Nikolay V. Luparev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Nikolay V. Luparev has a total of 64 co-authors. Here are the top co-authors by number of shared publications:
- Sergey A. Tarelkin
Технологический институт сверхтвердых и новых углеродных материалов
11 shared publications - Andrey V. Golovanov
Liquid Crystal Laboratory, Department of Polymers and Crystals, Moscow State University, Moscow, Russia
6 shared publications - Boris P. Sorokin
Federal State Budgetary Institution «Technological Institute for Superhard and Novel Carbon Materials of National Research Centre «Kurchatov Institute», 108840 Moscow, Troitsk, Russian Federation; Moscow Institute of Physics and Technology, 141700 Dolgoprudny, Russian Federation
6 shared publications - Dmitrii D. Prikhodko
Технологический институт сверхтвердых и новых углеродных материалов
6 shared publications - Nikita O. Asafiev
Технологический институт сверхтвердых и новых углеродных материалов Национального исследовательского центра «Курчатовский институт
5 shared publications - Vera O. Timoshenko
Технологический институт сверхтвердых и новых углеродных материалов
5 shared publications
Latest Publications
- 8 November 2025
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 68 (12) , 41-50
APPLICATION OF A MICROWAVE ACOUSTOELECTRONIC SENSOR ON A DIAMOND SUBSTRATE FOR THE ANALYSIS OF THE CHEMICAL COMPOSITION OF SOLUTIONS AND SUSPENSIONS
For the first time, an acoustoelectronic sensor on a diamond substrate with the "Al/Al0.72S0.28N/Mo/(100) diamond" structure using a longitudinal bulk acoustic wave as an operating mode on microwave frequency band up to 9 GHz has been applied for studying solutions and suspensions. The sensor design excluded the effect of the studied liquids on the sensing element as a thin-film piezoelectric transducer Al/Al0.72Sc0.28N/Mo. Using acoustic overtones in the vicinity of frequencies of 4.8, 5.6 and 9.3 GHz, the change in the informative parameters of the sensor (amplitude, quality factor, reflection coefficient) was investigated as a result of applying aqueous solutions of sodium chloride (up to the concentration of a saturated solution) or glycerin (0 - 100 wt.%), as well as a precipitated suspension with carbon nanotubes (CNTs). A monotonous decrease in the informative parameters of a sensor was found with an increase in the concentration of solutions, as well as during the transition from the liquid fraction of the suspension to the dried one. Loading the sensor with samples of aqueous solutions of NaCl and glycerin, or suspensions with CNT did not lead to a significant decrease in the quality of the microwave signal. For this type of sensor, the actual accuracy of measuring the concentration of solute using aqueous solutions of sodium chloride or glycerin as an example was ~1 wt.%. The minimum sample of the studied solutions, leading to a change in the informative parameters of the sensor, for water turned out to be ~0.8 milligrams (~8·10-4 ml). The use of type IIa single crystalline synthetic diamond as a sensor substrate ensures high chemical and biological stability of the operation surface, resistance to temperature loads and abrasive wear, and the possibility of repeated use. For citation: Sorokin B.P., Yashin D.V., Asafiev N.O., Khaskov M.A., Luparev N.V. Application of a microwave acoustoelectronic sensor on a diamond substrate for the analysis of the chemical composition of solutions and suspensions. ChemChemTech [Izv. Vyssh. Uchebn. Zaved. Khim. Khim. Tekhnol.]. 2025. V. 68. N 12. P. 41-50. DOI: 10.6060/ivkkt.20256812.17y.
- 8 November 2025
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 68 (12) , 41-50
APPLICATION OF A MICROWAVE ACOUSTOELECTRONIC SENSOR ON A DIAMOND SUBSTRATE FOR THE ANALYSIS OF THE CHEMICAL COMPOSITION OF SOLUTIONS AND SUSPENSIONS
For the first time, an acoustoelectronic sensor on a diamond substrate with the "Al/Al0.72S0.28N/Mo/(100) diamond" structure using a longitudinal bulk acoustic wave as an operating mode on microwave frequency band up to 9 GHz has been applied for studying solutions and suspensions. The sensor design excluded the effect of the studied liquids on the sensing element as a thin-film piezoelectric transducer Al/Al0.72Sc0.28N/Mo. Using acoustic overtones in the vicinity of frequencies of 4.8, 5.6 and 9.3 GHz, the change in the informative parameters of the sensor (amplitude, quality factor, reflection coefficient) was investigated as a result of applying aqueous solutions of sodium chloride (up to the concentration of a saturated solution) or glycerin (0 - 100 wt.%), as well as a precipitated suspension with carbon nanotubes (CNTs). A monotonous decrease in the informative parameters of a sensor was found with an increase in the concentration of solutions, as well as during the transition from the liquid fraction of the suspension to the dried one. Loading the sensor with samples of aqueous solutions of NaCl and glycerin, or suspensions with CNT did not lead to a significant decrease in the quality of the microwave signal. For this type of sensor, the actual accuracy of measuring the concentration of solute using aqueous solutions of sodium chloride or glycerin as an example was ~1 wt.%. The minimum sample of the studied solutions, leading to a change in the informative parameters of the sensor, for water turned out to be ~0.8 milligrams (~8·10-4 ml). The use of type IIa single crystalline synthetic diamond as a sensor substrate ensures high chemical and biological stability of the operation surface, resistance to temperature loads and abrasive wear, and the possibility of repeated use. For citation: Sorokin B.P., Yashin D.V., Asafiev N.O., Khaskov M.A., Luparev N.V. Application of a microwave acoustoelectronic sensor on a diamond substrate for the analysis of the chemical composition of solutions and suspensions. ChemChemTech [Izv. Vyssh. Uchebn. Zaved. Khim. Khim. Tekhnol.]. 2025. V. 68. N 12. P. 41-50. DOI: 10.6060/ivkkt.20256812.17y.
