V. A. Bershtein
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
V. A. Bershtein has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
P. N. Yakushev
Ioffe Physico‐Technical Institute, Russian Academy of Sciences, 194021 St. Petersburg, Russia
2 shared publications- Alexander Fainleib
Institute of Macromolecular Chemistry of the National Academy of Sciences of Ukraine, 48 Kharkivske Shose, 02155 Kyiv, Ukraine
1 shared publication I. Bey
Institute of Macromolecular Chemistry, National Academy of Sciences of Ukraine, 02160 Kyiv, Ukraine
1 shared publicationL. Brozova
Institute of Macromolecular Chemistry, Heyrovsky square 2, 16206 Prague, Czech Republic
1 shared publicationL. David
Laboratoire des Materiaux Polymeres et Biomateriaux, CNRS 5627, Universite Claude Bernard, Villeurbanne, France
1 shared publicationL. M. Egorova
Ioffe Physico-Technical Institute, Russian Academy of Sciences, 194021 St. Petersburg, Russia
1 shared publication
Latest Publications
- 3 October 2005
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 43 (22) , 3261-3272
Structural/compositional nanoheterogeneity and glass‐transition plurality in amorphous polycyanurate–poly(tetramethylene glycol) hybrid networks
The nanostructure and dynamics over the temperature range of −140 to 300 °C were studied in a series of polycyanurate (PCN)–poly(tetramethylene glycol) (PTMG) hybrid networks by wide‐angle X‐ray diffraction and small‐angle X‐ray scattering, with a synchrotron radiation setup, and by differential scanning calorimetry (DSC) and laser‐interferometric creep rate spectroscopy (CRS) techniques, respectively. The networks were synthesized from the dicyanate ester of bisphenol A and hydroxyl‐terminated PTMG with a number‐average molecular weight of 1.000 g/mol; the PTMG content varied from 0 to 40 wt %, and the degree of its chemical incorporation into the PCN network changed from 78.8 to 97%. The noncrystalline structure and considerable structural nanoheterogeneity of the hybrid networks were shown. CRS/DSC analysis revealed a complicated dynamic behavior, that is, a wide dispersion of glass transitions in the hybrid networks due to the presence of nanodomains with different degrees of rigid crosslinking (i.e., compositional nanoheterogeneity). Besides the physical significance, the plurality of glass transitions found in the PCN–PTMG hybrid networks was also of practical interest because it resulted in increasing mechanical strength of the brittle PCN network due to microplasticity arising at room temperature and moderate temperatures and the retention of some rigidity and creep resistance at temperatures much higher than the basic glass‐transition temperature. © 2005 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 43: 3261–3272, 2005
- 3 October 2005
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 43 (22) , 3261-3272
Structural/compositional nanoheterogeneity and glass‐transition plurality in amorphous polycyanurate–poly(tetramethylene glycol) hybrid networks
The nanostructure and dynamics over the temperature range of −140 to 300 °C were studied in a series of polycyanurate (PCN)–poly(tetramethylene glycol) (PTMG) hybrid networks by wide‐angle X‐ray diffraction and small‐angle X‐ray scattering, with a synchrotron radiation setup, and by differential scanning calorimetry (DSC) and laser‐interferometric creep rate spectroscopy (CRS) techniques, respectively. The networks were synthesized from the dicyanate ester of bisphenol A and hydroxyl‐terminated PTMG with a number‐average molecular weight of 1.000 g/mol; the PTMG content varied from 0 to 40 wt %, and the degree of its chemical incorporation into the PCN network changed from 78.8 to 97%. The noncrystalline structure and considerable structural nanoheterogeneity of the hybrid networks were shown. CRS/DSC analysis revealed a complicated dynamic behavior, that is, a wide dispersion of glass transitions in the hybrid networks due to the presence of nanodomains with different degrees of rigid crosslinking (i.e., compositional nanoheterogeneity). Besides the physical significance, the plurality of glass transitions found in the PCN–PTMG hybrid networks was also of practical interest because it resulted in increasing mechanical strength of the brittle PCN network due to microplasticity arising at room temperature and moderate temperatures and the retention of some rigidity and creep resistance at temperatures much higher than the basic glass‐transition temperature. © 2005 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 43: 3261–3272, 2005
