EMEduard Monakhov

Eduard Monakhov

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Eduard Monakhov has a total of 70 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Defect evolution and nitrogen incorporation in ion-implanted β-Ga2O3

    by Alexander Azarov, Augustinas Galeckas, Alexey Mikhaylov, Alena Nikolskaya, David Tetelbaum, Dmitry Korolev, Eduard Monakhov, Andrej Kuznetsov

    Nitrogen plays an important role in the Ga2O3-based device fabrication since it demonstrates a deep acceptor behavior and it can be used as a compensation impurity. In the present work, we introduced N into the monoclinic β-Ga2O3 single crystals by ion implantation using different dose-rates. The thermal evolution of the structural and optical properties of the implanted samples was studied by combining Rutherford backscattering/channeling spectrometry and x-ray diffraction with photoluminescence spectroscopy. We demonstrate that crystal disorder in N-implanted β-Ga2O3 is a strong function of ion flux even for room temperature implantation. Unlike other implanted species, the defect annealing kinetics for N exhibit a distinct two-stage behavior, where the low-temperature stage (400 °C). These trends are discussed in the framework of the disorder stabilization induced by the incorporation of the implanted N atoms into the Ga2O3 lattice. The obtained results can be used to better understand the interaction between N and intrinsic defects as well as to push forward the development of β-Ga2O3-based electronic devices.


  • Open Access

    Doping dependence of boron–hydrogen dynamics in crystalline silicon

    by P. Vieira Rodrigues, B. Hammann, N. Aßmann, J. Schön, W. Kwapil, T. Niewelt, F. Schindler, E. V. Monakhov, M. C. Schubert

    In this contribution, we investigate the formation and dissociation of boron–hydrogen (BH) pairs in crystalline silicon under thermal equilibrium conditions. Our samples span doping concentrations of nearly two orders of magnitude and are passivated with a layer stack consisting of thin aluminum oxide and hydrogen-rich silicon nitride (Al2O3/SiNx:H). This layer stack acts as a hydrogen source during a following rapid thermal annealing. We characterize the samples using low-temperature Fourier-transform infrared spectroscopy and four-point-probe resistivity measurements. Our findings show that the proportion of hydrogen atoms initially bound to boron (BH pairs) rises with increasing boron concentration. Upon isothermal dark annealing at (163 ± 2) °C, hydrogen present in molecular form, H2, dissociates at a rate directly proportional to the concentration of boron atoms, ∝ [B−], leading to the formation of BH pairs. With prolonged annealing, an unknown hydrogen complex is formed at a rate that is inversely proportional to the square of the boron concentration, ∝ 1/[B−]2, resulting in the disappearance of BH pairs. Based on experimental observations, we derive a kinetic model in which we describe the formation of the unknown complex through neutral hydrogen H0 binding to a sink. Additionally, we investigate the temperature dependence of the reaction rates and find that the H2 dissociation process has an activation energy of (1.11 ± 0.05) eV, which is in close agreement with theoretical predictions.


  • Open Access

    Reducing Time and Costs of FT-IR Studies of the Effect of SiNx, Dopants, and Emitter on Hydrogen Species in Si Wafers and Solar Cell Structures

    by Nicole Aßmann, Rune Søndenå, Benjamin Hammann, Wolfram Kwapil, Eduard Monakhov