- Open Access
- 20 June 2025
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 68 (9) , 60-65
FEATURES OF THE TECHNOLOGY OF HOMOEPITAXIAL CHEMICAL DEPOSITION OF THIN DIAMOND LAYERS ON A NITROGEN-DOPED SINGLE-CRYSTAL DIAMOND SUBSTRATE
В данной работе исследованы особенности формирования и свойств алмазных структур, предназначенных для преобразования энергии бета-распада радиоактивного изотопа 63Ni в электрическую энергию. Были выращены алмазные подложки с различной концентрацией азота (300 ppm и 60 ppm) методом температурного градиента при высоких давлениях (TG-HPHT). Анализ показал, что высокое содержание азота приводит к значительному увеличению количества структурных дефектов в подложках. На подготовленных алмазных подложках методом химического осаждения из газовой фазы синтезированы гомоэпитаксиальные слои с низким содержанием примесных центров и изготовлены диоды Шоттки n-типа. Подробно исследованы электрические свойства диодов при воздействии бета-излучения при температурах выше комнатной. Показано, что гомоэпитаксиальные слои на подложках с высокой концентрацией азота наследуют структурные дефекты, которые приводят к высоким токам утечки в диодах и делают такие диоды непригодными для создания эффективных преобразователей энергии. В то же время диоды, изготовленные на подложках с концентрацией азота 60 ppm, обеспечивают низкий ток утечки и эффективное преобразование энергии при температурах до 500 °C. Максимальная электрическая мощность составила 170 пВт при КПД около 1%. Результаты демонстрируют важность оптимизации уровня легирования азотом и кристаллического качества подложек для создания эффективных и долговечных радиоизотопных преобразователей энергии с использованием алмазных PiN структур. Для цитирования: Тарелкин С.А., Корнилов Н.В., Кузнецов М.С., Лупарев Н.В., Мартюшов С.Ю., Тимошенко В.О. Особенности технологии гомоэпитаксиального химического осаждения тонких алмазных слоев на монокристаллическую алмазную подложку, легированную азотом. Изв. вузов. Химия и хим. технология. 2025. Т. 68. Вып. 9. С. 60-65. DOI: 10.6060/ivkkt.20256809.11y.
- 20 June 2025
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 68 (9) , 60-65
Open AccessFEATURES OF THE TECHNOLOGY OF HOMOEPITAXIAL CHEMICAL DEPOSITION OF THIN DIAMOND LAYERS ON A NITROGEN-DOPED SINGLE-CRYSTAL DIAMOND SUBSTRATE
В данной работе исследованы особенности формирования и свойств алмазных структур, предназначенных для преобразования энергии бета-распада радиоактивного изотопа 63Ni в электрическую энергию. Были выращены алмазные подложки с различной концентрацией азота (300 ppm и 60 ppm) методом температурного градиента при высоких давлениях (TG-HPHT). Анализ показал, что высокое содержание азота приводит к значительному увеличению количества структурных дефектов в подложках. На подготовленных алмазных подложках методом химического осаждения из газовой фазы синтезированы гомоэпитаксиальные слои с низким содержанием примесных центров и изготовлены диоды Шоттки n-типа. Подробно исследованы электрические свойства диодов при воздействии бета-излучения при температурах выше комнатной. Показано, что гомоэпитаксиальные слои на подложках с высокой концентрацией азота наследуют структурные дефекты, которые приводят к высоким токам утечки в диодах и делают такие диоды непригодными для создания эффективных преобразователей энергии. В то же время диоды, изготовленные на подложках с концентрацией азота 60 ppm, обеспечивают низкий ток утечки и эффективное преобразование энергии при температурах до 500 °C. Максимальная электрическая мощность составила 170 пВт при КПД около 1%. Результаты демонстрируют важность оптимизации уровня легирования азотом и кристаллического качества подложек для создания эффективных и долговечных радиоизотопных преобразователей энергии с использованием алмазных PiN структур. Для цитирования: Тарелкин С.А., Корнилов Н.В., Кузнецов М.С., Лупарев Н.В., Мартюшов С.Ю., Тимошенко В.О. Особенности технологии гомоэпитаксиального химического осаждения тонких алмазных слоев на монокристаллическую алмазную подложку, легированную азотом. Изв. вузов. Химия и хим. технология. 2025. Т. 68. Вып. 9. С. 60-65. DOI: 10.6060/ivkkt.20256809.11y.
