CSChanggen Shi

Changgen Shi

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Changgen Shi has a total of 24 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Study on interface characteristics of TC4/7075 explosive welding based on molecular dynamics algorithm

    by Wu Xiaoming, Cai Yonggen, Shi Changgen

    The preparation of TC4/7075 composites for ultra-thin flyer plates is a significant challenge in the field of explosive welding. A weldability window for multi-layer metal explosive welding and a configuration for ultra-thin flyer plate explosive welding were established in this study. TC4/7075 composite materials were successfully prepared with a flyer plate thickness of only 0.3 mm. An analysis was conducted on the material bonding ability, element diffusion, crystal evolution, and microscopic morphology during the explosive welding process of TC4/7075, utilizing the weldability window, molecular dynamics algorithm, and electron backscattered diffraction testing. The results show that various dislocations are present at the interface, predominantly 1/6 ⟨112⟩ dislocations. Element diffusion primarily occurs during the unloading stage at high temperature and zero external pressure; the interface has the best bonding ability when titanium exhibits FCC lattice structure. The prepared composite material demonstrates high intra-grain and grain boundary stresses; the rolling texture is observed on the aluminum side while an equiaxed twin structure forms on the titanium side due to interactions between stacking faults, Stair-rod dislocations, and Hirth immovable dislocations.


  • Open Access

    Atomic motion behavior calculation and bonding mechanism analysis of explosive welding of high-strength and high-hardness titanium alloy Ti6Al4V/aluminum alloy 7075

    by Wu Xiaoming, Shi Changgen, Wang Haitao, Luo Xuchuan, Sun Zerui

    The explosive welding technology of titanium alloy Ti6Al4V/aluminum alloy 7075 is the most valuable research problem in the field of Ti/Al explosive welding. In this paper, the smooth particle hydrodynamics and molecular dynamics algorithms are used to conduct multi-scale numerical calculations on the explosive welding of Ti6Al4V and 7075. The interface morphology, interface atomic movement, lattice changes and crystal defects are comprehensively analyzed. With the calculation as a reference, the Ti6Al4V/7075 composite with a flat interface is prepared. The calculation results indicate that with the transformation of titanium aluminum crystal structure, a large number of various dislocations, mainly 1/6〈110〉dislocations, are generated on the titanium side; During explosive welding, uniform and stable element diffusion occurred. Element diffusion mainly occurred in the unloading stage when the pressure was 0. The melting zone and ablation zone were composed of TiAl and TiAl3, respectively; The fundamental reason for the combination of Ti6Al4V/7075 is the diffusion of elements and the solid-phase binding of atoms.


  • Open Access

    Analysis and Characterization of Three Charge Thicknesses in TA1/Al1060/Al7075 Explosive Welding Composite Process

    by Zhiqun Xia, Haitao Wang, Changgen Shi, Zerui Sun, Qiang Wang, Xvchuan Luo

    The titanium/aluminum composite materials overcome the limitations of single metal materials and achieve lightweight, high-strength, and corrosion-resistant properties. However, there have been no reports on explosion-welded composites of titanium alloys and seven-series aluminum alloys. Therefore, TA1/Al1060/Al7075 explosion-welded plates with three different explosive thicknesses were successfully prepared using Al1060 as the transition layer. The SPH-FEM coupled algorithm was employed to analyze the detonation process in detail and predict the interface under different explosive thicknesses. The results showed that during the explosion welding process, the high temperature, pressure, and high-speed impact resulted in significant plastic deformation and jetting phenomena at the bonding interface, which were in good agreement with the experimental observations. With the increase in explosive thickness, the TA1/Al1060 bonding interface exhibited a flat shape, while the Al1060/Al7075 interface transitioned from a flat to a wavy morphology. Moreover, the crack, vortex, and TiAl3 were observed at the interface. Mechanical testing results revealed that the composite plate with a 35 mm explosive thickness exhibited the best tensile, shear, and bending performance, indicating the optimal process parameter. This study provides significant support and reference for the application of explosion welding technology in titanium alloys and seven-series aluminum alloy composite materials.


  • Open Access

    Experimental and numerical approach to titanium-aluminum explosive welding

    by Xiaoming Wu, Changgen Shi, Ke Feng, Li Gao, Wenxuan Li, Kun Qian

    The welding parameters of TA2/1060/5083 were calculated accurately through a combination of explosive welding weldability window and numerical simulation, based on which explosion welding experiments were conducted using these parameters obtained. Then, a test was carried out on the mechanical properties of the composite plates obtained from the experiments and microstructure characterization was performed. As suggested by the results, TA2/1060 was a excellent straight bond, and the interface of 1060/5083 was a sine-wave featuring both vortex structure and splashing molten block structure, with an average wavelength of 700μm and a wave height of 100μm. The tensile strength and shear strength of the composite materials reached 354 MPa and 110 MPa, respectively, while the material showed the signs of ductile fracture. Moreover, work hardening and fine grain strengthening occurred at the interface, as did the element diffusion of Ti-Al, with a maximum diffusion depth of 32μm.


  • Comprehensive investigation of effect of the charge thickness and stand-off gap on interface characteristics of explosively welded TA2 and Q235B

    by Zerui Sun, Changgen Shi, Xiaoming Wu, Hang Shi

    The current work is all a matter of the separate study of the effect of charge thickness or stand-off gap on the quality of the bonding interface. The relationship among collision velocity, charge thickness and stand-off gap in parallel explosive welding was illustrated. Four TA2/Q235B composite plates with different parameters were manufactured to investigate the effect of the collision velocity on the bonding interface. The interface morphology, element diffusion and mechanical properties of samples with different parameters were discussed, respectively. The results indicated all samples were corrugated combination and the higher-speed samples obtained larger waves with more pronounced vortex regions and melted layers. The composite interfaces presented six different grain structures due to plastic deformation, respectively. In addition, high-speed samples had a wider element diffusion layer. TiFe3 and TiFe2 were found in the vortex region and the melting layer, respectively. The mechanical tests showed that the hardness of the interface was the highest and decreased gradually to both sides. The tensile strength and shear strength were higher than the raw material. The higher collision velocity increased the tensile strength but decreased the shear strength. The intermetallic compounds with cleavage fracture existed at the interface and ductile fracture occurred at other positions.


  • Open Access

    Influence of Explosive Ratio on Morphological and Structural Properties of Ti/Al Clads

    by Zhonghang Fang, Changgen Shi, Hesheng Shi, Zerui Sun

    The current work focuses on the effect of explosive ratio R on the comprehensive properties of Ti/Al clads manufactured via explosive welding. The lower and upper limits of explosive ratio, namely R1 and R2, were determined according to the R–δf (flyer plate thickness) welding window. Two TA2/1060 explosive cladding plates were successfully manufactured at the different explosive ratios. Microstructure investigation was conducted by optical microscopy (OM), scanning electron microscopy (SEM), and energy dispersive spectrometer (EDS). The small wave bonding interface was observed at R1, where the vortex structure containing the ingot structure appeared periodically. The bonding interface presented a big wave bonding morphology and a locally continuous melting layer at R2. Many prolonged grains and adiabatic shear bands (ASBs) were found near the interface for a greater explosive load. Intermetallic compounds were formed in the bonding zones of the two plates. The thickness of element diffusion area increased with an increasing explosive ratio. Comparative tests of mechanical properties indicated that the tensile shear strength at R1 was higher. The microhardness, tensile strength, and bending performance of the two plates are similar and acceptable. Tensile fracture analysis indicated the fracture mode at R1 was ductile fracture, while the explosive cladding plate at R2 had mainly ductile fracture with quasi-cleavage fracture as the supplement.