Basak Tuna
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Basak Tuna has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Hadj Benkreira
Department of Chemical Engineering, University of Bradford, Bradford, UK
3 shared publications Guralp Ozkoc
Department of Chemical Engineering Kocaeli University 41380 Kocaeli Turkey
1 shared publication- Guralp Ozkoc
Kocaeli University
1 shared publication Humeyra Sirin
Department of Chemical Engineering Kocaeli University 41380 Kocaeli Turkey
1 shared publication
Latest Publications
- Open Access
Investigation into the Reprocessability of Polycarbonate/Organoclay Nanocomposites
With the rapid expansion in the use of nanomaterials, ensuring their reprocessability has become a critical consideration for the sustainable development of polymer-based nanocomposites. In this study, the effects of repetitive thermo-mechanical processing cycles on the properties of polycarbonate (PC)/organoclay nanocomposites, as well as the impact of reactive extrusion of reprocessed PC/organoclay nanocomposites using a chain extender, were investigated for the first time. The nanocomposites were processed three times using a twin-screw extruder, and a multi-anhydride functional chain extender was incorporated to counteract the thermo-mechanical degradation observed after the third extrusion cycle. Morphological analysis indicated that the delamination of clay nanolayers within the polymer matrix was slightly enhanced with increasing extrusion cycles, while the addition of the chain extender further promoted nanoclay exfoliation. Despite the improved clay dispersion in PC, both rheological and tensile measurements revealed the detrimental effects of repeated reprocessing on the nanocomposites. The chain extender effectively mitigated this degradation by relinking cleaved polymer chains; consequently, the complex viscosity and storage modulus at 0.1 Hz of the three-times-extruded nanocomposite increased by 248% and 426%, respectively, following chain extender incorporation. The effectiveness of the chain extender was further evidenced by a 27% enhancement in tensile strength. The glass transition temperatures of the samples were not significantly affected by either the extrusion cycles or the addition of the chain extender. The thermal stability of the nanocomposites decreased with increasing numbers of extrusion cycles; however, the incorporation of the chain extender imparted enhanced resistance to thermal degradation, as confirmed by thermogravimetric analysis.
Open AccessInvestigation into the Reprocessability of Polycarbonate/Organoclay Nanocomposites
With the rapid expansion in the use of nanomaterials, ensuring their reprocessability has become a critical consideration for the sustainable development of polymer-based nanocomposites. In this study, the effects of repetitive thermo-mechanical processing cycles on the properties of polycarbonate (PC)/organoclay nanocomposites, as well as the impact of reactive extrusion of reprocessed PC/organoclay nanocomposites using a chain extender, were investigated for the first time. The nanocomposites were processed three times using a twin-screw extruder, and a multi-anhydride functional chain extender was incorporated to counteract the thermo-mechanical degradation observed after the third extrusion cycle. Morphological analysis indicated that the delamination of clay nanolayers within the polymer matrix was slightly enhanced with increasing extrusion cycles, while the addition of the chain extender further promoted nanoclay exfoliation. Despite the improved clay dispersion in PC, both rheological and tensile measurements revealed the detrimental effects of repeated reprocessing on the nanocomposites. The chain extender effectively mitigated this degradation by relinking cleaved polymer chains; consequently, the complex viscosity and storage modulus at 0.1 Hz of the three-times-extruded nanocomposite increased by 248% and 426%, respectively, following chain extender incorporation. The effectiveness of the chain extender was further evidenced by a 27% enhancement in tensile strength. The glass transition temperatures of the samples were not significantly affected by either the extrusion cycles or the addition of the chain extender. The thermal stability of the nanocomposites decreased with increasing numbers of extrusion cycles; however, the incorporation of the chain extender imparted enhanced resistance to thermal degradation, as confirmed by thermogravimetric analysis.
