Rıza Gürbüz
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Rıza Gürbüz has a total of 31 co-authors. Here are the top co-authors by number of shared publications:
Ali Motameni
Department of Metallurgical and Materials Engineering, Middle East Technical University, Ankara, Turkey
1 shared publication- Ali Motameni
Department of Metallurgical and Materials Engineering, Middle East Technical University, Ankara, Turkey
1 shared publication Bettina Chang
Walter de Gruyter GmbH, Berlin/Boston, Genthiner Straße 13, 10785 Berlin, Germany
1 shared publication- Can Hakan Sarikaya
Department of Prosthetic Dentistry, Graduate School of Health Sciences, Ankara University, Ankara, Türkiye
1 shared publication - Cemil Hakan Gür
Metallurgical and Materials Engineering Department, Middle East Technical University, 06530 Ankara, Türkiye
1 shared publication Druckerei Typesetting
Walter de Gruyter GmbH Genthiner Straße 13 10785 Berlin Germany www
1 shared publication
Latest Publications
- 30 June 2025
- Published by SAGE Publications in Bio-Medical Materials and Engineering
- Vol. 37 (1) , 33-41
Experimental and numerical failure analysis of Thompson hip prosthesis
Background: There are different surgical procedures to fix femoral head-neck fractures, such as total hip arthroplasty and hemiarthroplasty. Under optimal conditions, the inserted prosthesis should last a long time, possibly a lifetime, with only trace amounts of wear each year due to the friction between the femur bone and the prosthesis stem. However, in some cases, failure due to excessive wear, creep, fatigue, corrosion, etc., can occur. Objective: This study investigates the failure causes of a Thompson hip prosthesis both experimentally and numerically. Methods: The stem of the prosthesis, which is inserted into the femur, broke inside a patient's body over time. Following the removal surgery, the severely damaged and fractured stem was examined to determine the root causes of the failure. For this purpose, fractographic examination of the fractured surfaces was conducted with scanning electron microscope (SEM). Microstructural analyses were performed using optical microscope, and the chemical composition of the prosthesis was analyzed with energy dispersive spectroscopy (EDS). Vickers hardness (HV30) test was conducted on the femoral stem. Additionally, finite element method (FEM) was applied to estimate the forces acting on the prosthesis. Results: It was observed that fatigue cracks initiated and propagated from the outer surface of the femoral stem at locations very close to the maximum von Mises stresses observed in the FEM analysis. However, the load magnitudes in the FEM analysis were not high enough to initiate any cracks. Conclusion: It is considered that crack initiation occurred due to material defects from the prosthesis manufacturing process, and the cyclic loading during body motion propagated these cracks. Ultimately, the fracture of the Thompson hip prosthesis occurred.
- 30 June 2025
- Published by SAGE Publications in Bio-Medical Materials and Engineering
- Vol. 37 (1) , 33-41
Experimental and numerical failure analysis of Thompson hip prosthesis
Background: There are different surgical procedures to fix femoral head-neck fractures, such as total hip arthroplasty and hemiarthroplasty. Under optimal conditions, the inserted prosthesis should last a long time, possibly a lifetime, with only trace amounts of wear each year due to the friction between the femur bone and the prosthesis stem. However, in some cases, failure due to excessive wear, creep, fatigue, corrosion, etc., can occur. Objective: This study investigates the failure causes of a Thompson hip prosthesis both experimentally and numerically. Methods: The stem of the prosthesis, which is inserted into the femur, broke inside a patient's body over time. Following the removal surgery, the severely damaged and fractured stem was examined to determine the root causes of the failure. For this purpose, fractographic examination of the fractured surfaces was conducted with scanning electron microscope (SEM). Microstructural analyses were performed using optical microscope, and the chemical composition of the prosthesis was analyzed with energy dispersive spectroscopy (EDS). Vickers hardness (HV30) test was conducted on the femoral stem. Additionally, finite element method (FEM) was applied to estimate the forces acting on the prosthesis. Results: It was observed that fatigue cracks initiated and propagated from the outer surface of the femoral stem at locations very close to the maximum von Mises stresses observed in the FEM analysis. However, the load magnitudes in the FEM analysis were not high enough to initiate any cracks. Conclusion: It is considered that crack initiation occurred due to material defects from the prosthesis manufacturing process, and the cyclic loading during body motion propagated these cracks. Ultimately, the fracture of the Thompson hip prosthesis occurred.
