Ahmed Elloumi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Ahmed Elloumi has a total of 36 co-authors. Here are the top co-authors by number of shared publications:
- Slim Souissi
Laboratory of Electromechanical Systems (LASEM), National Engineering School of Sfax, University of Sfax, Sfax, Tunisia
5 shared publications - Ahmed Koubaa
Université du Québec en Abitibi-Témiscamingue (UQAT)
3 shared publications A. Elleuchi
Laboratoire Des Systèmes Electro Mécaniques (LASEM) Unité Physique Et Mécaniques Des Matériaux(UPMM), Université De Sfax, Tunisie Sfax Tunisie North Africa
2 shared publicationsAfef Mansouri
Electromechanical Systems Laboratory LASEM, National Engineering School of Sfax, University of Sfax, Sfax, Tunisia
2 shared publicationsAli Gargouri
Eukaryotic Molecular Biotechnology Laboratory, Sfax Biotechnology Center, Sfax, Tunisia
2 shared publicationsCh. Bradai
Laboratoire Des Systèmes Electro Mécaniques (LASEM) Unité Physique Et Mécaniques Des Matériaux(UPMM), Université De Sfax, Tunisie Sfax Tunisie North Africa
2 shared publications
Latest Publications
- Open Access
Development and Characterization of Scented PLA-Based Biocomposites Reinforced with Spent Coffee Grounds and Lignin for FDM 3D Printing
This study investigates the development of biodegradable, scented bio-composite filaments incorporating industrial residues, specifically spent coffee grounds (SCG) and lignin (LI), into a PLA matrix for FDM 3D printing. Two fragrance additives, essential oil (EO) and microencapsulated fragrance powder (FP), were introduced (3%) to enhance sensory properties. The research investigates the effects of filler content (5%, 10%, and 15%) and fragrance additives on the surface chemistry (FTIR), thermal stability (TGA and DSC), mechanical properties (Tensile, flexural and impact), microstructure, and dimensional stability (Water absorption test and thickness swelling). Incorporating industrial residues and additives into PLA reduced the thermal stability, the degradation temperature and the glass transition temperature but increased the residual mass and the crystallinity. The effect of lignin was more pronounced than that of SCG, significantly influencing these thermal properties. Increasing the filler content of spent coffee grounds and lignin also led to a progressive decrease in tensile, flexural, and impact strength due to poor interfacial adhesion and increased void formation. However, lignin-based biocomposites exhibited enhanced stiffness at lower concentrations (≤10%), while biocomposites containing 15% SCG doubled their elongation at break compared to pure PLA. Adding fragrance reduced the mechanical strength but improved ductility due to plasticizer-like interactions. Microstructural analysis revealed heterogeneity in the biocomposites’ fracture surface characterized by the presence of pores, filler agglomeration, and delamination, indicating uneven filler dispersion and limited interfacial adhesion, particularly at high filler concentrations. The water absorption and dimensional stability of 3D-printed biocomposites increased progressively with the addition of residues. The presence of essential oil slightly improved water resistance by forming hydrogen bonds that limited moisture absorption. This article adds significant value by extending the potential applications of biocomposites beyond conventional engineering uses, making them particularly suitable for the fashion and design sectors, where multi-sensory and sustainable materials are increasingly sought after.
