Dashuang Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Dashuang Liu has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
Ping Wei
School of Material Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang, China
2 shared publicationsAnzhe Shen
School of Material Science and Engineering, Hefei University of Technology, Hefei, China
1 shared publicationChun Li
School of Material Science and Engineering, Hefei University of Technology, Hefei, China
1 shared publicationJiayou Wang
School of Material Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang, People’s Republic of China
1 shared publicationMingfang Wu
School of Material Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang, People’s Republic of China
1 shared publicationR. P. Liu
College of Material Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016, China
1 shared publication
Latest Publications
- 17 February 2025
- Published by Springer Nature in Welding in the World
- Vol. 70 (1) , 19-33
Effect of laser power on microstructure and mechanical properties of W/Ni/Cu laser welded joints
- 17 February 2025
- Published by Springer Nature in Welding in the World
- Vol. 70 (1) , 19-33
Effect of laser power on microstructure and mechanical properties of W/Ni/Cu laser welded joints
- 23 September 2020
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 26 (1) , 1-10
Effect of welding wires on fatigue property of 7N01-T4 aluminium alloy joints
The effect of ER5356 and ER5087 welding wires on fatigue property of MIG-welded 7N01-T4 aluminium alloy joints was investigated. The microstructure of ER5087 welded joint is similar to that of ER5356 joint. However, the fusion zone of the welding joint with ER5087 has a smaller grain size than that of the joint with ER5356. The fatigue strength of joints welded with ER5356 and ER5087 is 105.9 and 103.2 MPa at 107 cycles. During the fatigue process, the crack initiation for joints welded using ER5087 is due to porosity while for ER5356 is due to microcracks from eutectic melting in the heat-affected zone.
- 23 September 2020
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 26 (1) , 1-10
Effect of welding wires on fatigue property of 7N01-T4 aluminium alloy joints
The effect of ER5356 and ER5087 welding wires on fatigue property of MIG-welded 7N01-T4 aluminium alloy joints was investigated. The microstructure of ER5087 welded joint is similar to that of ER5356 joint. However, the fusion zone of the welding joint with ER5087 has a smaller grain size than that of the joint with ER5356. The fatigue strength of joints welded with ER5356 and ER5087 is 105.9 and 103.2 MPa at 107 cycles. During the fatigue process, the crack initiation for joints welded using ER5087 is due to porosity while for ER5356 is due to microcracks from eutectic melting in the heat-affected zone.
- 1 November 2015
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 20 (8) , 693-701
Microstructure and wear mechanism change by Nb added in slag free self-shielded flux cored wire
The iron based hardfacing alloys were produced using slag free self-shielded flux cored wires with varying niobium contents. The results show that NbC acted as the nucleus of primary M7(C, B)3 (M = Cr, Fe mainly) carbides and decreased the amount of M7(C,B)3 carbides when niobium was added into the alloys. When 18 wt-%Fe–Nb (60 wt-%Nb) was added, the microstructure of hardfacing alloy transformed from hypereutectic structure to a eutectic one due to the formation of NbC, which consumed a mass of carbon. The microstructure changed into a hypoeutectic structure when the Fe–Nb content was up to 24 wt-%. With the increase in Fe–Nb content, the main abrasive wear mechanism changed from microcracking to microcutting and microploughing due to the formation of NbC and the reduction of primary M7(C, B)3 carbides. The wear loss of the alloy with 18 wt-%Fe–Nb addition was the smallest among all the alloys.
- 1 November 2015
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 20 (8) , 693-701
Microstructure and wear mechanism change by Nb added in slag free self-shielded flux cored wire
The iron based hardfacing alloys were produced using slag free self-shielded flux cored wires with varying niobium contents. The results show that NbC acted as the nucleus of primary M7(C, B)3 (M = Cr, Fe mainly) carbides and decreased the amount of M7(C,B)3 carbides when niobium was added into the alloys. When 18 wt-%Fe–Nb (60 wt-%Nb) was added, the microstructure of hardfacing alloy transformed from hypereutectic structure to a eutectic one due to the formation of NbC, which consumed a mass of carbon. The microstructure changed into a hypoeutectic structure when the Fe–Nb content was up to 24 wt-%. With the increase in Fe–Nb content, the main abrasive wear mechanism changed from microcracking to microcutting and microploughing due to the formation of NbC and the reduction of primary M7(C, B)3 carbides. The wear loss of the alloy with 18 wt-%Fe–Nb addition was the smallest among all the alloys.