- 1 April 2002
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 40 (10) , 1056-1069
Molecular dynamics in nanostructured polyimide–silica hybrid materials and their thermal stability
Molecular motion and thermal stability in two series of nanophase‐separated polyimide–silica (PI–SiO2) hybrid materials with chemically bound components were studied. The hybrids were synthesized from p‐aminophenyltrimethoxysilane‐terminated poly(amic acid)s as PI precursors and tetramethoxysilane as a silica precursor via a sol–gel process. The hybrids differed in their PI chemical structure and chain length (number‐average molecular weight = 5.000, 7.500, or 10.000) and in their SiO2 content, which ranged from 0 to 50 wt %. Differential scanning calorimetry, laser‐interferometric creep rate spectroscopy, and thermally stimulated depolarization current techniques were used for studying the dynamics from 100 to 650 K and from 10−3 to 10−2 Hz. Comparative thermogravimetric measurements were also carried out from 300 to 900 K. Silica nano‐ or submicrodomains that formed affected PI dynamics in two opposite directions. Because of the loosening of the molecular packing of PI chains confined to nanometer‐scale spaces between silica constraints, an enhancement of small‐scale motion, mostly at temperatures below the β‐relaxation region, occurred. However, a partial or total suppression of segmental motion could be observed above the β‐relaxation temperature, drastically so for the shortest PI chains at elevated silica contents and within or close to the glass‐transition range, because of the covalent anchoring of chain ends to silica domains. Large changes in thermal stability, including a 2.5‐fold increase in the apparent activation energy of degradation, were observed in the hybrids studied. A greater than 100 °C rise in long‐term thermal stability could be predicted for some hybrids with respect to pure PI. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 1056–1069, 2002
- 1 April 2002
- Published by Wiley in Journal of Polymer Science Part B: Polymer Physics
- Vol. 40 (10) , 1056-1069
Molecular dynamics in nanostructured polyimide–silica hybrid materials and their thermal stability
Molecular motion and thermal stability in two series of nanophase‐separated polyimide–silica (PI–SiO2) hybrid materials with chemically bound components were studied. The hybrids were synthesized from p‐aminophenyltrimethoxysilane‐terminated poly(amic acid)s as PI precursors and tetramethoxysilane as a silica precursor via a sol–gel process. The hybrids differed in their PI chemical structure and chain length (number‐average molecular weight = 5.000, 7.500, or 10.000) and in their SiO2 content, which ranged from 0 to 50 wt %. Differential scanning calorimetry, laser‐interferometric creep rate spectroscopy, and thermally stimulated depolarization current techniques were used for studying the dynamics from 100 to 650 K and from 10−3 to 10−2 Hz. Comparative thermogravimetric measurements were also carried out from 300 to 900 K. Silica nano‐ or submicrodomains that formed affected PI dynamics in two opposite directions. Because of the loosening of the molecular packing of PI chains confined to nanometer‐scale spaces between silica constraints, an enhancement of small‐scale motion, mostly at temperatures below the β‐relaxation region, occurred. However, a partial or total suppression of segmental motion could be observed above the β‐relaxation temperature, drastically so for the shortest PI chains at elevated silica contents and within or close to the glass‐transition range, because of the covalent anchoring of chain ends to silica domains. Large changes in thermal stability, including a 2.5‐fold increase in the apparent activation energy of degradation, were observed in the hybrids studied. A greater than 100 °C rise in long‐term thermal stability could be predicted for some hybrids with respect to pure PI. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 1056–1069, 2002