Aigul A. Sarkeeva
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Aigul A. Sarkeeva has a total of 33 co-authors. Here are the top co-authors by number of shared publications:
- Aleksey Kruglov
Russian Academy of Sciences
4 shared publications - Ramil Ya. Lutfullin
Институт проблем сверхпластичности металлов РАН, ул. Степана Халтурина, 39, 450001, Уфа, Россия; Уфимский государственный нефтяной технический университет, ул. Космонавтов, 1, 450064, г. Уфа, Россия
4 shared publications - Carmen María Cepeda-Jiménez
CENIM, CSIC
2 shared publications - Fernando Carreno
Physical Metallurgy Department, CENIM-CSIC, Av. Gregorio del Amo 8, 28040 Madrid, Spain
2 shared publications - Oscar Antonio Ruano
Physical Metallurgy Department, CENIM-CSIC, Av. Gregorio del Amo 8, 28040 Madrid, Spain
2 shared publications A A Kruglov
Institute for Metals Superplasticity Problems of Russian Academy of Sciences, 39 Khalturin St., 450001 Ufa, Russia
1 shared publication
Latest Publications
- Open Access
Local Plastic Deformation and Quality of Cu-Cu Joints Obtained by Ultrasonic Welding
Joints of copper sheets with a thickness of 0.8 mm were produced by ultrasonic welding. To assess the quality of the joints, tensile lap-shear strength, area fraction of bonding, distributions of normal strains in the cross sections of welded samples, linear weld density at a magnification of ×1000, and the microstructure and microhardness of welded samples were analyzed. It was proved that the arrangement of microbonds and length of gaps in joint zones significantly depended on the local normal strains of welded samples caused by the penetration of tool ridges under the clamping pressure. Joint regions with a linear weld density of more than 70% were observed if the local compression strains of the sample exceeded 15%. The appearance of local tensile strains was accompanied by a drop in the linear weld density of the joints in some regions, down to 5%. The distribution of normal strains depends on the mutual positions of the ridges of the welding tip and anvil. It is concluded that in order to improve the quality of joints obtained by ultrasonic welding and reduce the scatter of their strength values, welding tools should provide sufficiently high normal compression strains in the weld spot area.
Open AccessLocal Plastic Deformation and Quality of Cu-Cu Joints Obtained by Ultrasonic Welding
Joints of copper sheets with a thickness of 0.8 mm were produced by ultrasonic welding. To assess the quality of the joints, tensile lap-shear strength, area fraction of bonding, distributions of normal strains in the cross sections of welded samples, linear weld density at a magnification of ×1000, and the microstructure and microhardness of welded samples were analyzed. It was proved that the arrangement of microbonds and length of gaps in joint zones significantly depended on the local normal strains of welded samples caused by the penetration of tool ridges under the clamping pressure. Joint regions with a linear weld density of more than 70% were observed if the local compression strains of the sample exceeded 15%. The appearance of local tensile strains was accompanied by a drop in the linear weld density of the joints in some regions, down to 5%. The distribution of normal strains depends on the mutual positions of the ridges of the welding tip and anvil. It is concluded that in order to improve the quality of joints obtained by ultrasonic welding and reduce the scatter of their strength values, welding tools should provide sufficiently high normal compression strains in the weld spot area.
- 11 January 2023
- Published by Elsevier in Materialia
- Vol. 27
The mechanical behavior of the Ti6Al4V/Ti/Ti6Al4V composite produced by directed energy deposition under impact loading
- 11 January 2023
- Published by Elsevier in Materialia
- Vol. 27
The mechanical behavior of the Ti6Al4V/Ti/Ti6Al4V composite produced by directed energy deposition under impact loading
- 1 December 2022
- Published by Institute for Metals Superplasticity Problems of RAS in Letters on Materials
- Vol. 12 (4) , 499-503
Impact fracture characteristics of multilayer laminate based on near-alpha titanium alloy
Titanium near-alpha alloy Ti-6Al-2Zr-1.2\Mo-1.3V was used to manufacture a multilayer laminate by diffusion bonding. The laminate consisted of thirteen sheets stacked relative to each other in a way that they all had common rolling direction. The influence of cutting orientation of specimens on the mechanical behavior under impact loading of the laminate was determined. The results of quantitative assessment of the impact fracture characteristics for the studied specimens was analyzed. The transverse specimens had a higher impact strength value in comparison to the longitudinal specimens. The results of fractographic studies showed the presence of minor delaminations on the surfaces of fractured specimens.
- 1 December 2022
- Published by Institute for Metals Superplasticity Problems of RAS in Letters on Materials
- Vol. 12 (4) , 499-503
Impact fracture characteristics of multilayer laminate based on near-alpha titanium alloy
Titanium near-alpha alloy Ti-6Al-2Zr-1.2\Mo-1.3V was used to manufacture a multilayer laminate by diffusion bonding. The laminate consisted of thirteen sheets stacked relative to each other in a way that they all had common rolling direction. The influence of cutting orientation of specimens on the mechanical behavior under impact loading of the laminate was determined. The results of quantitative assessment of the impact fracture characteristics for the studied specimens was analyzed. The transverse specimens had a higher impact strength value in comparison to the longitudinal specimens. The results of fractographic studies showed the presence of minor delaminations on the surfaces of fractured specimens.
