Sheng Zhang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Sheng Zhang has a total of 75 co-authors. Here are the top co-authors by number of shared publications:
Zhiyi Zou
4 shared publications- Yuqi Zhang
School of Mechanical Engineering, University of Science and Technology Beijing, Beijing 100089, China
3 shared publications Luo Zhang
2 shared publicationsQingdong Zhang
2 shared publicationsShan Huang
2 shared publications- Viswanathan S. Saji
King Fahd University of Petroleum & Minerals
2 shared publications
Latest Publications
- Open Access
- 15 May 2026
- Published by Elsevier in SSRN Electronic Journal
A high strength-ductility combination governed by deformation mechanism transition in an SLMed FeCoNiCrMo0.2 HEA over a wide temperature range
The rapid development of aerospace, advanced energy, and related fields has prompted an urgent demand for high-performance structural materials capable of operating over extreme temperature ranges. High-entropy alloys (HEAs) are promising candidates in this regard, and selective laser melting (SLM) leverages their potential by enabling the fabrication of complex components. This study systematically investigates the mechanical behavior and deformation mechanisms of an SLM-fabricated (SLMed) FeCoNiCrMo₀.₂ HEA over a temperature range from 173 K to 923 K. The results demonstrate a pronounced and systematic temperature dependence of mechanical performance. At 173 K and 298 K, the alloy achieves an excellent synergy of high strength and ductility. In contrast, at elevated temperatures (623 K, 773 K, 923 K), both strength and ductility decrease concurrently, accompanied by the emergence of pronounced serrated flow associated with the Portevin–Le Chatelier (PLC) effect. By innovatively combining electron backscatter diffraction (EBSD) with refined composite multi scale entropy (RCMSE) analysis, this work quantitatively correlates the evolving complexity of serrated flow with the underlying micro-deformation mechanisms across the temperature range. Microstructural characterization indicates that the superior low- and room-temperature performance originates from synergistic strengthening due to high-density dislocation storage and twinning induced plasticity (TWIP). Conversely, the degradation of mechanical properties at high temperatures is attributed to dynamic recovery (DRV) dominated softening coupled with plastic instability induced by dynamic strain aging (DSA).
- 15 May 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessA high strength-ductility combination governed by deformation mechanism transition in an SLMed FeCoNiCrMo0.2 HEA over a wide temperature range
The rapid development of aerospace, advanced energy, and related fields has prompted an urgent demand for high-performance structural materials capable of operating over extreme temperature ranges. High-entropy alloys (HEAs) are promising candidates in this regard, and selective laser melting (SLM) leverages their potential by enabling the fabrication of complex components. This study systematically investigates the mechanical behavior and deformation mechanisms of an SLM-fabricated (SLMed) FeCoNiCrMo₀.₂ HEA over a temperature range from 173 K to 923 K. The results demonstrate a pronounced and systematic temperature dependence of mechanical performance. At 173 K and 298 K, the alloy achieves an excellent synergy of high strength and ductility. In contrast, at elevated temperatures (623 K, 773 K, 923 K), both strength and ductility decrease concurrently, accompanied by the emergence of pronounced serrated flow associated with the Portevin–Le Chatelier (PLC) effect. By innovatively combining electron backscatter diffraction (EBSD) with refined composite multi scale entropy (RCMSE) analysis, this work quantitatively correlates the evolving complexity of serrated flow with the underlying micro-deformation mechanisms across the temperature range. Microstructural characterization indicates that the superior low- and room-temperature performance originates from synergistic strengthening due to high-density dislocation storage and twinning induced plasticity (TWIP). Conversely, the degradation of mechanical properties at high temperatures is attributed to dynamic recovery (DRV) dominated softening coupled with plastic instability induced by dynamic strain aging (DSA).
- Open Access
- 9 February 2026
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 41, 4757-4770
Composition modification and experimental verification of Hastelloy X superalloy with superior mechanical properties fabricated by laser powder bed fusion
- 9 February 2026
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 41, 4757-4770
Open AccessComposition modification and experimental verification of Hastelloy X superalloy with superior mechanical properties fabricated by laser powder bed fusion
- Open Access
- 25 June 2025
- Published by Elsevier in Materials & Design
- Vol. 256
Multi-nanoprecipitate strengthened aluminium-scandium alloy for additive manufacturing
- 25 June 2025
- Published by Elsevier in Materials & Design
- Vol. 256
Open AccessMulti-nanoprecipitate strengthened aluminium-scandium alloy for additive manufacturing
- Open Access
- 23 October 2024
- Published by MDPI AG in Applied Sciences
- Vol. 14 (21) , 9686
The Effects of Laser Power on the Performance and Microstructure of Inconel 718 Formed by Selective Laser Melting
In this study, the effects of laser power on the microstructure and mechanical properties of Inconel 718 formed by SLM were systematically studied. The results show that with the increase in laser power from 285 W to 360 W, the increase in working temperature in the molten pool promoted the evaporation of gas and the vaporization of the low-melting-point alloy components, and the relative density gradually increased from 99.31% to 99.79%. In addition, with the increase in laser energy density, the microstructure gradually coarsened from columnar dendrites to cellular crystals. The nano-hardness of the material decreased with the increase in laser power. The nano-hardness of four groups of samples from 285 W to 360 W decreased form 3.43 GPa to 2.09 GPa, and the elastic modulus decreased form 205.72 GPa to 199.91 GPa.
