  • Influence of Rare Earth Element Additions on the Microstructure, Corrosion Resistance, and Joinability of AZ31 Magnesium Alloys

    by Ziadoon Tareq Mhawesh, İsmail Hakkı Kara, Fatih Hayat

    Magnesium alloys are increasingly prioritized for lightweight engineering applications; however, their industrial utility is often limited by microstructural stability and corrosion susceptibility. In the present study, the microstructure, corrosion behavior, and joinability of AZ31 magnesium alloys modified by varying concentrations of rare earth elements, specifically neodymium (Nd) and lanthanum (La), were comprehensively investigated. Two specific compositions, AZ31-0.5Nd-0.2La and AZ31-0.5Nd-0.5La, were synthesized via induction melting and subsequently processed through hot rolling to produce sheets with a precise thickness of 1.5 mm. To evaluate their structural integration potential, these processed alloys were successfully joined with interstitial-free (IF) steel through a mechanical clinching process. Detailed microstructural characterization was performed utilizing scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDX). The analysis revealed that secondary intermetallic phases, primarily enriched with Al-Mn-Nd and Al-La-Nd, were predominantly distributed along the grain boundaries in both alloy variants. Potentiodynamic polarization tests were executed in a 3.5% NaCl solution across three distinct cross-sections (S1, S2, and S3) to ensure experimental consistency. Quantitative data indicated that the AZ31-0.5Nd-0.5La alloy exhibited superior corrosion resistance compared to the AZ31-0.5Nd-0.2La alloy, as evidenced by significantly lower icorr and mpy values. Long-term immersion corrosion tests further confirmed these findings, showing that while metal loss generally increased with duration, the AZ31-0.5Nd-0.5La alloy achieved the lowest metal loss (0.79 g) after 16 hours. Ultimately, the results demonstrate that an increased lanthanum content is highly favorable for enhancing the microstructural stability and corrosion resistance of AZ31 magnesium alloys.

  • Open Access

    The Effect of Sc on the Biocorrosion Properties of Selected Zinc-Based Biomaterials

    by Ismail Hakkı KARA, Salem A G Saleh

    In this study, Zn-based alloys were produced by the conventional casting technique. After homogenization heat treatment, microstructural properties and corrosion life of pure zinc, Zn-Mg, Zn-Mg-Al, and Zn-Mg-Al-Sc alloys were investigated. Effects of additional elements, heat treatment, and phases formed in the structures affecting corrosion resistance were systematically investigated. To evaluate corrosion, we performed electrochemical and immersion tests in Hank's salt solution. Corrosion resistance deteriorated in scandium-added Zn-Mg-Al-Sc alloys due to localized galvanic coupling, whereas we observed improvements in microstructure. On a positive note, the Zn-Mg-Al alloy showed the best corrosion resistance. Our findings on the microstructural changes and corrosion resistance effects of Sc addition to biodegradable Zn-based alloys helped to explain the complex role played by Sc. The previous studies focused mostly on binary and ternary systems of Zn alloys. However, new insight into the role of Sc adding in Zn-based alloys is contributed by this study. The findings of our study clarify the effect of Sc on the microstructure and bio-corrosion behavior of Zn-based alloys. As a result, more reliable biodegradable Zn-based alloys will be designed thanks to this study.


  • Open Access

    Experimental and Numerical Investigation of Thinning Behavior in Deep Drawing of AISI 1008, CuZn30, and Aluminum 1100

    by Riham Raad Ahmed, İsmail Hakkı KARA, Muhsin J. Jweeg

    This study investigates the thickness distribution behavior of deep drawing cup products under the influence of various forming parameters, die radius, punch velocity, blank holder force, sheet thickness, and sheet metal type. Three types of sheet metal were used: low carbon steel (AISI 1008), aluminum (1100), and brass (CuZn30), in sheets of 80 mm diameter circular blanks with thicknesses of 0.7 and 1 mm, formed by a tooling set (die, punch, and blank holder). The die radius profile at R4 and R6 was used, where the punch velocities were 100, 150, and 200 mm/min. ABAQUS/CAE was used for numerical simulation, and a dynamic explicit solver was employed to form cylindrical cup products. The results show that for three metals, higher punch speeds tend to increase strain localization, and maximum thinning occurs at the punch nose radius; the maximum thickening in the sidewall region and thinning are increased with the decrease of die radius. It was also found that the r-value of the Lankford coefficients plays a significant role in thinning behavior in relation to rolling (r-value direction). The results also indicate that aluminum alloys are relatively formable, but they are highly sensitive to process variables, specifically blank holder pressure and sheet thickness. Wrinkles are reduced by increased blank holder force, but higher values cause tearing near the punch corners. All of the materials showed a similar thinning behavior during the deep drawing process, in spite of the variations in their mechanical properties. The results have shown a strong agreement between experimental and numerical work with a maximum discrepancy of 5 %.