- Open Access
- 1 January 2025
- Published by Wiley in Case Reports in Dentistry
- Vol. 2025 (1)
Implant Body Fracture Due to Fatigue in a Maxillary Implant‐Retained Overdenture Treatment
The aim of this study was to determine the causes of fatigue and implant failures in an implant‐retained overdenture case. One out of four implants portrayed inadequate osseointegration during healing abutment placement, and one was fractured from the middle to the apical third after 1 year of denture use. Various aspects, such as insufficient cooling while implant socket preparation, incorrect prosthodontic planning, and erroneous design of the denture, were evaluated. Macroscopic and microscopic inspections of the fractured implant body were assessed by scanning electron microscopy (SEM) and optical microscopy. Consequently, metallic fatigue along with secondary cracks and beach marks were evident. It was deduced that the failed and fractured implants depicted substandard osseointegration; thus, they were susceptible to the wear out effect of the occlusal forces. Unfavorable osseointegration caused the fulcrum axis to move apically instead of forming on the neck part of the implant, and micromovements around the fulcrum axis mustered the fracture.
- 1 January 2025
- Published by Wiley in Case Reports in Dentistry
- Vol. 2025 (1)
Open AccessImplant Body Fracture Due to Fatigue in a Maxillary Implant‐Retained Overdenture Treatment
The aim of this study was to determine the causes of fatigue and implant failures in an implant‐retained overdenture case. One out of four implants portrayed inadequate osseointegration during healing abutment placement, and one was fractured from the middle to the apical third after 1 year of denture use. Various aspects, such as insufficient cooling while implant socket preparation, incorrect prosthodontic planning, and erroneous design of the denture, were evaluated. Macroscopic and microscopic inspections of the fractured implant body were assessed by scanning electron microscopy (SEM) and optical microscopy. Consequently, metallic fatigue along with secondary cracks and beach marks were evident. It was deduced that the failed and fractured implants depicted substandard osseointegration; thus, they were susceptible to the wear out effect of the occlusal forces. Unfavorable osseointegration caused the fulcrum axis to move apically instead of forming on the neck part of the implant, and micromovements around the fulcrum axis mustered the fracture.
- 31 January 2024
- Published by Demiryolu Muhendisligi Dergisi, Demiryolu Muhendisleri Dernegi in Demiryolu Mühendisliği
- No. 19,p. 56-66
Experimental Failure Analysis of SKL-21 Type Tension Clamps
- 31 January 2024
- Published by Demiryolu Muhendisligi Dergisi, Demiryolu Muhendisleri Dernegi in Demiryolu Mühendisliği
- No. 19,p. 56-66
Experimental Failure Analysis of SKL-21 Type Tension Clamps
- Open Access
- 25 September 2021
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 15 (58) , 344-364
Determining the endurance limit of AISI 4340 steels in terms of different statistical approaches
In engineering applications, fatigue phenomenon is a key issue and needs to be analyzed in the beginning of design phase in case of any component exposed to alternating loading on operation otherwise catastrophic fatigue failure may cause. Component can be designed with safe-life, fail-safe, and damage tolerant approach based on whether redundant load path and damage sensitive. Before starting analyzing the structure, material allowable data needs to be presented in a reliable way to predict fatigue life of components. SN curves with presented confidence levels are the robust approach to make a prediction on safe life of a structure in terms of fatigue. In this point, there are so many approaches to determine fatigue limit of materials and issue shall be handled by statistical manner. In literature, different staircase and curve fitting methods were presented to estimate endurance limit of materials and some reliability manuscript published. In this paper, fatigue limit of AISI 4340 steel will be investigated through most convinced staircase and curve fitting approaches and their reliability will be queried.
