Guoquan Qi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Guoquan Qi has a total of 25 co-authors. Here are the top co-authors by number of shared publications:
- Houbu Li
State Key Laboratory for Performance and Structure Safety of Petroleum Tubular Goods and Equipment Materials, CNPC Tubular Goods Research Institute, Xi’an 710077, China
7 shared publications - Xuemin Zhang
School of Materials Science and Engineering, Chang’an University, Xi’an 710064, China
4 shared publications - Dongtao Qi
State Key Laboratory of Performance and Structural Safety for Petroleum Tubular Goods and Equipment Materials, CNPC Tubular Goods Research Institute, Xi’an 710077, China
3 shared publications - Han Ding
Department of Applied Chemistry, School of Science, Northwestern Polytechnical University, Xi’an, China
3 shared publications - Xiong Gao
Shaanxi Yanchang Petroleum Northwest Rubber LLC, Xianyang 712023, China
3 shared publications - Huifang Chu
School of Materials Science and Engineering, Chang’an University, Xi’an 710064, China
2 shared publications
Latest Publications
- Open Access
Activated Carbon Based on Recycled Epoxy Boards and Their Adsorption toward Methyl Orange
With the swift progress of the electronics industry, discarded circuit boards have become an important source of non-degradable waste. In this work, discarded epoxy resin was collected as a precursor to prepare activated carbon (AC) through stepwise carbonization/activation methods. The rough carbon materials with a certain graphite and amorphous structure reveal the multiple oxygen-containing groups on their surface. In the process of studying the adsorption of methyl orange by activated carbon, it is found that the adsorption is in accordance with the quasi-secondary kinetic model, and equilibrium adsorption amounts can reach 41.051 mg/g. The adsorption isotherm of AC is more in line with the Langmuir model, and the saturation adsorption amount at three different temperatures is 23.137 mg/g, 30.358 mg/g, and 37.202 mg/g, respectively. The enthalpy (ΔH) is 17.30 KJ/mol in the adsorption process, which indicates that is a physical process with heat-absorbing capabilities. This work is of great significance with regard to the recycling of waste to reduce pollution and in terms of gaining economic benefits.
Open AccessActivated Carbon Based on Recycled Epoxy Boards and Their Adsorption toward Methyl Orange
With the swift progress of the electronics industry, discarded circuit boards have become an important source of non-degradable waste. In this work, discarded epoxy resin was collected as a precursor to prepare activated carbon (AC) through stepwise carbonization/activation methods. The rough carbon materials with a certain graphite and amorphous structure reveal the multiple oxygen-containing groups on their surface. In the process of studying the adsorption of methyl orange by activated carbon, it is found that the adsorption is in accordance with the quasi-secondary kinetic model, and equilibrium adsorption amounts can reach 41.051 mg/g. The adsorption isotherm of AC is more in line with the Langmuir model, and the saturation adsorption amount at three different temperatures is 23.137 mg/g, 30.358 mg/g, and 37.202 mg/g, respectively. The enthalpy (ΔH) is 17.30 KJ/mol in the adsorption process, which indicates that is a physical process with heat-absorbing capabilities. This work is of great significance with regard to the recycling of waste to reduce pollution and in terms of gaining economic benefits.
- Open Access
Molecular Simulation Study on the Hydrogen Permeation Behavior and Mechanism of Common Polymers
This research aimed to provide an understanding of the selection and safe application of pipeline liner materials for hydrogen transport by examining the permeation properties and mechanisms of hydrogen within polymers commonly used for this purpose, such as high-density polyethylene (HDPE) and ethylene-vinyl alcohol copolymer (EVOH), through molecular simulation. The study was carried out within defined operational parameters of temperature (ranging from room temperature to 80 °C) and pressure (from 2.5 to 10 MPa) that are pertinent to hydrogen pipeline infrastructures. The results reveal that with an increase in temperature from 30 °C to 80 °C, the solubility, diffusion, and permeability coefficients of hydrogen in HDPE increase by 18.7%, 92.9%, and 129.0%, respectively. Similarly, in EVOH, these coefficients experience increments of 15.9%, 81.6%, and 112.7%. Conversely, pressure variations have a negligible effect on permeability in both polymers. HDPE exhibits significantly higher hydrogen permeability compared to EVOH. The unique chain segment configuration of EVOH leads to the formation of robust hydrogen bonds among the hydroxyl groups, thereby impeding the permeation of hydrogen. The process by which hydrogen is adsorbed in polymers involves aggregation at low potential energy levels. During diffusion, the hydrogen molecule primarily vibrates within a limited range, with intermittent occurrences of significant hole-to-hole transitions over larger distances. Hydrogen exhibits a stronger interaction with HDPE compared to EVOH, leading to a higher number of adsorption sites and increased hydrogen adsorption capacity in HDPE. Hydrogen molecules move more actively in HDPE than in EVOH, exhibiting greater hole amplitude and more holes in transition during the diffusion process.