- Open Access
- 20 June 2025
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 68 (9) , 53-59
ELECTRON IRRADIATION OF AN UNDOPED HOMOEPITAXIAL DIAMOND TO SUPPRESS HOLE CONDUCTIVITY
Использование нелегированного монокристаллического алмаза в качестве материла для изготовления детекторов высокоэнергетических частиц и различных типов ионизирующего излучения ограничивается наличием фоновой проводимости, вызванной примесью бора, что приводит к высокому темновому току в структурах типа металл-полупроводник-металл или металл-диэлектрик-металл. В данной работе исследуется возможность подавления фоновой проводимости в нелегированном гомоэпитаксиальном алмазе с помощью облучения алмаза небольшими дозами электронов высокой энергии (3,5 МэВ). Объектом исследования стали монокристаллы алмаза с концентрацией примесей менее 1014 см-3, но обладающие удельным сопротивлением при комнатной температуре ~5 кОм∙см. Образцы были подвергнуты электронному облучению с дозами 2∙1015 см-2 и 1016 см-2. Контроль результатов осуществлялся с помощью анализа температурной зависимости электрофизических свойств материала и вольт-амперных характеристик образцов детекторов из него. Полученные в работе результаты показывают, что облучение эффективно снижает проводимость алмаза на несколько порядков. Исследования температурных зависимостей электрофизических параметров подтверждают стабильность материала после облучения в диапазоне температур до 1000 К, что делает возможным создание омических контактов в детекторных структурах без ухудшения характеристик. Измерения вольт-амперных характеристик демонстрируют существенное уменьшение темнового тока детекторов после облучения. Кроме того, величина темнового тока облученных образцов с омическими контактами, обладающими повышенной механической и температурной стабильностью, сопоставима с результатами для необлученных образцов с контактами Шоттки. Полученные данные открывают перспективы разработки детекторов на основе гомоэпитаксиального алмаза, устойчивых к экстремальным условиям эксплуатации. Для цитирования: Тимошенко В.О., Приходько Д.Д., Тарелкин С.А., Жолудев С.И., Лупарев Н.В., Корнилов Н.В. Электронное облучение нелегированного гомоэпитаксиального алмаза для подавления дырочной проводимости. Изв. вузов. Химия и хим. технология. 2025. Т. 68. Вып. 9. С. 53-59. DOI: 10.6060/ivkkt.20256809.12y.
- 20 June 2025
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 68 (9) , 53-59
Open AccessELECTRON IRRADIATION OF AN UNDOPED HOMOEPITAXIAL DIAMOND TO SUPPRESS HOLE CONDUCTIVITY
Использование нелегированного монокристаллического алмаза в качестве материла для изготовления детекторов высокоэнергетических частиц и различных типов ионизирующего излучения ограничивается наличием фоновой проводимости, вызванной примесью бора, что приводит к высокому темновому току в структурах типа металл-полупроводник-металл или металл-диэлектрик-металл. В данной работе исследуется возможность подавления фоновой проводимости в нелегированном гомоэпитаксиальном алмазе с помощью облучения алмаза небольшими дозами электронов высокой энергии (3,5 МэВ). Объектом исследования стали монокристаллы алмаза с концентрацией примесей менее 1014 см-3, но обладающие удельным сопротивлением при комнатной температуре ~5 кОм∙см. Образцы были подвергнуты электронному облучению с дозами 2∙1015 см-2 и 1016 см-2. Контроль результатов осуществлялся с помощью анализа температурной зависимости электрофизических свойств материала и вольт-амперных характеристик образцов детекторов из него. Полученные в работе результаты показывают, что облучение эффективно снижает проводимость алмаза на несколько порядков. Исследования температурных зависимостей электрофизических параметров подтверждают стабильность материала после облучения в диапазоне температур до 1000 К, что делает возможным создание омических контактов в детекторных структурах без ухудшения характеристик. Измерения вольт-амперных характеристик демонстрируют существенное уменьшение темнового тока детекторов после облучения. Кроме того, величина темнового тока облученных образцов с омическими контактами, обладающими повышенной механической и температурной стабильностью, сопоставима с результатами для необлученных образцов с контактами Шоттки. Полученные данные открывают перспективы разработки детекторов на основе гомоэпитаксиального алмаза, устойчивых к экстремальным условиям эксплуатации. Для цитирования: Тимошенко В.О., Приходько Д.Д., Тарелкин С.А., Жолудев С.И., Лупарев Н.В., Корнилов Н.В. Электронное облучение нелегированного гомоэпитаксиального алмаза для подавления дырочной проводимости. Изв. вузов. Химия и хим. технология. 2025. Т. 68. Вып. 9. С. 53-59. DOI: 10.6060/ivkkt.20256809.12y.
