Joachim Seland Graff
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Joachim Seland Graff has a total of 37 co-authors. Here are the top co-authors by number of shared publications:
- Spyros Diplas
SINTEF Industry, 0373 Oslo, Norway
5 shared publications - Leonidas Gargalis
Conify, Panteli Nikolaidi 23A, Agios Ioannis Rentis, 182 33 Athens, Greece
4 shared publications - Leonidas Karavias
Conify, Panteli Nikolaidi 23A, Agios Ioannis Rentis, 182 33 Athens, Greece
4 shared publications - Elias P. Koumoulos
IRES—Innovation in Research & Engineering Solutions, Silversquare Europe, Square de Meeûs 35, 1000 Brussels, Belgium
3 shared publications - Evangelia K. Karaxi
Conify, Panteli Nikolaidi 23A, Agios Ioannis Rentis, 182 33 Athens, Greece
3 shared publications - Aggeliki Lekatou
Department of Materials Science and Engineering, University of Ioannina, 45110 Ioannina, Greece
1 shared publication
Latest Publications
- Open Access
- 20 August 2026
- Published by IOP Publishing in Journal of Physics: Materials
- Vol. 9 (3) , 035020
Tailoring Alnico magnets through micromagnetic simulations and machine learning
Alnico magnets have gained renewed interest in the search for rare-earth free permanent magnets due to their high thermal stability and magnetisation. However, the limited coercivity of these shape-anisotropy-based alloys constrains their performance. Their coercivity can be improved by tailoring their structure at the micro- and nano-levels and by identifying the elemental composition and crystal structure that would increase anisotropy. Alnico alloys are composed of millimetre-to-micrometer-sized grains of different sizes and orientations. Inside each grain, magnetic nanorods embedded in a non-magnetic matrix form as a result of thermo-magnetic treatment of the cast alloy. Starting from a reference Alnico sample, we realised a finite elements micromagnetic study of exchange-decoupled rods by varying their dimensions and interrod spacing across those observed experimentally. We computed the hysteresis properties by progressing from micromagnetic simulations of a small number of rods within the magnetostatic field of their neighbours to large systems treated statistically based on the distribution of orientations of the grains. We compared the coercivity of an isolated rod with that of the exchange-decoupled system to highlight the effect of magnetostatic interactions. We computed analytically the stray field acting on a single rod as a consequence of its surrounding rods in order to confirm the scaling of the coercivity with the packing fraction p . We explored how intrinsic material properties influence magnetic behaviour by examining materials with different magnetocrystalline anisotropy constants and saturation polarisation values. Results from several hundred simulations were used to train a multi-layer perceptron regressor and predict the magnetic properties as function of the dimensions of the rods, interrod spacing and orientation of the grains. With this approach, we highlight the underlying trends by which nanoscale structuring, intrinsic material properties and grain alignment can be tailored to improve the magnetic properties of Alnico alloys.
- 20 August 2026
- Published by IOP Publishing in Journal of Physics: Materials
- Vol. 9 (3) , 035020
Open AccessTailoring Alnico magnets through micromagnetic simulations and machine learning
Alnico magnets have gained renewed interest in the search for rare-earth free permanent magnets due to their high thermal stability and magnetisation. However, the limited coercivity of these shape-anisotropy-based alloys constrains their performance. Their coercivity can be improved by tailoring their structure at the micro- and nano-levels and by identifying the elemental composition and crystal structure that would increase anisotropy. Alnico alloys are composed of millimetre-to-micrometer-sized grains of different sizes and orientations. Inside each grain, magnetic nanorods embedded in a non-magnetic matrix form as a result of thermo-magnetic treatment of the cast alloy. Starting from a reference Alnico sample, we realised a finite elements micromagnetic study of exchange-decoupled rods by varying their dimensions and interrod spacing across those observed experimentally. We computed the hysteresis properties by progressing from micromagnetic simulations of a small number of rods within the magnetostatic field of their neighbours to large systems treated statistically based on the distribution of orientations of the grains. We compared the coercivity of an isolated rod with that of the exchange-decoupled system to highlight the effect of magnetostatic interactions. We computed analytically the stray field acting on a single rod as a consequence of its surrounding rods in order to confirm the scaling of the coercivity with the packing fraction p . We explored how intrinsic material properties influence magnetic behaviour by examining materials with different magnetocrystalline anisotropy constants and saturation polarisation values. Results from several hundred simulations were used to train a multi-layer perceptron regressor and predict the magnetic properties as function of the dimensions of the rods, interrod spacing and orientation of the grains. With this approach, we highlight the underlying trends by which nanoscale structuring, intrinsic material properties and grain alignment can be tailored to improve the magnetic properties of Alnico alloys.