Open AccessMolecular Simulation Study on the Hydrogen Permeation Behavior and Mechanism of Common Polymers
This research aimed to provide an understanding of the selection and safe application of pipeline liner materials for hydrogen transport by examining the permeation properties and mechanisms of hydrogen within polymers commonly used for this purpose, such as high-density polyethylene (HDPE) and ethylene-vinyl alcohol copolymer (EVOH), through molecular simulation. The study was carried out within defined operational parameters of temperature (ranging from room temperature to 80 °C) and pressure (from 2.5 to 10 MPa) that are pertinent to hydrogen pipeline infrastructures. The results reveal that with an increase in temperature from 30 °C to 80 °C, the solubility, diffusion, and permeability coefficients of hydrogen in HDPE increase by 18.7%, 92.9%, and 129.0%, respectively. Similarly, in EVOH, these coefficients experience increments of 15.9%, 81.6%, and 112.7%. Conversely, pressure variations have a negligible effect on permeability in both polymers. HDPE exhibits significantly higher hydrogen permeability compared to EVOH. The unique chain segment configuration of EVOH leads to the formation of robust hydrogen bonds among the hydroxyl groups, thereby impeding the permeation of hydrogen. The process by which hydrogen is adsorbed in polymers involves aggregation at low potential energy levels. During diffusion, the hydrogen molecule primarily vibrates within a limited range, with intermittent occurrences of significant hole-to-hole transitions over larger distances. Hydrogen exhibits a stronger interaction with HDPE compared to EVOH, leading to a higher number of adsorption sites and increased hydrogen adsorption capacity in HDPE. Hydrogen molecules move more actively in HDPE than in EVOH, exhibiting greater hole amplitude and more holes in transition during the diffusion process.
- Open Access
The Aging Performance of PVDF in Acid Oil and Gas Medium
In the process of transporting oil and gas, the service performance of thermoplastic pipes will decline due to the multiple influences of medium, temperature, and pressure. In order to study the service performance changes of PVDF pipes under oil and gas transportation conditions, the high-temperature autoclave is used to simulate the service state of the pipe in the mediums. The PVDF samples are exposed to simulated oil and gas mediums for 1 week, 3 weeks, 5 weeks, and 7 weeks under 60 °C and 90 °C conditions. After the exposure test, the physical and chemical properties of the PVDF pipe are tested and compared with the initial samples. Compared with the initial sample, the sample quality after the exposure test has a slight increase, with growth rates of 2% and 3% at 60 °C and 90 °C, respectively. Meanwhile, the tensile strength of the samples is about 13% and 21% lower than that of the initial sample, respectively. According to the microscopic morphology analyses, there are some crack defects on the surface of the sample after the exposure test. Through infrared analysis, it is shown that no molecular chain breakage, crosslinking, or other reactions are found after the exposure test. The above analysis shows that the PVDF sample has slight penetration and swelling during the exposure test. However, due to the large force between the PVDF molecules, its mechanical properties have a small downward trend, showing excellent environmental stress crack resistance.
Open AccessThe Aging Performance of PVDF in Acid Oil and Gas Medium
In the process of transporting oil and gas, the service performance of thermoplastic pipes will decline due to the multiple influences of medium, temperature, and pressure. In order to study the service performance changes of PVDF pipes under oil and gas transportation conditions, the high-temperature autoclave is used to simulate the service state of the pipe in the mediums. The PVDF samples are exposed to simulated oil and gas mediums for 1 week, 3 weeks, 5 weeks, and 7 weeks under 60 °C and 90 °C conditions. After the exposure test, the physical and chemical properties of the PVDF pipe are tested and compared with the initial samples. Compared with the initial sample, the sample quality after the exposure test has a slight increase, with growth rates of 2% and 3% at 60 °C and 90 °C, respectively. Meanwhile, the tensile strength of the samples is about 13% and 21% lower than that of the initial sample, respectively. According to the microscopic morphology analyses, there are some crack defects on the surface of the sample after the exposure test. Through infrared analysis, it is shown that no molecular chain breakage, crosslinking, or other reactions are found after the exposure test. The above analysis shows that the PVDF sample has slight penetration and swelling during the exposure test. However, due to the large force between the PVDF molecules, its mechanical properties have a small downward trend, showing excellent environmental stress crack resistance.