- 12 October 2024
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 67 (10) , 73-79
DIAMOND VERTICAL PN SCHOTTKY DIODES WITH PRESISION NITROGEN-DOPED n- LAYER
В данной работе были проведены эксперименты, направленные на оптимизацию вертикальных Шоттки pn диодов с концентрацией азота в n- слое 2. Были исследованы вольт-амперные и вольт-фарадные характеристики диодов. Вольт-фарадные характеристики показали независимость емкости диодов на среднелегированной подложке от запирающего напряжения, что говорит о полном обеднении дрейфового слоя диода. Это подтверждает, что данные диоды являются pn Шоттки диодами. Максимальное интегральное значение прямого тока было ограничено сопротивлением подложки и составило 0,1 А при 10 В и площади Шоттки контакта 6,25 мм2. Это значительно ниже рекордных характеристик алмазных Шоттки диодов. Была обнаружена прямая зависимость концентрации бора в выращенном слое и концентрацией бора в подложке. Таким образом сделан вывод о том, что для достижения максимально низких концентраций донорных центров в n- слое и предотвращения перекомпенсации их акцепторами необходимо использовать легированные бором подложки с концентрацией бора ~1017 см-3. Для цитирования: Тимошенко В.О., Приходько Д.Д., Тарелкин С.А., Корнилов Н.В., Лупарев Н.В., Голованов А.В. Алмазные вертикальные pn диоды Шоттки с прецизионно легированным азотом слоем n-. Изв. вузов. Химия и хим. технология. 2024. Т. 67. Вып. 10. С. 73-79. DOI: 10.6060/ivkkt.20246710.11y.
- 12 October 2024
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 67 (10) , 73-79
DIAMOND VERTICAL PN SCHOTTKY DIODES WITH PRESISION NITROGEN-DOPED n- LAYER
В данной работе были проведены эксперименты, направленные на оптимизацию вертикальных Шоттки pn диодов с концентрацией азота в n- слое 2. Были исследованы вольт-амперные и вольт-фарадные характеристики диодов. Вольт-фарадные характеристики показали независимость емкости диодов на среднелегированной подложке от запирающего напряжения, что говорит о полном обеднении дрейфового слоя диода. Это подтверждает, что данные диоды являются pn Шоттки диодами. Максимальное интегральное значение прямого тока было ограничено сопротивлением подложки и составило 0,1 А при 10 В и площади Шоттки контакта 6,25 мм2. Это значительно ниже рекордных характеристик алмазных Шоттки диодов. Была обнаружена прямая зависимость концентрации бора в выращенном слое и концентрацией бора в подложке. Таким образом сделан вывод о том, что для достижения максимально низких концентраций донорных центров в n- слое и предотвращения перекомпенсации их акцепторами необходимо использовать легированные бором подложки с концентрацией бора ~1017 см-3. Для цитирования: Тимошенко В.О., Приходько Д.Д., Тарелкин С.А., Корнилов Н.В., Лупарев Н.В., Голованов А.В. Алмазные вертикальные pn диоды Шоттки с прецизионно легированным азотом слоем n-. Изв. вузов. Химия и хим. технология. 2024. Т. 67. Вып. 10. С. 73-79. DOI: 10.6060/ivkkt.20246710.11y.
- 3 June 2024
- Published by Pleiades Publishing Ltd in Technical Physics
- Vol. 69 (8) , 2416-2420
Compensation Ratio of Acceptor Centers in Different Growth Sectors of Boron-Doped High-Pressure High-Temperature Diamond
In the production of power diamond electronic elements that are intended for high integral current, low-resistivity active substrates with a low concentration of lattice defects are used. Boron-doped diamond grown by the method of temperature gradient at high pressure and high temperature seems to be most promising for such substrates. Due to the incomplete ionization of acceptor centers in diamond at room temperature, the compensation ratio of these centers strongly influences the free carrier concentration in the material and, hence, on its electrical conductivity. In this article, the subject of research has been the temperature dependence of the electrical conductivity and Hall effect of moderately boron-doped diamond in different crystal growth sectors. It has been shown that the compensation ratio in the {111} growth sector is two to three orders of magnitude greater than in the {001} and {311} sectors. As a result, the electrical conductivity of the {001} and {311} sectors is roughly ~25 times as high as that of the {111} sector, although the boron total concentration in the latter is about ten times higher. Thus, the formation probability of donor centers in {001} and {311} sectors is more than 100 times lower than in the {111} sector. Results indicate that wafers cut from the {001} and {311} sectors are most promising for the production of electron devices with the proviso that a high boron concentration is achieved and the donor concentration remains low.
