Oscar Kwame Segbefia
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Oscar Kwame Segbefia has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
Naureen Akhtar
2 shared publicationsTor Oskar Sætre
2 shared publications- Tor Oskar Sætre
Department of Engineering Sciences, University of Agder, 4879 Grimstad, Norway
1 shared publication
Latest Publications
- Open Access
- 11 June 2023
- Published by Elsevier in Solar Energy Materials and Solar Cells
- Vol. 258
Moisture induced degradation in field-aged multicrystalline silicon photovoltaic modules
- 11 June 2023
- Published by Elsevier in Solar Energy Materials and Solar Cells
- Vol. 258
Open AccessMoisture induced degradation in field-aged multicrystalline silicon photovoltaic modules
- Open Access
- 13 February 2023
- Published by Elsevier in Energy Reports
- Vol. 9, 3104-3119
Defects and fault modes of field-aged photovoltaic modules in the Nordics
- 13 February 2023
- Published by Elsevier in Energy Reports
- Vol. 9, 3104-3119
Open AccessDefects and fault modes of field-aged photovoltaic modules in the Nordics
- Open Access
Investigation of the Temperature Sensitivity of 20-Years Old Field-Aged Photovoltaic Panels Affected by Potential Induced Degradation
One effect of moisture ingress on solar panels is potential induced degradation (PID). Solar panels affected by PID experience large leakage currents between the solar cells and the module’s frame, which leads to substantial power degradation. In the present work, the temperature coefficients of 3 old PV panels affected by PID were investigated. In the electroluminescence images, solar cells nearer to the edge of the modules appear darker due to ohmic shunting. IR thermal images acquired under clear sky outdoor conditions show that the majority of the warmer cells (hotspots) were located closer to the edge of the modules. The difference in cell temperature (∆T) due to PID effect ranges from 7 °C to 15 °C for the 3 field-aged modules. The average temperature coefficient of efficiency (βηm) was found to be −0.5%/°C. Also, it was observed that the temperature coefficients of open circuit voltage (βVoc = −0.4%/°C), maximum power point voltage (βVmpp = −0.5%/°C), and fill factor (βFF = −0.2%/°C), were the underlying factors for the degradation in the Pmax of the old solar panels affected by PID. This accounted for an average 1.2%/year overall degradation in the efficiency of these modules. Most notably, it was discovered that the PV modules affected by PID show negative temperature coefficients of maximum power point current (βJmpp) due to large leakage currents. This observed negative βJmpp we believe is characteristic of PV panels affected by PID.
Open AccessInvestigation of the Temperature Sensitivity of 20-Years Old Field-Aged Photovoltaic Panels Affected by Potential Induced Degradation
One effect of moisture ingress on solar panels is potential induced degradation (PID). Solar panels affected by PID experience large leakage currents between the solar cells and the module’s frame, which leads to substantial power degradation. In the present work, the temperature coefficients of 3 old PV panels affected by PID were investigated. In the electroluminescence images, solar cells nearer to the edge of the modules appear darker due to ohmic shunting. IR thermal images acquired under clear sky outdoor conditions show that the majority of the warmer cells (hotspots) were located closer to the edge of the modules. The difference in cell temperature (∆T) due to PID effect ranges from 7 °C to 15 °C for the 3 field-aged modules. The average temperature coefficient of efficiency (βηm) was found to be −0.5%/°C. Also, it was observed that the temperature coefficients of open circuit voltage (βVoc = −0.4%/°C), maximum power point voltage (βVmpp = −0.5%/°C), and fill factor (βFF = −0.2%/°C), were the underlying factors for the degradation in the Pmax of the old solar panels affected by PID. This accounted for an average 1.2%/year overall degradation in the efficiency of these modules. Most notably, it was discovered that the PV modules affected by PID show negative temperature coefficients of maximum power point current (βJmpp) due to large leakage currents. This observed negative βJmpp we believe is characteristic of PV panels affected by PID.