- Open Access
- 21 November 2024
- Published by Elsevier in Engineering Science and Technology, an International Journal
- Vol. 60
Chain extension of poly(butylene terephthalate)/organically modified clay nanocomposites
- 21 November 2024
- Published by Elsevier in Engineering Science and Technology, an International Journal
- Vol. 60
Open AccessChain extension of poly(butylene terephthalate)/organically modified clay nanocomposites
- 1 February 2023
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry B
- Vol. 17 (1) , 196-205
Reactive Extrusion of Recycled Polycarbonate Using Chain Extenders
Electronic waste (e-waste) problem becomes more critical due to increasing demand on upgrading of electrical-electronic devices in accordance with the latest technology nowadays. Polycarbonate (PC) is one of the most used plastics to produce computers, mobile phones and televisions thus recovering of PC wastes to develop new value-adding products has been an important task. The challenge of the PC recycling is thermal degradation under multiple thermo-mechanical processing cycles, which deteriorates molecular weight and properties of the polymer. In this study, a multi-functional anhydride chain extender (ANHY) and a multi-functional epoxy chain extender (EPOX) were used to offset thermal degradation of recycled PC (rPC) during extrusion. The effect of chain extenders on the properties of resulting materials was evaluated by rheology, tensile test, thermogravimetric analysis (TGA), dynamic mechanical analysis (DMA) and differential scanning calorimetry (DSC). Both types of chain extenders enhanced the viscoelastic and mechanical properties of rPC, however ANHY had much higher chain extension reactivity than EPOX. ANHY increased complex viscosity by 58% and tensile modulus by 39%, whilst EPOX showed 26% increment in complex viscosity and 10% enhancement in tensile modulus on the base rPC. The formation of long chain branching in the samples containing chain extenders was observed from the rheology tests. TGA results also confirmed the efficiency of ANHY chain extender that shifted decomposition temperature of rPC to higher value than that of EPOX. The incorporation of chain extenders slightly increased glass transition temperature (Tg) of rPC in DMA and DSC test results.
- 1 February 2023
- Published by Pleiades Publishing Ltd in Russian Journal of Physical Chemistry B
- Vol. 17 (1) , 196-205
Reactive Extrusion of Recycled Polycarbonate Using Chain Extenders
Electronic waste (e-waste) problem becomes more critical due to increasing demand on upgrading of electrical-electronic devices in accordance with the latest technology nowadays. Polycarbonate (PC) is one of the most used plastics to produce computers, mobile phones and televisions thus recovering of PC wastes to develop new value-adding products has been an important task. The challenge of the PC recycling is thermal degradation under multiple thermo-mechanical processing cycles, which deteriorates molecular weight and properties of the polymer. In this study, a multi-functional anhydride chain extender (ANHY) and a multi-functional epoxy chain extender (EPOX) were used to offset thermal degradation of recycled PC (rPC) during extrusion. The effect of chain extenders on the properties of resulting materials was evaluated by rheology, tensile test, thermogravimetric analysis (TGA), dynamic mechanical analysis (DMA) and differential scanning calorimetry (DSC). Both types of chain extenders enhanced the viscoelastic and mechanical properties of rPC, however ANHY had much higher chain extension reactivity than EPOX. ANHY increased complex viscosity by 58% and tensile modulus by 39%, whilst EPOX showed 26% increment in complex viscosity and 10% enhancement in tensile modulus on the base rPC. The formation of long chain branching in the samples containing chain extenders was observed from the rheology tests. TGA results also confirmed the efficiency of ANHY chain extender that shifted decomposition temperature of rPC to higher value than that of EPOX. The incorporation of chain extenders slightly increased glass transition temperature (Tg) of rPC in DMA and DSC test results.