  • Development and Evaluation of Hybrid Sol-Gel Coatings for Enhanced Corrosion Resistance on Mild Steel

    by Mohammed Jaber Abed Al-Owaidi1, İsmail Hakkı Kara, Fatih Hayat

    This article describes the design, synthesis, and characterization of sol–gel hybrid coatings to improve corrosion protection for low-carbon steel. We intensively studied System A (TEOS/MPTS) and System B (TEOS/MPTS/PhTMS). The process included dip-coating, then temperature curing, and we applied techniques like SEM, XRD, FTIR, contact angle measurements, and potentiodynamic Tafel polarization tests to characterize the results. The SEM and FTIR analyses confirmed that we properly developed dense, cross-linked siloxane networks, and XRD patterns suggested mainly amorphous structures. The contact angle measurements demonstrated a significant improvement in hydrophobicity, with System A exhibiting a contact angle value of 89.8° for the TE3 sample. Electrochemical measurements indicated significant corrosion current density decreases for System A (i_corr = 8.13 µA/cm², 91% improvement in comparison to bare steel), while System B showed a relatively less significant enhancement. Contrary to expectations, films cast from freshly synthesized sols outperformed those from aged sols, underlining the significance of sol aging in film homogeneity and barrier performance. Overall, the hybrid sol–gel coatings, especially TEOS/MPTS formulations, exhibit effective physical and chemical protective properties against corrosion and enhanced hydrophobicity and barrier properties. The precursor mixture, sol aging, and deposition parameters must be optimized to ensure optimal performance and uniformity. These findings portend a promising future for these green, scalable, and long-lasting protective coatings in industrial applications.

  • Microstructural Evolution and Corrosion Characteristics of Zn-RE-Mg-Al-Mn Cast Alloys

    by Ziadoon Tareq Mhawesh Mhawesh, İsmail Hakkı KARA

    In this work, the effects of adding rare earth elements (Nd and Gd) and Mg, Al, and Mn on the microstructure and corrosion characteristics of Zn-based cast alloys were comprehensively studied. Eight different alloy samples were synthesized and analyzed by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDX), potentiodynamic polarization (Tafel) experiments, and immersion corrosion tests. Microstructural analysis revealed the presence of dendritic α-Zn phases in the Zn matrix and Nd-rich and Gd-rich intermetallic phases, whose morphology varied depending on the kind and quantity of the additives. The Tafel test values of corrosion potential (Ecorr) and current density (Icorr), and the immersion test-derived values of annual corrosion rates (mm/year), were well correlated with the degree of microstructural degradation. Sample Zn + 5 Mg + 0.1 Al + 0.01 Mn + 0.5 Nd + 2.0 Gd, which had the highest corrosion resistance with a higher percentage of Nd and more homogeneous in structure, followed by Sample Zn + 5 Mg + 0.1 Al + 0.01 Mn + 0.1 Nd with the poorest performance. Post-immersion SEM micrographs substantiated the corrosion and electrochemical as well as immersion results, and reiterated that the distribution of intermetallic phases, grain size, and homogeneity of alloying elements are the major parameters governing the corrosion behavior.

  • Comparative Study for Corrosion Resistance of Ferrous and Non-ferrous Pipes Immersed in Magnetized Water

    by Bilal Ali Abbas Al-Halboosi, İsmail Hakkı KARA

    This study aims to investigate the corrosion resistance of galvanized steel (GS) and AZ31 pipe materials immersed in a magnetized water treatment (MWT) applied river water source. The potentiodynamic corrosion test results showed that a better corrosion rate is obtained by the AZ31(corr.rate: 0.0442 mm/y) specimen than GS (corr.rate: 0.0764 mm/y) due to the passivation efficiency resulting from the calcite and MgO particles on the surface.

  • Mg-2,5Al-1,0Sn-0,3Mn-0,4La-1,33Gd Mg Alaşımının Yüksek Sıcaklık Aşınma Davranışına Haddeleme Hızının Etkisinin İncelenmesi

    by İsmail Hakkı KARA

    Bu çalışmanın amacı otomotiv ve uzay taşıtlarında kullanım potansiyeli yüksek olan hafif magnezyum (Mg) alaşımların yüksek sıcaklık aşınma davranışına farklı haddeleme hızlarının etkisini incelemektir. Sürtünme nedeniyle oluşan veya kullanım çevresine bağlı artan sıcaklığın aşınmaya maruz kalan fren balataları gibi uygulamalarda Mg alaşımın nasıl tepki verdiğini anlamak önem arz etmektedir. Yapısal olarak geliştirilmiş nadir toprak elementi içeren Mg alaşımları buna çözüm olarak düşünülmüştür. Burada yüksek sıcaklığa dayanımı zayıf olan ikincil fazlar yerine yapıda daha kararlı ikincil fazlar oluşturmak esas alınmıştır. Bu amaçla sıcak haddelenmiş Mg-2.5Al-1.0Sn-0.3Mn-0.4La-1.33Gd Mg alaşımına 225°C de aşınma testleri uygulanmıştır. 1.5, 4.7 ve 10 m/dk olmak üzere üç farklı hadde hızıyla elde edilen sac malzemelerin mikroyapısal karakterizasyonu ışık optik mikroskop (LOM) ve taramalı elektron mikroskobu (SEM) vasıtasıyla incelenmiştir. Hadde hızına bağlı ikizlenmeler ve yeniden kristalleşen taneler elde edilmiştir. Sıcak aşınma davranışının mikroyapıya bağlı olarak değiştiği ve oluşan sert ikincil fazların daha yumuşak olan matrisle birleşerek aşınma direncine katkı sağladığı anlaşılmıştır. Artan hadde hızına bağlı aşınma hızında düşüş meydana gelmiştir. 10m/dk ve 1.5m/dk hadde hızlarının aşınma hızları karşılaştırıldığında iki kattan daha fazla fark olduğu görülmüştür. Aşınma mekanizmaları incelenen aşınmış yüzeylerin plastik akma, adhezif ve plastik deformasyon türünde mekanizmalara sahip olduğu görülmüştür.