St. Ulfawanti Intan Subadra
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
St. Ulfawanti Intan Subadra has a total of 38 co-authors. Here are the top co-authors by number of shared publications:
- Ahmad Taufiq
Department of Physics Universitas Negeri Malang Malang Indonesia
7 shared publications - Nurul Hidayat
Universitas Negeri Malang
3 shared publications Arif Hidayat
Department of Physics Universitas Negeri Malang Malang Indonesia
2 shared publicationsMunasir
2 shared publicationsSunaryono
2 shared publications- Wisnu Ari Adi
Research Center for Energy Materials, National Research and Innovation Agency, Kawasan Sains Teknologi Habibie, Serpong, Indonesia
2 shared publications
Latest Publications
- 17 October 2026
- Published by Wiley in Macromolecular Symposia
Structural, Optical, and Magnetic Properties of Mn x Fe 3‐x O 4 Ferrofluids Derived From Iron Sand for Energy Harvesting Application
In this research, we report the synthesis of iron sand‐based Mn x Fe 3‐x O 4 ferrofluids along with the characterization of their structural, optical, and magnetic properties, as well as their energy harvesting performance. The Mn x Fe 3‐x O 4 nanoparticles in the ferrofluids constructed an inverse spinel structure, with their diffraction peaks shifting to lower angles as the Mn 2+ content increased. FTIR spectra showed the Fe‐O and Mn‐O stretching detected at wavenumbers of 430–521 cm −1 and 411 cm −1 , respectively. The magnetic nanoparticles tended to agglomerate with particle sizes ranging from 24.0 nm to 39.6 nm. The bandgap energy increased as the Mn 2+ content increased. Furthermore, the energy harvesting performance was represented by voltage values in the range of 16.17–96.20 µV as a function of Mn 2+ content. Although the voltage was relatively low, the obtained results indicate promising potential for future energy harvesting applications.
- 17 October 2026
- Published by Wiley in Macromolecular Symposia
Structural, Optical, and Magnetic Properties of Mn x Fe 3‐x O 4 Ferrofluids Derived From Iron Sand for Energy Harvesting Application
In this research, we report the synthesis of iron sand‐based Mn x Fe 3‐x O 4 ferrofluids along with the characterization of their structural, optical, and magnetic properties, as well as their energy harvesting performance. The Mn x Fe 3‐x O 4 nanoparticles in the ferrofluids constructed an inverse spinel structure, with their diffraction peaks shifting to lower angles as the Mn 2+ content increased. FTIR spectra showed the Fe‐O and Mn‐O stretching detected at wavenumbers of 430–521 cm −1 and 411 cm −1 , respectively. The magnetic nanoparticles tended to agglomerate with particle sizes ranging from 24.0 nm to 39.6 nm. The bandgap energy increased as the Mn 2+ content increased. Furthermore, the energy harvesting performance was represented by voltage values in the range of 16.17–96.20 µV as a function of Mn 2+ content. Although the voltage was relatively low, the obtained results indicate promising potential for future energy harvesting applications.
- Open Access
- 4 March 2026
- Published by Ecletica Quimica in Ecletica Quimica
- Vol. 51
Synthesis of chitosan/AC/Fe3O4 nanocomposite and its structural, magnetic, and heavy metal adsorption characteristics
The chitosan/activated carbon (AC)/Fe3O4 nanocomposite has been successfully synthesized. The nanocomposite was then characterized to investigate its structural, magnetic, and heavy metal Cr(III) adsorption characteristics using XRD, SEM, FTIR, VSM, and ICP-OES. The chitosan/AC/Fe3O4 nanocomposite performed a single phase with a cubic inverse spinel structure with a lattice parameter and crystallite size of 8.38 ± 0.01 Å and 5.04 ± 0.09 nm, respectively. The SEM image showed that the morphology of chitosan/AC/Fe3O4 tended to be spherical with an average particle size of 51.4 ± 0.4 nm. The FTIR spectrum showed that the chitosan/AC/Fe3O4 nanocomposite exhibited the presence of a β-1,4-glycosidic bond at 858 cm–1 originating from chitosan. The C=C functional group and Fe-O bonds appeared at 1606 and 439–642 cm–1, indicating the presence of AC and Fe3O4. The chitosan/AC/Fe3O4 nanocomposite had superparamagnetic properties with a saturation magnetization value of 36.27 ± 0.05 emu/g. Furthermore, the chitosan/AC/Fe3O4 nanocomposite had a capacity and efficiency for Cr(III) adsorption of 13.95 mg/g and 27.88% at a contact time of 240 min, respectively.
