Etienne Copin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Etienne Copin has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
Philippe Lours
Institut Clément Ader (ICA), Université de Toulouse, CNRS, IMT Mines Albi, INSA, ISAE‐SUPAERO, UPS Toulouse France
5 shared publicationsThierry Sentenac
Université de Toulouse
3 shared publicationsFlorence Ansart
Université Toulouse 3 Paul-Sabatier
2 shared publications- Yankuan Liu
Tianjin Key Laboratory of Civil Aircraft Airworthiness and Maintenance, College of Aeronautical Engineering, Civil Aviation University of China, Tianjin, China
2 shared publications Yannick Le Maoult
2 shared publicationsZhiping Wang
2 shared publications
Latest Publications
- 1 April 2026
- Published by Agence Bibliographique de l'Enseignement Supérieur
Fonctionnalisation de barrières thermiques aéronautiques YSZ issues de la voie sol-gel : mesure de température et diagnostic de l'endommagement par fluorescence
L'objectif de la thèse est de développer des systèmes de Barrières Thermiques (BT) « capteurs » base zircone yttriée (ZrO2 + 9.8mol% Y2O3, YSZ) déposés par voie sol-gel selon un procédé de trempage-retrait. Ceux-ci sont dédiés à la mesure de la température par des méthodes de thermométrie par fluorescence et au suivi de l'endommagement dans l'épaisseur des revêtements. Les méthodes proposées sont basées sur le suivi de l'évolution, notamment avec la température, des propriétés de photoluminescence de marqueurs fluorescents lanthanides Ln3+, tels que l'europium Eu3+, le dysprosium Dy3+, l'erbium Er3+, le samarium Sm3+ ou encore le thulium Tm3+. Ceux-ci sont directement incorporés dans la structure de la zircone, semi-transparente dans le domaine d'émission visible de ces marqueurs. Un banc de mesure des propriétés de fluorescence (spectres, intensités et temps de vie) a spécifiquement été développé dans ce but. La caractérisation des différents couples YSZ:Ln3+ sous forme de poudres synthétisées par voie sol-gel a permis d'optimiser les compositions de manière à maximiser l'intensité du signal de fluorescence tout en préservant les propriétés microstructurales requises pour une BT. Les dépôts sol-gel réalisés par trempage-retrait permettent la fabrication de prototypes de BT multicouches fonctionnalisées intégrant jusqu'à trois couches fluorescentes de longueurs d'onde d'émission distinctes. De tels systèmes architecturés permettent de sonder optiquement la totalité de l'épaisseur de zircone déposée pour de futures applications visant à évaluer les gradients thermiques siégeant dans le volume des revêtements. Des BT fonctionnalisées contenant des défauts de délamination pré-calibrés à l'interface métal/céramique ont été également utilisées pour comparer l'intérêt d'une méthode de fluorescence accrue par réflectance et d'une méthode de thermographie infrarouge pour le suivi et l'évaluation des processus d'endommagement précurseurs de l'écaillage. Enfin, le potentiel qu'offrent les poudres de zircone YSZ:Ln3+ dopées en tant que marqueurs fluorescents de l'histoire thermique, alternatifs aux peintures thermiques utilisées industriellement, a aussi été analysé.