- 31 December 2021
- Published by Bilecik Seyh Edebali Universitesi Fen Bilimleri Dergisi in Bilecik Şeyh Edebali Üniversitesi Fen Bilimleri Dergisi
- Vol. 8 (2) , 882-892
Investigation of Effects of a Polymeric Chain Extender on the Properties of Recycled Poly (Butylene Terephthalate)
Poli(bütilen tereftalat) (PBT) günümüzde en fazla kullanılan poliesterlerdendir, ancak PBT atıkların geri dönüşüm kapsamında katma değerli ürünlere dönüşmesine yönelik girişimler hala sınırlıdır. PBT geri dönüşümünün en önemli zorluklarından birisi çoklu eriyik işleme döngüleri sırasındaki termal bozunma olup, polimerin molekül ağırlığı ve özelliklerinde kayıplara yol açmaktadır. Bu çalışmada geri dönüştürülmüş PBT (Gd. PBT) farklı yükleme oranındaki (%ağ. 0.5, 1, 1.5) polimerik bir zincir uzatıcı (Joncryl ADR 4368) ile çift vidalı ekstrüderde harmanlanmıştır. Örneklerin reolojik, mekanik ve termal özellikleri farklı karakterizasyon yöntemleri ile incelenmiştir. Reolojik sonuçlar zincir uzatıcının eklenmesiyle kopan zincirlerin tekrar bağlanarak Gd. PBT’nin viskoelastik özelliklerinin geliştiğini göstermiştir. Zincir uzatıcının Gd. PBT’nin özelliklerine olan önemli etkisi çekme testi sonuçlarından da doğrulanmıştır. Zincir uzatıcı içeren örneklerin elastik modül ve çekme dayanımları artış gösterirken, kopmadaki uzama değerleri zincir dallanmasına bağlı olarak düşmüştür. Zincir uzatıcının örneklerin dallanmış yapısına etkisi düşük kristalinite değerlerinden de gözlemlenmiştir. Termogravimetrik analiz zincir uzatıcının Gd. PBT’nin termal bozunma sıcaklığını arttırdığını göstermiştir. Zincir uzatıcı içeren örneklerin özelliklerindeki iyileşme artan zincir uzatıcı konsantrasyonu ile daha belirgin olmuştur.
- 31 December 2021
- Published by Bilecik Seyh Edebali Universitesi Fen Bilimleri Dergisi in Bilecik Şeyh Edebali Üniversitesi Fen Bilimleri Dergisi
- Vol. 8 (2) , 882-892
Investigation of Effects of a Polymeric Chain Extender on the Properties of Recycled Poly (Butylene Terephthalate)
Poli(bütilen tereftalat) (PBT) günümüzde en fazla kullanılan poliesterlerdendir, ancak PBT atıkların geri dönüşüm kapsamında katma değerli ürünlere dönüşmesine yönelik girişimler hala sınırlıdır. PBT geri dönüşümünün en önemli zorluklarından birisi çoklu eriyik işleme döngüleri sırasındaki termal bozunma olup, polimerin molekül ağırlığı ve özelliklerinde kayıplara yol açmaktadır. Bu çalışmada geri dönüştürülmüş PBT (Gd. PBT) farklı yükleme oranındaki (%ağ. 0.5, 1, 1.5) polimerik bir zincir uzatıcı (Joncryl ADR 4368) ile çift vidalı ekstrüderde harmanlanmıştır. Örneklerin reolojik, mekanik ve termal özellikleri farklı karakterizasyon yöntemleri ile incelenmiştir. Reolojik sonuçlar zincir uzatıcının eklenmesiyle kopan zincirlerin tekrar bağlanarak Gd. PBT’nin viskoelastik özelliklerinin geliştiğini göstermiştir. Zincir uzatıcının Gd. PBT’nin özelliklerine olan önemli etkisi çekme testi sonuçlarından da doğrulanmıştır. Zincir uzatıcı içeren örneklerin elastik modül ve çekme dayanımları artış gösterirken, kopmadaki uzama değerleri zincir dallanmasına bağlı olarak düşmüştür. Zincir uzatıcının örneklerin dallanmış yapısına etkisi düşük kristalinite değerlerinden de gözlemlenmiştir. Termogravimetrik analiz zincir uzatıcının Gd. PBT’nin termal bozunma sıcaklığını arttırdığını göstermiştir. Zincir uzatıcı içeren örneklerin özelliklerindeki iyileşme artan zincir uzatıcı konsantrasyonu ile daha belirgin olmuştur.
