J. E. Gruzleski
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
J. E. Gruzleski has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
A. Abdollahi
Department of Mining and Metallurgical Engineering, McGill University, 3610 University Street, Montreal, Quebec, Canada H3A 2B2
1 shared publicationA. Tronche
Department of Materials Science and Metallurgy, Cambridge University, Pembroke St., Cambridge, UK, CB2 3QZ
1 shared publicationD. Gloria
Department of Mining and Metallurgical Engineering, McGill University. M. H. Wong Building, 3610 University St., Montreal, Quebec, Canada H3A 2B2
1 shared publicationF. Mucciardi
Department of Mining and Metallurgical Engineering, McGill University, 3610 University St., Montréal, Québec, Canada H3A 2B2
1 shared publicationM. Mahfoud
Department of Mining and Metallurgical Engineering, McGill University, 3610 University St., Montréal, Québec, Canada H3A 2B2
1 shared publicationR. I. Mackay
Department of Mining and Metallurgical Engineering, McGill University, Montreal, Quebec, Canada
1 shared publication
Latest Publications
- 1 January 1999
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (4) , 211-218
A general grain size determination technique for Al-Si casting alloys
Grain size determination is of great importance to metallurgists and foundry alloy producers since grain size can be related to many fundamental casting and mechanical properties. Conventional techniques for grain size measurement, developed mainly for wrought aluminium alloys, consist of the grinding and fine polishing of a sample, an often difficult to achieve anodizing step, and examination under crossed polarizers. Such techniques give good results, but are long and difficult to accomplish. A more simple technique, which is less time consuming, easier to achieve, and relatively inexpensive has been developed. It gives good results for a wide range of alloy compositions, and is particularly effective on Al-Si foundry alloys. The technique is not influenced by the presence of common grain refining elements and does not depend on the grain size of the sample. The application of this method to commercial alloys such as 319,356 and others is discussed.
- 1 January 1999
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (4) , 211-218
A general grain size determination technique for Al-Si casting alloys
Grain size determination is of great importance to metallurgists and foundry alloy producers since grain size can be related to many fundamental casting and mechanical properties. Conventional techniques for grain size measurement, developed mainly for wrought aluminium alloys, consist of the grinding and fine polishing of a sample, an often difficult to achieve anodizing step, and examination under crossed polarizers. Such techniques give good results, but are long and difficult to accomplish. A more simple technique, which is less time consuming, easier to achieve, and relatively inexpensive has been developed. It gives good results for a wide range of alloy compositions, and is particularly effective on Al-Si foundry alloys. The technique is not influenced by the presence of common grain refining elements and does not depend on the grain size of the sample. The application of this method to commercial alloys such as 319,356 and others is discussed.
- 29 November 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (3) , 145-155
An evaluation of calcium as a eutectic modifier in A357 alloy
Modification of the eutectic silicon in Al-Si alloys is traditionally performed by sodium and strontium addition to alter the form of the silicon from an acicular shape to a fine fibrous one. This modification results in a considerable improvement in mechanical properties, especially elongation. Although not commonly used as a modifier, calcium also has the potential to modify the eutectic silicon in Al-Si alloys. Metallographic observation and thermal analysis studies in A357 alloy indicate that, when the cooling rate is quite low, Ca modifies the eutectic silicon, but the effect of Ca as a modifier is not as strong as is Na or Sr. When the cooling rate is high, a fully modified structure can be obtained with calcium. Recovery of Ca in the melt is high and certain. It does not fade with long holding times, and retains its effect after repeated remeltings. Calcium addition does increase porosity in the cast alloys. The reduced pressure test (RPT) shows that the density of samples decreases with calcium addition, and observation of polished sections confirms the porosity increase. Tatur tests indicate that Ca modification increases microporosity, and decreases macroporosity. Calcium and strontium interact together to reduce the effectiveness of each other as a modifier. This interaction can be seen by thermal analysis as well as by microstructural studies.
- 29 November 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 11 (3) , 145-155
An evaluation of calcium as a eutectic modifier in A357 alloy
Modification of the eutectic silicon in Al-Si alloys is traditionally performed by sodium and strontium addition to alter the form of the silicon from an acicular shape to a fine fibrous one. This modification results in a considerable improvement in mechanical properties, especially elongation. Although not commonly used as a modifier, calcium also has the potential to modify the eutectic silicon in Al-Si alloys. Metallographic observation and thermal analysis studies in A357 alloy indicate that, when the cooling rate is quite low, Ca modifies the eutectic silicon, but the effect of Ca as a modifier is not as strong as is Na or Sr. When the cooling rate is high, a fully modified structure can be obtained with calcium. Recovery of Ca in the melt is high and certain. It does not fade with long holding times, and retains its effect after repeated remeltings. Calcium addition does increase porosity in the cast alloys. The reduced pressure test (RPT) shows that the density of samples decreases with calcium addition, and observation of polished sections confirms the porosity increase. Tatur tests indicate that Ca modification increases microporosity, and decreases macroporosity. Calcium and strontium interact together to reduce the effectiveness of each other as a modifier. This interaction can be seen by thermal analysis as well as by microstructural studies.
- 1 January 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 10 (4) , 191-200
On-line control of heat extraction during thermal analysis of aluminium alloys
Thermal analysis is a non-destructive and quantitative technique used to assess the quality of liquid metal prior to casting. Conventional thermal analysis is carried out by pouring a relatively small sample of the melt into a sampling cup. The liquid metal is then allowed to solidify, and its temperature is recorded as a function of time. One of the shortcomings associated with this method is that the physical and thermal characteristics of the sampling cup in any one given test determine the effective cooling rate. Moreover, the method is a batch operation which is difficult to automate and to computerise. To overcome these shortcomings, a new technique of performing thermal analysis has been devised. This new technique, which is based on heat pipe technology, is in-situ, semi-continuous, easy to use, dependable, and most importantly, capable of performing thermal analysis tests at controlled and variable cooling rates throughout the entire solidification process. In the present paper, the characteristics of the new system, as well as the technique of controlling the cooling rate (heat extraction) during thermal analysis of aluminium alloys are described.
