D. A. Rozhentsev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
D. A. Rozhentsev has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
N. K. Tkachev
Institute of High Temperature Electrochemistry, Ural Branch of the RAS
2 shared publicationsN. I. Shurov
Institute of High-Temperature Electrochemistry, Ural Branch of RAS, Russian Federation
1 shared publicationN. K Tkachev
Institute of High-Temperature Electrochemistry, Ural Branch of the Russian Academy of Sciences
1 shared publicationN.I. Shurov
1 shared publicationN.K. Tkachev
1 shared publication- Nickolai K. Tkachev
Institute of Metallurgy, Ural Branch of the Russian Academy of Sciences, Ekaterinburg, Russia
1 shared publication
Latest Publications
- 1 November 2023
- Published by The Russian Academy of Sciences in Расплавы
- No. 6,p. 570-576
FORMATION OF NANO-POROUS IRON BY ELECTROCHEMICAL DEALLOYING OF FERROTITANIUM IN MELTED EUTECTIC LiCl–KCl
Porous iron is considered one of the most promising biodegradable or resorbable materials in traumatology. To date, only a few works on the preparation of nanoporous iron by dealloying or selective dissolution of ferroalloys are known. Among the promising candidates for precursor alloys, ferrotitanium is of great interest. The difference of iron and titanium release potentials in chloride melts can be about 700 mV. However, two intermetallides are present in the phase diagram: Fe2Ti and FeTi with melting temperatures of 1427 and 1317°C, respectively. A sample of the composition Fe0.6Ti0.4 was melted with the congruent Fe2Ti compound as its base. Dealloying was carried out in the molten chloride eutectic LiCl–KCl at two temperatures of 400 and 600°C in the potentiostatic mode at the following potentials relative to the platinum quasi-electrode –0.23 and +0.1 V, respectively. The potentials were chosen to provide sufficiently large currents at the beginning of the electrode process, but to avoid mechanical cracking of the sample. Bi-continuous iron nanostructure with characteristic pore sizes of the order of 100 nm at dealloying slightly below its recrystallization start temperature (400°C) was obtained. The residual titanium content found by EDS spectroscopy did not exceed 5 at % by surface. At increasing, the process temperature up to 600°C the expected enlargement of pores and ligaments was observed, and extended areas of larger voids appeared – of the order of several microns, arising, apparently, due to more intensive destruction of micro-inclusions of the FeTi phase in the precursor alloy. The XRD of the samples after dealloying unequivocally testifies to the formation of the cermet iron phase on the surface of the samples. The weak XRD reflections of impurities of the defective wustite phase (FeO) are noted, as there is a partial oxidation of the active nanoporous iron surface already after the sample removal and washing in the air at room temperature. The conclusion is made that it is fundamentally possible to obtain nanoporous iron with a bicontinuous pore structure and ligaments (≈100 nm) from ferrotitanium in molten chloride eutectics by electrochemical dealloying at temperatures slightly below the beginning of iron recrystallization (400°C).
- 1 November 2023
- Published by The Russian Academy of Sciences in Расплавы
- No. 6,p. 570-576
FORMATION OF NANO-POROUS IRON BY ELECTROCHEMICAL DEALLOYING OF FERROTITANIUM IN MELTED EUTECTIC LiCl–KCl
Porous iron is considered one of the most promising biodegradable or resorbable materials in traumatology. To date, only a few works on the preparation of nanoporous iron by dealloying or selective dissolution of ferroalloys are known. Among the promising candidates for precursor alloys, ferrotitanium is of great interest. The difference of iron and titanium release potentials in chloride melts can be about 700 mV. However, two intermetallides are present in the phase diagram: Fe2Ti and FeTi with melting temperatures of 1427 and 1317°C, respectively. A sample of the composition Fe0.6Ti0.4 was melted with the congruent Fe2Ti compound as its base. Dealloying was carried out in the molten chloride eutectic LiCl–KCl at two temperatures of 400 and 600°C in the potentiostatic mode at the following potentials relative to the platinum quasi-electrode –0.23 and +0.1 V, respectively. The potentials were chosen to provide sufficiently large currents at the beginning of the electrode process, but to avoid mechanical cracking of the sample. Bi-continuous iron nanostructure with characteristic pore sizes of the order of 100 nm at dealloying slightly below its recrystallization start temperature (400°C) was obtained. The residual titanium content found by EDS spectroscopy did not exceed 5 at % by surface. At increasing, the process temperature up to 600°C the expected enlargement of pores and ligaments was observed, and extended areas of larger voids appeared – of the order of several microns, arising, apparently, due to more intensive destruction of micro-inclusions of the FeTi phase in the precursor alloy. The XRD of the samples after dealloying unequivocally testifies to the formation of the cermet iron phase on the surface of the samples. The weak XRD reflections of impurities of the defective wustite phase (FeO) are noted, as there is a partial oxidation of the active nanoporous iron surface already after the sample removal and washing in the air at room temperature. The conclusion is made that it is fundamentally possible to obtain nanoporous iron with a bicontinuous pore structure and ligaments (≈100 nm) from ferrotitanium in molten chloride eutectics by electrochemical dealloying at temperatures slightly below the beginning of iron recrystallization (400°C).
