    Features of a local biointerface formed upon integration of a knitted nickel-titanium mesh into striated muscle tissue

    by E. B. Topolnitskiy, N. A. Shefer, E. S. Marchenko, T. I. Fomina, A. S. Garin

    Особенности локального биоинтерфейса при интеграции трикотажной никелид-титановой сетки в поперечнополосатую мышечную ткань

  • Open Access

    Study of the biocompatibility of porous 3D-TiNi implants in vivo

    by E. S. Marchenko, I. I. Gordienko, A. A. Kozulin, G. A. Baigonakova, S. A. Borisov, A. S. Garin, S. P. Cherny, E. L. Choinzonov, Д. Е. Кульбакин

    Introduction. Porous TiNi alloys are widely used in medicine as osteoreplacement implants due to their unique properties of superelasticity and biocompatibility, but their clinical use is severely limited by time-consuming manual fabrication and the inability to create precise geometries. Reconstructive surgery for the replacement of bone defects requires biocompatible endoprostheses of individual shape and complex geometry. The use of porous 3D-TiNi implants can be a solution to many problems in traumatology and bone oncology.Aim: To evaluate the possibility of using porous 3D-TiNi implants in osteoplastic surgery based on a study of the structure and biocompatibility of the material under in vivo conditions.Material and Methods. Porous samples in the form of cones and a single implant for maxillofacial surgery were prepared from TiNi powder by selective laser melting. To print an individual implant for maxillofacial surgery, the personal data of the patient at the Oncology Research Institute were used. The macrostructure, elemental and phase composition of porous titanium nickelide samples were investigated using scanning microscopy and X-ray diffraction analysis. The biocompatibility of porous cone-shaped samples was evaluated in vivo using guinea pigs whose condition was analysed by CT scanning.Results. Structural studies of porous titanium nickelide samples showed that selective laser melting can be used to obtain a continuous porous structure with strong contact bridges between particles of a three-phase powder. In vivo testing of the cone-shaped implants showed no local inflammatory changes, rejection or deformation of the hind limb axes of the experimental animals. The basic feasibility of fabricating a custom implant of complex geometry from TiNi powder using selective laser melting according to a patient’s MSCT data was demonstrated.Conclusions. Porous 3D-TiNi implants obtained by selective laser melting showed high biocompatibility under in vivo conditions. An experimental study confirmed the efficacy and ease of use of 3D TiNi implants, their excellent self-fixation in bone tissue, and bone tissue augmentation at the interface with the implant. The macrostructure, chemical and phase composition of the implant material was found to be close to traditional porous TiNi alloys. It was shown that the method of selective laser melting makes it possible to create complex geometric defects in bone tissue from TiNi.


  • Open Access

    Features of the integration of two-layer metal knitwear made of titanium nickelide during the replacement of a thoracoabdominal defect in the experiment

    by E. B. Topolnitskiy, N. A. Shefer, E. S. Marchenko, T. I. Fomina, R. A. Mikhed, А. N. Tsydenova, A. S. Garin

    The aim of investigation was to study experimentally the morphological features of tissue integration of two-layer titanium nickelide (TiNi) knitwear when replacing thoracoabdominal defects.Materials and methods. The experiments were carried out on 40 Wistar rats. The experimental animals were divided into two comparison groups: in Group A (n = 20) the defect was replaced using a two-layer knitted tape made of TiNi, in Group B (n = 20) a polypropylene mesh implant was used. The technique of the operation and the peculiarities of keeping the animals did not differ. Animals were taken out after 14, 30, 60 and 90 days of experiment. The macroscopic structural features at the site of implant fixation to tissues and at the sites of contact with underlying organs were studied, and the inflammatory process was assessed. The histological and electron microscopic study was carried out with an assessment of the features of tissue integration through the mesh structure of knitwear.Results. Thirty days after the surgery in four cases of Group B the appearance of the chest wall deformation at the site of implant fixation was noted, in one case the deformation site was located along the lateral edge of the abdominal wall. Among the animals of Group A no such changes were recorded. The histological and electron microscopy examination revealed that the porous structure of the TiNi wire, as well as the biomechanical and biochemical properties of the two-layer metal knitwear, ensure optimal integration of the endoprosthesis in the body tissues, forming an elastic frame close to natural. In Group B, on the contrary, the reaction of the body caused by the implanted polypropylene prosthesis was characterized by more pronounced fibrosis, and tissue integration through the mesh structure of the implant was not observed.Conclusion. Two-layer TiNi knitwear in the replacement of complex structures of the thoracoabdominal zone showed promising results, which opens up prospects for further clinical research.