- Open Access
Highly Thermal Conductive and Electrically Insulating Epoxy Composites Based on Zinc-Oxide-Coated Silver Nanowires
Nano-ZnO particles were deposited on the surface of silver nanowires (AgNWs) by the precipitation method, and the obtained AgNW@ZnO filler with core-shell structure was added to epoxy resin to prepare AgNW@ZnO/EP thermally conductive composites. The ZnO coating on the surface of AgNWs effectively improves the thermal conductivity of the composites. When 8 wt% AgNW@ZnO filler was added to the epoxy resin, the thermal conductivity of the AgNW@ZnO/EP composite increased to 0.77 W/(m·K). The enhancement of the thermal conductivity is attributed to the fact that ZnO effectively improves the interface bonding between AgNWs and the epoxy matrix, thus strengthening the contact between AgNWs. In addition, the electrical insulation of the AgNW@ZnO/EP composites was improved upon the introduction of the ZnO coating over AgNWs. For the filler content of 8 wt%, the volume resistivity of the AgNW@ZnO/EP composites was found to be higher than 1013 Ω·cm. AgNW@ZnO/EP composites have also exhibited low dielectric constant and good thermal stability.
Open AccessHighly Thermal Conductive and Electrically Insulating Epoxy Composites Based on Zinc-Oxide-Coated Silver Nanowires
Nano-ZnO particles were deposited on the surface of silver nanowires (AgNWs) by the precipitation method, and the obtained AgNW@ZnO filler with core-shell structure was added to epoxy resin to prepare AgNW@ZnO/EP thermally conductive composites. The ZnO coating on the surface of AgNWs effectively improves the thermal conductivity of the composites. When 8 wt% AgNW@ZnO filler was added to the epoxy resin, the thermal conductivity of the AgNW@ZnO/EP composite increased to 0.77 W/(m·K). The enhancement of the thermal conductivity is attributed to the fact that ZnO effectively improves the interface bonding between AgNWs and the epoxy matrix, thus strengthening the contact between AgNWs. In addition, the electrical insulation of the AgNW@ZnO/EP composites was improved upon the introduction of the ZnO coating over AgNWs. For the filler content of 8 wt%, the volume resistivity of the AgNW@ZnO/EP composites was found to be higher than 1013 Ω·cm. AgNW@ZnO/EP composites have also exhibited low dielectric constant and good thermal stability.
- Open Access
Permeation Characteristics of CH4 in PVDF with Crude Oil-Containing
The liner of reinforced thermoplastic composite pipes (RTPs) used for oil and gas gathering and transportation experienced blister failure due to gas permeation. Few reports have appeared on the problem of gas permeation in thermoplastics with absorbed crude oil. Accordingly, the permeability of CH4 in polyvinylidene fluoride (PVDF) containing crude oil was studied at the normal service conditions by molecular simulations. The results showed that the solubility coefficients of CH4 in PVDF containing crude oil were much lower than those in pure PVDF. It can be concluded that the crude oil molecules absorbed into PVDF occupied certain adsorption sites, resulting in a decrease in the adsorption capacity of CH4 molecules in PVDF. The diffusion coefficients of CH4 in oil-containing PVDF were significantly greater than in PVDF. This is because the absorption of oil molecules leads to the volume swelling of PVDF and then increases the free volume for diffusion. The permeation process showed that CH4 molecules were selective-aggregate adsorbed in the region with low potential energy in oil-containing PVDF firstly, and then they vibrated within the holes of PVDF containing oil in most cases and jumped into the neighboring holes at high temperatures and pressures.
