    Investigation on the Solidification Structure of Q355 in 475 mm Extra-Thick Slabs Adopting Cellular Automaton-Finite Element Model

    by Kezai Yu, Minglin Wang, Haihan Fan, Zhonghua Zhan, Zixiang Ren, Lijun Xu

    The solidification structure characteristics are decisive for the production of extra-thick slabs. This study developed a solidification heat transfer model and a cellular automaton–finite element coupled model to investigate the solidification behavior and structure characteristics of a 475 mm extra-thick slab. The models were applied under various continuous casting process parameters and different alloy element content. The simulation results reveal that casting speed has the most significant effect on the solidification behavior of extra-thick slabs, surpassing the impact of specific water flow and superheat. The solidification structure characteristics of the 475 mm extra-thick slabs were investigated under various conditions. The findings indicate that at higher casting speeds and superheats, the average grain size increases and the grain number decreases. The average grain size initially decreases and then increases with the rise in specific water flow, reaching its minimum at approximately 0.17 L·kg−1. Additionally, the average grain radius first decreases and then slightly increases with an increase in carbon content, achieving the minimum value of about 0.17% carbon. Compared with carbon and manganese, silicon has a greater impact on the solidification structure of ultra-thick slabs, and a moderate increase in silicon content can effectively refine the grain size. This study provides a theoretical foundation for understanding the changes in solidification structure characteristics and optimizing continuous casting process parameters for 475 mm extra-thick slabs.


  • Open Access

    Formation Mechanism and Improvement of Magnetic Particle Inspection Defects in Cr5 Backup Roller Forged Ingot

    by Weifeng Zhang, Guanbo Wang, Yanling Zhang, Guoguang Cheng, Zhonghua Zhan

    Industrial tests and thermodynamic calculations were utilized to investigate the source and formation of magnetic particle inspection defects identified on the near-surface of the Cr5 back-up roll forged ingot, which was used in large cold rolling mills. The results showed that the linear aggregating SiO2-MnO-Al2O3 liquid inclusions up to 3 mm led to the flaw detection failure. SiO2-MnO-Al2O3 liquid inclusions were firstly formed in the inductive furnace. Due to its low contact angle, a huge amount of SiO2-MnO-Al2O3 liquid inclusions were inherited into the forged ingot. The formation of SiO2-MnO-Al2O3 liquid inclusions was attributed to the over-oxidation and relatively low aluminum content in the molten steel, as calculated by Factsage 8.1. Controlling the amount of aluminum in molten steel during the smelting process could modify the formation of SiO2-MnO-Al2O3 and CaO-SiO2-Al2O3 liquid oxide into solid Al2O3 type inclusions that were easily removed. Besides, the CaO-SiO2-Al2O3 liquid oxide could be transformed from CaO-Al2O3 type oxide by the significant loss of aluminum content during the VD process or slag entrapment. Certain content of aluminum in the molten steel could improve the flaw detection caused by the aggregating SiO2-MnO-Al2O3 inclusions effectively.


  • Open Access

    Formation and Evolution of DS-Type Inclusions in 15-5PH Stainless Steel

    by Zhonghua Zhan, Weifeng Zhang, Yanling Zhang, Ruxing Shi, Guoguang Cheng

    15-5PH stainless steel castings are key components in fracturing trucks. However, DS-type inclusions can lead to fatigue failure of the material. To elucidate the formation mechanism of large-size DS-type inclusions, the evolution, growth, and aggregation of inclusions during vacuum oxygen decarburization, ladle refining, and vacuum casting were studied. The results show that the DS-type inclusions with sizes larger than 20 μm were CaO–Al2O3–SiO2–MgO–CaS composite inclusions. After Si–Al additions in vacuum degassing, typical inclusions were spinel or Al2O3. After Ca–Si additions during ladle treatment, typical inclusions were liquid or dual-phase Al2O3–CaO–SiO2–MgO. During the solidification process, due to the segregation of S and the decrease in solubility, the typical inclusions in the final casting became Al2O3–CaO–SiO2–MgO–CaS. For optimal fatigue performance of stainless steel castings, slag and refractory composition control were also necessary because the [Mg] contents mainly come from the slag and lining.