Anant Shukla
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Anant Shukla has a total of 26 co-authors. Here are the top co-authors by number of shared publications:
- Manoranjan Kar
Department of Physics, Indian Institute of Technology Patna, Bihta, Patna, India
7 shared publications - Jyotirekha Mallick
Department of Physics, Indian Institute of Technology Patna 1 , Bihta, Patna 801106, India
3 shared publications - Amar Dev
Indian Institute of Technology Patna , Bihta, Bihar 801106
2 shared publications Murli Kumar Manglam
2 shared publications- Murli Kumar Manglam
Department of Material Science and Engineering Indian Institute of Technology Kanpur Kalyanpur Kanpur 208016 Uttar Pradesh India
2 shared publications - Suman Kumari
Department of Physics Indian Institute of Technology Patna Bihta Patna 801106 Bihar India
2 shared publications
Latest Publications
- Open Access
- 13 January 2025
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 137 (2)
Investigation on coupling between ferro-orderings and energy harvesting properties of nickel ferrite and strontium modified barium titanate composites
Environment-friendly, low power-consuming magnetoelectric composites possess the interesting coupling between various ferro-order parameters and find applications in magnetic sensors, waveguides, transducers, spintronics, four-state memory devices, etc. The particulate composites (x)NiFe2O4–(1 − x)Ba0.9Sr0.1TiO3 were prepared using the hybrid sol-gel method using the conventional ceramic double-sintering method. The ferromagnetic nickel ferrite crystallized into a cubic crystal structure whose x-ray diffraction (XRD) peaks could be indexed to Fd3¯m space group. The ferroelectric strontium-substituted barium titanate crystallized to a tetragonal crystal structure with P4mm space group. Presence of both crystal symmetries and elemental compositions as per the proposed stoichimetry were observed from experimental results (XRD and electron microscopy techniques). Koop's phenomenological theory could be employed to explain the impedance spectra in the range of 1 kHz to 1 MHz. The effect of Maxwell–Wagner polarization and space charge polarization on the dielectric properties of composites have been observed. The Arrott plot technique successfully explains the suitability of composites for high-energy storage applications. The coupling between both ferro-orderings has been revealed from the magneto-dielectric curves and its dependency on the microstructure has been observed. The magnetocapacitance increased with the increase in NiFe2O4 composition in the (x)NiFe2O4–(1 − x)Ba0.9Sr0.1TiO3 composite. The 30% NiFe2O4 in (x)NiFe2O4–(1 − x)Ba0.9Sr0.1TiO3 composite exhibited overall better energy harvesting (η = 62.9%) and magnetodielectric properties (MC = 1.4%, MI = 20% at 1 kHz).
- 13 January 2025
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 137 (2)
Open AccessInvestigation on coupling between ferro-orderings and energy harvesting properties of nickel ferrite and strontium modified barium titanate composites
Environment-friendly, low power-consuming magnetoelectric composites possess the interesting coupling between various ferro-order parameters and find applications in magnetic sensors, waveguides, transducers, spintronics, four-state memory devices, etc. The particulate composites (x)NiFe2O4–(1 − x)Ba0.9Sr0.1TiO3 were prepared using the hybrid sol-gel method using the conventional ceramic double-sintering method. The ferromagnetic nickel ferrite crystallized into a cubic crystal structure whose x-ray diffraction (XRD) peaks could be indexed to Fd3¯m space group. The ferroelectric strontium-substituted barium titanate crystallized to a tetragonal crystal structure with P4mm space group. Presence of both crystal symmetries and elemental compositions as per the proposed stoichimetry were observed from experimental results (XRD and electron microscopy techniques). Koop's phenomenological theory could be employed to explain the impedance spectra in the range of 1 kHz to 1 MHz. The effect of Maxwell–Wagner polarization and space charge polarization on the dielectric properties of composites have been observed. The Arrott plot technique successfully explains the suitability of composites for high-energy storage applications. The coupling between both ferro-orderings has been revealed from the magneto-dielectric curves and its dependency on the microstructure has been observed. The magnetocapacitance increased with the increase in NiFe2O4 composition in the (x)NiFe2O4–(1 − x)Ba0.9Sr0.1TiO3 composite. The 30% NiFe2O4 in (x)NiFe2O4–(1 − x)Ba0.9Sr0.1TiO3 composite exhibited overall better energy harvesting (η = 62.9%) and magnetodielectric properties (MC = 1.4%, MI = 20% at 1 kHz).
