Alexander Thoemmes
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Alexander Thoemmes has a total of 27 co-authors. Here are the top co-authors by number of shared publications:
- Alexey A. Ruktuev
Novosibirsk State Technical University, Novosibirsk, Russia
5 shared publications Ivan V. Ivanov
Novosibirsk State Technical University
5 shared publications- Daria Viktorovna Lazurenko
Novosibirsk State Technical University, Novosibirsk, Russia
4 shared publications Adelya A. Kashimbetova
Novosibirsk State Technical University
3 shared publications- Ivan V. Ivanov
Novosibirsk State Technical University
3 shared publications Alexander G. Anisimov
Lavrentyev Institute of Hydrodynamics SB RAS
2 shared publications
Latest Publications
- Open Access
- 1 March 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 795 (1)
Relationship between phase composition and wear resistance of titanium alloys
The wide use of titanium alloys is often due to their unique properties. Availability of a wide variety of mechanical, physical and chemical properties is associated with a large number of polymorphic modifications of titanium alloys. During the last decade, the metastable omega phase piques the largest interest among all titanium modifications. This study attempts to explain the different wear behavior of some titanium alloys with different Nb content during dry friction impact.
- 1 March 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 795 (1)
Open AccessRelationship between phase composition and wear resistance of titanium alloys
The wide use of titanium alloys is often due to their unique properties. Availability of a wide variety of mechanical, physical and chemical properties is associated with a large number of polymorphic modifications of titanium alloys. During the last decade, the metastable omega phase piques the largest interest among all titanium modifications. This study attempts to explain the different wear behavior of some titanium alloys with different Nb content during dry friction impact.
- 14 June 2019
- Published by Springer Nature in Metals and Materials International
- Vol. 26 (1) , 83-93
Application of Different Diffraction Peak Profile Analysis Methods to Study the Structure Evolution of Cold-Rolled Hexagonal α-Titanium
- 14 June 2019
- Published by Springer Nature in Metals and Materials International
- Vol. 26 (1) , 83-93
Application of Different Diffraction Peak Profile Analysis Methods to Study the Structure Evolution of Cold-Rolled Hexagonal α-Titanium
- Open Access
- 24 April 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 511 (1) , 012020
Microstructure and mechanical properties of annealed, quenched and suction cast Ti-6Al-4V
The effect of heat treatment or processing method on microstructure, mechanical properties and phase formation in Ti-6Al-4V alloys has been researched. The alloys in as-delivered, annealed, quenched and suction cast conditions were investigated using scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX) and synchrotron X-ray diffraction (SXRD) analysis. The different processing- or heat treatment routes lead to significant changes in the phase composition. The quenched and suction cast alloys exhibited a mixture of martensitic α' / α'' and BCC β phase. In annealed and as-delivered alloys α' + β phase mixtures was detected. The properties of alloys strongly depend on heat treatment and / or processing route.
- 24 April 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 511 (1) , 012020
Open AccessMicrostructure and mechanical properties of annealed, quenched and suction cast Ti-6Al-4V
The effect of heat treatment or processing method on microstructure, mechanical properties and phase formation in Ti-6Al-4V alloys has been researched. The alloys in as-delivered, annealed, quenched and suction cast conditions were investigated using scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX) and synchrotron X-ray diffraction (SXRD) analysis. The different processing- or heat treatment routes lead to significant changes in the phase composition. The quenched and suction cast alloys exhibited a mixture of martensitic α' / α'' and BCC β phase. In annealed and as-delivered alloys α' + β phase mixtures was detected. The properties of alloys strongly depend on heat treatment and / or processing route.
- 1 February 2019
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 946, 287-292
Characterization of Ti-xNb (x = 25 – 35) Alloys in as Melt and Annealed States
The effect of Nb content on microstructure, mechanical properties and phase formation in as-melt and annealed binary Ti-Nb alloys were investigated using scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX) and X-ray diffraction (XRD) analysis. The content of Nb varied in the range 25-35 mass % leading to significant changes in the microstructure. The annealed and furnace-cooled binary Ti-Nb samples exhibited HCP martensitic α` phase at a Nb content below 27.5 mass % and metastable BCC β phase at higher contents of Nb. The mechanical properties of alloys depended strongly on the Nb content and type of the dominating phase.