- Open Access
Tensile Properties and Fracture Analysis of Duplex (2205) and Super Duplex (2507) Stainless Steels, Produced via Laser Powder Bed Fusion Additive Manufacturing
Additive manufacturing of duplex (DSS) and super duplex stainless steel (SDSS) has been successfully demonstrated using laser powder bed fusion (LPBF) in recent years. Owing to the high cooling rates, as-built LPBF-processed DSS and SDSS exhibit close to 100% ferritic microstructures and require heat treatment at 1000–1300 °C to obtain the desired duplex microstructure. In this work, the mechanical properties of DSS and SDSS processed via LPBF were investigated in three building directions (vertical, horizontal, diagonal) and three processing conditions (as-built, stress-relieved, annealed, and quenched) using uniaxial tensile testing. As-built samples exhibited tensile and yield strength greater than 1000 MPa accompanied by less than 20% elongation at break. In comparison, the water-quenched samples and samples annealed at 1100 °C exhibited elongation at break greater than 34% with yield and tensile strength values less than 950 MPa. Stress relief annealing at 300 °C had a negligible impact on the mechanical properties. Austenite formation upon high-temperature annealing restored the reduced ductility of the as-built samples. The as-built and stress-relieved SDSS showed the highest yield and tensile strength values in the horizontal build direction, reaching up to ≈1400 and ≈1500 MPa (for SDSS), respectively, as compared to the vertical and diagonal directions. Fractographic investigation after tensile testing revealed predominantly a quasi-ductile failure mechanism, showing fine size dimple formation and cleavage facets in the as-built state and a fully ductile fracture in the annealed and quenched conditions. The findings in this study demonstrate the mechanical anisotropy of DSS and SDSS along three different build orientations, 0°, 45°, 90°, and three post-processing conditions.
Open AccessTensile Properties and Fracture Analysis of Duplex (2205) and Super Duplex (2507) Stainless Steels, Produced via Laser Powder Bed Fusion Additive Manufacturing
Additive manufacturing of duplex (DSS) and super duplex stainless steel (SDSS) has been successfully demonstrated using laser powder bed fusion (LPBF) in recent years. Owing to the high cooling rates, as-built LPBF-processed DSS and SDSS exhibit close to 100% ferritic microstructures and require heat treatment at 1000–1300 °C to obtain the desired duplex microstructure. In this work, the mechanical properties of DSS and SDSS processed via LPBF were investigated in three building directions (vertical, horizontal, diagonal) and three processing conditions (as-built, stress-relieved, annealed, and quenched) using uniaxial tensile testing. As-built samples exhibited tensile and yield strength greater than 1000 MPa accompanied by less than 20% elongation at break. In comparison, the water-quenched samples and samples annealed at 1100 °C exhibited elongation at break greater than 34% with yield and tensile strength values less than 950 MPa. Stress relief annealing at 300 °C had a negligible impact on the mechanical properties. Austenite formation upon high-temperature annealing restored the reduced ductility of the as-built samples. The as-built and stress-relieved SDSS showed the highest yield and tensile strength values in the horizontal build direction, reaching up to ≈1400 and ≈1500 MPa (for SDSS), respectively, as compared to the vertical and diagonal directions. Fractographic investigation after tensile testing revealed predominantly a quasi-ductile failure mechanism, showing fine size dimple formation and cleavage facets in the as-built state and a fully ductile fracture in the annealed and quenched conditions. The findings in this study demonstrate the mechanical anisotropy of DSS and SDSS along three different build orientations, 0°, 45°, 90°, and three post-processing conditions.
- Open Access
High-Rate Epitaxial Growth of Silicon Using Electron Beam Evaporation at High Temperatures
This paper describes the high-rate (~1.5 μm/min) growth of Si films on Si supporting substrates with (100) crystallographic orientation at 600 °C, 800 °C, and 1000 °C in a vacuum environment of ~1 × 10−5 mbar using electron beam (e-beam) evaporation. The microstructure, crystallinity, and conductivity of such films were investigated. It was established that fully crystalline (Raman spectroscopy, EBSD) and stress-free epi-Si layers with a thickness of approximately 50 µm can be fabricated at 1000 °C, while at 600 °C and 800 °C, some poly-Si inclusions were observed using Raman spectroscopy. Hall effect measurements showed that epi-Si layers deposited at 1000 °C had resistivity, carrier concentration, and mobility comparable to those obtained for c-Si wafers fabricated through ingot growth and wafering using the same solar grade Si feedstock used for the e-beam depositions. The dislocation densities were determined to be ∼2 × 107 cm−2 and ∼5 × 106 cm−2 at 800 and 1000 °C, respectively, using Secco etch. The results highlight the potential of e-beam evaporation as a promising and cost-effective alternative to conventional CVD for the growth of epi-Si layers and, potentially, epi-Si wafers. Some of the remaining technical challenges of this deposition technology are briefly indicated and discussed.