- 1 December 2021
- Published by Institute for Metals Superplasticity Problems of RAS in Letters on Materials
- Vol. 11 (4) , 457-461
The role of stop-off material in three-layer corrugated structures made of titanium alloys
In the manufacture of three-layer corrugated structures made of titanium alloys by diffusion bonding followed by superplastic forming, stop-off materials are used. The use of stop-off material makes it possible to selectively connect sheet blanks with each other and, as a result, get a hollow structure with an internal set of stiffeners in the form of a corrugation. The effect of stop-off materials based on boron nitride and yttrium oxide on the structure and mechanical properties of the titanium alloy Ti-6Al-4V is studied. Special attention is paid to the influence of stop-off materials on the quality of solid-phase joints in a corrugated structure. It is shown that the stop-off material based on yttrium oxide leads to the least degradation of the mechanical properties of the titanium alloy. It is established that the quality of the design depends not only on the composition of the stop-off materials, but also on the procedure of its processing before diffusion bonding of blanks. The composition of stop-off materials as binders includes organic components that contain light elements: nitrogen, carbon, oxygen and hydrogen. The latter are known to be harmful impurities for titanium and its alloys, and their chemical interaction with titanium is sharply intensified at high temperatures. The traditional temperatures of diffusion bonding and superplastic forming of the Ti-6Al-4V alloy are in the range of 900 - 950 degrees C. Therefore, it is necessary to control and prevent the process of adsorption of hydrogen, nitrogen, oxygen and carbon atoms on the connected surfaces of titanium blanks, since this can have a noticeable effect on the quality of diffusion joints, will lead to defects, and the fatigue strength of the entire structure already depends on this.
- 1 December 2021
- Published by Institute for Metals Superplasticity Problems of RAS in Letters on Materials
- Vol. 11 (4) , 457-461
The role of stop-off material in three-layer corrugated structures made of titanium alloys
In the manufacture of three-layer corrugated structures made of titanium alloys by diffusion bonding followed by superplastic forming, stop-off materials are used. The use of stop-off material makes it possible to selectively connect sheet blanks with each other and, as a result, get a hollow structure with an internal set of stiffeners in the form of a corrugation. The effect of stop-off materials based on boron nitride and yttrium oxide on the structure and mechanical properties of the titanium alloy Ti-6Al-4V is studied. Special attention is paid to the influence of stop-off materials on the quality of solid-phase joints in a corrugated structure. It is shown that the stop-off material based on yttrium oxide leads to the least degradation of the mechanical properties of the titanium alloy. It is established that the quality of the design depends not only on the composition of the stop-off materials, but also on the procedure of its processing before diffusion bonding of blanks. The composition of stop-off materials as binders includes organic components that contain light elements: nitrogen, carbon, oxygen and hydrogen. The latter are known to be harmful impurities for titanium and its alloys, and their chemical interaction with titanium is sharply intensified at high temperatures. The traditional temperatures of diffusion bonding and superplastic forming of the Ti-6Al-4V alloy are in the range of 900 - 950 degrees C. Therefore, it is necessary to control and prevent the process of adsorption of hydrogen, nitrogen, oxygen and carbon atoms on the connected surfaces of titanium blanks, since this can have a noticeable effect on the quality of diffusion joints, will lead to defects, and the fatigue strength of the entire structure already depends on this.
- Open Access
- 1 December 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 1008 (1) , 012071
Methods of controlling mechanical behavior of layered titanium material under impact loading
The results of studies on the mechanical behavior of a Ti-6Al-4V laminated material obtained by diffusion welding are analyzed. It is shown that the impact behavior of the layered material depends on many factors including the interface defects, the orientation of the notch tip relative to interface, the number and microstructural state of the layers and their crystallographic texture.
- 1 December 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 1008 (1) , 012071
Open AccessMethods of controlling mechanical behavior of layered titanium material under impact loading
The results of studies on the mechanical behavior of a Ti-6Al-4V laminated material obtained by diffusion welding are analyzed. It is shown that the impact behavior of the layered material depends on many factors including the interface defects, the orientation of the notch tip relative to interface, the number and microstructural state of the layers and their crystallographic texture.