- 1 February 2019
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 946, 287-292
Characterization of Ti-xNb (x = 25 – 35) Alloys in as Melt and Annealed States
The effect of Nb content on microstructure, mechanical properties and phase formation in as-melt and annealed binary Ti-Nb alloys were investigated using scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX) and X-ray diffraction (XRD) analysis. The content of Nb varied in the range 25-35 mass % leading to significant changes in the microstructure. The annealed and furnace-cooled binary Ti-Nb samples exhibited HCP martensitic α` phase at a Nb content below 27.5 mass % and metastable BCC β phase at higher contents of Nb. The mechanical properties of alloys depended strongly on the Nb content and type of the dominating phase.
- 1 February 2019
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 946, 73-78
Corrosion Resistance of Medical Stainless Steel Obtained by Non-Vacuum Electron Beam Cladding
Pitting and crevice corrosion resistance of 321 stainless steel and non-vacuum electron-beam cladded stainless steel have been investigated by using potentio-dynamic polarization curve plotting. Lock-Ringer Salt Solution (LRSS) was used as biological media for corrosion test measurements. Microstructural research of samples after corrosion was carried out by using scanning electron microscopy. The experimental results show that the cladded stainless steel possesses higher pitting and crevice corrosion resistance.
- 1 February 2019
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 946, 73-78
Corrosion Resistance of Medical Stainless Steel Obtained by Non-Vacuum Electron Beam Cladding
Pitting and crevice corrosion resistance of 321 stainless steel and non-vacuum electron-beam cladded stainless steel have been investigated by using potentio-dynamic polarization curve plotting. Lock-Ringer Salt Solution (LRSS) was used as biological media for corrosion test measurements. Microstructural research of samples after corrosion was carried out by using scanning electron microscopy. The experimental results show that the cladded stainless steel possesses higher pitting and crevice corrosion resistance.
- 1 January 2019
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 60 (9-10) , 659-665
Structure and Phase Composition of Biomedical Alloys of the Ti – Nb System in Cast Condition and After Heat Treatment
- 1 January 2019
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 60 (9-10) , 659-665
Structure and Phase Composition of Biomedical Alloys of the Ti – Nb System in Cast Condition and After Heat Treatment
- 1 January 2019
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 60 (9-10) , 625-632
Effect of Electron Beam Power Density on the Structure of Titanium Under Non-Vacuum Electron-Beam Treatment
- 1 January 2019
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 60 (9-10) , 625-632
Effect of Electron Beam Power Density on the Structure of Titanium Under Non-Vacuum Electron-Beam Treatment
- 12 December 2018
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2051 (1) , 020258
Producing of Ti–Ta–Nb layers on Ti-substrate by electron beam treatment
This paper presents the results of studies of the microstructure, phase formation and mechanical properties in non-vacuum electron beam cladded Ti–Ta–Nb alloys. The defect-free surface layer had a content of 21 mass. % Nb and 33 mass. % Ta and a thickness of 2 mm. The samples were investigated using optical microscopy (OM), X-ray diffraction (XRD) analysis, energy dispersive X-ray spectroscopy (EDX). The results of OM and XRD analysis showed that the material inhibits a finely dispersed lamellar structure, which consists of a mixture of martensitic phases (α′ + α″) and β phase. The average microhardness is between 300–400 HV and the ultimate tensile strength (UTS) 400–450 MPa. The results of Charpy impact strength test showed that due to the coated surfaced layer the impact strength decreases to 210 J/cm2.
- 12 December 2018
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2051 (1) , 020258
Producing of Ti–Ta–Nb layers on Ti-substrate by electron beam treatment
This paper presents the results of studies of the microstructure, phase formation and mechanical properties in non-vacuum electron beam cladded Ti–Ta–Nb alloys. The defect-free surface layer had a content of 21 mass. % Nb and 33 mass. % Ta and a thickness of 2 mm. The samples were investigated using optical microscopy (OM), X-ray diffraction (XRD) analysis, energy dispersive X-ray spectroscopy (EDX). The results of OM and XRD analysis showed that the material inhibits a finely dispersed lamellar structure, which consists of a mixture of martensitic phases (α′ + α″) and β phase. The average microhardness is between 300–400 HV and the ultimate tensile strength (UTS) 400–450 MPa. The results of Charpy impact strength test showed that due to the coated surfaced layer the impact strength decreases to 210 J/cm2.
