Guangwei Yang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Guangwei Yang has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
Xinhua Wang
University of Science and Technology Beijing
3 shared publicationsFuxiang Huang
University of Science and Technology Beijing
2 shared publicationsWanjun Wang
School of Metallurgical and Ecological Engineering University of Science and Technology Beijing Beijing 100083 China
2 shared publicationsYuqun Yin
Technical Research Institute Nanjing Iron and Steel United Corporation Nanjing 210035 China
2 shared publicationsChunxia Tang
Technical Research Institute Nanjing Iron and Steel United Corporation Nanjing 210035 China
1 shared publicationDie Yang
University of Science and Technology Beijing
1 shared publication
Latest Publications
- 30 September 2014
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 46 (1) , 145-154
Influence of Calcium Addition on Inclusions in LCAK Steel with Ultralow Sulfur Content
- 30 September 2014
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 46 (1) , 145-154
Influence of Calcium Addition on Inclusions in LCAK Steel with Ultralow Sulfur Content
- 11 November 2013
- Published by Wiley in Steel Research International
- Vol. 85 (5) , 784-792
Influence of Reoxidation in Tundish on Inclusion for Ca‐Treated Al‐Killed Steel
Reoxidation usually happens during steelmaking, especially in tundish. Severe reoxidation contaminates the steel cleanliness, and detrimentally affects the steel quality and performance. The purpose of this study is to highlight the adverse effect of reoxidation in tundish on non‐metallic inclusion in liquid steel and the end product for Ca‐treated Al‐killed steel. Inclusions of RH refining, tundish, slab, and plate were investigated on API‐X70 pipeline steel. To get a more reliable result, automatic scanning electron microscopy ASPEX PSEM EXPLORER was employed to analyze the inclusion with a much larger scan area. It was found that reoxidation in tundish converted the well‐modified liquid calcium aluminates into solid Al2O3‐rich inclusions, which are more likely to cause nozzle clogging than pure Al2O3, and the inclusion number dramatically increased form 2.8 µm−2 after RH treatment to 13.5 µm−2 in tundish, further decreased to about 6.0 µm−2 in slab and plate. It indicated that reoxidation in tundish put the calcium treatment and strong capacity of inclusion removal during RH treatment in vain. The ratio of liquid inclusions was proportional to average CaO/Al2O3 in inclusions. Big aggregates and stringer shaped inclusions with CaO/Al2O3 locating between 0.08 and 0.13 were found at the 1/2 and 1/4 slab and plate thickness. The stringer shaped inclusions in the plate were the product of big aggregates in the slab after rolling, and made the plate fail to pass ultrasonic testing.
- 11 November 2013
- Published by Wiley in Steel Research International
- Vol. 85 (5) , 784-792
Influence of Reoxidation in Tundish on Inclusion for Ca‐Treated Al‐Killed Steel
Reoxidation usually happens during steelmaking, especially in tundish. Severe reoxidation contaminates the steel cleanliness, and detrimentally affects the steel quality and performance. The purpose of this study is to highlight the adverse effect of reoxidation in tundish on non‐metallic inclusion in liquid steel and the end product for Ca‐treated Al‐killed steel. Inclusions of RH refining, tundish, slab, and plate were investigated on API‐X70 pipeline steel. To get a more reliable result, automatic scanning electron microscopy ASPEX PSEM EXPLORER was employed to analyze the inclusion with a much larger scan area. It was found that reoxidation in tundish converted the well‐modified liquid calcium aluminates into solid Al2O3‐rich inclusions, which are more likely to cause nozzle clogging than pure Al2O3, and the inclusion number dramatically increased form 2.8 µm−2 after RH treatment to 13.5 µm−2 in tundish, further decreased to about 6.0 µm−2 in slab and plate. It indicated that reoxidation in tundish put the calcium treatment and strong capacity of inclusion removal during RH treatment in vain. The ratio of liquid inclusions was proportional to average CaO/Al2O3 in inclusions. Big aggregates and stringer shaped inclusions with CaO/Al2O3 locating between 0.08 and 0.13 were found at the 1/2 and 1/4 slab and plate thickness. The stringer shaped inclusions in the plate were the product of big aggregates in the slab after rolling, and made the plate fail to pass ultrasonic testing.
- 26 April 2013
- Published by Wiley in Steel Research International
- Vol. 85 (1) , 26-34
Transient Inclusion Evolution during RH Degassing
Inclusion morphology, composition and number at different times of RH vacuum treatment were investigated on API‐X70 pipeline steel with ASPEX. It is found that the inclusions are mainly globular CaO–Al2O3–MgO. The inclusion number decreases with time during RH treatment and the removal ratio can reach 72% after 28 min treatment. The initial number of inclusion plays a vital role in final inclusion number, so efforts must be made to eliminate the inclusion before RH treatment to get a highly clean steel. Non‐liquid inclusions including C3A (C is CaO and A is Al2O3) and Al2O3 · MgO decrease much more quickly and thoroughly than liquid ones, C12A7. This can be explained by the fact that non‐liquid inclusions have a much higher contact angle and interfacial energy but a much lower work of adhesion than liquid ones between inclusion and steel melt.
- 26 April 2013
- Published by Wiley in Steel Research International
- Vol. 85 (1) , 26-34
Transient Inclusion Evolution during RH Degassing
Inclusion morphology, composition and number at different times of RH vacuum treatment were investigated on API‐X70 pipeline steel with ASPEX. It is found that the inclusions are mainly globular CaO–Al2O3–MgO. The inclusion number decreases with time during RH treatment and the removal ratio can reach 72% after 28 min treatment. The initial number of inclusion plays a vital role in final inclusion number, so efforts must be made to eliminate the inclusion before RH treatment to get a highly clean steel. Non‐liquid inclusions including C3A (C is CaO and A is Al2O3) and Al2O3 · MgO decrease much more quickly and thoroughly than liquid ones, C12A7. This can be explained by the fact that non‐liquid inclusions have a much higher contact angle and interfacial energy but a much lower work of adhesion than liquid ones between inclusion and steel melt.