Emil Żmuda
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Emil Żmuda has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Andrzej Radomski
Department of Wood Science and Wood Protection, Institute of Wood Sciences and Furniture, Warsaw University of Life Sciences in Warsaw, Nowoursynowska 166 Street, 02-787 Warsaw, Poland
3 shared publications - Andrzej Antczak
Institute of Wood Sciences and Furniture, Warsaw University of Life Sciences—SGGW, 159 Nowoursynowska St., 02-776 Warsaw, Poland
1 shared publication - Anita Wronka
Institute of Wood Science and Furniture, Warsaw University of Life Sciences—SGGW, Nowoursynowska St. 159, 02-776 Warsaw, Poland
1 shared publication - Dominika Szadkowska
Department of Wood Science and Wood Protection, Institute of Wood Sciences and Furniture, Warsaw University of Life Sciences, 166 Nowoursynowska St., 02-787 Warsaw, Poland
1 shared publication - Florentyna Akus-Szylberg
Warsaw University of Life Science – SGGW Department of Wood Science and Wood Protection, Institute of Wood Sciences and Furniture
1 shared publication - Grzegorz Kowaluk
Department of Technology and Entrepreneurship in Wood Industry, Institute of Wood Sciences and Furniture, Warsaw University of Life Sciences—SGGW, Nowoursynowska St. 159, 02-787 Warsaw, Poland
1 shared publication
Latest Publications
- Open Access
Influence of In Situ Polymerization on the Compressive Strength of Scots Pine (Pinus sylvestris L.) Recovered from Demolition Timber and Two Forest-Sourced Species: European Beech (Fagus sylvatica) and Black Alder (Alnus glutinosa)
This study investigated the effect of in situ polymerization on the compressive strength of demolition-derived Scots pine, European beech, and black alder wood. The treatment applied was based on previously confirmed in situ polymerization systems in wood, which are known to lead to polymer formation and composite-like structures. In this study, we assumed similar behavior and focused on a mechanical evaluation of the modified wood. Three different polymer systems were applied to evaluate differences in performance. After modification, the compressive strength levels increased by 60% in beech, 119% in alder, and 150% in pine, with corresponding increases in density and weight percent gain (WPG). The highest relative improvement was observed in the least dense species, pine. The findings suggest that polymer treatment can significantly enhance the mechanical properties, likely due to the incorporation of polymer into the wood matrix; however, this inference is based on indirect physical evidence.
Open AccessInfluence of In Situ Polymerization on the Compressive Strength of Scots Pine (Pinus sylvestris L.) Recovered from Demolition Timber and Two Forest-Sourced Species: European Beech (Fagus sylvatica) and Black Alder (Alnus glutinosa)
This study investigated the effect of in situ polymerization on the compressive strength of demolition-derived Scots pine, European beech, and black alder wood. The treatment applied was based on previously confirmed in situ polymerization systems in wood, which are known to lead to polymer formation and composite-like structures. In this study, we assumed similar behavior and focused on a mechanical evaluation of the modified wood. Three different polymer systems were applied to evaluate differences in performance. After modification, the compressive strength levels increased by 60% in beech, 119% in alder, and 150% in pine, with corresponding increases in density and weight percent gain (WPG). The highest relative improvement was observed in the least dense species, pine. The findings suggest that polymer treatment can significantly enhance the mechanical properties, likely due to the incorporation of polymer into the wood matrix; however, this inference is based on indirect physical evidence.
- Open Access
Effect of Styrene Polymerization on the Bondability of Beech and Alder Wood with Different Adhesives
This study aimed to evaluate the bondability of beech and alder wood modified through styrene polymerization within the wood lumen. Unmodified wood samples served as the reference material. Bondability was tested using four adhesive types commonly used in wood technology: polyvinyl acetate (PVAc), urea-formaldehyde (UF), phenol-resorcinol-formaldehyde (PRF), and epoxy resin. In addition to shear strength measurements, the adhesive density profile was also assessed. Results indicated that styrene modification generally reduced wood bondability, with reductions in shear strength ranging from 8% to 23% for beech wood and 1.6% to 29% for alder wood, depending on the adhesive type. The only exception was observed with the epoxy adhesive, which showed a 13% improvement in bonding quality for modified wood. These findings suggest that while styrene modification may enhance specific properties of wood, it can adversely affect its adhesion performance with some adhesive systems, except epoxy, which displayed improved compatibility with styrene-modified wood. The study offers insights for selecting suitable adhesives when using modified wood in structural applications.