- 23 October 2024
- Published by MDPI AG in Applied Sciences
- Vol. 14 (21) , 9686
Open AccessThe Effects of Laser Power on the Performance and Microstructure of Inconel 718 Formed by Selective Laser Melting
In this study, the effects of laser power on the microstructure and mechanical properties of Inconel 718 formed by SLM were systematically studied. The results show that with the increase in laser power from 285 W to 360 W, the increase in working temperature in the molten pool promoted the evaporation of gas and the vaporization of the low-melting-point alloy components, and the relative density gradually increased from 99.31% to 99.79%. In addition, with the increase in laser energy density, the microstructure gradually coarsened from columnar dendrites to cellular crystals. The nano-hardness of the material decreased with the increase in laser power. The nano-hardness of four groups of samples from 285 W to 360 W decreased form 3.43 GPa to 2.09 GPa, and the elastic modulus decreased form 205.72 GPa to 199.91 GPa.
- Top Cited Papers
- 9 May 2024
- Published by Elsevier in International Journal of Machine Tools and Manufacture
- Vol. 199
Additive manufacturing of metallic metamaterials with enhanced mechanical properties enabled by microstructural and structural design
- 9 May 2024
- Published by Elsevier in International Journal of Machine Tools and Manufacture
- Vol. 199
Top Cited PapersAdditive manufacturing of metallic metamaterials with enhanced mechanical properties enabled by microstructural and structural design
- Open Access
- 17 May 2023
- Published by Elsevier in The Lancet Respiratory Medicine
- Vol. 11 (8) , 698-708
Safety and immunogenicity of heterologous boosting with orally aerosolised or intramuscular Ad5-nCoV vaccine and homologous boosting with inactivated vaccines (BBIBP-CorV or CoronaVac) in children and adolescents: a randomised, open-label, parallel-controlled, non-inferiority, single-centre study
- 17 May 2023
- Published by Elsevier in The Lancet Respiratory Medicine
- Vol. 11 (8) , 698-708
Open AccessSafety and immunogenicity of heterologous boosting with orally aerosolised or intramuscular Ad5-nCoV vaccine and homologous boosting with inactivated vaccines (BBIBP-CorV or CoronaVac) in children and adolescents: a randomised, open-label, parallel-controlled, non-inferiority, single-centre study
- Open Access
Effect of Heat Treatment on the Microstructure and Mechanical Properties of Additive Manufactured Ti-6.5Al-2Zr-1Mo-1V Alloy
Ti-6.5Al-2Zr-1Mo-1V (TA15), widely used in the aerospace industry, is a medium- to high-strength, near-α titanium alloy with high aluminium equivalent value. The TA15 fabricated via laser powder bed fusion (L-PBF) normally presents a typical brittle appearance in as-built status, with high strength and low ductility. In this study, the microstructure and properties of L-PBF TA15 were engineered by various heat treatments below the β-transus temperature (1022 °C). After heat treatment, the original acicular martensite gradually transforms into a typical lamellar α + β dual-phase structure. Withannealing temperature increases, the lamellar α phase thickened with a decreased aspect ratio. Globularisation of the α grain can be noticed when annealing above 800 °C, which leads to a balance between strength and ductility. After heat treatment between 800–900 °C, the desired combination of strength and ductility can be achieved, with elongation of about 12.5% and ultimate tensile strength of about 1100 Mpa.
Open AccessEffect of Heat Treatment on the Microstructure and Mechanical Properties of Additive Manufactured Ti-6.5Al-2Zr-1Mo-1V Alloy
Ti-6.5Al-2Zr-1Mo-1V (TA15), widely used in the aerospace industry, is a medium- to high-strength, near-α titanium alloy with high aluminium equivalent value. The TA15 fabricated via laser powder bed fusion (L-PBF) normally presents a typical brittle appearance in as-built status, with high strength and low ductility. In this study, the microstructure and properties of L-PBF TA15 were engineered by various heat treatments below the β-transus temperature (1022 °C). After heat treatment, the original acicular martensite gradually transforms into a typical lamellar α + β dual-phase structure. Withannealing temperature increases, the lamellar α phase thickened with a decreased aspect ratio. Globularisation of the α grain can be noticed when annealing above 800 °C, which leads to a balance between strength and ductility. After heat treatment between 800–900 °C, the desired combination of strength and ductility can be achieved, with elongation of about 12.5% and ultimate tensile strength of about 1100 Mpa.