- 3 June 2024
- Published by Pleiades Publishing Ltd in Technical Physics
- Vol. 69 (8) , 2416-2420
Compensation Ratio of Acceptor Centers in Different Growth Sectors of Boron-Doped High-Pressure High-Temperature Diamond
In the production of power diamond electronic elements that are intended for high integral current, low-resistivity active substrates with a low concentration of lattice defects are used. Boron-doped diamond grown by the method of temperature gradient at high pressure and high temperature seems to be most promising for such substrates. Due to the incomplete ionization of acceptor centers in diamond at room temperature, the compensation ratio of these centers strongly influences the free carrier concentration in the material and, hence, on its electrical conductivity. In this article, the subject of research has been the temperature dependence of the electrical conductivity and Hall effect of moderately boron-doped diamond in different crystal growth sectors. It has been shown that the compensation ratio in the {111} growth sector is two to three orders of magnitude greater than in the {001} and {311} sectors. As a result, the electrical conductivity of the {001} and {311} sectors is roughly ~25 times as high as that of the {111} sector, although the boron total concentration in the latter is about ten times higher. Thus, the formation probability of donor centers in {001} and {311} sectors is more than 100 times lower than in the {111} sector. Results indicate that wafers cut from the {001} and {311} sectors are most promising for the production of electron devices with the proviso that a high boron concentration is achieved and the donor concentration remains low.
- 4 March 2024
- Published by AIP Publishing in Applied Physics Letters
- Vol. 124 (10)
Hall measurements on nitrogen-doped Ib-type synthetic single crystal diamonds at temperatures 550–1143 K
Synthetic nitrogen-doped diamond single crystals have various high-tech applications, but their electronic properties have not been sufficiently studied. In this research, we investigated temperature dependencies in the range T = (550–1143) K of the electrical resistivity and Hall mobility in synthetic single-crystal Ib-type diamonds doped with nitrogen during growth. A series of experimental samples were cut from diamond crystals grown by temperature gradient high-pressure high-temperature (TG-HPHT) and chemical vapor deposition (CVD) methods. They contain (0.085–6.5) × 1019 cm−3 single substitutional nitrogen atoms (C-centers) as measured by optical spectrometry methods. The Hall mobility of free electrons decreases from 600 to 150 cm2 V−1 s−1 in the CVD grown sample with the lowest N content and from 300 to 100 cm2 V−1 s−1 in highly doped HPHT grown samples in the temperature range of 550–900 K. At T = (900–1100) K, the mobility decreases to 50 cm2 V−1 s−1 in highly doped samples. The activation energies of electrical conductivity Ea and impurity-to-band energies of nitrogen donors ED decrease with increasing N concentration in the ranges (1.55–1.32) and (1.63–1.33) eV, respectively. The lowest compensation ratio k ∼ 1% in the moderately doped CVD diamond is unique for n-type diamonds. Typical values of k in highly N-doped crystals are in the range of 10%–20%, facilitating the use of N-doped diamonds in durable high-temperature electronic devices.
- 4 March 2024
- Published by AIP Publishing in Applied Physics Letters
- Vol. 124 (10)
Hall measurements on nitrogen-doped Ib-type synthetic single crystal diamonds at temperatures 550–1143 K
Synthetic nitrogen-doped diamond single crystals have various high-tech applications, but their electronic properties have not been sufficiently studied. In this research, we investigated temperature dependencies in the range T = (550–1143) K of the electrical resistivity and Hall mobility in synthetic single-crystal Ib-type diamonds doped with nitrogen during growth. A series of experimental samples were cut from diamond crystals grown by temperature gradient high-pressure high-temperature (TG-HPHT) and chemical vapor deposition (CVD) methods. They contain (0.085–6.5) × 1019 cm−3 single substitutional nitrogen atoms (C-centers) as measured by optical spectrometry methods. The Hall mobility of free electrons decreases from 600 to 150 cm2 V−1 s−1 in the CVD grown sample with the lowest N content and from 300 to 100 cm2 V−1 s−1 in highly doped HPHT grown samples in the temperature range of 550–900 K. At T = (900–1100) K, the mobility decreases to 50 cm2 V−1 s−1 in highly doped samples. The activation energies of electrical conductivity Ea and impurity-to-band energies of nitrogen donors ED decrease with increasing N concentration in the ranges (1.55–1.32) and (1.63–1.33) eV, respectively. The lowest compensation ratio k ∼ 1% in the moderately doped CVD diamond is unique for n-type diamonds. Typical values of k in highly N-doped crystals are in the range of 10%–20%, facilitating the use of N-doped diamonds in durable high-temperature electronic devices.