Open AccessHigh-Rate Epitaxial Growth of Silicon Using Electron Beam Evaporation at High Temperatures
This paper describes the high-rate (~1.5 μm/min) growth of Si films on Si supporting substrates with (100) crystallographic orientation at 600 °C, 800 °C, and 1000 °C in a vacuum environment of ~1 × 10−5 mbar using electron beam (e-beam) evaporation. The microstructure, crystallinity, and conductivity of such films were investigated. It was established that fully crystalline (Raman spectroscopy, EBSD) and stress-free epi-Si layers with a thickness of approximately 50 µm can be fabricated at 1000 °C, while at 600 °C and 800 °C, some poly-Si inclusions were observed using Raman spectroscopy. Hall effect measurements showed that epi-Si layers deposited at 1000 °C had resistivity, carrier concentration, and mobility comparable to those obtained for c-Si wafers fabricated through ingot growth and wafering using the same solar grade Si feedstock used for the e-beam depositions. The dislocation densities were determined to be ∼2 × 107 cm−2 and ∼5 × 106 cm−2 at 800 and 1000 °C, respectively, using Secco etch. The results highlight the potential of e-beam evaporation as a promising and cost-effective alternative to conventional CVD for the growth of epi-Si layers and, potentially, epi-Si wafers. Some of the remaining technical challenges of this deposition technology are briefly indicated and discussed.
- Open Access
A Comparative Investigation of Duplex and Super Duplex Stainless Steels Processed through Laser Powder Bed Fusion
The aim of this paper was to compare duplex (DSS) and super duplex stainless steel processed by laser powder bed fusion (LPBF) based on the process parameters and microstructure–nanomechanical property relationships. Each alloy was investigated with respect to its feedstock powder characteristics. Optimum process parameters including scanning speed, laser power, beam diameter, laser energy density, and layer thickness were defined for each alloy, and near-fully dense parts (>99.9%) were produced. Microstructural analysis was performed via optical (OM), scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD). The samples were subjected to stress relief and high-temperature annealing. EBSD revealed the crystallographic orientation and quantified the phases in the as-built and annealed sample conditions. The as-built samples revealed a fully ferritic microstructure with a small amount of grain boundary austenite in the SDSS microstructure. High-temperature solution annealing resulted in the desired duplex microstructure for both alloys. There were no secondary phases present in the microstructure after both heat treatments. Nanoindentation generated nanomechanical (modulus) mapping grids and quantified the nanomechanical (both hardness and modulus) response; plasticity and stress relief were also assessed in all three conditions (as-built, stress-relieved, and annealed) in both DSS and SDSS. Austenite formation in the annealed condition contributed to lower hardness levels (~4.3–4.8 Gpa) and higher plastic deformation compared to the as-built (~5.7–6.3 Gpa) and stress-relieved conditions (~4.8–5.8 Gpa) for both alloys. SDSS featured a ~60% austenite volume fraction in its annealed and quenched microstructure, attributed to its higher nickel and nitrogen contents compared to DSS, which exhibited a ~30% austenite volume fraction.
Open AccessA Comparative Investigation of Duplex and Super Duplex Stainless Steels Processed through Laser Powder Bed Fusion
The aim of this paper was to compare duplex (DSS) and super duplex stainless steel processed by laser powder bed fusion (LPBF) based on the process parameters and microstructure–nanomechanical property relationships. Each alloy was investigated with respect to its feedstock powder characteristics. Optimum process parameters including scanning speed, laser power, beam diameter, laser energy density, and layer thickness were defined for each alloy, and near-fully dense parts (>99.9%) were produced. Microstructural analysis was performed via optical (OM), scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD). The samples were subjected to stress relief and high-temperature annealing. EBSD revealed the crystallographic orientation and quantified the phases in the as-built and annealed sample conditions. The as-built samples revealed a fully ferritic microstructure with a small amount of grain boundary austenite in the SDSS microstructure. High-temperature solution annealing resulted in the desired duplex microstructure for both alloys. There were no secondary phases present in the microstructure after both heat treatments. Nanoindentation generated nanomechanical (modulus) mapping grids and quantified the nanomechanical (both hardness and modulus) response; plasticity and stress relief were also assessed in all three conditions (as-built, stress-relieved, and annealed) in both DSS and SDSS. Austenite formation in the annealed condition contributed to lower hardness levels (~4.3–4.8 Gpa) and higher plastic deformation compared to the as-built (~5.7–6.3 Gpa) and stress-relieved conditions (~4.8–5.8 Gpa) for both alloys. SDSS featured a ~60% austenite volume fraction in its annealed and quenched microstructure, attributed to its higher nickel and nitrogen contents compared to DSS, which exhibited a ~30% austenite volume fraction.
