Sanjay Kumar Bhattacharyya
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Sanjay Kumar Bhattacharyya has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Koushik Pal
Hari Shankar Singhania Elastomer and Tyre research Institute, Plot No. 437, Hebbal Industrial Area, Mysore, Karnataka, 570016, India
2 shared publications Rabindra Mukhopadhyay
Hari Shankar Singhania Elastomer and Tire Research Institute Mysore India
2 shared publicationsBarun Kumar Samui
R&D Centre Hari Shankar Singhania Elastomer and Tyre Research Institute Mysore India
1 shared publication- Dipankar Chattopadhyay
University of Calcutta 92 A.P.C. Road
1 shared publication Dipankar Mondal
Department of Polymer Science and Technology University of Calcutta Kolkata India
1 shared publication- Hirak Satpathi
Hari Shankar Singhania Elastomer and Tyre Research Institute, Hebbal Industrial Area, Mysore, Karnataka, 570016, India
1 shared publication
Latest Publications
- 26 September 2021
- Published by Wiley in Polymer Engineering & Science
- Vol. 61 (12) , 3017-3028
Impact of α‐cellulose as a green filler on physico‐mechanical properties of a solution grade styrene‐butadiene rubber based tire‐tread compound
Physico‐mechanical and dynamic mechanical properties of typical solution grade styrene‐butadiene rubber (S‐SBR) and polybutadiene rubber (PBR) based tire‐tread compound were investigated by partially replacing highly dispersible (HD) silica with naturally occurring α‐cellulose. Fourier transform infrared spectrum detected abundance of hydroxyl group in α‐cellulose, which has created keenness to investigate its reinforcement characteristics in an S‐SBR and PBR based compound. Scanning electron microscope and transmission electron microscope were employed to investigate the microstructure and dispersion of α‐cellulose at higher magnification. Thermo‐gravimetric analysis was performed to understand the degradation behavior of α‐cellulose. Differential scanning calorimeter was engaged to detect phase transition and degree of purity of α‐cellulose. An increase in cure rate was observed with partial replacement of HD silica by α‐cellulose. The cure rate index was increased by 13% over control one at 10% replacement of silica with α‐cellulose. It was noticed that at an optimum level of replacement (10%), α‐cellulose containing compounds exhibited lower viscoelastic energy dissipation (both loss modulus [E″] and loss tangent [tan δ]) at the slight expense of tensile moduli. Beside these, substitution of silica with α‐cellulose found to have no effect on wet grip property of the compounds.
- 26 September 2021
- Published by Wiley in Polymer Engineering & Science
- Vol. 61 (12) , 3017-3028
Impact of α‐cellulose as a green filler on physico‐mechanical properties of a solution grade styrene‐butadiene rubber based tire‐tread compound
Physico‐mechanical and dynamic mechanical properties of typical solution grade styrene‐butadiene rubber (S‐SBR) and polybutadiene rubber (PBR) based tire‐tread compound were investigated by partially replacing highly dispersible (HD) silica with naturally occurring α‐cellulose. Fourier transform infrared spectrum detected abundance of hydroxyl group in α‐cellulose, which has created keenness to investigate its reinforcement characteristics in an S‐SBR and PBR based compound. Scanning electron microscope and transmission electron microscope were employed to investigate the microstructure and dispersion of α‐cellulose at higher magnification. Thermo‐gravimetric analysis was performed to understand the degradation behavior of α‐cellulose. Differential scanning calorimeter was engaged to detect phase transition and degree of purity of α‐cellulose. An increase in cure rate was observed with partial replacement of HD silica by α‐cellulose. The cure rate index was increased by 13% over control one at 10% replacement of silica with α‐cellulose. It was noticed that at an optimum level of replacement (10%), α‐cellulose containing compounds exhibited lower viscoelastic energy dissipation (both loss modulus [E″] and loss tangent [tan δ]) at the slight expense of tensile moduli. Beside these, substitution of silica with α‐cellulose found to have no effect on wet grip property of the compounds.
- 21 August 2021
- Published by Wiley in Polymer Engineering & Science
- Vol. 61 (10) , 2616-2629
Understanding the influence of anti‐reversion agent and metal oxide dose on natural rubber–carbon black system
Sulfidic linkages that are formed during the vulcanization process of natural rubber (NR) are unstable at a higher temperature and can be reversed into conjugated diene. To overcome such issue and to build a compound that is hostile to inversion and with increasing service life, anti‐reversion agent (ARA), for example, N,N′‐4,4′‐diphenylmethyene bismaleimide (BMDM), is added into the formulation. This work explains the conjugation reaction mechanism of conjugated diene and BMDM by means of gas chromatography–mass spectrometry and Fourier transform infrared spectroscopy. The first phase of this study is associated with the change in ARA dosage keeping ZnO dosage the same. It is observed that 5 phr of BMDM and 2 phr ZnO combination (ARA4) shows lowest reversion at 160°C. The modulus value at 300% elongation increased 12% by the incorporation of BMDM as compared to the compound of no BMDM (ARA1). The second part is all about keeping BMDM dosage the same at 5 phr level and varying ZnO phr by 3, 4, and 5. From the overall results, it is observed that at a suitable dosage of BMDM and ZnO (5 phr BMDM and 3 phr ZnO combination [ARA5]), least reversion can be achieved and vulcanizates containing optimized BMDM and ZnO show better retention properties after aerobic aging as compared to ARA1.
- 21 August 2021
- Published by Wiley in Polymer Engineering & Science
- Vol. 61 (10) , 2616-2629
Understanding the influence of anti‐reversion agent and metal oxide dose on natural rubber–carbon black system
Sulfidic linkages that are formed during the vulcanization process of natural rubber (NR) are unstable at a higher temperature and can be reversed into conjugated diene. To overcome such issue and to build a compound that is hostile to inversion and with increasing service life, anti‐reversion agent (ARA), for example, N,N′‐4,4′‐diphenylmethyene bismaleimide (BMDM), is added into the formulation. This work explains the conjugation reaction mechanism of conjugated diene and BMDM by means of gas chromatography–mass spectrometry and Fourier transform infrared spectroscopy. The first phase of this study is associated with the change in ARA dosage keeping ZnO dosage the same. It is observed that 5 phr of BMDM and 2 phr ZnO combination (ARA4) shows lowest reversion at 160°C. The modulus value at 300% elongation increased 12% by the incorporation of BMDM as compared to the compound of no BMDM (ARA1). The second part is all about keeping BMDM dosage the same at 5 phr level and varying ZnO phr by 3, 4, and 5. From the overall results, it is observed that at a suitable dosage of BMDM and ZnO (5 phr BMDM and 3 phr ZnO combination [ARA5]), least reversion can be achieved and vulcanizates containing optimized BMDM and ZnO show better retention properties after aerobic aging as compared to ARA1.