- Open Access
Microwave Diamond-Based HBAR as a Highly Sensitive Sensor for Multiple Applications: Acoustic Attenuation in the Mo Film
The application of microwave diamond-based HBAR as a sensor of microwave acoustic attenuation α was considered, using the Mo film as an object of research. A multilayered piezoelectric structure, as the Al/Al0.73Sc0.27N/Mo/(100) diamond/Mo, was produced using aluminum–scandium nitride composition, and was studied in detail for a number of the Mo films with different thicknesses obtained by magnetron deposition. The operational frequency band of 3.3 … 18 GHz was used. It was found that the dependence of the resonant frequency shift vs. the h(Mo) thickness for all the overtones to be investigated was linear. For a given sensor, it was found that the mass sensitivity per unit area rm was equal to −26 × 10−12 and −8.7 × 10−12 g/(cm2∙Hz) at 6.0 GHz and 18.3 GHz, respectively. The frequency dependencies of quality factor Q, which changed as a result of Mo film deposition, were considered as the basic experimental data. A method for extracting the α(Mo) values was proposed. The Q-factor under the complete deposition of Mo film was 936 nm, and dropped moderately to ~25%. Such values were enough for an aim of the given experiment. The α(f) in molybdenum was obtained, and demonstrated a dependence that was close to quadratic, corresponding to the Akhiezer attenuation law.
Open AccessMicrowave Diamond-Based HBAR as a Highly Sensitive Sensor for Multiple Applications: Acoustic Attenuation in the Mo Film
The application of microwave diamond-based HBAR as a sensor of microwave acoustic attenuation α was considered, using the Mo film as an object of research. A multilayered piezoelectric structure, as the Al/Al0.73Sc0.27N/Mo/(100) diamond/Mo, was produced using aluminum–scandium nitride composition, and was studied in detail for a number of the Mo films with different thicknesses obtained by magnetron deposition. The operational frequency band of 3.3 … 18 GHz was used. It was found that the dependence of the resonant frequency shift vs. the h(Mo) thickness for all the overtones to be investigated was linear. For a given sensor, it was found that the mass sensitivity per unit area rm was equal to −26 × 10−12 and −8.7 × 10−12 g/(cm2∙Hz) at 6.0 GHz and 18.3 GHz, respectively. The frequency dependencies of quality factor Q, which changed as a result of Mo film deposition, were considered as the basic experimental data. A method for extracting the α(Mo) values was proposed. The Q-factor under the complete deposition of Mo film was 936 nm, and dropped moderately to ~25%. Such values were enough for an aim of the given experiment. The α(f) in molybdenum was obtained, and demonstrated a dependence that was close to quadratic, corresponding to the Akhiezer attenuation law.
- 1 January 2023
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 66 (10) , 38-43
COMPENSATION RATIO OF ACCEPTOR CENTERS IN DIFFERENT GROWTH SECTORS OF BORON-DOPED HPHT DIAMOND
Создание элементов силовой алмазной электроники, рассчитанных на высокий интегральный ток, требует использования активных подложек с низким электрическим сопротивлением и низким содержанием дефектов кристаллической решетки. Наиболее перспективным материалом для создания таких подложек является легированный бором алмаз, выращенный методом температурного градиента при высоком давлении и температуре. Неполная ионизация акцепторных центров в алмазе при комнатной температуре приводит к тому, что степень компенсации данных центров оказывает значительное влияние на концентрацию свободных носителей в материале, а, следовательно, и на его проводимость. В данной работе исследовались температурные зависимости электропроводности и эффекта Холла среднелегированного бором алмаза в разных секторах роста кристалла. Показано, что степень компенсации в секторе роста {111} на 2-3 порядка выше по сравнению с секторами {001} и {311}. В связи с этим электропроводность секторов {001} и {311} оказалась в ~25 раз выше, чем в секторе {111}, при том, что общая концентрация бора в секторе {111} примерно в 10 раз выше. Таким образом, вероятность образования донорных центров в секторах {001} и {311} более чем в 100 раз ниже по сравнению с сектором {111}. Полученные результаты говорят о том, что наиболее перспективным с точки зрения создания электронных устройств являются пластины, вырезанные из секторов {001} и {311}, при условии достижения достаточно высокой концентрации бора и сохранения низкой концентрации доноров. Для цитирования: Приходько Д.Д., Тимошенко В.О., Тарелкин С.А., Кузнецов М.С., Лупарев Н.В., Бланк В.Д. Степень компенсации акцепторов в легированном бором HPHT алмазе в разных секторах роста. Изв. вузов. Химия и хим. технология. 2023. Т. 66. Вып. 10. С. 38-43. DOI: 10.6060/ivkkt.20236610.7y.
