spectroscopy (FTIR) and scanning electron microscopy (SEM). The findings indicated that the incorporation of LECA up to 100% as an alternative to siliceous sand aggregate in geopolymer mortar has an adverse effect on compressive strength and water absorption, but has a positive effect on workability, thermal conductivity, and relative strength after exposure to elevated temperatures.
- 15 January 2021
- Published by Taylor & Francis in European Journal of Environmental and Civil Engineering
- Vol. 26 (10) , 4827-4846
Effect of high temperature on physical, mechanical and microstructure properties of alkali-activated slag pastes blended with ceramic waste material
This paper presents the influence of ceramic waste powder (CWP) inclusion on the physico-mechanical properties and microstructure analysis of alkali-activated pastes prior and after exposure to elevated temperatures. Such geopolymer specimens were designed upon replacing ground granulated blast-furnace slag (GGBFS) with CWP at ratios of 0%, 5%, 10%, 15% and 20%, by mass. The water absorption and compressive strength (wet and dry) of non-exposed samples were determined at curing ages of 1, 7, 14 and 28 days. After that, the specimens were exposed to high temperatures of 200, 400, 600 and 1000 °C with a heating rate of 5 °C/min. The characteristics of tested samples such as visual inspection, residual compressive strength and microstructure were evaluated. Techniques as Fourier Transform Infrared spectroscopy (FTIR), Thermogravimetric Analysis (TGA/DTG) and Scanning Electron Microscopy (SEM) were used for studying molecular and microstructure of geopolymer composite. Results indicated that the inclusion of CWP with slag in composite structure based geopolymer enhanced the physico-mechanical properties and microstructure of mixtures before and after thermal exposure. The specimens made of 15% CWP displayed superior thermal stability in terms of remaining compressive strength and microstructure than the reference ones.
- 15 January 2021
- Published by Taylor & Francis in European Journal of Environmental and Civil Engineering
- Vol. 26 (10) , 4827-4846
Effect of high temperature on physical, mechanical and microstructure properties of alkali-activated slag pastes blended with ceramic waste material
This paper presents the influence of ceramic waste powder (CWP) inclusion on the physico-mechanical properties and microstructure analysis of alkali-activated pastes prior and after exposure to elevated temperatures. Such geopolymer specimens were designed upon replacing ground granulated blast-furnace slag (GGBFS) with CWP at ratios of 0%, 5%, 10%, 15% and 20%, by mass. The water absorption and compressive strength (wet and dry) of non-exposed samples were determined at curing ages of 1, 7, 14 and 28 days. After that, the specimens were exposed to high temperatures of 200, 400, 600 and 1000 °C with a heating rate of 5 °C/min. The characteristics of tested samples such as visual inspection, residual compressive strength and microstructure were evaluated. Techniques as Fourier Transform Infrared spectroscopy (FTIR), Thermogravimetric Analysis (TGA/DTG) and Scanning Electron Microscopy (SEM) were used for studying molecular and microstructure of geopolymer composite. Results indicated that the inclusion of CWP with slag in composite structure based geopolymer enhanced the physico-mechanical properties and microstructure of mixtures before and after thermal exposure. The specimens made of 15% CWP displayed superior thermal stability in terms of remaining compressive strength and microstructure than the reference ones.
- 1 January 2020
- Published by Elsevier in Journal of Building Engineering
- Vol. 27
Development the properties of brick geopolymer pastes using concrete waste incorporating dolomite aggregate
- 1 January 2020
- Published by Elsevier in Journal of Building Engineering
- Vol. 27
Development the properties of brick geopolymer pastes using concrete waste incorporating dolomite aggregate
- 3 July 2019
- Published by Taylor & Francis in Transactions of the Indian Ceramic Society
- Vol. 78 (3) , 146-154
Effect of Concrete Waste on Compressive Strength and Microstructure Development of Ceramic Geopolymer Pastes
Ceramic industry generates a large amount of wastes, which pollutes and damages the environment. This paper presents the effects of concrete waste incorporating dolomite aggregate on ceramic-based geopolymer pastes in terms of microstructure and compressive strength. Recently, attention has been drawn to the use of geopolymer technology in the production of building units. Geopolymers were prepared from alkali activation of ceramic waste by 6%, 8%, 10% and 12% NaOH. To enhance the mechanical properties, alkali-activated ceramic geopolymer with 10% and 12% NaOH was partially substituted with concrete waste containing dolomite coarse aggregate at proportions of 5%, 10%, 15%, 20% and 30% by weight. Likewise, other geopolymer mixtures were manufactured by replacing ceramics with 5%, 10%, 15%, 20% and 30% calcined concrete waste at 850oC. Water/binder ratio as well as compressive strength of all mixtures was determined at 1, 7, 14 and 28 days. Phase composition and microstructure of geopolymer were identified using Fourier transform infrared spectroscopy and scanning electron microscopy techniques. Incorporation of 10% concrete waste and 20% calcined concrete waste enhanced the compressive strength and the microstructure of ceramic geopolymer pastes, while embedding extra amounts led to adverse effects.
