Han-Wen Xiao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Han-Wen Xiao has a total of 27 co-authors. Here are the top co-authors by number of shared publications:
Tao Jiang
Ministry-of-Education Key Laboratory of the Green Preparation and Application of Functional Materials, Faculty of Materials Science and Engineering, Hubei University, Wuhan 430062, China
4 shared publicationsJen‐Taut Yeh
Ministry-of-Education Key Laboratory of the Green Preparation and Application of Functional Materials, Faculty of Materials Science and Engineering, Hubei University, Wuhan 430062, China
3 shared publications- Chi-Min Shu
National Yunlin University of Science and Technology
2 shared publications - Fang-Chang Tsai
Hubei Key Laboratory of Polymer Materials, Key Laboratory for the Green Preparation and Application of Functional Materials (Ministry of Education), Hubei Collaborative Innovation Center for Advanced Organic Chemical Materials, School of Materials Science and Engineering, Faculty of Life Sciences, Hubei University, Wuhan 430062, China
2 shared publications Lung-Chang Tsai
Department of Safety, Health, and Environmental Engineering, National Yunlin Universi-ty of Science and Technology, Douliou, Yunlin, Taiwan ROC
2 shared publications- Sheng Wen
Faculty of Chemistry and Materials Science, Hubei Engineering University, P. R. China
2 shared publications
Latest Publications
- Open Access
- 9 May 2013
- Published by IntechOpen
Adsorption of Methylene Blue on Multi-Walled Carbon Nanotubes in Sodium Alginate Gel Beads
- 9 May 2013
- Published by IntechOpen
Open AccessAdsorption of Methylene Blue on Multi-Walled Carbon Nanotubes in Sodium Alginate Gel Beads
- 18 November 2010
- Published by Wiley in Polymer Composites
- Vol. 31 (12) , 2057-2068
Kinetics and crystal structure of poly(lactic acid) crystallized nonisothermally: Effect of plasticizer and nucleating agent
The kinetics of neat poly(lactic acid) (PLA) and its composites with triphenyl phosphate (TPP) and/or talc crystallized nonisothermally at different cooling rates of 1, 2.5, 5, 7.5, and 10°C/min was analyzed by differential scanning calorimetry and described by Avrami equation and combined Avrami‐Ozawa equation. The results showed that talc acted as PLA nucleating agent accelerated crystallization rate by decreasing the crystallization half‐time t1/2 or rate parameter F(T), whereas TPP acted as PLA plasticizer decreased crystallization rate. For neat PLA and plasticized PLA, the average values of Avrami exponent n were almost close to each other, but added TPP decreased crystallization rate constant k. As for PLA composites with talc, the crystallization process was relatively complex, and was divided into three regimes. At a given cooling rate, the value of n2 was almost larger than that that of n1 or n3, whereas the value of k2 was less than that of k1 or k3. The effective activation energy ΔEx calculated from Friedman formula increased with the increase of relative crystallinity and TPP content, whereas decreased with the presence of talc. Wide angle X‐ray diffraction verified that all samples crystallized nonisothermally in cooling rate range of 1–10°C/min form α‐form. POLYM. COMPOS., 31:2057–2068, 2010. © 2010 Society of Plastics Engineers
- 18 November 2010
- Published by Wiley in Polymer Composites
- Vol. 31 (12) , 2057-2068
Kinetics and crystal structure of poly(lactic acid) crystallized nonisothermally: Effect of plasticizer and nucleating agent
The kinetics of neat poly(lactic acid) (PLA) and its composites with triphenyl phosphate (TPP) and/or talc crystallized nonisothermally at different cooling rates of 1, 2.5, 5, 7.5, and 10°C/min was analyzed by differential scanning calorimetry and described by Avrami equation and combined Avrami‐Ozawa equation. The results showed that talc acted as PLA nucleating agent accelerated crystallization rate by decreasing the crystallization half‐time t1/2 or rate parameter F(T), whereas TPP acted as PLA plasticizer decreased crystallization rate. For neat PLA and plasticized PLA, the average values of Avrami exponent n were almost close to each other, but added TPP decreased crystallization rate constant k. As for PLA composites with talc, the crystallization process was relatively complex, and was divided into three regimes. At a given cooling rate, the value of n2 was almost larger than that that of n1 or n3, whereas the value of k2 was less than that of k1 or k3. The effective activation energy ΔEx calculated from Friedman formula increased with the increase of relative crystallinity and TPP content, whereas decreased with the presence of talc. Wide angle X‐ray diffraction verified that all samples crystallized nonisothermally in cooling rate range of 1–10°C/min form α‐form. POLYM. COMPOS., 31:2057–2068, 2010. © 2010 Society of Plastics Engineers
- 14 July 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 118 (6) , 3558-3569
Isothermal crystallization kinetics and crystal structure of poly(lactic acid): Effect of triphenyl phosphate and talc
In this article, kinetics of neat poly(lactic acid) (PLA) and its blends with triphenyl phosphate (TPP) and/or talc crystallized isothermally in the temperature range of 113–128°C was analyzed by differential scanning calorimetry (DSC) and described by the Avrami equation. The results showed that the average value of Avrami exponents n is around 2.0 for neat PLA and the PLA/15TPP blend, and around 3.0 for the PLA/1.2Talc blend and the PLA/15TPP/1.2Talc blend. The crystallization rate constants k for neat PLA and its blends were increased in the following order: the PLA/15TPP blend, neat PLA, the PLA/15TPP/1.2Talc blend, and PLA/1.2Talc blend. The half‐time of crystallization t1/2 was increased with an increase of crystallization temperature Tc and the presence of TPP, and was decreased sharply with the incorporation of talc. Further investigation into crystallization activation energy ΔEa of neat PLA and its blends with 15 wt % TPP and/or 1.2 wt % talc showed that the values of ΔEa were increased with the incorporation of TPP and/or talc compared to that of neat PLA. It was verified by wide angle X‐ray diffraction (WAXD) that neat PLA and its blends with TPP and/or talc crystallized isothermally in the temperature range of 113–128°C, and all formed the α‐form crystal after enough annealing time. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 14 July 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 118 (6) , 3558-3569