- 1 January 2023
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 66 (10) , 38-43
COMPENSATION RATIO OF ACCEPTOR CENTERS IN DIFFERENT GROWTH SECTORS OF BORON-DOPED HPHT DIAMOND
Создание элементов силовой алмазной электроники, рассчитанных на высокий интегральный ток, требует использования активных подложек с низким электрическим сопротивлением и низким содержанием дефектов кристаллической решетки. Наиболее перспективным материалом для создания таких подложек является легированный бором алмаз, выращенный методом температурного градиента при высоком давлении и температуре. Неполная ионизация акцепторных центров в алмазе при комнатной температуре приводит к тому, что степень компенсации данных центров оказывает значительное влияние на концентрацию свободных носителей в материале, а, следовательно, и на его проводимость. В данной работе исследовались температурные зависимости электропроводности и эффекта Холла среднелегированного бором алмаза в разных секторах роста кристалла. Показано, что степень компенсации в секторе роста {111} на 2-3 порядка выше по сравнению с секторами {001} и {311}. В связи с этим электропроводность секторов {001} и {311} оказалась в ~25 раз выше, чем в секторе {111}, при том, что общая концентрация бора в секторе {111} примерно в 10 раз выше. Таким образом, вероятность образования донорных центров в секторах {001} и {311} более чем в 100 раз ниже по сравнению с сектором {111}. Полученные результаты говорят о том, что наиболее перспективным с точки зрения создания электронных устройств являются пластины, вырезанные из секторов {001} и {311}, при условии достижения достаточно высокой концентрации бора и сохранения низкой концентрации доноров. Для цитирования: Приходько Д.Д., Тимошенко В.О., Тарелкин С.А., Кузнецов М.С., Лупарев Н.В., Бланк В.Д. Степень компенсации акцепторов в легированном бором HPHT алмазе в разных секторах роста. Изв. вузов. Химия и хим. технология. 2023. Т. 66. Вып. 10. С. 38-43. DOI: 10.6060/ivkkt.20236610.7y.
- 7 November 2022
- Published by AIP Publishing in Applied Physics Letters
- Vol. 121 (19) , 194102
Microwave acoustic studies of materials in diamond anvil cell under high pressure
This paper presents an integrated measuring system combining a diamond anvil cell (DAC) and a high overtone bulk acoustic resonator (HBAR) operating at the microwave frequency band as 2.8–8.8 GHz. We have studied several metallic (W, Zr) and semiconductor (Si) samples under pressure up to ∼16 GPa. As an HBAR, we have used the “Al/Al0.72Sc0.28N/Mo/(100) diamond” structure utilizing a piezoelectric aluminum–scandium nitride film. We have observed that under pressure, the Q-factor of the HBAR decreases but remains at the value of 2500–3000, which is suitable for our experiments. It is demonstrated that the above system can be used for studying the behavior of various solids under high pressure, the pressure-induced phase transition in Zr, the registration of plastic deformations, and their relaxation in metals. Here, we discussed the phenomenon of an acoustic wave passing through a tungsten layer under a pressure of ∼5.5 GPa. The integrated DAC&HBAR measuring system has demonstrated some practical advantages over known ultrasonic systems combined with the DAC as the possibility of applying a microwave operational frequency, the measurement of a Q-factor change under pressure, and the miniature size of a sensitive HBAR element. The application of the built-in DAC&HBAR system will hopefully allow more accurate studies on materials in the GPa pressure range of a DAC.
- 7 November 2022
- Published by AIP Publishing in Applied Physics Letters
- Vol. 121 (19) , 194102
Microwave acoustic studies of materials in diamond anvil cell under high pressure
This paper presents an integrated measuring system combining a diamond anvil cell (DAC) and a high overtone bulk acoustic resonator (HBAR) operating at the microwave frequency band as 2.8–8.8 GHz. We have studied several metallic (W, Zr) and semiconductor (Si) samples under pressure up to ∼16 GPa. As an HBAR, we have used the “Al/Al0.72Sc0.28N/Mo/(100) diamond” structure utilizing a piezoelectric aluminum–scandium nitride film. We have observed that under pressure, the Q-factor of the HBAR decreases but remains at the value of 2500–3000, which is suitable for our experiments. It is demonstrated that the above system can be used for studying the behavior of various solids under high pressure, the pressure-induced phase transition in Zr, the registration of plastic deformations, and their relaxation in metals. Here, we discussed the phenomenon of an acoustic wave passing through a tungsten layer under a pressure of ∼5.5 GPa. The integrated DAC&HBAR measuring system has demonstrated some practical advantages over known ultrasonic systems combined with the DAC as the possibility of applying a microwave operational frequency, the measurement of a Q-factor change under pressure, and the miniature size of a sensitive HBAR element. The application of the built-in DAC&HBAR system will hopefully allow more accurate studies on materials in the GPa pressure range of a DAC.