Open AccessPermeation Characteristics of CH4 in PVDF with Crude Oil-Containing
The liner of reinforced thermoplastic composite pipes (RTPs) used for oil and gas gathering and transportation experienced blister failure due to gas permeation. Few reports have appeared on the problem of gas permeation in thermoplastics with absorbed crude oil. Accordingly, the permeability of CH4 in polyvinylidene fluoride (PVDF) containing crude oil was studied at the normal service conditions by molecular simulations. The results showed that the solubility coefficients of CH4 in PVDF containing crude oil were much lower than those in pure PVDF. It can be concluded that the crude oil molecules absorbed into PVDF occupied certain adsorption sites, resulting in a decrease in the adsorption capacity of CH4 molecules in PVDF. The diffusion coefficients of CH4 in oil-containing PVDF were significantly greater than in PVDF. This is because the absorption of oil molecules leads to the volume swelling of PVDF and then increases the free volume for diffusion. The permeation process showed that CH4 molecules were selective-aggregate adsorbed in the region with low potential energy in oil-containing PVDF firstly, and then they vibrated within the holes of PVDF containing oil in most cases and jumped into the neighboring holes at high temperatures and pressures.
- Open Access
- 25 February 2022
- Published by MDPI AG in Preprints.org
Analyses and the cause of corrosion and materials loss at the base of a three-phase separator in petroleum-based processing
The three-phase separator was perforated after four years’ service. The perforation position is at the bottom of the vessel under the baffle plate in an oil transfer station. The cause of perforation was investigated by chemical analysis using a direct-reading spectrometer, microstructure examined by optical microscope(OM), and lab simulated corrosion experiments by electrochemical workstation, and the corrosion products examined with scanning electron microscopy(SEM), energy dispersive spectrometer(EDS) in this paper. The analyses indicated that the coating at the base of the pressure vessel failed and this led to the direct exposure of the carbon steel plate to the corrosive medium. The electrical contact between the carbon steel and the stainless steel, sets up a galvanic cell that accelerated the corrosion of the pressure vessel which eventually led leads to the perforation.
- 25 February 2022
- Published by MDPI AG in Preprints.org
Open AccessAnalyses and the cause of corrosion and materials loss at the base of a three-phase separator in petroleum-based processing
The three-phase separator was perforated after four years’ service. The perforation position is at the bottom of the vessel under the baffle plate in an oil transfer station. The cause of perforation was investigated by chemical analysis using a direct-reading spectrometer, microstructure examined by optical microscope(OM), and lab simulated corrosion experiments by electrochemical workstation, and the corrosion products examined with scanning electron microscopy(SEM), energy dispersive spectrometer(EDS) in this paper. The analyses indicated that the coating at the base of the pressure vessel failed and this led to the direct exposure of the carbon steel plate to the corrosive medium. The electrical contact between the carbon steel and the stainless steel, sets up a galvanic cell that accelerated the corrosion of the pressure vessel which eventually led leads to the perforation.
- Open Access
Molecular Simulation on Permeation Behavior of CH4/CO2/H2S Mixture Gas in PVDF at Service Conditions
Reinforced thermoplastic composite pipes (RTPs) have been widely used for oil and gas gathering and transportation. Polyvinylidene fluoride (PVDF) has the greatest potential as a thermoplastic liner of RTPs due to its excellent thermal and mechanical properties. However, permeation of gases is inevitable in the thermoplastic liner, which may lead to blister failure of the liner and damage the safe operation of the RTPs. In order to clarify the permeation behavior and obtain the permeation mechanism of the mixture gas (CH4/CO2/H2S) in PVDF at the normal service conditions, molecular simulations were carried out by combining the Grand Canonical Monte Carlo (GCMC) method and the Molecular Dynamics (MD) method. The simulated results showed that the solubility coefficients of gases increased with the decrease in temperature and the increase in pressure. The adsorption isotherms of all gases were consistent with the Langmuir model. The order of the adsorption concentration for different gases was H2S > CO2> CH4. The isosteric heats of gases at all the actual service conditions were much less than 42 kJ/mol, which indicated that the adsorption for all the gases belonged to the physical adsorption. Both of the diffusion and permeation coefficients increased with the increase in temperature and pressure. The diffusion belonged to Einstein diffusion and the diffusion coefficients of each gas followed the order of CH4 > CO2 > H2S. During the permeation process, the adsorption of gas molecules in PVDF exhibited selective aggregation, and most of them were adsorbed in the low potential energy region of PVDF cell. The mixed-gas molecules vibrated within the hole of PVDF at relatively low temperature and pressure. As the temperature and pressure increase, the gas molecules jumped into the neighboring holes occasionally and then dwelled in the holes, moving around their equilibrium positions.