    Accurately measuring the hydrogen content in silicon (Si) solar cells is essential due to its connection to surface degradation and light and elevated temperature induced degradation (LeTID). Fourier Transform-Infrared (FT-IR) spectroscopy provides a quantitative technique for determining the content of various hydrogen species in Si wafers that have undergone various process steps. In this study, we examine both the effect of a silicon nitride (SiNx:H) layer during FT-IR spectroscopic measurements on hydrogen species, as well as the impact of an emitter present during firing on the amount of hydrogen introduced into Si wafers. We find that the presence of SiNx:H during measurements has negligible effects on the measured hydrogen species, potentially simplifying the preparation steps for FT-IR. For the emitter investigation we analyze boron (B)- and gallium (Ga)-doped p-type wafers to detect H-B, H-Ga, Oi-H2, and H2. We observe that hydrogen species initially present in B- and Ga-doped Si wafers differ significantly. Only H-Ga is detected in Ga-doped wafers, while H-B, Oi-H2, and H2 signals are measured in B-doped wafers. Moreover, we cannot confirm an increased release of H through the emitter into the bulk during the firing process. Finally, we conduct measurements at different temperatures and confirm that cryogenic temperatures are more effective for detecting H-B and H2 with concentrations in the 1014 cm-3 range. Nevertheless, useful spectra can still be obtained at liquid nitrogen (N2) temperatures.


  • Open Access

    Inverse dynamic defect annealing in ZnO

    by Alexander Azarov, Augustinas Galeckas, Elke Wendler, Eduard Monakhov, Andrej Kuznetsov

    Radiation tolerance of semiconductors depends on the dynamic defect annealing efficiency during irradiation. Consequently, it matters at what temperature one keeps the sample during irradiation, so that elevated temperatures typically result in lower remaining disorder. In the present work, we observed an opposite trend for the nitrogen ion implants into zinc oxide. Combining ion channeling technique, x-ray diffraction, and photoluminescence spectroscopy, we demonstrate that the interaction of nitrogen with radiation defects promotes an inverse dynamic annealing process, so that the increase in irradiation temperature leads to a more efficient defect formation. As a result, the residual radiation disorder is maximized at 650 °C and this state is characterized by the appearance of prominent optical signatures associated with zinc interstitials and strongly reduced strain accumulation as compared to the samples implanted at lower temperatures. However, for higher implantation temperatures, the impact of the inverse annealing decreases correlating with the surface degradation and loss of nitrogen.


  • Open Access

    Gamma-radiation hardness and long-term stability of ALD-Al2O3 surface passivated Si

    by Michael N. Getz, Marco Povoli, Ozhan Koybasi, Tomas Slavicek, Eduard Monakhov

    Al2O3 has emerged as the surface passivation material of choice for p-type silicon in photovoltaics and has also become a candidate for passivating Si-based radiation sensors. However, the surface passivation of Al2O3 has been shown to degrade when exposed to gamma-radiation, making it of interest to determine methods of depositing Al2O3 that minimize the radiation-induced degradation on the surface passivation. In this study, we investigate the long-term stability and gamma-radiation hardness of Al2O3 prepared using the TMA+H2O+O3 precursor combination and how the pretreatment, the deposition temperature, and the film thickness affect the density of interface states, Dit, and fixed oxide charge, Qfix, before and after gamma-irradiation. We find that the surface saturation current density, J0s, of silicon passivated by Al2O3 increases after annealing but stabilizes over time depending on the Al2O3 thickness. Samples with thicknesses of 60 nm stabilize over days. J0s stabilizes at lower values with increased Al2O3 thickness. After exposure to 1 Mrad gamma-radiation, the samples still exhibit low Dit and high Qfix, with the best performing sample having a Dit of 1.5 × 1010 eV−1 cm−2 and a Qfix of −3.1 × 1012 cm−2. The deposition temperature appears to indirectly affect radiation hardness, owing to its impact on the hydrogen concentration in the film and at the Si–SiOx–Al2O3 interface. Lifetime measurements after irradiation indicate that Al2O3 still passivates the surface effectively. The carrier lifetime and Qfix can largely be recovered by annealing samples in O2 at 435 °C.