- 1 April 2018
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 769, 29-34
Comparison of Mechanical Properties and Microstructure of Annealed and Quenched Ti-Nb Alloys
The effect of Nb content on microstructure, mechanical properties and phase formation in annealed and quenched binary Ti-Nb alloys were investigated using scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX) and X-ray diffraction (XRD) analysis. The content of Nb varied in the range 0-37 mass % leading to significant changes in the microstructure. The annealed and furnace-cooled binary Ti-Nb samples exhibited HCP martensitic α` phase at a Nb content below 14 mass % and stable BCC β phase at higher contents of Nb. The structure of the quenched samples changed with increase of Nb content in the following order: coarse primary martensite → fine acicular (α`+α``) martensite → single β phase structure. The mechanical properties of alloys strongly depended on the Nb content and type of the dominating phase.
- 1 April 2018
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 769, 29-34
Comparison of Mechanical Properties and Microstructure of Annealed and Quenched Ti-Nb Alloys
The effect of Nb content on microstructure, mechanical properties and phase formation in annealed and quenched binary Ti-Nb alloys were investigated using scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX) and X-ray diffraction (XRD) analysis. The content of Nb varied in the range 0-37 mass % leading to significant changes in the microstructure. The annealed and furnace-cooled binary Ti-Nb samples exhibited HCP martensitic α` phase at a Nb content below 14 mass % and stable BCC β phase at higher contents of Nb. The structure of the quenched samples changed with increase of Nb content in the following order: coarse primary martensite → fine acicular (α`+α``) martensite → single β phase structure. The mechanical properties of alloys strongly depended on the Nb content and type of the dominating phase.
- 1 April 2018
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 769, 48-53
Structural Transformations Occurring during the Formation of TiAl3-Based Composites Reinforced by TiB2 or TiC Hard Particles
This work is devoted to investigation of the structure of Ti-TiAl3 composites reinforced by TiB2 or TiC hard particles and obtained by spark plasma sintering of elemental foils and ceramic powders. Sintering was carried out at the temperature of 830 oC under the pressure of 40 MPa during 10 minutes. Microstructure of the composites obtained was represented by alternated layers of titanium and intermetallic compound TiAl3. Also, it was found that at the Ti-TiAl3 interfaces thin intermediate layers were formed. Quantitative elemental analysis of these layers showed that Ti3Al, TiAl, and TiAl2 compounds, as well as Ti (Al) solid solution could be formed in these zones. Diffraction analysis did not reveal any transformations of initial reinforcing phases after sintering. Interlayers with titanium diboride had the average microhardness level of 3988 HV, and the average microhardness level of interlayers with TiC was 1610 HV.
- 1 April 2018
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 769, 48-53
Structural Transformations Occurring during the Formation of TiAl3-Based Composites Reinforced by TiB2 or TiC Hard Particles
This work is devoted to investigation of the structure of Ti-TiAl3 composites reinforced by TiB2 or TiC hard particles and obtained by spark plasma sintering of elemental foils and ceramic powders. Sintering was carried out at the temperature of 830 oC under the pressure of 40 MPa during 10 minutes. Microstructure of the composites obtained was represented by alternated layers of titanium and intermetallic compound TiAl3. Also, it was found that at the Ti-TiAl3 interfaces thin intermediate layers were formed. Quantitative elemental analysis of these layers showed that Ti3Al, TiAl, and TiAl2 compounds, as well as Ti (Al) solid solution could be formed in these zones. Diffraction analysis did not reveal any transformations of initial reinforcing phases after sintering. Interlayers with titanium diboride had the average microhardness level of 3988 HV, and the average microhardness level of interlayers with TiC was 1610 HV.