- 19 April 2019
- Published by Wiley in Polymer Engineering & Science
- Vol. 59 (6) , 1233-1241
Chain extension of polyamide 6/organoclay nanocomposites
Thermal degradation of polyamide 6 (PA6)/organoclay nanocomposites is a serious impediment to wider applications of these nanocomposites. In this study, a solution is proposed based on the well‐established use of chain extenders. As in PA6, thermal degradation, in the absence of moisture, produces broken polymer chains with amide end groups, a chain extender with anhydride functionalities, known to be strongly reactive with amide groups, was used to reconnect the chains. Experiments conducted using a laboratory twin‐screw extruder were first checked, through transmission electron microscopy observations, to have produced good organoclay intercalation and exfoliation into PA6. Following from this, samples with the chain extender added were produced and characterized. The data obtained were conclusive in the effectiveness of the chain extender: for the chain extended nanocomposites, there is an enhancement in the value of the complex viscosity by 7 times and in the storage modulus by 88 times, while the tensile modulus increased by 57% compared with the neat PA6. The nonchain extended nanocomposite achieved in comparison an enhancement of 2 times the value of the complex viscosity and 19 times the storage modulus while the tensile modulus increased by 53% compared to the neat PA6. These data provide conclusive proof on the rationale that anhydride functionalities should be sought when developing chain extenders for PA6 nanocomposites. POLYM. ENG. SCI., 59:1233–1241 2019. © 2019 Society of Plastics Engineers
- 19 April 2019
- Published by Wiley in Polymer Engineering & Science
- Vol. 59 (6) , 1233-1241
Chain extension of polyamide 6/organoclay nanocomposites
Thermal degradation of polyamide 6 (PA6)/organoclay nanocomposites is a serious impediment to wider applications of these nanocomposites. In this study, a solution is proposed based on the well‐established use of chain extenders. As in PA6, thermal degradation, in the absence of moisture, produces broken polymer chains with amide end groups, a chain extender with anhydride functionalities, known to be strongly reactive with amide groups, was used to reconnect the chains. Experiments conducted using a laboratory twin‐screw extruder were first checked, through transmission electron microscopy observations, to have produced good organoclay intercalation and exfoliation into PA6. Following from this, samples with the chain extender added were produced and characterized. The data obtained were conclusive in the effectiveness of the chain extender: for the chain extended nanocomposites, there is an enhancement in the value of the complex viscosity by 7 times and in the storage modulus by 88 times, while the tensile modulus increased by 57% compared with the neat PA6. The nonchain extended nanocomposite achieved in comparison an enhancement of 2 times the value of the complex viscosity and 19 times the storage modulus while the tensile modulus increased by 53% compared to the neat PA6. These data provide conclusive proof on the rationale that anhydride functionalities should be sought when developing chain extenders for PA6 nanocomposites. POLYM. ENG. SCI., 59:1233–1241 2019. © 2019 Society of Plastics Engineers
- 17 October 2018
- Published by Wiley in Polymer Engineering & Science
- Vol. 59 (s2) , E25-E31
Reactive Extrusion of Polyamide 6 Using a Novel Chain Extender
Polyamide 6 (PA6) is an important engineering thermoplastic, very widely used but prone to thermal degradation during extrusion at temperature not far from its melt temperature (220°C). Typically, and as measured in this study, PA6 extruded at temperature of 300°C shows a 40% decrease in tensile modulus compared with non‐extruded PA6. To rebuild PA6 molecular weight, the easiest and cheapest method is to use an appropriate chain extender. Many chain extenders have been used in the past but they are essentially suited to nucleophile induced degradation, targeting split PA6 chains carboxyl COOH and amine NH2 end groups. What have been lacking are effective chain extenders for thermally only induced degradation, i.e. for the