Isothermal crystallization kinetics and crystal structure of poly(lactic acid): Effect of triphenyl phosphate and talc
In this article, kinetics of neat poly(lactic acid) (PLA) and its blends with triphenyl phosphate (TPP) and/or talc crystallized isothermally in the temperature range of 113–128°C was analyzed by differential scanning calorimetry (DSC) and described by the Avrami equation. The results showed that the average value of Avrami exponents n is around 2.0 for neat PLA and the PLA/15TPP blend, and around 3.0 for the PLA/1.2Talc blend and the PLA/15TPP/1.2Talc blend. The crystallization rate constants k for neat PLA and its blends were increased in the following order: the PLA/15TPP blend, neat PLA, the PLA/15TPP/1.2Talc blend, and PLA/1.2Talc blend. The half‐time of crystallization t1/2 was increased with an increase of crystallization temperature Tc and the presence of TPP, and was decreased sharply with the incorporation of talc. Further investigation into crystallization activation energy ΔEa of neat PLA and its blends with 15 wt % TPP and/or 1.2 wt % talc showed that the values of ΔEa were increased with the incorporation of TPP and/or talc compared to that of neat PLA. It was verified by wide angle X‐ray diffraction (WAXD) that neat PLA and its blends with TPP and/or talc crystallized isothermally in the temperature range of 113–128°C, and all formed the α‐form crystal after enough annealing time. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 27 April 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 117 (5) , 2980-2992
Kinetics and crystal structure of isothermal crystallization of poly(lactic acid) plasticized with triphenyl phosphate
In this article, the spherulitic growth rate of neat and plasticized poly(lactic acid) (PLA) with triphenyl phosphate (TPP) was measured and analyzed in the temperature range of 104–142°C by polarizing optical microscopy. Neat PLA had the maximum value of 0.28 μm/s at 132°C, whereas plasticized PLA had higher value than that of neat PLA, but the temperature corresponding to the maximum value was shifted toward lower one with increasing TPP content. The isothermal crystallization kinetics of neat and plasticized PLA was also analyzed by differential scanning calorimetry and described by the Avrami equation. The results showed for neat PLA and its blends with various TPP contents, the average value of Avrami exponents n were close to around 2.5 at two crystallization temperatures of 113 and 128°C, the crystallization rate constant k was decreased, and the half‐life crystallization time t1/2 was increased with TPP content. For neat PLA and its blend with 15 wt % TPP content, the average value of n was 2.0 and 2.3, respectively, the value of k was decreased, and the value of t1/2 was increased with crystallization temperature (Tc). Further investigation into crystallization activation energy ΔEa of neat PLA and its blend with 15 wt % TPP showed that ΔEa of plasticized PLA was increased compared to neat PLA. It was verified by wide‐angle X‐ray diffraction that neat PLA and its blends containing various TPP contents crystallized isothermally in the temperature range of 113–128°C all form the α‐form crystal. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 27 April 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 117 (5) , 2980-2992
Kinetics and crystal structure of isothermal crystallization of poly(lactic acid) plasticized with triphenyl phosphate
In this article, the spherulitic growth rate of neat and plasticized poly(lactic acid) (PLA) with triphenyl phosphate (TPP) was measured and analyzed in the temperature range of 104–142°C by polarizing optical microscopy. Neat PLA had the maximum value of 0.28 μm/s at 132°C, whereas plasticized PLA had higher value than that of neat PLA, but the temperature corresponding to the maximum value was shifted toward lower one with increasing TPP content. The isothermal crystallization kinetics of neat and plasticized PLA was also analyzed by differential scanning calorimetry and described by the Avrami equation. The results showed for neat PLA and its blends with various TPP contents, the average value of Avrami exponents n were close to around 2.5 at two crystallization temperatures of 113 and 128°C, the crystallization rate constant k was decreased, and the half‐life crystallization time t1/2 was increased with TPP content. For neat PLA and its blend with 15 wt % TPP content, the average value of n was 2.0 and 2.3, respectively, the value of k was decreased, and the value of t1/2 was increased with crystallization temperature (Tc). Further investigation into crystallization activation energy ΔEa of neat PLA and its blend with 15 wt % TPP showed that ΔEa of plasticized PLA was increased compared to neat PLA. It was verified by wide‐angle X‐ray diffraction that neat PLA and its blends containing various TPP contents crystallized isothermally in the temperature range of 113–128°C all form the α‐form crystal. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 3 February 2004
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 92 (1) , 357-362
Morphology, rheology, and mechanical properties of dynamically cured EPDM/PP blend: Effect of curing agent dose variation
- 3 February 2004
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 92 (1) , 357-362
Morphology, rheology, and mechanical properties of dynamically cured EPDM/PP blend: Effect of curing agent dose variation