Ismail Akin Kiyici
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Ismail Akin Kiyici has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
F.N. Oktar
Marmara University
2 shared publicationsSimeon Agathopoulos
University of Ioannina
2 shared publications- Carmen Ristoscu
National Institute for Laser, Plasma and Radiation Physics, 409 Atomistilor Street, P.O. Box MG 36, 077125 Magurele, Romania
1 shared publication D. Bilgiç
Marmara University
1 shared publicationD. Kel
Marmara University
1 shared publication- Duygu Ağaoğulları
Istanbul Technical University
1 shared publication
Latest Publications
- 27 October 2011
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 493-494, 781-786
Sea Snail: An Alternative Source for Nano-Bioceramic Production
The production of nano-calcium phosphate, such as HA (hydroxyapatite), materials from synthetic chemicals could sometimes lead to a costly and tedious work. Sea creatures could be an alternative way to produce very fine and even nano-structured calcium phosphate materials. Nacres vastly consist of rich calcium carbonate and/or aragonite mater. With simple conversion methods, like hotplate stirring, various bioceramic structures could be produced suitable for thin film coatings with various methods, like pulsed laser deposition (MAPLE). This study is part of a bigger project which eventually and ultimately aims to produce nano-phases of calcium phosphate biocompatible bioceramics, which can be used for biomedical coatings. In this particular study, we focus at transforming chemically, using hotplate stirring method, local sea snail shells rapana thomasiana. Cleaned sea snail samples were provided from local markets in Istanbul. The shells were smashed down, ball-milled and the powder was sieved (3 content of the shells. According to these results, the required volume of H3PO4 was added in order to set the molar ratio of Ca/P (during hotplate stirring) either 10/6 or 3/2 (these ratios correspond to HA and TCP, respectively). SEM and X-ray diffraction analyses were conducted. The SEM observations showed brick-like particles were formed with sizes <5 µm. From the X-ray diffraction analysis, predominantly monetite, which can be considered as a precursor of HA and TCP, was detected. The results of this study showed that to produce HA and other bioceramic phases, hot-plate stirring method is a reliable, fast, rapid and economic method when compared to other tedious HA production methods. Moreover, sea snail shells are very good candidate materials to produce fine powders with hotplate stirring method for various tissue engineering applications.
- 27 October 2011
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 493-494, 781-786
Sea Snail: An Alternative Source for Nano-Bioceramic Production
The production of nano-calcium phosphate, such as HA (hydroxyapatite), materials from synthetic chemicals could sometimes lead to a costly and tedious work. Sea creatures could be an alternative way to produce very fine and even nano-structured calcium phosphate materials. Nacres vastly consist of rich calcium carbonate and/or aragonite mater. With simple conversion methods, like hotplate stirring, various bioceramic structures could be produced suitable for thin film coatings with various methods, like pulsed laser deposition (MAPLE). This study is part of a bigger project which eventually and ultimately aims to produce nano-phases of calcium phosphate biocompatible bioceramics, which can be used for biomedical coatings. In this particular study, we focus at transforming chemically, using hotplate stirring method, local sea snail shells rapana thomasiana. Cleaned sea snail samples were provided from local markets in Istanbul. The shells were smashed down, ball-milled and the powder was sieved (3 content of the shells. According to these results, the required volume of H3PO4 was added in order to set the molar ratio of Ca/P (during hotplate stirring) either 10/6 or 3/2 (these ratios correspond to HA and TCP, respectively). SEM and X-ray diffraction analyses were conducted. The SEM observations showed brick-like particles were formed with sizes <5 µm. From the X-ray diffraction analysis, predominantly monetite, which can be considered as a precursor of HA and TCP, was detected. The results of this study showed that to produce HA and other bioceramic phases, hot-plate stirring method is a reliable, fast, rapid and economic method when compared to other tedious HA production methods. Moreover, sea snail shells are very good candidate materials to produce fine powders with hotplate stirring method for various tissue engineering applications.
- 1 October 2011
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 493-494, 287-292
Production of Natural Bioceramic from Land Snails
There are thousands of land snail species, ranging in size from 1 mm to the Giant African Snail growing up to a foot long. Two species, known as escargot, helix aspersa and helix pomatia, are commercially important. Helix pomatia is abundant in Turkey. Those snails are exported usually without shells. Shells are damped to trash sites or used as substitute food for animals. The shell is rich in calcium carbonate and some other minor minerals. Thus, snails’ shells can be used as a source for bioceramic production. So far, in the literature there are lot of papers about converting calcite and aragonite structures to hydroxyapatite (HA), like corals, sea shells, sea urchin and other sea creatures. However, there is very limited information about converting land snail shells to HA and other bioceramic phases. The aim of this work was to produce various phases of bioceramic materials from land snails’ shells which are left as a residue waste after their export procedures. Empty local land snails’ shells (helix pomatia) were collected in Istanbul. They were washed, dried, crushed and ball milled until a powder of 100 µm particles size was obtained. Raw powders were stirred at 80°C for 15 min on a hotplate. A second part of the raw powder was stirred with an ultrasonic stirrer at 80°C for 15 min in an ultrasonic equipment. Equivalent amount of H3PO4 was added drop by drop into the solution. The reaction lasted for 8h. Then, to evaporate the liquid part, the mixtures were put into an incubator at 100°C for 24 h and the resultant dried sediments were collected. The produced powders were analyzed with X-ray diffraction, IR and scanning electron microscope (SEM). The experimental results confirmed the formation of various Ca-phosphates, specifically monetite, fluorapatite and some other minor calcium phosphate phases. Bioceramic production from land snail is a reliable and economic way comparing to other tedious methods of producing synthetic HA and other various bioceramics phases.
- 1 October 2011
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 493-494, 287-292
Production of Natural Bioceramic from Land Snails
There are thousands of land snail species, ranging in size from 1 mm to the Giant African Snail growing up to a foot long. Two species, known as escargot, helix aspersa and helix pomatia, are commercially important. Helix pomatia is abundant in Turkey. Those snails are exported usually without shells. Shells are damped to trash sites or used as substitute food for animals. The shell is rich in calcium carbonate and some other minor minerals. Thus, snails’ shells can be used as a source for bioceramic production. So far, in the literature there are lot of papers about converting calcite and aragonite structures to hydroxyapatite (HA), like corals, sea shells, sea urchin and other sea creatures. However, there is very limited information about converting land snail shells to HA and other bioceramic phases. The aim of this work was to produce various phases of bioceramic materials from land snails’ shells which are left as a residue waste after their export procedures. Empty local land snails’ shells (helix pomatia) were collected in Istanbul. They were washed, dried, crushed and ball milled until a powder of 100 µm particles size was obtained. Raw powders were stirred at 80°C for 15 min on a hotplate. A second part of the raw powder was stirred with an ultrasonic stirrer at 80°C for 15 min in an ultrasonic equipment. Equivalent amount of H3PO4 was added drop by drop into the solution. The reaction lasted for 8h. Then, to evaporate the liquid part, the mixtures were put into an incubator at 100°C for 24 h and the resultant dried sediments were collected. The produced powders were analyzed with X-ray diffraction, IR and scanning electron microscope (SEM). The experimental results confirmed the formation of various Ca-phosphates, specifically monetite, fluorapatite and some other minor calcium phosphate phases. Bioceramic production from land snail is a reliable and economic way comparing to other tedious methods of producing synthetic HA and other various bioceramics phases.