- 4 March 2026
- Published by Ecletica Quimica in Ecletica Quimica
- Vol. 51
Open AccessSynthesis of chitosan/AC/Fe3O4 nanocomposite and its structural, magnetic, and heavy metal adsorption characteristics
The chitosan/activated carbon (AC)/Fe3O4 nanocomposite has been successfully synthesized. The nanocomposite was then characterized to investigate its structural, magnetic, and heavy metal Cr(III) adsorption characteristics using XRD, SEM, FTIR, VSM, and ICP-OES. The chitosan/AC/Fe3O4 nanocomposite performed a single phase with a cubic inverse spinel structure with a lattice parameter and crystallite size of 8.38 ± 0.01 Å and 5.04 ± 0.09 nm, respectively. The SEM image showed that the morphology of chitosan/AC/Fe3O4 tended to be spherical with an average particle size of 51.4 ± 0.4 nm. The FTIR spectrum showed that the chitosan/AC/Fe3O4 nanocomposite exhibited the presence of a β-1,4-glycosidic bond at 858 cm–1 originating from chitosan. The C=C functional group and Fe-O bonds appeared at 1606 and 439–642 cm–1, indicating the presence of AC and Fe3O4. The chitosan/AC/Fe3O4 nanocomposite had superparamagnetic properties with a saturation magnetization value of 36.27 ± 0.05 emu/g. Furthermore, the chitosan/AC/Fe3O4 nanocomposite had a capacity and efficiency for Cr(III) adsorption of 13.95 mg/g and 27.88% at a contact time of 240 min, respectively.
- 12 March 2024
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 317
A novel Fe3O4/ZnO/PANI/rGO nanohybrid material for radar wave absorbing
- 12 March 2024
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 317
A novel Fe3O4/ZnO/PANI/rGO nanohybrid material for radar wave absorbing
- 31 July 2023
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 950, 39-45
Ferrofluid Mn0.5Zn0.5Fe2O4 as Harvesting Energy: Preliminary Study
Currently humans are still very dependent on resources derived from fossil fuels. Even though fossil fuels are no longer sufficient to meet energy needs. For this reason, renewable energy technology is developed in the form of energy harvesting from mechanical energy in the form of ferrofluid vibrations. The ferrofluid used in this study is composed of filler Mn0.5Zn0.5Fe2O4 where Zn doping is used to increase magnetization, surfactant tetramethylammonium hydroxide (TMAH), and H2O as a liquid carrier. This study aims to study ferrofluid Mn0.5Zn0.5Fe2O4 as energy harvesting. Mn0.5Zn0.5Fe2O4 nanoparticles were synthesized using the coprecipitation method accompanied by nanostructure studies in the form of XRD, FTIR and VSM tests to determine the diffraction peaks, functional groups and magnetic properties of the sample. The diffraction peaks of Mn0.5Zn0.5Fe2O4 are at the peaks (2 2 0), (3 1 1), (2 2 2), (4 0 0), (4 2 2), (5 1 1), and (4 4 0). The FTIR spectrum of Mn0.5Zn0.5Fe2O4 nanoparticles is shown in the wavelength range of 4000-500 cm−1. The band vibration peaks of O-H stretching, CO2, O-H, Mn-O, Zn-O, and Fe-O particles Mn0.5Zn0.5Fe2O4 are respectively at 3392 cm−1, 2309 and 2376 cm−1, 1635 cm−1, 861 and 1636 cm−1, 686 cm−1 and 539 cm−1. The functional group of the metal-oxygen group (M–O) originates from magnetic particles as fillers to form ferrofluids. The competition of Mn and Zn ions at octahedral and tetrahedral sites in the spinel system tends to change the lattice parameters of the Mn0.5Zn0.5Fe2O4 ferrofluid. The magnetization curve of the Mn0.5Zn0.5Fe2O4 ferrofluid has superparamagnetic characteristics with a saturation magnetization value of 31,727 emu/g so it can be used as an energy harvester. Based on the IV electrical test, the Mn0.5Zn0.5Fe2O4 ferrofluid has the potential for energy harvesting with a voltage value of 1.67 µV and a current of 136.6 µA.