- 3 July 2019
- Published by Taylor & Francis in Transactions of the Indian Ceramic Society
- Vol. 78 (3) , 146-154
Effect of Concrete Waste on Compressive Strength and Microstructure Development of Ceramic Geopolymer Pastes
Ceramic industry generates a large amount of wastes, which pollutes and damages the environment. This paper presents the effects of concrete waste incorporating dolomite aggregate on ceramic-based geopolymer pastes in terms of microstructure and compressive strength. Recently, attention has been drawn to the use of geopolymer technology in the production of building units. Geopolymers were prepared from alkali activation of ceramic waste by 6%, 8%, 10% and 12% NaOH. To enhance the mechanical properties, alkali-activated ceramic geopolymer with 10% and 12% NaOH was partially substituted with concrete waste containing dolomite coarse aggregate at proportions of 5%, 10%, 15%, 20% and 30% by weight. Likewise, other geopolymer mixtures were manufactured by replacing ceramics with 5%, 10%, 15%, 20% and 30% calcined concrete waste at 850oC. Water/binder ratio as well as compressive strength of all mixtures was determined at 1, 7, 14 and 28 days. Phase composition and microstructure of geopolymer were identified using Fourier transform infrared spectroscopy and scanning electron microscopy techniques. Incorporation of 10% concrete waste and 20% calcined concrete waste enhanced the compressive strength and the microstructure of ceramic geopolymer pastes, while embedding extra amounts led to adverse effects.
- 19 August 2018
- Published by Springer Nature in Journal of Thermal Analysis and Calorimetry
- Vol. 136 (2) , 609-620
Thermal resistance of alkali-activated metakaolin pastes containing nano-silica particles
- 19 August 2018
- Published by Springer Nature in Journal of Thermal Analysis and Calorimetry
- Vol. 136 (2) , 609-620
Thermal resistance of alkali-activated metakaolin pastes containing nano-silica particles
- 1 August 2018
- Published by American Society of Civil Engineers (ASCE) in Journal of Materials in Civil Engineering
- Vol. 30 (8)
Behavior of Alkali-Activated Metakaolin Pastes Blended with Quartz Powder Exposed to Seawater Attack
The purpose of this work is to investigate the resistance of alkali-activated metakaolin (AAMK) paste specimens blended with different amounts of quartz powder (QP) against different environmental conditions. Metakaolin (MK) was partially substituted with QP at levels of 10, 20, 30, and 40%, by weight. After initial curing, specimens were exposed to different conditions including air, potable fresh water, and seawater up to 12 months. Compressive strength before exposure as well as strength deterioration ratio (SDR) after exposure were determined. The mineralogical compositions for selected mixtures before and after exposure to seawater attack were identified by X-ray diffraction (XRD) and thermogravimetric analysis (TGA) and compared with those cured in lab air. The microstructure and morphology were identified using scanning electron microscopy (SEM). The results showed that the incorporation of QP in MK-based geopolymers seemed as promising candidates for marine structure applications.
- 1 August 2018
- Published by American Society of Civil Engineers (ASCE) in Journal of Materials in Civil Engineering
- Vol. 30 (8)
Behavior of Alkali-Activated Metakaolin Pastes Blended with Quartz Powder Exposed to Seawater Attack
The purpose of this work is to investigate the resistance of alkali-activated metakaolin (AAMK) paste specimens blended with different amounts of quartz powder (QP) against different environmental conditions. Metakaolin (MK) was partially substituted with QP at levels of 10, 20, 30, and 40%, by weight. After initial curing, specimens were exposed to different conditions including air, potable fresh water, and seawater up to 12 months. Compressive strength before exposure as well as strength deterioration ratio (SDR) after exposure were determined. The mineralogical compositions for selected mixtures before and after exposure to seawater attack were identified by X-ray diffraction (XRD) and thermogravimetric analysis (TGA) and compared with those cured in lab air. The microstructure and morphology were identified using scanning electron microscopy (SEM). The results showed that the incorporation of QP in MK-based geopolymers seemed as promising candidates for marine structure applications.