- 1 August 2020
- Published by Institute for Metals Superplasticity Problems of RAS in Letters on Materials
- Vol. 10 (3) , 345-350
Features of manufactured and impact failure of a layered material based on Ti-6Al-4V alloy
Structural methods for controlling the properties of a layered material (LM) based on Ti-6Al-4V alloy are presented in this work. The layered materials were manufactured by diffusion bonding. They consist of seven and thirteen sheets of the thickness about 1.5 and 0.8 mm, respectively. Two methods of assembling the sheets were used: in one case, they were stacked relative to each other so that the rolling direction (RD) in them coincided (LM of type 1), and in the other, they did not match (LM of type 2), the angle between the RD in the neighboring sheets was 0 and 90 degrees, respectively. It was found that the prismatic texture (texture with datum planes oriented perpendicular to the rolling plane) present in the as-received sheets is inherited by the layered material of type 1 that it causes the anisotropy of impact strength. Almost the same distribution of the pole density of basis in the rolling direction and in the transverse direction determines the isotropy of impact strength in the layered material of type 2. A comparative evaluation of the test results has shown that when the crack propagates simultaneously through all layers (the crack divider orientation) the impact strength value is higher for the 7-layer material when the crack propagates sequentially from one layer to another (the crack arrester orientation) it is higher for the 13-layer material. The quantitative assessment of the fracture characteristics made it possible to establish that the decrease in the impact strength of the samples tested in the crack divider orientation with the number of layers increasing is conditioned by decreasing both the crack initiation energy and the crack propagation energy. In contrast, the improvement of impact strength of the samples tested in the crack arrester orientation occurs due to the significant increasing the crack propagation energy at an insignificant decreasing the crack initiation energy.
- 1 August 2020
- Published by Institute for Metals Superplasticity Problems of RAS in Letters on Materials
- Vol. 10 (3) , 345-350
Features of manufactured and impact failure of a layered material based on Ti-6Al-4V alloy
Structural methods for controlling the properties of a layered material (LM) based on Ti-6Al-4V alloy are presented in this work. The layered materials were manufactured by diffusion bonding. They consist of seven and thirteen sheets of the thickness about 1.5 and 0.8 mm, respectively. Two methods of assembling the sheets were used: in one case, they were stacked relative to each other so that the rolling direction (RD) in them coincided (LM of type 1), and in the other, they did not match (LM of type 2), the angle between the RD in the neighboring sheets was 0 and 90 degrees, respectively. It was found that the prismatic texture (texture with datum planes oriented perpendicular to the rolling plane) present in the as-received sheets is inherited by the layered material of type 1 that it causes the anisotropy of impact strength. Almost the same distribution of the pole density of basis in the rolling direction and in the transverse direction determines the isotropy of impact strength in the layered material of type 2. A comparative evaluation of the test results has shown that when the crack propagates simultaneously through all layers (the crack divider orientation) the impact strength value is higher for the 7-layer material when the crack propagates sequentially from one layer to another (the crack arrester orientation) it is higher for the 13-layer material. The quantitative assessment of the fracture characteristics made it possible to establish that the decrease in the impact strength of the samples tested in the crack divider orientation with the number of layers increasing is conditioned by decreasing both the crack initiation energy and the crack propagation energy. In contrast, the improvement of impact strength of the samples tested in the crack arrester orientation occurs due to the significant increasing the crack propagation energy at an insignificant decreasing the crack initiation energy.
- 1 April 2020
- Published by Elsevier in Composites Part B: Engineering
- Vol. 187
Characteristics of the mechanical behavior of Ti–6Al–4V multilayer laminate under impact loading
- 1 April 2020
- Published by Elsevier in Composites Part B: Engineering
- Vol. 187
Characteristics of the mechanical behavior of Ti–6Al–4V multilayer laminate under impact loading
- 1 July 2015
- Published by Pleiades Publishing Ltd in Physical Mesomechanics
- Vol. 18 (3) , 250-260
Micromechanisms of deformation and fracture in a VT6 titanium laminate under impact load
The paper studies the phase composition, microstructure, and mechanisms of plastic deformation and fracture under impact load in a laminate obtained by pressure welding of VT6 titanium alloy sheets. Under impact loading at 20 and -196°C, the material is delaminated into sheet piles with attendant changes in their fracture rate. At fracture surfaces, the initial crystal structure experiences structural phase decomposition which results in dynamic rotations. In fracture and delamination sublayers, the material is fragmented. The effects are more pronounced at = -196°C.
- 1 July 2015
- Published by Pleiades Publishing Ltd in Physical Mesomechanics
- Vol. 18 (3) , 250-260
Micromechanisms of deformation and fracture in a VT6 titanium laminate under impact load
The paper studies the phase composition, microstructure, and mechanisms of plastic deformation and fracture under impact load in a laminate obtained by pressure welding of VT6 titanium alloy sheets. Under impact loading at 20 and -196°C, the material is delaminated into sheet piles with attendant changes in their fracture rate. At fracture surfaces, the initial crystal structure experiences structural phase decomposition which results in dynamic rotations. In fracture and delamination sublayers, the material is fragmented. The effects are more pronounced at = -196°C.
- 29 May 2013
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 44 (10) , 4743-4753
Effect of Processing Temperature on the Texture and Shear Mechanical Properties of Diffusion Bonded Ti-6Al-4V Multilayer Laminates
- 29 May 2013
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 44 (10) , 4743-4753
Effect of Processing Temperature on the Texture and Shear Mechanical Properties of Diffusion Bonded Ti-6Al-4V Multilayer Laminates
- 1 February 2013
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 563, 28-35
Influence of interfacial defects on the impact toughness of solid state diffusion bonded Ti–6 Al–4 V alloy based multilayer composites
- 1 February 2013
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 563, 28-35
Influence of interfacial defects on the impact toughness of solid state diffusion bonded Ti–6 Al–4 V alloy based multilayer composites