- 15 April 2023
- Published by The Russian Academy of Sciences in Žurnal obŝej himii
- Vol. 93 (4) , 628-634
Peculiarities of oxidation of nanoporous iron produced by ferromanganese dealloying in molten salt
A wuestite phase metastable at room temperature in the form of a whisker conglomerate was found on the surface of nanoporous iron obtained by electrochemical dealloying (selective anodic dissolution of a less noble metal) of ferromanganese. The features of the further oxidation of iron by TG-DSC and Х-ray phase analysis with a temperature sweep were studied. A wide range of coexistence of three forms of iron oxides and relative stability of the magnetite phase up to 900°C were described.
- 15 April 2023
- Published by The Russian Academy of Sciences in Žurnal obŝej himii
- Vol. 93 (4) , 628-634
Peculiarities of oxidation of nanoporous iron produced by ferromanganese dealloying in molten salt
A wuestite phase metastable at room temperature in the form of a whisker conglomerate was found on the surface of nanoporous iron obtained by electrochemical dealloying (selective anodic dissolution of a less noble metal) of ferromanganese. The features of the further oxidation of iron by TG-DSC and Х-ray phase analysis with a temperature sweep were studied. A wide range of coexistence of three forms of iron oxides and relative stability of the magnetite phase up to 900°C were described.
- 1 April 2023
- Published by Pleiades Publishing Ltd in Russian Journal of General Chemistry
- Vol. 93 (4) , 886-891
Features of Oxidation of Nanoporous Iron Obtained by Ferromanganese Dealloying in Molten Salts
A wustite phase in the form of a whisker conglomerate, which is metastable at room temperature, was found on the surface of nanoporous iron obtained by electrochemical dealloying (selective anodic dissolution of a less noble metal) of ferromanganese. Features of the further iron oxidation were studied by TG-DSC and Х-ray phase analysis with a temperature sweep. A wide range of coexistence of three forms of iron oxides and relative stability of the magnetite phase up to 900°C have been described.
- 1 April 2023
- Published by Pleiades Publishing Ltd in Russian Journal of General Chemistry
- Vol. 93 (4) , 886-891
Features of Oxidation of Nanoporous Iron Obtained by Ferromanganese Dealloying in Molten Salts
A wustite phase in the form of a whisker conglomerate, which is metastable at room temperature, was found on the surface of nanoporous iron obtained by electrochemical dealloying (selective anodic dissolution of a less noble metal) of ferromanganese. Features of the further iron oxidation were studied by TG-DSC and Х-ray phase analysis with a temperature sweep. A wide range of coexistence of three forms of iron oxides and relative stability of the magnetite phase up to 900°C have been described.
- 3 January 2023
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 48 (59) , 22513-22521
Potentiostatic dealloying of PdIn in molten LiCl–KCl eutectic
- 3 January 2023
- Published by Elsevier in International Journal of Hydrogen Energy
- Vol. 48 (59) , 22513-22521
Potentiostatic dealloying of PdIn in molten LiCl–KCl eutectic
- 29 October 2021
- Published by Royal Society of Chemistry (RSC) in Dalton Transactions
- Vol. 50 (45) , 16720-16725
Synthesis of a Pd 2 In–Pd 3 In bi-continuous nanoporous structure by electrochemical dealloying in molten salts
High-temperature dealloying in molten alkali chlorides has been demonstrated and nanoporous coherent structures consisting of the intermetallic compounds Pd 2 In and Pd 3 In in a ratio of 2 : 1 have been observed.
- 29 October 2021
- Published by Royal Society of Chemistry (RSC) in Dalton Transactions
- Vol. 50 (45) , 16720-16725
Synthesis of a Pd 2 In–Pd 3 In bi-continuous nanoporous structure by electrochemical dealloying in molten salts
High-temperature dealloying in molten alkali chlorides has been demonstrated and nanoporous coherent structures consisting of the intermetallic compounds Pd 2 In and Pd 3 In in a ratio of 2 : 1 have been observed.
- 1 June 2021
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 168 (6) , 061504
Communication—High-Temperature Electrochemical Synthesis of Nanoporous Iron by Dealloying of Ferromanganese in a LiCl-KCl Eutectic
A bi-continuous structure of nanoporous iron was synthesized by the high-temperature electrochemical dealloying of Fe 0.5 Mn 0.5 in a molten LiCl-KCl eutectic. It was found that the characteristic bi-continuous structure of pores and ligaments of the order of 100 nm is formed at the lower temperature of 400 °C. At 500 °C another morphology of dendrite-like structure is formed since the number of ligaments decreases due to coarse-graining during processing. Surprisingly, at 600 °C, the formation of a new bi-continuous structure with “ginger-root-like” ligaments of several microns was observed.
- 1 June 2021
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 168 (6) , 061504
Communication—High-Temperature Electrochemical Synthesis of Nanoporous Iron by Dealloying of Ferromanganese in a LiCl-KCl Eutectic
A bi-continuous structure of nanoporous iron was synthesized by the high-temperature electrochemical dealloying of Fe 0.5 Mn 0.5 in a molten LiCl-KCl eutectic. It was found that the characteristic bi-continuous structure of pores and ligaments of the order of 100 nm is formed at the lower temperature of 400 °C. At 500 °C another morphology of dendrite-like structure is formed since the number of ligaments decreases due to coarse-graining during processing. Surprisingly, at 600 °C, the formation of a new bi-continuous structure with “ginger-root-like” ligaments of several microns was observed.