Open AccessDevelopment and Characterization of Scented PLA-Based Biocomposites Reinforced with Spent Coffee Grounds and Lignin for FDM 3D Printing
This study investigates the development of biodegradable, scented bio-composite filaments incorporating industrial residues, specifically spent coffee grounds (SCG) and lignin (LI), into a PLA matrix for FDM 3D printing. Two fragrance additives, essential oil (EO) and microencapsulated fragrance powder (FP), were introduced (3%) to enhance sensory properties. The research investigates the effects of filler content (5%, 10%, and 15%) and fragrance additives on the surface chemistry (FTIR), thermal stability (TGA and DSC), mechanical properties (Tensile, flexural and impact), microstructure, and dimensional stability (Water absorption test and thickness swelling). Incorporating industrial residues and additives into PLA reduced the thermal stability, the degradation temperature and the glass transition temperature but increased the residual mass and the crystallinity. The effect of lignin was more pronounced than that of SCG, significantly influencing these thermal properties. Increasing the filler content of spent coffee grounds and lignin also led to a progressive decrease in tensile, flexural, and impact strength due to poor interfacial adhesion and increased void formation. However, lignin-based biocomposites exhibited enhanced stiffness at lower concentrations (≤10%), while biocomposites containing 15% SCG doubled their elongation at break compared to pure PLA. Adding fragrance reduced the mechanical strength but improved ductility due to plasticizer-like interactions. Microstructural analysis revealed heterogeneity in the biocomposites’ fracture surface characterized by the presence of pores, filler agglomeration, and delamination, indicating uneven filler dispersion and limited interfacial adhesion, particularly at high filler concentrations. The water absorption and dimensional stability of 3D-printed biocomposites increased progressively with the addition of residues. The presence of essential oil slightly improved water resistance by forming hydrogen bonds that limited moisture absorption. This article adds significant value by extending the potential applications of biocomposites beyond conventional engineering uses, making them particularly suitable for the fashion and design sectors, where multi-sensory and sustainable materials are increasingly sought after.
- 25 July 2025
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 139 (7-8) , 3989-3998
Optimization of FDM 3D printing parameters of PLA and composite materials using definitive screening design
- 25 July 2025
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 139 (7-8) , 3989-3998
Optimization of FDM 3D printing parameters of PLA and composite materials using definitive screening design
- 20 May 2025
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 57 (6) , 1050-1071
Parametric optimization and modeling of the fused filament fabrication (FFF) manufacturing using recycled polyethylene terephthalate (PET) from water bottles
Most earlier studies on distributed recycling additive manufacturing (DRAM) have focused on using recycle-bots—waste plastic extruders—to produce raw materials for fused fluid fabrication (FFF). In the present study, an innovative recycling method designed explicitly for post-consumer water bottles was introduced and evaluated for its effectiveness in producing high-quality PET filament. The PET material was thoroughly characterized before and after filament production and following the 3D printing process. This approach successfully preserved the crystallinity of PET and prevented its thermal degradation. Key parameters, including infill density, printing speed, and layer thickness, were investigated using Taguchi’s method in conjunction with Grey Relational Analysis (GRA) to optimize the printing of recycled PET. This methodology aimed to maximize Young’s modulus and tensile strength while minimizing printing time and material usage. The results highlighted a trade-off between mechanical performance and printing efficiency. The best mechanical properties were achieved with a layer thickness of 0.1 mm and 100% infill density, yielding a tensile strength of 30 MPa and a Young’s modulus of 2311 MPa—values comparable to commercially available recycled PET and PLA filaments.
- 20 May 2025
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 57 (6) , 1050-1071
Parametric optimization and modeling of the fused filament fabrication (FFF) manufacturing using recycled polyethylene terephthalate (PET) from water bottles
Most earlier studies on distributed recycling additive manufacturing (DRAM) have focused on using recycle-bots—waste plastic extruders—to produce raw materials for fused fluid fabrication (FFF). In the present study, an innovative recycling method designed explicitly for post-consumer water bottles was introduced and evaluated for its effectiveness in producing high-quality PET filament. The PET material was thoroughly characterized before and after filament production and following the 3D printing process. This approach successfully preserved the crystallinity of PET and prevented its thermal degradation. Key parameters, including infill density, printing speed, and layer thickness, were investigated using Taguchi’s method in conjunction with Grey Relational Analysis (GRA) to optimize the printing of recycled PET. This methodology aimed to maximize Young’s modulus and tensile strength while minimizing printing time and material usage. The results highlighted a trade-off between mechanical performance and printing efficiency. The best mechanical properties were achieved with a layer thickness of 0.1 mm and 100% infill density, yielding a tensile strength of 30 MPa and a Young’s modulus of 2311 MPa—values comparable to commercially available recycled PET and PLA filaments.