practical cases where the PA6 is thoroughly dried before extrusion. For such a case, the degradation reaction mechanism dictates that the solution is to develop chain extenders that target the split PA6 chains amide CONH2 groups not the carboxyl COOH and amine NH2 end groups. As amide groups strongly react with anhydride functionalities, we test the effectiveness of a novel chain extender, Joncryl® ADR 3400, a styrene maleic anhydride copolymer with multiple, repeating anhydride functionality. Assessment of chain extension in this study is done as with previous work, using rheology, mechanical and thermal properties of PA6 extruded on its own and with the chain extender. The viscoelastic data conclusively show the efficacy of such chain extender with more than 10‐fold changes in the comparative values of the extruded sample storage modulus G’ and as much as an 85% increase in the tensile modulus. POLYM. ENG. SCI., 59:E25–E31, 2019. © 2018 Society of Plastics Engineers
- 17 October 2018
- Published by Wiley in Polymer Engineering & Science
- Vol. 59 (s2) , E25-E31
Reactive Extrusion of Polyamide 6 Using a Novel Chain Extender
Polyamide 6 (PA6) is an important engineering thermoplastic, very widely used but prone to thermal degradation during extrusion at temperature not far from its melt temperature (220°C). Typically, and as measured in this study, PA6 extruded at temperature of 300°C shows a 40% decrease in tensile modulus compared with non‐extruded PA6. To rebuild PA6 molecular weight, the easiest and cheapest method is to use an appropriate chain extender. Many chain extenders have been used in the past but they are essentially suited to nucleophile induced degradation, targeting split PA6 chains carboxyl COOH and amine NH2 end groups. What have been lacking are effective chain extenders for thermally only induced degradation, i.e. for the practical cases where the PA6 is thoroughly dried before extrusion. For such a case, the degradation reaction mechanism dictates that the solution is to develop chain extenders that target the split PA6 chains amide CONH2 groups not the carboxyl COOH and amine NH2 end groups. As amide groups strongly react with anhydride functionalities, we test the effectiveness of a novel chain extender, Joncryl® ADR 3400, a styrene maleic anhydride copolymer with multiple, repeating anhydride functionality. Assessment of chain extension in this study is done as with previous work, using rheology, mechanical and thermal properties of PA6 extruded on its own and with the chain extender. The viscoelastic data conclusively show the efficacy of such chain extender with more than 10‐fold changes in the comparative values of the extruded sample storage modulus G’ and as much as an 85% increase in the tensile modulus. POLYM. ENG. SCI., 59:E25–E31, 2019. © 2018 Society of Plastics Engineers
- 1 August 2017
- Published by Wiley in Polymer Engineering & Science
- Vol. 58 (7) , 1037-1042
Chain extension of recycled PA6
Recycling of polymers is a necessity in our intensively consuming polymer world but the nature of polymers is such that they are prone to thermal degradation when re‐extruded and this poses technical challenges to recycling. This article describes research that seeks to rebuild the structure of degraded PA6. We present data from controlled experiments with pristine pPA6 extruded to form a base recycle rPA6 to which we added two chain extenders, separately: one with anhydride multifunctionality (ANHY), highly reactive with amide groups and one with epoxy multifunctionality (EPOX), less reactive. We found from rheological data carried out in the linear viscoelastic region (so as to study structural changes) a striking difference in the ability of the chain extenders to rebuild structure: 306% increase in the complex viscosity of rPA6/ANHY compared to 25% in that of rPA6/EPOX of the base rPA6. Mechanical and thermal (DSC and TGA) tests confirmed the superior efficacy of the multifunctional anhydride chain extender. Beside the practical benefit that ensues from this research, it also provides a strategic platform to develop chain extenders for other degrading polymers on the basis of understanding the degradation chemical reaction and targeting the most reactive end group of the split chains. POLYM. ENG. SCI., 58:1037–1042, 2018. © 2017 Society of Plastics Engineers