- 31 July 2023
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 950, 39-45
Ferrofluid Mn0.5Zn0.5Fe2O4 as Harvesting Energy: Preliminary Study
Currently humans are still very dependent on resources derived from fossil fuels. Even though fossil fuels are no longer sufficient to meet energy needs. For this reason, renewable energy technology is developed in the form of energy harvesting from mechanical energy in the form of ferrofluid vibrations. The ferrofluid used in this study is composed of filler Mn0.5Zn0.5Fe2O4 where Zn doping is used to increase magnetization, surfactant tetramethylammonium hydroxide (TMAH), and H2O as a liquid carrier. This study aims to study ferrofluid Mn0.5Zn0.5Fe2O4 as energy harvesting. Mn0.5Zn0.5Fe2O4 nanoparticles were synthesized using the coprecipitation method accompanied by nanostructure studies in the form of XRD, FTIR and VSM tests to determine the diffraction peaks, functional groups and magnetic properties of the sample. The diffraction peaks of Mn0.5Zn0.5Fe2O4 are at the peaks (2 2 0), (3 1 1), (2 2 2), (4 0 0), (4 2 2), (5 1 1), and (4 4 0). The FTIR spectrum of Mn0.5Zn0.5Fe2O4 nanoparticles is shown in the wavelength range of 4000-500 cm−1. The band vibration peaks of O-H stretching, CO2, O-H, Mn-O, Zn-O, and Fe-O particles Mn0.5Zn0.5Fe2O4 are respectively at 3392 cm−1, 2309 and 2376 cm−1, 1635 cm−1, 861 and 1636 cm−1, 686 cm−1 and 539 cm−1. The functional group of the metal-oxygen group (M–O) originates from magnetic particles as fillers to form ferrofluids. The competition of Mn and Zn ions at octahedral and tetrahedral sites in the spinel system tends to change the lattice parameters of the Mn0.5Zn0.5Fe2O4 ferrofluid. The magnetization curve of the Mn0.5Zn0.5Fe2O4 ferrofluid has superparamagnetic characteristics with a saturation magnetization value of 31,727 emu/g so it can be used as an energy harvester. Based on the IV electrical test, the Mn0.5Zn0.5Fe2O4 ferrofluid has the potential for energy harvesting with a voltage value of 1.67 µV and a current of 136.6 µA.
- Open Access
- 30 December 2021
- Published by Indonesian Magnetics Society in Journal of Magnetism and Its Applications
- Vol. 1 (2) , 40-45
Effect of ZnO Mass on Nanostructure, Magnetic and Optical Properties of Fe2O3/MWCNT/ZnO Nanocomposites
Fe2O3/MWCNT/ZnO nanocomposites were successfully synthesized through the precipitation method. The synthesis was carried out through a variation of ZnO mass, with (Fe2O3/MWCNT):ZnO mass ratio of 1:0, 1:0.5, 1:1, 1:1.5, and 0:1. The XRD analysis results suggested that the nanocomposites were composed of two phases, namely Fe2O3 with centered hexagonal structure and ZnO with hexagonal wurtzite structure. The ZnO diffraction peak tended to increase following the increasing ZnO composition within the nanocomposites. The presence of MWCNT was confirmed by the FTIR results signifying the detection of C=C vibration at wavenumbers of 1631–1640 cm-1. The crystallite size of Fe2O3 and ZnO was in the range of 30.97–31.12 nm and 30.46–35.64 nm, respectively. The nanocomposites were comprised of the spherical, tube, and sheet particles, representing Fe2O3, MWCNT, and ZnO, respectively, with particle size ranged from 33.97 nm to 55.19 nm. The nanocomposites were observed to present weak ferromagnetic, with a decrease in saturation magnetization value following the increase of ZnO composition. The optical properties of the nanocomposites tended to decrease as the increasing ZnO composition.