- Open Access
- 24 June 2024
- Published by MDPI AG in Journal of Composites Science
- Vol. 8 (7) , 236
Characterization of Posidonia oceanica Fibers High-Density Polyethylene Composites: Reinforcing Potential and Effect of Coupling Agent
This study investigated the influence of fiber loading and maleated polyethylene (MAPE) coupling agent on the structural, thermal, mechanical, morphological properties, and torque rheology of high-density polyethylene (HDPE) reinforced with Posidonia oceanica fiber (POF) composites. HDPE/POF composites, both with and without MAPE, were manufactured using a two-step process: composite pellets extrusion, followed by test samples injection molding with various POF loadings (0, 20, 30, and 40 wt%). HDPE/POF composites reinforced with higher loading of POF (40 wt%) exhibit superior stiffness, better crystallinity, and higher stabilized torque and mechanical energy (Em) compared to other composite formulations. Therefore, varying the POF loading leads to extrusion and injection processing variations. Furthermore, the coupling agent significantly enhances the tensile strength, ductility, impact strength, crystallinity, stabilized torque, and Em of the HDPE/POF composite. This improvement is due to the enhanced interfacial adhesion between the POF and the HDPE matrix with the addition of the MAPE, as supported by the Scanning Electron Microscopy (SEM) micrographs.
- 24 June 2024
- Published by MDPI AG in Journal of Composites Science
- Vol. 8 (7) , 236
Open AccessCharacterization of Posidonia oceanica Fibers High-Density Polyethylene Composites: Reinforcing Potential and Effect of Coupling Agent
This study investigated the influence of fiber loading and maleated polyethylene (MAPE) coupling agent on the structural, thermal, mechanical, morphological properties, and torque rheology of high-density polyethylene (HDPE) reinforced with Posidonia oceanica fiber (POF) composites. HDPE/POF composites, both with and without MAPE, were manufactured using a two-step process: composite pellets extrusion, followed by test samples injection molding with various POF loadings (0, 20, 30, and 40 wt%). HDPE/POF composites reinforced with higher loading of POF (40 wt%) exhibit superior stiffness, better crystallinity, and higher stabilized torque and mechanical energy (Em) compared to other composite formulations. Therefore, varying the POF loading leads to extrusion and injection processing variations. Furthermore, the coupling agent significantly enhances the tensile strength, ductility, impact strength, crystallinity, stabilized torque, and Em of the HDPE/POF composite. This improvement is due to the enhanced interfacial adhesion between the POF and the HDPE matrix with the addition of the MAPE, as supported by the Scanning Electron Microscopy (SEM) micrographs.
- 31 May 2024
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 56 (5) , 675-692
A Comparative study of gray relational analysis and VlseKriterijumska Optimizacija I Kompromisno Resenje approaches for enhancing mechanical properties and productivity in 3D-Printed copper-filled PLA parts
Fused Filament Fabrication (FDM) has emerged as a prominent and innovative manufacturing technique, facilitating the creation of intricate, lightweight components at reduced time and cost. Despite its advantages, the productivity and mechanical performance of 3D-printed parts remain challenging areas. Hence, there is a growing interest in investigating the interplay between FDM build time and mechanical properties. Structural parameters such as layer thickness (Lt), raster angle (Ia), and air gap distance (Ifd) can exhibit conflicting effects on productivity and mechanical properties. This study employs GRA and VIKOR techniques for the multi-criteria selection of 3D printing, aiming to optimize both printing time and specific flexural properties of PLA/copper composite beams constructed in the edge direction. We compare the parameters selected by both methods and evaluate their impact on the responses. The behaviors of the two models differ: GRA optimizes two responses the specific stiffness ans specific strength, while VIKOR is more effective for minimising printing time. Both models select the lower raster angle of 0° as optimuim. Lt significantly influences printing time, being the primary parameter in the VIKOR method, whereas Ifd primarily contributes to mechanical properties.