- 1 April 2026
- Published by Agence Bibliographique de l'Enseignement Supérieur
Fonctionnalisation de barrières thermiques aéronautiques YSZ issues de la voie sol-gel : mesure de température et diagnostic de l'endommagement par fluorescence
L'objectif de la thèse est de développer des systèmes de Barrières Thermiques (BT) « capteurs » base zircone yttriée (ZrO2 + 9.8mol% Y2O3, YSZ) déposés par voie sol-gel selon un procédé de trempage-retrait. Ceux-ci sont dédiés à la mesure de la température par des méthodes de thermométrie par fluorescence et au suivi de l'endommagement dans l'épaisseur des revêtements. Les méthodes proposées sont basées sur le suivi de l'évolution, notamment avec la température, des propriétés de photoluminescence de marqueurs fluorescents lanthanides Ln3+, tels que l'europium Eu3+, le dysprosium Dy3+, l'erbium Er3+, le samarium Sm3+ ou encore le thulium Tm3+. Ceux-ci sont directement incorporés dans la structure de la zircone, semi-transparente dans le domaine d'émission visible de ces marqueurs. Un banc de mesure des propriétés de fluorescence (spectres, intensités et temps de vie) a spécifiquement été développé dans ce but. La caractérisation des différents couples YSZ:Ln3+ sous forme de poudres synthétisées par voie sol-gel a permis d'optimiser les compositions de manière à maximiser l'intensité du signal de fluorescence tout en préservant les propriétés microstructurales requises pour une BT. Les dépôts sol-gel réalisés par trempage-retrait permettent la fabrication de prototypes de BT multicouches fonctionnalisées intégrant jusqu'à trois couches fluorescentes de longueurs d'onde d'émission distinctes. De tels systèmes architecturés permettent de sonder optiquement la totalité de l'épaisseur de zircone déposée pour de futures applications visant à évaluer les gradients thermiques siégeant dans le volume des revêtements. Des BT fonctionnalisées contenant des défauts de délamination pré-calibrés à l'interface métal/céramique ont été également utilisées pour comparer l'intérêt d'une méthode de fluorescence accrue par réflectance et d'une méthode de thermographie infrarouge pour le suivi et l'évaluation des processus d'endommagement précurseurs de l'écaillage. Enfin, le potentiel qu'offrent les poudres de zircone YSZ:Ln3+ dopées en tant que marqueurs fluorescents de l'histoire thermique, alternatifs aux peintures thermiques utilisées industriellement, a aussi été analysé.
- 22 April 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (20) , 30618-30631
Photoluminescence evolution in APS-deposited YSZ:Eu3+ thermal barrier coatings: mechanisms and sensitivity to thermal history over 0–800 h isothermal exposure at 1100 °C
- 22 April 2025
- Published by Elsevier in Ceramics International
- Vol. 51 (20) , 30618-30631
Photoluminescence evolution in APS-deposited YSZ:Eu3+ thermal barrier coatings: mechanisms and sensitivity to thermal history over 0–800 h isothermal exposure at 1100 °C
- 11 January 2022
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 45 (4) , 1258-1275
Impact of annealing treatment on the fatigue behavior of Inconel 625 produced by laser‐based powder bed fusion
Laser‐based powder bed fusion (LPBF) is attractive to build complex parts in spite of the low machinability of Inconel 625. The LPBF microstructures and tensile properties are well documented in literature. But fatigue properties and impact of the LPBF intrinsic defects and microstructures on the crack initiation and propagation mechanisms are uncommon. Low and high‐cycle fatigue tests at room and service temperature presented in this paper prove that the LPBF defects shorten the crack initiation stage. After annealing heat treatment, the microstructure adapts to the defects, and the fatigue response becomes similar to a free defect material. The fatigue life of as‐built Inconel 625 is lower than 50% of its monotonic yield tensile strength (YTS) while the annealed material reaches 100% of its YTS. The propagation rate is slowed by the homogeneous annealed microstructure and improved ductility resulting from removal of dislocation cells and changes in grain morphology.
- 11 January 2022
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 45 (4) , 1258-1275
Impact of annealing treatment on the fatigue behavior of Inconel 625 produced by laser‐based powder bed fusion
Laser‐based powder bed fusion (LPBF) is attractive to build complex parts in spite of the low machinability of Inconel 625. The LPBF microstructures and tensile properties are well documented in literature. But fatigue properties and impact of the LPBF intrinsic defects and microstructures on the crack initiation and propagation mechanisms are uncommon. Low and high‐cycle fatigue tests at room and service temperature presented in this paper prove that the LPBF defects shorten the crack initiation stage. After annealing heat treatment, the microstructure adapts to the defects, and the fatigue response becomes similar to a free defect material. The fatigue life of as‐built Inconel 625 is lower than 50% of its monotonic yield tensile strength (YTS) while the annealed material reaches 100% of its YTS. The propagation rate is slowed by the homogeneous annealed microstructure and improved ductility resulting from removal of dislocation cells and changes in grain morphology.