  • АНАЛИЗ ДЕФОРМАЦИОННЫХ ДИАГРАММ ОДНООСНОГО ЦИКЛИЧЕСКОГО РАСТЯЖЕНИЯ ПРОВОЛОК И МЕТАЛЛАТРИКОТАЖА ИЗ TiNi СПЛАВА

    by Е.с. Марченко, Г.а. Байгонакова, М.а. Ковалёва, С.в. Гюнтер, А.а. Шишелова, А.с. Гарин, А.в. Ветрова, К.м. Дубовиков, О. Мамазакиров

    В работе рассмотрено деформационное поведение тонких TiNi проволок диаметрами 40-90 мкм при одноосном растяжении. Деформационные зависимости напряжение-деформация, полученные в результате эксперимента, полностью соответствуют типовым диаграммам растяжения нитинола и подтверждают наличие мартенситного перехода, вызванного напряжением. Испытания на циклическое растяжение показали, что деформация проволоки характеризуется сверхэластичным поведением. Были получены деформационные диаграммы для металлотрикотажа из проволоки толщиной 60 мкм, и проведен сравнительный анализ с деформационным поведением проволоки. Результаты показали, что при одноосном растяжении металлотрикотажа на деформационных зависимостях отсутствует участок текучести, вызванный мартенситным переходом. Несмотря на сверхэластичное поведение проволок, сам металлотрикотаж, изготовленный из сверхэластисных проволок, ведет себя гиперупруго. Обнаружена закономерность, согласно которой предел прочности металлотрикотажа значительно ниже предела прочности проволоки.

  • ОСОБЕННОСТИ СТРУКТУРНО-ФАЗОВОГО СОСТОЯНИЯ НА ПОВЕРХНОСТИ НИКЕЛИД ТИТАНОВЫХ ЛИТЫХ И ПОРИСТЫХ СПЛАВОВ ПРИ ВЫСОКОТЕМПЕРАТУРНОЙ ГАЗОВОЙ КОРРОЗИИ

    by Е.с. Марченко, Г.а. Байгонакова, К.м. Дубовиков, А.с. Гарин, А.а. Шишелова, М.а. Ковалёва, А.а. Клопотов

    В статье дана сравнительная оценка окисленной поверхности монолитных и пористых сплавов на основе никелида титана после отжига на воздухе при 1000 °С. Представлен анализ стойкости поверхности пористого СВС никелида титана сопротивляться высокотемпературному окислению на воздухе при 1000 °С на основе исследований структурно-фазовых состояний приповерхностных слоев. Установлено, что для монолитных и пористых сплавов на основе никелида титана, полученных разными методами, отжиг при 1000 °С на воздухе приводит к разным структурно-фазовым состояниям в приповерхностных слоях. На окисленной поверхности монолитного сплава на основе никелида титана обнаружено многофазное состояние: диоксид титана TiO2, карбид TiC, оксид никеля NiO и никель Ni. Установлено, что окисная пленка толщиной 8¸10 мкм имеет градиентное строение с разными структурами: пористой, зернистой и островковой. На поверхности окисленного пористого спеченного сплава на основе никелида титана кроме фаз диоксида титана обнаружен свободный никель и его оксид. Высокотемпературный отжиг на воздухе приводит к образованию рыхлого окисленного слоя толщиной до 50¸60 мкм. Установлено, что на поверхности пористого образца, полученного методом высокотемпературного синтеза, содержание Ni значительно меньше, по сравнению с пористымми спеченными образцами из сплава на основе никелида титана. Изучение особенностей структурно-фазовых состояний приповерхностных слоев показало, что высокотемпературному окислению наиболее подвержены спеченные и монолитные сплавы на основе никелида титана из-за большей незащищенной реакционной поверхности, где на поверхности обнаружены оксид никеля и свободный никель (Ni, NiO). Показано, что наличие защитного тонкого и плотного оксикарбонитридного поверхностного слоя на основе соединения Ti4Ni2O(N,C) в пористом сплаве, полученного методом высокотемпературного синтеза, значительно уменьшает интенсивность окисления по сравнению с другими исследуемыми сплавами на основе никелида титана.