- 31 May 2024
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 56 (5) , 675-692
A Comparative study of gray relational analysis and VlseKriterijumska Optimizacija I Kompromisno Resenje approaches for enhancing mechanical properties and productivity in 3D-Printed copper-filled PLA parts
Fused Filament Fabrication (FDM) has emerged as a prominent and innovative manufacturing technique, facilitating the creation of intricate, lightweight components at reduced time and cost. Despite its advantages, the productivity and mechanical performance of 3D-printed parts remain challenging areas. Hence, there is a growing interest in investigating the interplay between FDM build time and mechanical properties. Structural parameters such as layer thickness (Lt), raster angle (Ia), and air gap distance (Ifd) can exhibit conflicting effects on productivity and mechanical properties. This study employs GRA and VIKOR techniques for the multi-criteria selection of 3D printing, aiming to optimize both printing time and specific flexural properties of PLA/copper composite beams constructed in the edge direction. We compare the parameters selected by both methods and evaluate their impact on the responses. The behaviors of the two models differ: GRA optimizes two responses the specific stiffness ans specific strength, while VIKOR is more effective for minimising printing time. Both models select the lower raster angle of 0° as optimuim. Lt significantly influences printing time, being the primary parameter in the VIKOR method, whereas Ifd primarily contributes to mechanical properties.
- 12 July 2023
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 55 (6) , 917-936
Enzymatic treatments of pine wood flour for high-density polyethylene composites: Impact on thermomechanical, aging, and wear behavior
The use of pine wood in wood-plastic composite WPC promotes sustainability by incorporating recycled or renewable materials, reducing the reliance on traditional wood sources, and minimizing environmental impact. This study focuses on treating pine wood flour (WF) with biological treatments (xylanase, pectinase, laccase, steam explosion) for use in WPC. The Scanning Electron Microscopy (SEM), Fourier Transform Infared spectroscopy (FTIR), biochemical analysis, and Thermo Gravimetric Analysis (TGA) were used to evaluate the effectiveness of the treatments in terms of the morphological, compositional, surface, and thermal stability of WF. The wear behavior of WPC was exanimate before and after hydrothermal aging. Morphological analysis of WF revealed that the enzymatic treatment produced a clean surface; it removed Xylan and led to a higher cellulose content (70%), and more porosity, and improved thermal stability and adhesion between WF and high density polyethylene (HDPE). Through analysis of wear and aging, we found the best wear resistance for laccase treatment among all WPC before and after aging, and it was lower than the HDPE. These findings highlight the positive impact of the enzymatic treatment on the adhesion between WF and HDPE, leading to reduced water absorption and increased wear resistance.
- 12 July 2023
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 55 (6) , 917-936
Enzymatic treatments of pine wood flour for high-density polyethylene composites: Impact on thermomechanical, aging, and wear behavior
The use of pine wood in wood-plastic composite WPC promotes sustainability by incorporating recycled or renewable materials, reducing the reliance on traditional wood sources, and minimizing environmental impact. This study focuses on treating pine wood flour (WF) with biological treatments (xylanase, pectinase, laccase, steam explosion) for use in WPC. The Scanning Electron Microscopy (SEM), Fourier Transform Infared spectroscopy (FTIR), biochemical analysis, and Thermo Gravimetric Analysis (TGA) were used to evaluate the effectiveness of the treatments in terms of the morphological, compositional, surface, and thermal stability of WF. The wear behavior of WPC was exanimate before and after hydrothermal aging. Morphological analysis of WF revealed that the enzymatic treatment produced a clean surface; it removed Xylan and led to a higher cellulose content (70%), and more porosity, and improved thermal stability and adhesion between WF and high density polyethylene (HDPE). Through analysis of wear and aging, we found the best wear resistance for laccase treatment among all WPC before and after aging, and it was lower than the HDPE. These findings highlight the positive impact of the enzymatic treatment on the adhesion between WF and HDPE, leading to reduced water absorption and increased wear resistance.