- 1 August 2017
- Published by Wiley in Polymer Engineering & Science
- Vol. 58 (7) , 1037-1042
Chain extension of recycled PA6
Recycling of polymers is a necessity in our intensively consuming polymer world but the nature of polymers is such that they are prone to thermal degradation when re‐extruded and this poses technical challenges to recycling. This article describes research that seeks to rebuild the structure of degraded PA6. We present data from controlled experiments with pristine pPA6 extruded to form a base recycle rPA6 to which we added two chain extenders, separately: one with anhydride multifunctionality (ANHY), highly reactive with amide groups and one with epoxy multifunctionality (EPOX), less reactive. We found from rheological data carried out in the linear viscoelastic region (so as to study structural changes) a striking difference in the ability of the chain extenders to rebuild structure: 306% increase in the complex viscosity of rPA6/ANHY compared to 25% in that of rPA6/EPOX of the base rPA6. Mechanical and thermal (DSC and TGA) tests confirmed the superior efficacy of the multifunctional anhydride chain extender. Beside the practical benefit that ensues from this research, it also provides a strategic platform to develop chain extenders for other degrading polymers on the basis of understanding the degradation chemical reaction and targeting the most reactive end group of the split chains. POLYM. ENG. SCI., 58:1037–1042, 2018. © 2017 Society of Plastics Engineers
- 21 October 2016
- Published by Springer Nature in Journal of Polymers and the Environment
- Vol. 25 (4) , 983-993
Effects of Diisocyanate and Polymeric Epoxidized Chain Extenders on the Properties of Recycled Poly(Lactic Acid)
- 21 October 2016
- Published by Springer Nature in Journal of Polymers and the Environment
- Vol. 25 (4) , 983-993
Effects of Diisocyanate and Polymeric Epoxidized Chain Extenders on the Properties of Recycled Poly(Lactic Acid)
- 6 August 2014
- Published by Wiley in Advances in Polymer Technology
- Vol. 33 (S1)
The Effects of Thermomechanical Cycles on the Properties of PLA/TPS Blends
In this study, it is aimed to investigate the physical properties of poly(lactic acid)/thermoplastic starch (PLA/TPS) blends as a function of number of recycling (NOR) for different blend compositions. The flexural and impact properties, dynamic mechanical behavior, thermal transitions, thermal stability, phase, and fracture morphology are presented. Thermogravimetric analysis shows that the thermal stability of blends diminished by the increasing amount of TPS. It is revealed from differential scanning calorimetry results that the glass transition temperature (Tg) and melting temperature (Tm) are negatively affected by the NOR. Flexural and impact tests show that the mechanical properties are deteriorated by NOR. The TPS phase size becomes coarser with NOR as observed from scanning electron microscopy. It is concluded that the properties of PLA/TPS blends are very sensitive to NOR and the PLA/TPS concentration as well.
- 6 August 2014
- Published by Wiley in Advances in Polymer Technology
- Vol. 33 (S1)
The Effects of Thermomechanical Cycles on the Properties of PLA/TPS Blends
In this study, it is aimed to investigate the physical properties of poly(lactic acid)/thermoplastic starch (PLA/TPS) blends as a function of number of recycling (NOR) for different blend compositions. The flexural and impact properties, dynamic mechanical behavior, thermal transitions, thermal stability, phase, and fracture morphology are presented. Thermogravimetric analysis shows that the thermal stability of blends diminished by the increasing amount of TPS. It is revealed from differential scanning calorimetry results that the glass transition temperature (Tg) and melting temperature (Tm) are negatively affected by the NOR. Flexural and impact tests show that the mechanical properties are deteriorated by NOR. The TPS phase size becomes coarser with NOR as observed from scanning electron microscopy. It is concluded that the properties of PLA/TPS blends are very sensitive to NOR and the PLA/TPS concentration as well.