  • Open Access

    The Impact of Different Hydrogen Configurations on Light- and Elevated-Temperature- Induced Degradation

    by Benjamin Hammann, Nicole Assmann, Philip M. Weiser, Wolfram Kwapil, Tim Niewelt, Florian Schindler, Rune Sondena, Eduard V. Monakhov, Martin C. Schubert

    In this article, the impact of different hydrogen configurations and their evolution on the extent and kinetics of light- and elevated-temperature-induced degradation (LeTID) is investigated in float-zone silicon via charge carrier lifetime measurements, low-temperature Fourier-transform infrared spectroscopy, and four-point-probe resistance measurements. Degradation conditions were light soaking at 77 °C and 1 sun-equivalent illumination intensity and dark anneal at 175 °C. The initial configuration of hydrogen is manipulated by varying the wafer thickness, the cooling ramp of the fast-firing process, and the dopant type (B- or P-doped). We find lower hydrogen concentrations in thinner samples and samples with a slower cooling ramp. This suggests that hydrogen diffuses out of the sample during the cool-down, which strongly affects the final concentration of hydrogen molecules H 2 , and to a smaller degree the concentration of boron-hydrogen (BH) pairs. A regeneration of potential LeTID defects and a presumed LeTID degradation during dark annealing is found in n-type Si. In p-type Si, the LeTID extent was found to scale with H 2 , suggesting a direct link between both. The temporal evolution of BH pairs, LeTID degradation/regeneration, and surface degradation depends on wafer thickness and the cooling ramp of the fast-firing process. Based upon these findings, we formulate a theory of the hydrogen-related mechanism behind LeTID: Hydrogen originating from H 2 moves between different temporary traps. First, hydrogen binds to LeTID precursors and acceptor atoms in the silicon bulk, later moving toward the surface. This leads first to the LeTID degradation and regeneration and then to the degradation of surface passivation.


  • Defects in semiconductors

    by L. Vines, E. Monakhov, A. Kuznetsov


  • Open Access

    Improving ALD-Al2O3 Surface Passivation of Si Utilizing Pre-Existing SiOx

    by Michael N. Getz, Marco Povoli, Eduard Monakhov

    Al 2 O 3 has rapidly become the surface passivation material of choice for p + layers of solar cells because of its high negative fixed charge, good long-term and thermal stability, and no parasitic absorption. In this article, the surface saturation current density, fixed charge, and interface state density are compared for Al 2 O 3 deposited on Si substrates where the pre-existing out-of-the-box SiO x layer was not removed, with substrates where the SiO x was removed by hydrofluoric acid. The depositions are performed by atomic layer deposition at temperatures in the 150–300 °C range, using trimethylaluminium, H 2 O, and O 3 as precursors. The samples where the native oxide was not removed achieve a higher level of surface passivation for every tested deposition temperature, with the sample deposited at 200 °C exhibiting a surface saturation current density of only 0.9 fA/cm 2 after annealing, a fixed charge of −4.2 × 10 12 cm −2 , and a density of interface states of 9.8 × 10 9 cm −2 eV −1 . Capacitance and conductance voltage characteristics reveal a strong correlation between the surface saturation current density and the density of interface states and fixed charges. It is also determined that the long-term stability of the surface passivation depends on the deposition temperature, with higher deposition temperatures resulting in improved long-term stability. The results indicate that H-terminated Si prior to Al 2 O 3 deposition may have a detrimental effect on the surface passivation.


  • Fine structure in electronic transitions attributed to nitrogen donor in silicon carbide

    by N. Assmann, C. Persson, A. Yu. Kuznetsov, E. V. Monakhov

    Nitrogen in group-IV semiconductors has become a well-established element of qubits capable of room-temperature operation. In silicon carbide, nitrogen can occupy different nonequivalent lattice sites, giving rise to different shallow donor states. We report a triplet fine structure in electronic transitions of nitrogen donors on the quasi-cubic carbon site in 4H silicon carbide with activation enthalpies of around 100 meV. The intensities of triplet components have a prominent dependence on the voltage bias. The activation enthalpies of the transitions exhibit the Poole–Frenkel effect, while no bias dependence is observed for the magnitude of splitting. A tentative explanation of the fine structure involves local symmetry changes due to stacking faults.