- Open Access
Novel Powder Feedstock towards Microstructure Engineering in Laser Powder Bed Fusion: A Case Study on Duplex/Super Duplex and Austenitic Stainless-Steel Alloys
Additive manufacturing of Duplex Stainless Steels (DSS) and Super Duplex Stainless Steels (SDSS) has been successfully demonstrated using LPBF in recent years, however, both alloys feature an almost fully ferritic microstructure in the as-built condition due to the fast cooling rates associated with the Laser Powder Bed Fusion (LPBF) process. Blends of DSS and SDSS powders were formulated with austenitic stainless-steel 316L powder, aiming to achieve increased austenite formation during in the LPBF as-built condition to potentially minimize the post heat treatments (solution annealing and quenching). Powder characteristics were investigated and process parameters were optimized to produce near fully dense parts. Nanoindentation (NI) tests were conducted to measure, not only the local mechanical properties and correlate them with the as-built microstructure, but also to gain a deeper understanding in the deformation behavior of individual phases that cannot be studied directly by macroscopic tensile tests. Scanning Electron Microscopy (SEM) and Electron Backscatter Diffraction (EBSD) were employed for microstructural analysis and phase quantification. The microstructural analysis and EBSD phase maps revealed an increase in austenite in the as-built microstructures. Blend 1 resulted in a duplex microstructure consisting of 10% austenite at the XY plane and 20% austenite at the XZ plane. The austenite content increased with increasing proportion of 316L stainless steel in the powder blends. The DSS blend required a much higher volumetric energy density for the fabrication of near fully dense parts. This imposed a slower solidification and a higher melt pool homogeneity, allowing for adequate diffusion of the austenite stabilizing elements. The presented workflow and findings from this study provide valuable insights into powder mixing for the development of custom alloys for rapid material screening in LPBF.
Open AccessNovel Powder Feedstock towards Microstructure Engineering in Laser Powder Bed Fusion: A Case Study on Duplex/Super Duplex and Austenitic Stainless-Steel Alloys
Additive manufacturing of Duplex Stainless Steels (DSS) and Super Duplex Stainless Steels (SDSS) has been successfully demonstrated using LPBF in recent years, however, both alloys feature an almost fully ferritic microstructure in the as-built condition due to the fast cooling rates associated with the Laser Powder Bed Fusion (LPBF) process. Blends of DSS and SDSS powders were formulated with austenitic stainless-steel 316L powder, aiming to achieve increased austenite formation during in the LPBF as-built condition to potentially minimize the post heat treatments (solution annealing and quenching). Powder characteristics were investigated and process parameters were optimized to produce near fully dense parts. Nanoindentation (NI) tests were conducted to measure, not only the local mechanical properties and correlate them with the as-built microstructure, but also to gain a deeper understanding in the deformation behavior of individual phases that cannot be studied directly by macroscopic tensile tests. Scanning Electron Microscopy (SEM) and Electron Backscatter Diffraction (EBSD) were employed for microstructural analysis and phase quantification. The microstructural analysis and EBSD phase maps revealed an increase in austenite in the as-built microstructures. Blend 1 resulted in a duplex microstructure consisting of 10% austenite at the XY plane and 20% austenite at the XZ plane. The austenite content increased with increasing proportion of 316L stainless steel in the powder blends. The DSS blend required a much higher volumetric energy density for the fabrication of near fully dense parts. This imposed a slower solidification and a higher melt pool homogeneity, allowing for adequate diffusion of the austenite stabilizing elements. The presented workflow and findings from this study provide valuable insights into powder mixing for the development of custom alloys for rapid material screening in LPBF.