- 30 December 2021
- Published by Indonesian Magnetics Society in Journal of Magnetism and Its Applications
- Vol. 1 (2) , 40-45
Open AccessEffect of ZnO Mass on Nanostructure, Magnetic and Optical Properties of Fe2O3/MWCNT/ZnO Nanocomposites
Fe2O3/MWCNT/ZnO nanocomposites were successfully synthesized through the precipitation method. The synthesis was carried out through a variation of ZnO mass, with (Fe2O3/MWCNT):ZnO mass ratio of 1:0, 1:0.5, 1:1, 1:1.5, and 0:1. The XRD analysis results suggested that the nanocomposites were composed of two phases, namely Fe2O3 with centered hexagonal structure and ZnO with hexagonal wurtzite structure. The ZnO diffraction peak tended to increase following the increasing ZnO composition within the nanocomposites. The presence of MWCNT was confirmed by the FTIR results signifying the detection of C=C vibration at wavenumbers of 1631–1640 cm-1. The crystallite size of Fe2O3 and ZnO was in the range of 30.97–31.12 nm and 30.46–35.64 nm, respectively. The nanocomposites were comprised of the spherical, tube, and sheet particles, representing Fe2O3, MWCNT, and ZnO, respectively, with particle size ranged from 33.97 nm to 55.19 nm. The nanocomposites were observed to present weak ferromagnetic, with a decrease in saturation magnetization value following the increase of ZnO composition. The optical properties of the nanocomposites tended to decrease as the increasing ZnO composition.
- 22 April 2020
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2232 (1) , 020007
Preparation of Fe3O4/MWCNT nanocomposite combined with titanium dioxide using sonochemical and precipitation methods
Regarding the physical and chemical performances, Fe3O4 and multi-wall carbon nanotubes (MWCNT) combined with other metal oxide such as titanium dioxide open new opportunity to be widely used for energy application such as supercapacitor. In this paper, we report the preparation of Fe3O4/MWCNT nanocomposite combined with titanium dioxide using sonochemical-precipitation method. The nanocomposite was characterized using X-ray diffractometer, Fourier transform infrared spectroscopy, scanning electron microscopy, and UV-Vis spectrometer. The results of diffraction data analysis showed the presence of crystalline phase in nanocomposite derived from Fe3O4 and titanium dioxide with cubic inverse spinel and anatase structures, respectively. The existence of MWCNT was then confirmed by functional groups data which indicated the vibration of C=C functional group at the wavenumber of 1400-1600 cm−1, while the vibration of Fe-O was detected at the wavenumber of 409 cm-1 and 667 cm−1 overlapped with Ti-O functional group. MWCNT was considered to be crosslinked the surface of Fe3O4 or titanium dioxide nanoparticles. The bandgap energy of the nanocomposite was 2.17 eV for Fe3O4/MWCNT, and 3.27 eV for Fe3O4/MWCNT. Furthermore, the magnetization value of the sample was 50 emu/g exhibited as a superparamagnetic character.
- 22 April 2020
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2232 (1) , 020007
Preparation of Fe3O4/MWCNT nanocomposite combined with titanium dioxide using sonochemical and precipitation methods
Regarding the physical and chemical performances, Fe3O4 and multi-wall carbon nanotubes (MWCNT) combined with other metal oxide such as titanium dioxide open new opportunity to be widely used for energy application such as supercapacitor. In this paper, we report the preparation of Fe3O4/MWCNT nanocomposite combined with titanium dioxide using sonochemical-precipitation method. The nanocomposite was characterized using X-ray diffractometer, Fourier transform infrared spectroscopy, scanning electron microscopy, and UV-Vis spectrometer. The results of diffraction data analysis showed the presence of crystalline phase in nanocomposite derived from Fe3O4 and titanium dioxide with cubic inverse spinel and anatase structures, respectively. The existence of MWCNT was then confirmed by functional groups data which indicated the vibration of C=C functional group at the wavenumber of 1400-1600 cm−1, while the vibration of Fe-O was detected at the wavenumber of 409 cm-1 and 667 cm−1 overlapped with Ti-O functional group. MWCNT was considered to be crosslinked the surface of Fe3O4 or titanium dioxide nanoparticles. The bandgap energy of the nanocomposite was 2.17 eV for Fe3O4/MWCNT, and 3.27 eV for Fe3O4/MWCNT. Furthermore, the magnetization value of the sample was 50 emu/g exhibited as a superparamagnetic character.
