Zhiwei Pan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Zhiwei Pan has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- Menglai Jiang
CAS Key Laboratory of Mechanical Behavior and Design of Materials, Department of Modern Mechanics, University of Science and Technology of China 1 , Hefei 230026, China
2 shared publications - Shenghong Huang
CAS Key Laboratory of Mechanical Behavior and Design of Materials, Department of Modern Mechanics, University of Science and Technology of China, Hefei 230027, China
2 shared publications Damao Yao
1 shared publication- Hang Li1 shared publication
He Shengnan
1 shared publicationHuang Shenghong
1 shared publication
Latest Publications
- Open Access
- 11 June 2025
- Published by Elsevier in Nuclear Engineering and Technology
- Vol. 57 (11)
In-situ diagnosis of heat loads on divertor tungsten targets using laser speckle digital image correlation
- 11 June 2025
- Published by Elsevier in Nuclear Engineering and Technology
- Vol. 57 (11)
Open AccessIn-situ diagnosis of heat loads on divertor tungsten targets using laser speckle digital image correlation
- 6 January 2022
- Published by IOP Publishing in Nuclear Fusion
- Vol. 62 (2) , 026040
Lifetime measurement of a particular deep crack failure on a flat-type divertor mockup under cyclic high heat flux loading conditions
Plasma facing components are key to enduring high heat flux (HHF) loading from high-temperature plasma in nuclear fusion reactors. Understanding their thermal-mechanical behavior and cracking failure mechanisms related to structural designs and fabrication technologies during HHF loading is of great significance for improving their servicing performance and R&D (research and development) levels. In this study, a particular deep cracking failure process on the tungsten layer of a flat-type divertor mockup during 1800 cycles of 10 MW m−2 HHF loadings is completely monitored and measured with a special improved digital image correlation (DIC) technique. It is found that the DIC measurement under the HHF loading environment is improved successfully to capture fine deformation and strain fields with a spatial resolution less than 0.35 mm so that field strain on a 1 mm thick copper interlayer and deep crack initiation at several microns scale on the tungsten layer are measured out. Based on both full field and local strain and displacement measurements of the target divertor mockup, the thermal mechanical behaviors from deformation to crack initiation and propagation are successfully measured and traced. It is revealed that for the baseline copper interlayer design of a flat-type divertor mockup, the accumulation of plastic strain in the copper interlayer during ratcheting damage induces enough tensile stress on the tungsten layer during HHF cycles, leading to cracking and fracture failures even in its elastic state earlier than the copper LCF lifetime. Current Structural Design Criteria for ITER In-Vessel Components rules fail to cover this kind of ratcheting cracking failure mode in the design stage. New design models or mechanical validation rules to resolve this design blind spot should be established in the future.
- 6 January 2022
- Published by IOP Publishing in Nuclear Fusion
- Vol. 62 (2) , 026040
Lifetime measurement of a particular deep crack failure on a flat-type divertor mockup under cyclic high heat flux loading conditions
Plasma facing components are key to enduring high heat flux (HHF) loading from high-temperature plasma in nuclear fusion reactors. Understanding their thermal-mechanical behavior and cracking failure mechanisms related to structural designs and fabrication technologies during HHF loading is of great significance for improving their servicing performance and R&D (research and development) levels. In this study, a particular deep cracking failure process on the tungsten layer of a flat-type divertor mockup during 1800 cycles of 10 MW m−2 HHF loadings is completely monitored and measured with a special improved digital image correlation (DIC) technique. It is found that the DIC measurement under the HHF loading environment is improved successfully to capture fine deformation and strain fields with a spatial resolution less than 0.35 mm so that field strain on a 1 mm thick copper interlayer and deep crack initiation at several microns scale on the tungsten layer are measured out. Based on both full field and local strain and displacement measurements of the target divertor mockup, the thermal mechanical behaviors from deformation to crack initiation and propagation are successfully measured and traced. It is revealed that for the baseline copper interlayer design of a flat-type divertor mockup, the accumulation of plastic strain in the copper interlayer during ratcheting damage induces enough tensile stress on the tungsten layer during HHF cycles, leading to cracking and fracture failures even in its elastic state earlier than the copper LCF lifetime. Current Structural Design Criteria for ITER In-Vessel Components rules fail to cover this kind of ratcheting cracking failure mode in the design stage. New design models or mechanical validation rules to resolve this design blind spot should be established in the future.
- 1 August 2021
- Published by Elsevier in Fusion Engineering and Design
- Vol. 169
Manufacturing and high heat flux testing of flat-type W/Cu/CuCrZr mock-up by HIP assisted brazing process
- 1 August 2021
- Published by Elsevier in Fusion Engineering and Design
- Vol. 169
Manufacturing and high heat flux testing of flat-type W/Cu/CuCrZr mock-up by HIP assisted brazing process
- 12 March 2009
- Published by Springer Nature in Advances in Computational Mathematics
- Vol. 33 (1) , 97-112
Learning from non-identical sampling for classification
- 12 March 2009
- Published by Springer Nature in Advances in Computational Mathematics
- Vol. 33 (1) , 97-112
Learning from non-identical sampling for classification