  • Open Access

    The 3D Taper Profile Machining of Superalloys and Composites Using WEDM: A Review

    by Krishnamoorthy Jayakumar, T. Suresh, S. Senthur Vaishnavan, M. Rajesh

    Wire electric discharge machine (WEDM) is a process used popularly in microsystems, tool and die industries, medicine, transportation, and spacecrafts to create intricate portions with high dimensional accuracy and surface finish. It is employed to process superalloys and materials made of composites which are conductive and strong materials. From the literature, an analysis of the WEDM process on different materials revealed that there were many variables involved and that each process parameter influences the different response variables. The removal process of a spark discharge for an inclined angle during the cutting of 3D profiles has different applications. Also, types of dielectric fluid, and the influence of wire material, diameter and pressure, wire tension, feed, Ton, Toff, current, and voltage on machining characteristics—like kerf, MRR, wire wear, surface finish and its characteristics, dimensional deviations, and corner errors—and on a variety of materials like Inconel, nickel, titanium, WC, steels, and other superalloys and composites (MMCs and CMCs) during taper WEDM were reviewed.

  • Performance analysis of TIG welded dissimilar aluminium alloy with scandium added ER5356 filler rods

    by S. Senthur Vaishnavan, K. Jayakumar

    The use of aluminum alloys has become far greater than ever with increasing needs for lighter and stronger structures leading to new aluminum alloys with rare earth admixtures. Scandium (Sc) is one such rare earth mineral used as an admixture for aluminum alloys. This study investigates the effect of using Standard ER5356 filler rod and Sc-added ER5356 filler rods in tungsten inert gas (TIG) welding dissimilar aluminum alloys AA5083-H111 and AA5754-H111. The investigations found that the presence of Sc during the welding process is a significant contributor toward enhanced grain refinement and producing dissimilar aluminum alloy with defect-free joint with improved tensile strength and hardness. In comparison, the TIG-welded joint using Sc-added filler rod exhibited enhanced yield strength of 128 MPa to the 117.5 MPa obtained for TIG weld without Sc in the filler rod. The microhardness evaluated by Vicker’s Hardness test displayed improved hardness of 124 HV1 due to the presence of Sc and 76 HV1 without presence of Sc during TIG welding.


  • Tungsten inert gas welding of two aluminum alloys using filler rods containing scandium: the role of process parameters

    by S. Senthur Vaishnavan, K. Jayakumar

    The present work investigates the effects of selected welding process parameters on the output responses for the tungsten inert gas welding of two aluminum alloys: 5083-H111 and 5754-H111. The tungsten inert gas welding was performed using design of experiments followed by the optimization of process parameter through response surface methodology technique. Tungsten inert gas welding was carried out by varying current, gas flow rate, and weight percentage of scandium addition on the filler rod and tensile strength and microhardness were measured as output responses. From the analysis of variance results, it was found that the significant influencing parameter to be input current for the tungsten inert gas welding. For predicting optimal ultimate tensile strength and microhardness, desirability approach was used. The optimized process parameters were found to be input current of 170 A, gas flow rate of 11 lit/min, and weight percentage of scandium added filler rod of 0.5%. The peak tensile strength and microhardness values observed for the optimum process parameters were 236.18 MPa and 105 HV, respectively. The validation of the optimization found these values from the experiments consistent with the predicted values with marginal error. The microstructure of the base alloys and the weld zone were analyzed.