- Open Access
- 1 February 2020
- Published by International Digital Organization for Scientific Information (IDOSI) in International Journal of Engineering
- Vol. 33 (2) , 304-313
Radar Absorption Performance of Fe3O4/AC/PANI Nanocomposites Prepared from Natural Iron Sand
In this work, the Fe3O4 nanoparticles from natural iron sand were combined with active carbon (AC) and polyaniline (PANI) to obtain Fe3O4/AC/PANI nanocomposites with mass variations of the AC of 0.1, 0.2, 0.3, 0.4, and 0.5 g. The crystalline phase of Fe3O4/AC/PANI nanocomposites formed from Fe3O4 with PANI having an amorphous phase. Meanwhile, the crystalline phase of AC was unmatched because of its very small composition. The presence of AC was observed through vibrations from the C-C and COOH functional groups. The existence of PANI was indicated by the vibrations of the benzoic ring and quinonoid bonds. Besides, the presence of Fe3O4 was confirmed by the presence of Fe-O functional groups from octahedral and tetrahedral positions. The optical properties of Fe3O4/AC/PANI nanocomposites were shown by increasing the energy gap along with decreasing absorption wavelength. Interestingly, increasing AC composition made the absorption bandwidth of the Fe3O4/AC/PANI nanocomposites wider, so that the radar absorption also increased marking by the greater reflection loss that reached -15.8 dB. The increase in the radar absorption performance of Fe3O4/AC/PANI nanocomposites came from the efficient complementarity between dielectric loss and magnetic loss and interfacial polarization between Fe3O4-AC or between Fe3O4-PANI.
- 1 February 2020
- Published by International Digital Organization for Scientific Information (IDOSI) in International Journal of Engineering
- Vol. 33 (2) , 304-313
Open AccessRadar Absorption Performance of Fe3O4/AC/PANI Nanocomposites Prepared from Natural Iron Sand
In this work, the Fe3O4 nanoparticles from natural iron sand were combined with active carbon (AC) and polyaniline (PANI) to obtain Fe3O4/AC/PANI nanocomposites with mass variations of the AC of 0.1, 0.2, 0.3, 0.4, and 0.5 g. The crystalline phase of Fe3O4/AC/PANI nanocomposites formed from Fe3O4 with PANI having an amorphous phase. Meanwhile, the crystalline phase of AC was unmatched because of its very small composition. The presence of AC was observed through vibrations from the C-C and COOH functional groups. The existence of PANI was indicated by the vibrations of the benzoic ring and quinonoid bonds. Besides, the presence of Fe3O4 was confirmed by the presence of Fe-O functional groups from octahedral and tetrahedral positions. The optical properties of Fe3O4/AC/PANI nanocomposites were shown by increasing the energy gap along with decreasing absorption wavelength. Interestingly, increasing AC composition made the absorption bandwidth of the Fe3O4/AC/PANI nanocomposites wider, so that the radar absorption also increased marking by the greater reflection loss that reached -15.8 dB. The increase in the radar absorption performance of Fe3O4/AC/PANI nanocomposites came from the efficient complementarity between dielectric loss and magnetic loss and interfacial polarization between Fe3O4-AC or between Fe3O4-PANI.
- Open Access
- 1 May 2019
- Published by IOP Publishing in IOP Conference Series: Earth and Environmental Science
- Vol. 276 (1) , 012041
Preparation and Characterization of Magnetite Nanoparticles Combined with Polyaniline and Activated Carbon
In this paper, we report the preparation of magnetite nanoparticles combined with polyaniline and activated carbon. The results of the X-Ray diffraction data analysis showed that the samples had a magnetite crystal phase without other phases. The existence of polyaniline and activated carbon was confirmed using Fourier transform infrared spectroscopy characterization shown by the presence of S=O, C-N, and C-C. The sample of synthesis results in this work had the band gap of 3.23 eV. Moreover, the results of data analysis using vector network analyzer revealed the maximum reflection loss value of -14 with the absorbance of 50%. Thereby, the synthesis optimization needs to be done to increase the sample absorbance to the radar wave.
- 1 May 2019
- Published by IOP Publishing in IOP Conference Series: Earth and Environmental Science
- Vol. 276 (1) , 012041
Open AccessPreparation and Characterization of Magnetite Nanoparticles Combined with Polyaniline and Activated Carbon
In this paper, we report the preparation of magnetite nanoparticles combined with polyaniline and activated carbon. The results of the X-Ray diffraction data analysis showed that the samples had a magnetite crystal phase without other phases. The existence of polyaniline and activated carbon was confirmed using Fourier transform infrared spectroscopy characterization shown by the presence of S=O, C-N, and C-C. The sample of synthesis results in this work had the band gap of 3.23 eV. Moreover, the results of data analysis using vector network analyzer revealed the maximum reflection loss value of -14 with the absorbance of 50%. Thereby, the synthesis optimization needs to be done to increase the sample absorbance to the radar wave.