Open AccessMolecular Simulation on Permeation Behavior of CH4/CO2/H2S Mixture Gas in PVDF at Service Conditions
Reinforced thermoplastic composite pipes (RTPs) have been widely used for oil and gas gathering and transportation. Polyvinylidene fluoride (PVDF) has the greatest potential as a thermoplastic liner of RTPs due to its excellent thermal and mechanical properties. However, permeation of gases is inevitable in the thermoplastic liner, which may lead to blister failure of the liner and damage the safe operation of the RTPs. In order to clarify the permeation behavior and obtain the permeation mechanism of the mixture gas (CH4/CO2/H2S) in PVDF at the normal service conditions, molecular simulations were carried out by combining the Grand Canonical Monte Carlo (GCMC) method and the Molecular Dynamics (MD) method. The simulated results showed that the solubility coefficients of gases increased with the decrease in temperature and the increase in pressure. The adsorption isotherms of all gases were consistent with the Langmuir model. The order of the adsorption concentration for different gases was H2S > CO2> CH4. The isosteric heats of gases at all the actual service conditions were much less than 42 kJ/mol, which indicated that the adsorption for all the gases belonged to the physical adsorption. Both of the diffusion and permeation coefficients increased with the increase in temperature and pressure. The diffusion belonged to Einstein diffusion and the diffusion coefficients of each gas followed the order of CH4 > CO2 > H2S. During the permeation process, the adsorption of gas molecules in PVDF exhibited selective aggregation, and most of them were adsorbed in the low potential energy region of PVDF cell. The mixed-gas molecules vibrated within the hole of PVDF at relatively low temperature and pressure. As the temperature and pressure increase, the gas molecules jumped into the neighboring holes occasionally and then dwelled in the holes, moving around their equilibrium positions.
- Open Access
Simulation Analysis of Limit Operating Specifications for Onshore Spoolable Reinforced Thermoplastic Pipes
Spoolable reinforced plastic line pipes (RTPs), exhibiting a series of advantages such as good flexibility, few joints, long single length, light weight, easy installation, etc., have been widely used in the onshore oil and gas industry such as oil and gas gathering and transportation, high pressure alcohol injection, water injection, sewage treatment, and other fields. However, due to the lack of clear standard specificationof the limit operating properties for RTPs, three typical failure modes, i.e., tensile, flexure, and torsion, frequently occur in terrain changes, construction operation, and subsequent application, which seriously affects the promotion and use of RTPs. In this paper, the stress distribution of a non-bonded polyester fiber reinforced high-density polyethylene (HDPE) pipe (DN 150, PN 2.5 MPa) was systematically studied by the finite element method (FEM), and then the limit operating values under the axial tensile, coiled bending, and torsion load were determined. The corresponding experiments were conducted to validate the reliability and accuracy of the FEM model. The FEM results showed that the critical strain for axial tensile was 3%, the minimum respooling bend radius was 1016.286 mm, and the limit torsion angle of this RTP was 58.77°, which are very close to the experimental results. These limit values will be useful to establish normative guidelines for field construction and failure prevention of onshore RTP.
Open AccessSimulation Analysis of Limit Operating Specifications for Onshore Spoolable Reinforced Thermoplastic Pipes
Spoolable reinforced plastic line pipes (RTPs), exhibiting a series of advantages such as good flexibility, few joints, long single length, light weight, easy installation, etc., have been widely used in the onshore oil and gas industry such as oil and gas gathering and transportation, high pressure alcohol injection, water injection, sewage treatment, and other fields. However, due to the lack of clear standard specificationof the limit operating properties for RTPs, three typical failure modes, i.e., tensile, flexure, and torsion, frequently occur in terrain changes, construction operation, and subsequent application, which seriously affects the promotion and use of RTPs. In this paper, the stress distribution of a non-bonded polyester fiber reinforced high-density polyethylene (HDPE) pipe (DN 150, PN 2.5 MPa) was systematically studied by the finite element method (FEM), and then the limit operating values under the axial tensile, coiled bending, and torsion load were determined. The corresponding experiments were conducted to validate the reliability and accuracy of the FEM model. The FEM results showed that the critical strain for axial tensile was 3%, the minimum respooling bend radius was 1016.286 mm, and the limit torsion angle of this RTP was 58.77°, which are very close to the experimental results. These limit values will be useful to establish normative guidelines for field construction and failure prevention of onshore RTP.