- 15 March 2023
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 55 (4) , 597-612
Biocomposites Films Based on Polylactic Acid and Olive Wood-Flour: Investigation on Physical, Thermal and Mechanical Properties
Considerable interest has been shown in the development of biocomposite films for food packaging in recent years. In this study, biocomposite films based on polylactic acid (PLA) were prepared with varying levels of olive wood flour (OWF) (0, 1, 3, 5, and 10 wt%) using the solvent casting method. To achieve better dispersion, 2% ethanol was added during the casting of the biocomposite films. The effect of OWF content on the physicochemical and mechanical properties of the PLA films was investigated. Interaction between the OWF cellulose and the PLA matrix was revealed by FTIR spectroscopy analysis, and the addition of ethanol was found to be suitable for better dispersion of OWF, which resulted in decreased agglomeration rate in the biocomposites. The biocomposite films with the addition of 1% of OWF (OW1) exhibited the best dispersion, thermal stability, and tensile strength, with a gain of 31.07% (29.65 ± 6.6 MPa) and an increase in Young’s modulus of 15% (1199.18 ± 98 MPa). It was demonstrated that the properties of the PLA/OWF biocomposites make them suitable for green applications, including as film packaging for food products.
- 15 March 2023
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 55 (4) , 597-612
Biocomposites Films Based on Polylactic Acid and Olive Wood-Flour: Investigation on Physical, Thermal and Mechanical Properties
Considerable interest has been shown in the development of biocomposite films for food packaging in recent years. In this study, biocomposite films based on polylactic acid (PLA) were prepared with varying levels of olive wood flour (OWF) (0, 1, 3, 5, and 10 wt%) using the solvent casting method. To achieve better dispersion, 2% ethanol was added during the casting of the biocomposite films. The effect of OWF content on the physicochemical and mechanical properties of the PLA films was investigated. Interaction between the OWF cellulose and the PLA matrix was revealed by FTIR spectroscopy analysis, and the addition of ethanol was found to be suitable for better dispersion of OWF, which resulted in decreased agglomeration rate in the biocomposites. The biocomposite films with the addition of 1% of OWF (OW1) exhibited the best dispersion, thermal stability, and tensile strength, with a gain of 31.07% (29.65 ± 6.6 MPa) and an increase in Young’s modulus of 15% (1199.18 ± 98 MPa). It was demonstrated that the properties of the PLA/OWF biocomposites make them suitable for green applications, including as film packaging for food products.
- 28 February 2023
- Published by Springer Nature in Polymer Bulletin
- Vol. 81 (1) , 719-737
Active bio composites films based on PLA/olive wood flour (Olea europaea L.)/cinnamon essential oil
- 28 February 2023
- Published by Springer Nature in Polymer Bulletin
- Vol. 81 (1) , 719-737
Active bio composites films based on PLA/olive wood flour (Olea europaea L.)/cinnamon essential oil
- 8 December 2022
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 55 (2) , 184-200
Mechanical properties of 3D printed parts: Effect of ultraviolet PLA filaments ageing and water absorption
In additive manufacturing, fused deposition modelling (FDM) is one of the most often-used technologies. Polylactic Acid (PLA) is the most frequently applied polymer for prototyping or for real uses. This study mainly focuses on the mechanical properties of PLA parts printed with filament exposed to UV light to mimic the effect of recycled filament. Three radiation periods were studied, respectively, 24 h, 48 h and 72 h. Tensile tests were carried out to characterize the influence of building orientation (On flat/on-edge) and raster angles (0°, 45°, 90°, 0°/90°, −45°/+45°). Failure modes were also discussed. Printed specimens were subjected to water absorption to assess the mechanical properties in real application. Generally with the same raster angle, the interlayer structure of specimens manufactured in on-edge orientation has greater adhesion than the specimens in flat orientation. The results show that mechanical properties are lower in case of flat building orientation and the raster angle has the same trend in both orientations. Elsewhere, edge orientation exhibited lower water absorption thanks to the inwall that protected the printed part. UV radiation enhances the interface between printed layers for the lower period. The mechanical properties were affected by the degradation of the bulk material in the direction of 90°.