Open AccessEffect of Styrene Polymerization on the Bondability of Beech and Alder Wood with Different Adhesives
This study aimed to evaluate the bondability of beech and alder wood modified through styrene polymerization within the wood lumen. Unmodified wood samples served as the reference material. Bondability was tested using four adhesive types commonly used in wood technology: polyvinyl acetate (PVAc), urea-formaldehyde (UF), phenol-resorcinol-formaldehyde (PRF), and epoxy resin. In addition to shear strength measurements, the adhesive density profile was also assessed. Results indicated that styrene modification generally reduced wood bondability, with reductions in shear strength ranging from 8% to 23% for beech wood and 1.6% to 29% for alder wood, depending on the adhesive type. The only exception was observed with the epoxy adhesive, which showed a 13% improvement in bonding quality for modified wood. These findings suggest that while styrene modification may enhance specific properties of wood, it can adversely affect its adhesion performance with some adhesive systems, except epoxy, which displayed improved compatibility with styrene-modified wood. The study offers insights for selecting suitable adhesives when using modified wood in structural applications.
- 26 December 2023
- Published by Index Copernicus in Annals of WULS, Forestry and Wood Technology
- Vol. 124, 99-106
Influence of selected treatment methods on the dry residue and sugars content extracted from wheat and rye bran.
In this paper 1% NaOH extraction and 1% NaOH extraction with α-amylase pre-treatment were conducted on wheat and rye bran. Different times of reaction (0.5, 1, 2 and 4 h) and different temperatures (40C, 45C, 50C and 95C) of process were applied during experiments. After the process, dry residue content was calculated. Additionally, monosaccharides content in liquid was determined after α-amylase pre-treatment and 1% NaOH extraction. Monosaccharides content (glucose, xylose and arabinose) after acid hydrolysis of obtained liquids was determined by the HPLC technique. Obtained results showed that there was a positive correlation between time, temperature and content of compounds extracted by 1% NaOH solution. The lowest dry residue content for wheat and rye bran after 1% NaOH extraction was obtained at 95 C during 4 hours of conducting the process (24.70.1 and 18.42.8 respectively). Additional pre-treatment by α-amylase increased solubility of compounds included in bran, especially for wheat bran. α-amylase influenced not only starch solubility but also other compounds from bran. The next advantage of pre-treatment by α-amylase was easier access to remaining sugars inside the bran, which in the form of xylose and arabinose can be obtained.
- 26 December 2023
- Published by Index Copernicus in Annals of WULS, Forestry and Wood Technology
- Vol. 124, 99-106
Influence of selected treatment methods on the dry residue and sugars content extracted from wheat and rye bran.
In this paper 1% NaOH extraction and 1% NaOH extraction with α-amylase pre-treatment were conducted on wheat and rye bran. Different times of reaction (0.5, 1, 2 and 4 h) and different temperatures (40C, 45C, 50C and 95C) of process were applied during experiments. After the process, dry residue content was calculated. Additionally, monosaccharides content in liquid was determined after α-amylase pre-treatment and 1% NaOH extraction. Monosaccharides content (glucose, xylose and arabinose) after acid hydrolysis of obtained liquids was determined by the HPLC technique. Obtained results showed that there was a positive correlation between time, temperature and content of compounds extracted by 1% NaOH solution. The lowest dry residue content for wheat and rye bran after 1% NaOH extraction was obtained at 95 C during 4 hours of conducting the process (24.70.1 and 18.42.8 respectively). Additional pre-treatment by α-amylase increased solubility of compounds included in bran, especially for wheat bran. α-amylase influenced not only starch solubility but also other compounds from bran. The next advantage of pre-treatment by α-amylase was easier access to remaining sugars inside the bran, which in the form of xylose and arabinose can be obtained.
- 30 June 2020
- Published by Index Copernicus in Annals of WULS, Forestry and Wood Technology
- Vol. 110, 35-40
Swelling and water resistance of black poplar wood (Populus nigra L.) modified by polymerisation in lumen with styrene
- 30 June 2020
- Published by Index Copernicus in Annals of WULS, Forestry and Wood Technology
- Vol. 110, 35-40
Swelling and water resistance of black poplar wood (Populus nigra L.) modified by polymerisation in lumen with styrene