- 23 May 2024
- Published by Elsevier in Ceramics International
- Vol. 50 (17) , 30514-30532
Structural and enhanced dielectric properties of Al-modified lanthanum strontium manganites
- 23 May 2024
- Published by Elsevier in Ceramics International
- Vol. 50 (17) , 30514-30532
Structural and enhanced dielectric properties of Al-modified lanthanum strontium manganites
- Open Access
- 1 May 2024
- Published by AIP Publishing in AIP Advances
- Vol. 14 (5)
Role of grain interface on dielectric and multiferroic properties of 0-3 type (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 nanocomposites
The (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 (0-3 type particulate) nanocomposites with x = 0.00, 0.02, 0.04, 0.06, 0.08, and 1.00 were prepared by the solid-state method. Cobalt ferrite crystallized into cubic crystal symmetry with an Fd3̄m space group. Strontium-substituted barium titanate crystallized into a tetragonal crystal structure with a P4mm space group. Field emission scanning electron microscopy and transmission electron microscopy techniques show the distribution of different sizes of particle. Polarization vs electric field curves show the highest maximum polarization (Pm) of 10.26 μC/cm2, remnant magnetization (Pr) of 11.70 μC/cm2, and coercivity (Ec) of 19.95 kV/cm for x = 0.04 composition at 35 kV/cm. However, it is smaller than the Ba0.8Sr0.2TiO3 phase (Pm = 16.86 μC/cm2, Pr = 13.20 μC/cm2, and EC = 10.80 kV/cm). The highest dielectric constant of around 9800 was found for x = 0.04 composition, with a very small dielectric loss factor of about 0.02, i.e., less than even 2%. This is ∼10 times compared to that of Ba0.8Sr0.2TiO3 (BSTO), which has been explained by considering interaction at the interface of CoFe2O4 (CFO) and BSTO, leakage current, and variation of the lattice parameter of BSTO in (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 nanocomposite. The magnetic hysteresis loops show squeezing near the origin. The magnetic parameters like coercivity, remnant magnetization, and saturation magnetization increased with the increase in the CoFe2O4 weight fraction. Magnetic interaction between surfaces of magnetic CFO and non-magnetic BSTO is evident from the ΔH vs M plots, and it also evidences the magnetism at the surface of BSTO due to uncompensated spins.
- 1 May 2024
- Published by AIP Publishing in AIP Advances
- Vol. 14 (5)
Open AccessRole of grain interface on dielectric and multiferroic properties of 0-3 type (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 nanocomposites
The (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 (0-3 type particulate) nanocomposites with x = 0.00, 0.02, 0.04, 0.06, 0.08, and 1.00 were prepared by the solid-state method. Cobalt ferrite crystallized into cubic crystal symmetry with an Fd3̄m space group. Strontium-substituted barium titanate crystallized into a tetragonal crystal structure with a P4mm space group. Field emission scanning electron microscopy and transmission electron microscopy techniques show the distribution of different sizes of particle. Polarization vs electric field curves show the highest maximum polarization (Pm) of 10.26 μC/cm2, remnant magnetization (Pr) of 11.70 μC/cm2, and coercivity (Ec) of 19.95 kV/cm for x = 0.04 composition at 35 kV/cm. However, it is smaller than the Ba0.8Sr0.2TiO3 phase (Pm = 16.86 μC/cm2, Pr = 13.20 μC/cm2, and EC = 10.80 kV/cm). The highest dielectric constant of around 9800 was found for x = 0.04 composition, with a very small dielectric loss factor of about 0.02, i.e., less than even 2%. This is ∼10 times compared to that of Ba0.8Sr0.2TiO3 (BSTO), which has been explained by considering interaction at the interface of CoFe2O4 (CFO) and BSTO, leakage current, and variation of the lattice parameter of BSTO in (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 nanocomposite. The magnetic hysteresis loops show squeezing near the origin. The magnetic parameters like coercivity, remnant magnetization, and saturation magnetization increased with the increase in the CoFe2O4 weight fraction. Magnetic interaction between surfaces of magnetic CFO and non-magnetic BSTO is evident from the ΔH vs M plots, and it also evidences the magnetism at the surface of BSTO due to uncompensated spins.
- 15 August 2023
- Published by Wiley in Physica Status Solidi (b)
- Vol. 260 (10)
Crystal Structure, Magnetic, and Dielectric Properties of (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 Multiferroics
The composites (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 are prepared by solid‐state reaction method using microwave double‐step sintering. Ba0.8Sr0.2TiO3 crystallizes to tetragonal crystal symmetry with P4mm space group and CoFe2O4 crystallizes to cubic crystal symmetry with space group. Electron microscopy techniques are used to understand the microstructure, elemental composition, and morphology of the composites. The dielectric properties are measured in the 1 Hz–1 MHz frequency range and 40–400 °C temperature range. Composite with x = 0.1 (ε′ ≈ 170, tan δ = 0.08 at 1 kHz) and 0.2 (ε′ ≈ 390, tan δ = 0.07 at 1 kHz) has better dielectric properties than the parent Ba0.8Sr0.2TiO3 ferroelectric (ε′ ≈ 125, tan δ = 0.16 at 1 kHz) and CoFe2O4 ferrimagnetic phases (ε′ ≈ 375, tan δ = 0.72 at 1 kHz), respectively. Composite with 10% cobalt ferrite has the highest saturation polarization (2.1 μC cm−2), the highest remanent polarization (0.9 μC cm−2), and coercive field (23.9 kV cm−1) compared to ferroelectric phase followed by x = 0.2 composite (PS = 1.6 μC cm−2, Pr = 0.8 μC cm−2, and EC = 19.2 kV cm−1). Composite with x = 0.2 shows the highest magnetic coercive field of 1.96 kOe. Hence, this article advocates that 20% ferrite in the composites is the optimized composition for multiferroic applications. The present study will help to explore piezoelectric, magnetostrictive, and magnetoelectric properties of (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 for the technological application.