- Open Access
- 12 April 2022
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 131 (14) , 145703
Investigation of veryintenseD3-band emission in multi-crystalline silicon wafers using electron microscopy and hyperspectral photoluminescence imaging
Defects in high performance multi-crystalline silicon wafers can be detrimental to the lifetime of the solar cell. It is, therefore, important to study and understand the underlying structure and chemical elements present at these defective areas in order to suppress them. The underlying cause of the D-band emission line “ ” (VID3) has not yet been understood, although many theories have been proposed. In this paper, we have investigated the underlying causes of the d-band emission peak VID3 by hyperspectral photoluminescence imaging, scanning electron microscopy, electron backscatter diffraction, scanning transmission electron microscopy, and density functional theory (DFT) to understand the defect structure in areas of a VID3 emission peak in more detail. We found a high VID3 peak intensity at sub-grain and twin boundaries bordering to grains with a small misorientation, which suggests higher stress in these regions. Defects close to the twin boundary indicate a light element dopant in the area, such as oxygen. DFT calculations show that oxygen is prone to segregate to this boundary.- 12 April 2022
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 131 (14) , 145703
Open AccessInvestigation of veryintenseD3-band emission in multi-crystalline silicon wafers using electron microscopy and hyperspectral photoluminescence imaging
Defects in high performance multi-crystalline silicon wafers can be detrimental to the lifetime of the solar cell. It is, therefore, important to study and understand the underlying structure and chemical elements present at these defective areas in order to suppress them. The underlying cause of the D-band emission line “ ” (VID3) has not yet been understood, although many theories have been proposed. In this paper, we have investigated the underlying causes of the d-band emission peak VID3 by hyperspectral photoluminescence imaging, scanning electron microscopy, electron backscatter diffraction, scanning transmission electron microscopy, and density functional theory (DFT) to understand the defect structure in areas of a VID3 emission peak in more detail. We found a high VID3 peak intensity at sub-grain and twin boundaries bordering to grains with a small misorientation, which suggests higher stress in these regions. Defects close to the twin boundary indicate a light element dopant in the area, such as oxygen. DFT calculations show that oxygen is prone to segregate to this boundary. - Open Access
- 26 May 2021
- Published by Springer Nature in npj Materials Degradation
- Vol. 5 (1) , 1-15
Corrosion performance and degradation mechanism of a bi-metallic aluminum structure processed by wire-arc additive manufacturing
An Al-5Mg alloy (AA5083) block, deposited over an AA6061 substrate by wire-arc additive manufacturing, was electrochemically tested along two different cross-sectional planes by cyclic polarization in 3.5 wt.% NaCl. The deposited layers and the interlayer boundaries showed similar polarization behavior regardless of the cross-sectional direction. The corrosion of both the substrate and the deposited layers was mainly attributed to the presence of relatively coarse intermetallic Al(Fe, Mn)Si particles. In the substrate, corrosion was governed by deep crevices along the interfaces of directionally aligned Al(Fe, Mn)Si particles with the Al matrix. The deposited layers and the interlayer boundaries showed pitting around numerous Al(Fe, Mn)Si particles and/or Al(Fe, Mn, Cr, Ti)Si at the interlayer boundaries, which were much finer compared to those of the substrate. The abundance of the fine precipitates and their intergranular location caused surface material removal, which was more extensive along the interlayer boundaries. The perpendicularz-yandz-xplanes of the deposited block did not show significant differences in anodic polarization behavior. Differences were more distinct in the case of cathodic polarization. Some anisotropy in polarization behavior was noted through the thickness of thez-yplane that complies with the obtained tensile behavior.
- 26 May 2021
- Published by Springer Nature in npj Materials Degradation
- Vol. 5 (1) , 1-15
Open AccessCorrosion performance and degradation mechanism of a bi-metallic aluminum structure processed by wire-arc additive manufacturing
An Al-5Mg alloy (AA5083) block, deposited over an AA6061 substrate by wire-arc additive manufacturing, was electrochemically tested along two different cross-sectional planes by cyclic polarization in 3.5 wt.% NaCl. The deposited layers and the interlayer boundaries showed similar polarization behavior regardless of the cross-sectional direction. The corrosion of both the substrate and the deposited layers was mainly attributed to the presence of relatively coarse intermetallic Al(Fe, Mn)Si particles. In the substrate, corrosion was governed by deep crevices along the interfaces of directionally aligned Al(Fe, Mn)Si particles with the Al matrix. The deposited layers and the interlayer boundaries showed pitting around numerous Al(Fe, Mn)Si particles and/or Al(Fe, Mn, Cr, Ti)Si at the interlayer boundaries, which were much finer compared to those of the substrate. The abundance of the fine precipitates and their intergranular location caused surface material removal, which was more extensive along the interlayer boundaries. The perpendicularz-yandz-xplanes of the deposited block did not show significant differences in anodic polarization behavior. Differences were more distinct in the case of cathodic polarization. Some anisotropy in polarization behavior was noted through the thickness of thez-yplane that complies with the obtained tensile behavior.