- 25 September 2021
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 15 (58) , 344-364
Open AccessDetermining the endurance limit of AISI 4340 steels in terms of different statistical approaches
In engineering applications, fatigue phenomenon is a key issue and needs to be analyzed in the beginning of design phase in case of any component exposed to alternating loading on operation otherwise catastrophic fatigue failure may cause. Component can be designed with safe-life, fail-safe, and damage tolerant approach based on whether redundant load path and damage sensitive. Before starting analyzing the structure, material allowable data needs to be presented in a reliable way to predict fatigue life of components. SN curves with presented confidence levels are the robust approach to make a prediction on safe life of a structure in terms of fatigue. In this point, there are so many approaches to determine fatigue limit of materials and issue shall be handled by statistical manner. In literature, different staircase and curve fitting methods were presented to estimate endurance limit of materials and some reliability manuscript published. In this paper, fatigue limit of AISI 4340 steel will be investigated through most convinced staircase and curve fitting approaches and their reliability will be queried.
- Open Access
- 1 September 2021
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 63 (9) , 789-791
Frontmatter
Article Frontmatter was published on September 1, 2021 in the journal Materials Testing (volume 63, issue 9).
- 1 September 2021
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 63 (9) , 789-791
Open AccessFrontmatter
Article Frontmatter was published on September 1, 2021 in the journal Materials Testing (volume 63, issue 9).
- Open Access
- 1 September 2013
- Published by FapUNIFESP (SciELO) in Soldagem & Inspeção
- Vol. 18 (3) , 207-216
Characterization of duplex stainless steel weld metals obtained by hybrid plasma-gas metal arc welding
Despite its high efficiency, autogenous keyhole welding is not well-accepted for duplex stainless steels because it causes excessive ferrite in as-welded duplex microstructure, which leads to a degradation in toughness and corrosion properties of the material. Combining the deep penetration characteristics of plasma arc welding in keyhole mode and metal deposition capability of gas metal arc welding, hybrid plasma - gas metal arc welding process has considered for providing a proper duplex microstructure without compromising the welding efficiency. 11.1 mm-thick standard duplex stainless steel plates were joined in a single-pass using this novel technique. Same plates were also subjected to conventional gas metal arc and plasma arc welding processes, providing benchmarks for the investigation of the weldability of the material. In the first place, the hybrid welding process enabled us to achieve less heat input compared to gas metal arc welding. Consequently, the precipitation of secondary phases, which are known to be detrimental to the toughness and corrosion resistance of duplex stainless steels, was significantly suppressed in both fusion and heat affected zones. Secondly, contrary to other keyhole techniques, proper cooling time and weld metal chemistry were achieved during the process, facilitating sufficient reconstructive transformation of austenite in the ferrite phase.
- 1 September 2013
- Published by FapUNIFESP (SciELO) in Soldagem & Inspeção
- Vol. 18 (3) , 207-216
Open AccessCharacterization of duplex stainless steel weld metals obtained by hybrid plasma-gas metal arc welding
Despite its high efficiency, autogenous keyhole welding is not well-accepted for duplex stainless steels because it causes excessive ferrite in as-welded duplex microstructure, which leads to a degradation in toughness and corrosion properties of the material. Combining the deep penetration characteristics of plasma arc welding in keyhole mode and metal deposition capability of gas metal arc welding, hybrid plasma - gas metal arc welding process has considered for providing a proper duplex microstructure without compromising the welding efficiency. 11.1 mm-thick standard duplex stainless steel plates were joined in a single-pass using this novel technique. Same plates were also subjected to conventional gas metal arc and plasma arc welding processes, providing benchmarks for the investigation of the weldability of the material. In the first place, the hybrid welding process enabled us to achieve less heat input compared to gas metal arc welding. Consequently, the precipitation of secondary phases, which are known to be detrimental to the toughness and corrosion resistance of duplex stainless steels, was significantly suppressed in both fusion and heat affected zones. Secondly, contrary to other keyhole techniques, proper cooling time and weld metal chemistry were achieved during the process, facilitating sufficient reconstructive transformation of austenite in the ferrite phase.