    Fusion Separation of Vanadium-Titanium Magnetite and Enrichment Test of Ti Element in Slag

    by Shuangping Yang, Shouman Liu, Shijie Guo, Tiantian Zhang, Jianghan Li

    In view of the problem that the enrichment and migration law of the Ti element in the slag of vanadium-titanium magnetite during the melting process is not clear, the phase transformation is not clear and the enrichment effect is not obvious, the single factor experiment and orthogonal experiment are used to optimize the melting conditions of Ti enrichment. Through XRD, SEM and EDS analysis, the effects of melting temperature, alkalinity and carbon content on the Ti phase in the slag are studied, and the occurrence form and migration law of the Ti element in the slag system under different melting conditions are clarified. The results demonstrate that increasing the basicity and melting temperature is beneficial to the enrichment of Ti, but it is too high it will lead to the formation of pyroxene, diopside and magnesia-alumina spinel, affecting the enrichment of Ti. The increase in carbon content can make Ti occur in slag in the form of titanium oxides such as TiO, TiO2, Ti2O3 and Ti3O5, but excessive carbon content leads to the excessive reduction of Ti compounds to TiCN and TiC. After optimization, under the melting conditions of alkalinity 1.2, the melting temperature 1500 °C and carbon content 15%, the content of Ti in slag can reach 18.84%, and the recovery rate is 93.54%. By detecting the content of Fe and V in molten iron, the recovery rates are 99.86% and 95.64%, respectively.


  • Open Access

    Study on Influencing Factors of High-Temperature Basic Characteristics of Iron Ore Powder and Optimization of Ore Blending

    by Shuangping Yang, Haijin Liu, Haixing Sun, Tiantian Zhang, Shouman Liu

    In order to explore the reasonable ore blending of low-silicon magnetite in sintering, it I necessary to realize the efficient utilization of low-silicon ore, further reduce cost, and increase yield. In this study, based on the high-temperature basic characteristics of iron ore powder used in the experiment, sinter pot tests were carried out with different low-silicon ore ratios, and the microstructure of the sinter was observed by scanning electron microscopy (SEM) and energy spectrum analysis (EDS) to determine the optimal matching law of low-silicon ore. The result showed that SiO2, Al2O3, and burning loss in iron ore powder composition were positively correlated with its assimilation, whereas MgO and basicity R2 were negatively correlated with the assimilation of iron ore powder. When the ratio of low-silicon ore was not more than 35%, increasing the ratio of hematite improved the liquid production and increased the production of acicular calcium ferrite. Therefore, the optimization of ore blending based on assimilation can improve the quality of sinter and strengthen the sintering process. This study has certain reference significance for the industrial production of low-silica sintering.


  • Open Access

    Mechanism of Microwave Activation on Molybdenite

    by Shuangping Yang, Tiantian Zhang, Shouman Liu, Haixing Sun

    The effect of microwave activation on the properties of oxidation roasting for molybdenite was investigated under the protection of inert gas, and the specific surface area, the oxidation properties, lattice constant, microstructure, and shape of molybdenite were analyzed and characterized by a laser particle size analyzer, thermogravimetry (TG), X-ray diffractometry (XRD) and scanning electron microscopy (SEM). The results show that microwave activation could effectively reduce the residual amount of sulfur in the molybdenum calcine and decrease the average particle size of molybdenite while increasing the specific surface area of molybdenite. On increasing the microwave activation power, the crystal cell volume and grain size of MoS2 reduced, and the microstrain increased slightly. At the same time, the surface shape of molybdenite became looser, but the layered structure is not changed. In addition, the oxidation property changed significantly; microwave activation promoted the oxidation reaction of molybdenite above 538 °C, and the rate of weight loss increased from 6.177% to 7.718% at 620 °C.