- 8 December 2022
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 55 (2) , 184-200
Mechanical properties of 3D printed parts: Effect of ultraviolet PLA filaments ageing and water absorption
In additive manufacturing, fused deposition modelling (FDM) is one of the most often-used technologies. Polylactic Acid (PLA) is the most frequently applied polymer for prototyping or for real uses. This study mainly focuses on the mechanical properties of PLA parts printed with filament exposed to UV light to mimic the effect of recycled filament. Three radiation periods were studied, respectively, 24 h, 48 h and 72 h. Tensile tests were carried out to characterize the influence of building orientation (On flat/on-edge) and raster angles (0°, 45°, 90°, 0°/90°, −45°/+45°). Failure modes were also discussed. Printed specimens were subjected to water absorption to assess the mechanical properties in real application. Generally with the same raster angle, the interlayer structure of specimens manufactured in on-edge orientation has greater adhesion than the specimens in flat orientation. The results show that mechanical properties are lower in case of flat building orientation and the raster angle has the same trend in both orientations. Elsewhere, edge orientation exhibited lower water absorption thanks to the inwall that protected the printed part. UV radiation enhances the interface between printed layers for the lower period. The mechanical properties were affected by the degradation of the bulk material in the direction of 90°.
- Open Access
- 24 May 2021
- Published by MDPI AG in Journal of Composites Science
- Vol. 5 (6) , 141
Dielectric Properties of Wood-Polymer Composites: Effects of Frequency, Fiber Nature, Proportion, and Chemical Composition
The characterization of the dielectric properties of wood–polymer composites (WPCs) is essential to understand their interaction with electromagnetic fields and evaluate their potential use for new applications. Thus, dielectric spectroscopy monitored the evolution of the dielectric properties of WPCs over a wide frequency range of 1 MHz to 1 GHz. WPCs were prepared using mixtures of different proportions (40%, 50%, and 60%) of wood and bark fibers from various species, high-density polyethylene, and maleated polyethylene (3%) by a two-step process, extrusion and compression molding. Results indicated that wood fibers modify the resistivity of polyethylene at low frequencies but have no effect at microwave frequencies. Increasing the fiber content increases the composites’ dielectric properties. The fibers’ cellulose content explains the variation in the dielectric properties of composites reinforced with fibers from different wood species. Indeed, composites with high cellulose content show higher dielectric constants.
- 24 May 2021
- Published by MDPI AG in Journal of Composites Science
- Vol. 5 (6) , 141
Open AccessDielectric Properties of Wood-Polymer Composites: Effects of Frequency, Fiber Nature, Proportion, and Chemical Composition
The characterization of the dielectric properties of wood–polymer composites (WPCs) is essential to understand their interaction with electromagnetic fields and evaluate their potential use for new applications. Thus, dielectric spectroscopy monitored the evolution of the dielectric properties of WPCs over a wide frequency range of 1 MHz to 1 GHz. WPCs were prepared using mixtures of different proportions (40%, 50%, and 60%) of wood and bark fibers from various species, high-density polyethylene, and maleated polyethylene (3%) by a two-step process, extrusion and compression molding. Results indicated that wood fibers modify the resistivity of polyethylene at low frequencies but have no effect at microwave frequencies. Increasing the fiber content increases the composites’ dielectric properties. The fibers’ cellulose content explains the variation in the dielectric properties of composites reinforced with fibers from different wood species. Indeed, composites with high cellulose content show higher dielectric constants.