- 1 January 1998
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 10 (4) , 191-200
On-line control of heat extraction during thermal analysis of aluminium alloys
Thermal analysis is a non-destructive and quantitative technique used to assess the quality of liquid metal prior to casting. Conventional thermal analysis is carried out by pouring a relatively small sample of the melt into a sampling cup. The liquid metal is then allowed to solidify, and its temperature is recorded as a function of time. One of the shortcomings associated with this method is that the physical and thermal characteristics of the sampling cup in any one given test determine the effective cooling rate. Moreover, the method is a batch operation which is difficult to automate and to computerise. To overcome these shortcomings, a new technique of performing thermal analysis has been devised. This new technique, which is based on heat pipe technology, is in-situ, semi-continuous, easy to use, dependable, and most importantly, capable of performing thermal analysis tests at controlled and variable cooling rates throughout the entire solidification process. In the present paper, the characteristics of the new system, as well as the technique of controlling the cooling rate (heat extraction) during thermal analysis of aluminium alloys are described.
- 29 November 1997
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 10 (3) , 131-145
Quantification of iron in aluminium-silicon foundry alloys via thermal analysis
Thermal analysis can provide a cost effective and reliable method to quantify the iron contents of aluminium-silicon alloy melts before the casting process is performed. The formation of the Al5FeSi intermetallic is resolvable on the cooling curves for aluminium-silicon alloys if the iron content is equal to or greater than 0.6% wt when the cooling rate of the thermal analysis sample is very slow. As the iron content gradually increases the nucleation temperature of Al5FeSi increases and results in extending the duration of the Al5FeSi thermal anomaly seen on cooling curves. Time and temperature based parameters associated with the Al5FeSi thermal anomaly are used to quantify the Fe content and the amount of iron rich intermetallic phases which appear in the microstructure. It is also shown that the duration of the eutectic growth, as determined from cooling curves, is influenced by the presence of iron.
- 29 November 1997
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 10 (3) , 131-145
Quantification of iron in aluminium-silicon foundry alloys via thermal analysis
Thermal analysis can provide a cost effective and reliable method to quantify the iron contents of aluminium-silicon alloy melts before the casting process is performed. The formation of the Al5FeSi intermetallic is resolvable on the cooling curves for aluminium-silicon alloys if the iron content is equal to or greater than 0.6% wt when the cooling rate of the thermal analysis sample is very slow. As the iron content gradually increases the nucleation temperature of Al5FeSi increases and results in extending the duration of the Al5FeSi thermal anomaly seen on cooling curves. Time and temperature based parameters associated with the Al5FeSi thermal anomaly are used to quantify the Fe content and the amount of iron rich intermetallic phases which appear in the microstructure. It is also shown that the duration of the eutectic growth, as determined from cooling curves, is influenced by the presence of iron.
- 1 May 1996
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 9 (1) , 17-26
Influence of melt cleanliness on pore formation in aluminium—silicon alloys
Porosity and inclusions are the most serious problems encountered in the production of aluminium castings. The formation of porosity during solidification can be affected by several factors such as melt hydrogen, cooling rate, alloying elements, modification and melt cleanliness. Of all these factors, melt cleanliness (i.e. inclusion concentration) is the most difficult to control and is often considered as a key factor influencing the pore nucleation. In the present paper, the effect of melt cleanliness on porosity formation in two aluminium foundry alloys (A356 and 319) was investigated systematically. Melts with different inclusion levels were prepared and tested by the reduced pressure test, and the melt cleanliness was quantified using a pressure filtration technique. In addition, the influence of filtration by ceramic foam filters on the porosity was studied. Results indicate that, at the same hydrogen level and with increased inclusion concentration, the density of reduced pressure samples decreases, and the amount of porosity and the number of pores increase. This trend is confirmed in both 356 and 319 alloys over a wide range of hydrogen levels. These results are discussed in the context of the nucleating effects of inclusions on pore formation during solidification. The practical application of the reduced pressure test for evaluation of both the melt cleanliness and the dissolved hydrogen level is outlined.
- 1 May 1996
- Published by Taylor & Francis in International Journal of Cast Metals Research
- Vol. 9 (1) , 17-26
Influence of melt cleanliness on pore formation in aluminium—silicon alloys
Porosity and inclusions are the most serious problems encountered in the production of aluminium castings. The formation of porosity during solidification can be affected by several factors such as melt hydrogen, cooling rate, alloying elements, modification and melt cleanliness. Of all these factors, melt cleanliness (i.e. inclusion concentration) is the most difficult to control and is often considered as a key factor influencing the pore nucleation. In the present paper, the effect of melt cleanliness on porosity formation in two aluminium foundry alloys (A356 and 319) was investigated systematically. Melts with different inclusion levels were prepared and tested by the reduced pressure test, and the melt cleanliness was quantified using a pressure filtration technique. In addition, the influence of filtration by ceramic foam filters on the porosity was studied. Results indicate that, at the same hydrogen level and with increased inclusion concentration, the density of reduced pressure samples decreases, and the amount of porosity and the number of pores increase. This trend is confirmed in both 356 and 319 alloys over a wide range of hydrogen levels. These results are discussed in the context of the nucleating effects of inclusions on pore formation during solidification. The practical application of the reduced pressure test for evaluation of both the melt cleanliness and the dissolved hydrogen level is outlined.