- Open Access
- 1 January 2022
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 65 (11) , 49-58
METHOD OF MICROWAVE ACOUSTIC RESEARCH OF MATERIALS UNDER THE HIGH PRESSURE
В статье рассмотрено устройство новой интегрированной измерительной системы (ИИС) "Mногообертонный СВЧ ОАВ-резонатор + камера высокого давления на алмазных наковальнях" и ее применение для исследования изменений акустических свойств образцов бумаги и поликристаллического молибдена под действием высокого давления. При создании ИИС для синтеза пьезоэлектрических пленок нитрида алюминия-скандия использовали метод магнетронного осаждения. Контроль качества и толщины пленок осуществляли методами рентгеноструктурного анализа и атомно-силовой микроскопии. Впервые показано, что ОАВ-резонатор в составе ИИС имеет хорошие операционные характеристики в области СВЧ вплоть до 8,8 ГГц при воздействии на образцы высокого давления. Уменьшение добротности ОАВ-резонатора как чувствительного элемента с ростом давления до 16 ГПа происходило до значений ~2500 – 3000, что вполне достаточно для точных измерений частот акустических обертонов. Продемонстрированы возможности применения ИИС для исследований особенностей поведения твердых тел при высоких давлениях и регистрации пластических деформаций в металлах. Было получено, что зависимость относительного сдвига частот обертонов от давления при сжатии образца бумаги имеет линейный характер. Благодаря этому выполнена калибровка камеры высокого давления на алмазных наковальнях, используя метод комбинационного рассеяния света. Получено, что сдвиг частот обертонов позволяет более точно определять напряжения в алмазной наковальне до 5 ГПа. При сжатии образца поликристаллического молибдена обнаружены явления пластической деформации и ползучести, а также сквозного прохождения акустической волны через образец, начиная с давления 3 ГПа. Полученные результаты будут полезны для исследователей, студентов и аспирантов в области физики высоких давлений и физической акустики. Для цитирования: Сорокин Б.П., Асафьев Н.О., Овсянников Д.А., Квашнин Г.М., Лупарев Н.В., Голованов А.В., Попов М.Ю., Аксененков В.В., Бланк В.Д. Метод СВЧ акустического исследования материалов под высоким давлением. Изв. вузов. Химия и хим. технология. 2022. Т. 65. Вып. 11. С. 49-58. DOI: 10.6060/ivkkt.20226511.4y.
- 1 January 2022
- Published by Ivanovo State University of Chemistry and Technology in ChemChemTech
- Vol. 65 (11) , 49-58
Open AccessMETHOD OF MICROWAVE ACOUSTIC RESEARCH OF MATERIALS UNDER THE HIGH PRESSURE
В статье рассмотрено устройство новой интегрированной измерительной системы (ИИС) "Mногообертонный СВЧ ОАВ-резонатор + камера высокого давления на алмазных наковальнях" и ее применение для исследования изменений акустических свойств образцов бумаги и поликристаллического молибдена под действием высокого давления. При создании ИИС для синтеза пьезоэлектрических пленок нитрида алюминия-скандия использовали метод магнетронного осаждения. Контроль качества и толщины пленок осуществляли методами рентгеноструктурного анализа и атомно-силовой микроскопии. Впервые показано, что ОАВ-резонатор в составе ИИС имеет хорошие операционные характеристики в области СВЧ вплоть до 8,8 ГГц при воздействии на образцы высокого давления. Уменьшение добротности ОАВ-резонатора как чувствительного элемента с ростом давления до 16 ГПа происходило до значений ~2500 – 3000, что вполне достаточно для точных измерений частот акустических обертонов. Продемонстрированы возможности применения ИИС для исследований особенностей поведения твердых тел при высоких давлениях и регистрации пластических деформаций в металлах. Было получено, что зависимость относительного сдвига частот обертонов от давления при сжатии образца бумаги имеет линейный характер. Благодаря этому выполнена калибровка камеры высокого давления на алмазных наковальнях, используя метод комбинационного рассеяния света. Получено, что сдвиг частот обертонов позволяет более точно определять напряжения в алмазной наковальне до 5 ГПа. При сжатии образца поликристаллического молибдена обнаружены явления пластической деформации и ползучести, а также сквозного прохождения акустической волны через образец, начиная с давления 3 ГПа. Полученные результаты будут полезны для исследователей, студентов и аспирантов в области физики высоких давлений и физической акустики. Для цитирования: Сорокин Б.П., Асафьев Н.О., Овсянников Д.А., Квашнин Г.М., Лупарев Н.В., Голованов А.В., Попов М.Ю., Аксененков В.В., Бланк В.Д. Метод СВЧ акустического исследования материалов под высоким давлением. Изв. вузов. Химия и хим. технология. 2022. Т. 65. Вып. 11. С. 49-58. DOI: 10.6060/ivkkt.20226511.4y.