- 15 August 2023
- Published by Wiley in Physica Status Solidi (b)
- Vol. 260 (10)
Crystal Structure, Magnetic, and Dielectric Properties of (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 Multiferroics
The composites (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 are prepared by solid‐state reaction method using microwave double‐step sintering. Ba0.8Sr0.2TiO3 crystallizes to tetragonal crystal symmetry with P4mm space group and CoFe2O4 crystallizes to cubic crystal symmetry with space group. Electron microscopy techniques are used to understand the microstructure, elemental composition, and morphology of the composites. The dielectric properties are measured in the 1 Hz–1 MHz frequency range and 40–400 °C temperature range. Composite with x = 0.1 (ε′ ≈ 170, tan δ = 0.08 at 1 kHz) and 0.2 (ε′ ≈ 390, tan δ = 0.07 at 1 kHz) has better dielectric properties than the parent Ba0.8Sr0.2TiO3 ferroelectric (ε′ ≈ 125, tan δ = 0.16 at 1 kHz) and CoFe2O4 ferrimagnetic phases (ε′ ≈ 375, tan δ = 0.72 at 1 kHz), respectively. Composite with 10% cobalt ferrite has the highest saturation polarization (2.1 μC cm−2), the highest remanent polarization (0.9 μC cm−2), and coercive field (23.9 kV cm−1) compared to ferroelectric phase followed by x = 0.2 composite (PS = 1.6 μC cm−2, Pr = 0.8 μC cm−2, and EC = 19.2 kV cm−1). Composite with x = 0.2 shows the highest magnetic coercive field of 1.96 kOe. Hence, this article advocates that 20% ferrite in the composites is the optimized composition for multiferroic applications. The present study will help to explore piezoelectric, magnetostrictive, and magnetoelectric properties of (x)CoFe2O4–(1−x)Ba0.8Sr0.2TiO3 for the technological application.
- 28 April 2023
- Published by Elsevier in Thin Solid Films
- Vol. 776
Directional dependent magnetization in BaFe12O19 thin film
- 28 April 2023
- Published by Elsevier in Thin Solid Films
- Vol. 776
Directional dependent magnetization in BaFe12O19 thin film
- 14 February 2023
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 133 (6) , 064102
Enhanced ferroelectricity and electrocaloric effect of Sm modified BSTO with temperature stability near room temperature
Lead-free ferroelectric materials are essential for environment-friendly solid-state cooling technology. In this respect, the electrocaloric effect of lead-free Ba0.8−xSr0.2SmxTiO3 (x = 0.01–0.05) ceramics has been investigated. The Rietveld refinement reveals that all the ceramics exhibit tetragonal symmetry and the tetragonality decreases for x > 0.03, which is the major reason behind the decrease in both isothermal entropy change and adiabatic temperature change. The degree of diffuseness parameter is enhanced by doping of Sm3+, which confirms the formation of polar nanoregion and the enhancement of the electrocaloric effect parameter by adding extra entropy. The relaxor behavior of the prepared samples is also confirmed by estimating the degree of deviation parameter from the curve. So, the temperature stability of the prepared ceramics is improved in a broad temperature window. The highest isothermal entropy change , adiabatic temperature change , and electrocaloric strength are found to be 1.230 Jkg−1 K−1, 0.862 K, and 0.028 73 K cm/kV at 316 K, respectively, for Ba0.77Sr0.2Sm0.03TiO3.- 14 February 2023
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 133 (6) , 064102
Enhanced ferroelectricity and electrocaloric effect of Sm modified BSTO with temperature stability near room temperature
Lead-free ferroelectric materials are essential for environment-friendly solid-state cooling technology. In this respect, the electrocaloric effect of lead-free Ba0.8−xSr0.2SmxTiO3 (x = 0.01–0.05) ceramics has been investigated. The Rietveld refinement reveals that all the ceramics exhibit tetragonal symmetry and the tetragonality decreases for x > 0.03, which is the major reason behind the decrease in both isothermal entropy change and adiabatic temperature change. The degree of diffuseness parameter is enhanced by doping of Sm3+, which confirms the formation of polar nanoregion and the enhancement of the electrocaloric effect parameter by adding extra entropy. The relaxor behavior of the prepared samples is also confirmed by estimating the degree of deviation parameter from the curve. So, the temperature stability of the prepared ceramics is improved in a broad temperature window. The highest isothermal entropy change , adiabatic temperature change , and electrocaloric strength are found to be 1.230 Jkg−1 K−1, 0.862 K, and 0.028 73 K cm/kV at 316 K, respectively, for Ba0.77Sr0.2Sm0.03TiO3.- 1 November 2021
- Published by Elsevier in Physica B: Condensed Matter
- Vol. 621
Optimization of magnetic properties and hyperthermia study on soft magnetic nickel ferrite fiber
- 1 November 2021
- Published by Elsevier in Physica B: Condensed Matter
- Vol. 621
Optimization of magnetic properties and hyperthermia study on soft magnetic nickel ferrite fiber