- 1 January 2020
- Published by Elsevier in Additive Manufacturing
- Vol. 31
A novel approach to the production of NiCrAlY bond coat onto IN625 superalloy by selective laser melting
- 1 January 2020
- Published by Elsevier in Additive Manufacturing
- Vol. 31
A novel approach to the production of NiCrAlY bond coat onto IN625 superalloy by selective laser melting
- 25 November 2019
- Published by Springer Nature in Journal of Thermal Spray Technology
- Vol. 29 (3) , 433-443
Apparent Interfacial Toughness of Undoped and Photoluminescent Eu3+-Doped Yttria-Stabilized Zirconia Thermal Barrier Coatings
- 25 November 2019
- Published by Springer Nature in Journal of Thermal Spray Technology
- Vol. 29 (3) , 433-443
Apparent Interfacial Toughness of Undoped and Photoluminescent Eu3+-Doped Yttria-Stabilized Zirconia Thermal Barrier Coatings
- 1 April 2018
- Published by Elsevier in Sensors and Actuators A: Physical
- Vol. 272, 42-52
On the thermal sensitivity and resolution of a YSZ:Er3+/YSZ:Eu3+ fluorescent thermal history sensor
- 1 April 2018
- Published by Elsevier in Sensors and Actuators A: Physical
- Vol. 272, 42-52
On the thermal sensitivity and resolution of a YSZ:Er3+/YSZ:Eu3+ fluorescent thermal history sensor
- 18 November 2016
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 26 (1) , 015001
Novel erbia-yttria co-doped zirconia fluorescent thermal history sensor
Thermochromic pigments are commonly used for off-line temperature mapping on components from systems operating at a temperature higher than 1073 K. However, their temperature resolution is often limited by the discrete number of color transitions they offer. This paper investigates the potential of erbia-yttria co-doped zirconia as a florescent thermal history sensor alternative to thermochromic pigments. Samples of yttria-stabilized zirconia powder (YSZ, 8.3 mol% YO 1.5 ) doped with 1.5 mol% ErO 1.5 and synthesized by a sol-gel route are calcined for 15 minutes under isothermal conditions between 1173 and 1423 K. The effects of temperature on their crystal structure and room temperature fluorescence properties are then studied. Results show a steady increase of the crystallinity of the powders with temperature, causing a significant and permanent increase of the emission intensity and fluorescence lifetime which could be used to determine temperature with a calculated theoretical resolution lower than 1 K for intensity. The intensity ratio obtained using a temperature insensitive YSZ:Eu 3+ reference phosphor is proposed as a more robust parameter regarding experimental conditions for determining thermal history. Finally, the possibilities for integrating this fluorescent marker into sol-gel deposited coatings for future practical thermal history sensing applications is also discussed.
- 18 November 2016
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 26 (1) , 015001
Novel erbia-yttria co-doped zirconia fluorescent thermal history sensor
Thermochromic pigments are commonly used for off-line temperature mapping on components from systems operating at a temperature higher than 1073 K. However, their temperature resolution is often limited by the discrete number of color transitions they offer. This paper investigates the potential of erbia-yttria co-doped zirconia as a florescent thermal history sensor alternative to thermochromic pigments. Samples of yttria-stabilized zirconia powder (YSZ, 8.3 mol% YO 1.5 ) doped with 1.5 mol% ErO 1.5 and synthesized by a sol-gel route are calcined for 15 minutes under isothermal conditions between 1173 and 1423 K. The effects of temperature on their crystal structure and room temperature fluorescence properties are then studied. Results show a steady increase of the crystallinity of the powders with temperature, causing a significant and permanent increase of the emission intensity and fluorescence lifetime which could be used to determine temperature with a calculated theoretical resolution lower than 1 K for intensity. The intensity ratio obtained using a temperature insensitive YSZ:Eu 3+ reference phosphor is proposed as a more robust parameter regarding experimental conditions for determining thermal history. Finally, the possibilities for integrating this fluorescent marker into sol-gel deposited coatings for future practical thermal history sensing applications is also discussed.