Hongfeng Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Hongfeng Li has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
- Liwei Zhao
Institute of Petrochemistry, Heilongjiang Academy of Sciences Harbin China
4 shared publications - Chunyan Qu
Institute of Petrochemistry, Heilongjiang Academy of Sciences, Harbin 150040, China
3 shared publications - Dezhi Wang
Institute of Petrochemistry, Heilongjiang Academy of Sciences, Harbin 150040, China
3 shared publications - Changwei Liu
Institute of Petrochemistry, Heilongjiang Academy of Sciences, Harbin 150040, China
2 shared publications - Hao Feng
Institute of Petrochemistry, Heilongjiang Academy of Sciences, Harbin 150040, China
2 shared publications - Wanbao Xiao
Institute of Petrochemistry, Heilongjiang Academy of Sciences, Harbin 150040, China
2 shared publications
Latest Publications
- Open Access
Rapid Crystallization and Fluorescence of Poly(ethylene terephthalate) Using Graphene Quantum Dots as Nucleating Agents
In this study, graphene quantum dots (GQDs) with a diameter of ~3 nm were successfully synthesized and incorporated into a poly(ethylene terephthalate) (PET) matrix to fabricate PET/GQDs nanocomposites. The impact of GQDs on the crystallization and thermal stability of the PET/GQDs nanocomposites was investigated. It was observed that the addition of only 0.5 wt% GQDs into the nanocomposites resulted in a significant increase in the crystallization temperature (peak temperature) of PET, from 194.3 °C to 206.0 °C during the cooling scan process. This suggested that an optimal concentration of GQDs could function as a nucleating agent and effectively enhance the crystallization temperature of PET. The isothermal crystallization method was employed to analyze the crystallization kinetics of the PET/GQDs nanocomposites, and the data showed that 0.5 wt% GQDs significantly accelerated the crystallization rate. Furthermore, the incorporation of GQDs into the PET matrix imparted photoluminescent properties to the resulting PET/GQDs nanocomposites. The PET crystals with GQDs as crystal nuclei and the crazes caused by defects played a vital role in isolating and suppressing the concentration quenching of GQDs. This effect facilitated the detection of defects in PET.
Open AccessRapid Crystallization and Fluorescence of Poly(ethylene terephthalate) Using Graphene Quantum Dots as Nucleating Agents
In this study, graphene quantum dots (GQDs) with a diameter of ~3 nm were successfully synthesized and incorporated into a poly(ethylene terephthalate) (PET) matrix to fabricate PET/GQDs nanocomposites. The impact of GQDs on the crystallization and thermal stability of the PET/GQDs nanocomposites was investigated. It was observed that the addition of only 0.5 wt% GQDs into the nanocomposites resulted in a significant increase in the crystallization temperature (peak temperature) of PET, from 194.3 °C to 206.0 °C during the cooling scan process. This suggested that an optimal concentration of GQDs could function as a nucleating agent and effectively enhance the crystallization temperature of PET. The isothermal crystallization method was employed to analyze the crystallization kinetics of the PET/GQDs nanocomposites, and the data showed that 0.5 wt% GQDs significantly accelerated the crystallization rate. Furthermore, the incorporation of GQDs into the PET matrix imparted photoluminescent properties to the resulting PET/GQDs nanocomposites. The PET crystals with GQDs as crystal nuclei and the crazes caused by defects played a vital role in isolating and suppressing the concentration quenching of GQDs. This effect facilitated the detection of defects in PET.
- Open Access
Epoxy-Modified Bismaleimide Structural Adhesive Film Toughened Synergistically with PEK-C and Core–Shell Polymers for Bonding CFRP
Bismaleimide (BMI) resin-based structural adhesives have excellent heat resistance, with important applications demonstrated in the bonding of high-temperature BMI composites. In this paper, we report an epoxy-modified BMI structural adhesive with excellent properties for bonding BMI-based CFRP. We prepared the BMI adhesive using epoxy-modified BMI as the matrix and PEK-C and core–shell polymers as synergistic tougheners. We found that the epoxy resins improve the process and bonding properties of BMI resin but slightly reduce thermal stability. PEK-C and core–shell polymers synergistically improve the toughness and bonding performances of the modified BMI adhesive system and allow the maintenance of heat resistance. The optimized BMI adhesive exhibits excellent heat resistance, with a high glass transition temperature of 208.6 °C and a high thermal degradation temperature of 425.4 °C. Most importantly, the optimized BMI adhesive exhibits satisfactory intrinsic bonding and thermal stability. It has a high shear strength of 32.0 MPa at room temperature and up to 17.9 MPa at 200 °C. The BMI adhesive-bonded composite joint has a high shear strength of 38.6 and 17.3 MPa at room temperature and 200 °C, respectively, indicating effective bonding and excellent heat resistance.
Open AccessEpoxy-Modified Bismaleimide Structural Adhesive Film Toughened Synergistically with PEK-C and Core–Shell Polymers for Bonding CFRP
Bismaleimide (BMI) resin-based structural adhesives have excellent heat resistance, with important applications demonstrated in the bonding of high-temperature BMI composites. In this paper, we report an epoxy-modified BMI structural adhesive with excellent properties for bonding BMI-based CFRP. We prepared the BMI adhesive using epoxy-modified BMI as the matrix and PEK-C and core–shell polymers as synergistic tougheners. We found that the epoxy resins improve the process and bonding properties of BMI resin but slightly reduce thermal stability. PEK-C and core–shell polymers synergistically improve the toughness and bonding performances of the modified BMI adhesive system and allow the maintenance of heat resistance. The optimized BMI adhesive exhibits excellent heat resistance, with a high glass transition temperature of 208.6 °C and a high thermal degradation temperature of 425.4 °C. Most importantly, the optimized BMI adhesive exhibits satisfactory intrinsic bonding and thermal stability. It has a high shear strength of 32.0 MPa at room temperature and up to 17.9 MPa at 200 °C. The BMI adhesive-bonded composite joint has a high shear strength of 38.6 and 17.3 MPa at room temperature and 200 °C, respectively, indicating effective bonding and excellent heat resistance.
- 16 February 2022
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 37 (4) , 740-754
Toughening of benzoxazine structural adhesives and surface films
In this paper, acrylic triblock copolymer (BMG) was used to toughen the benzoxazine/epoxy (BZ/EP) resin system and prepare a BZ/EP/DDS/BMG resin. BZ/EP/DDS/BMG resin curing characteristics, viscosity-temperature characteristics, heat resistance, toughness, morphology, and bonding performance were studied. The results show that the curing agent 4,4-diamino diphenyl sulfone (DDS) can lower the curing temperature of the BZ/EP/DDS system, making it suitable for co-curing of benzoxazine prepreg. The BMG did not affect the curing temperature of the BZ/EP resin. When 15 phr BMG was added, the viscosity of the BZ/EP/BMG resin at 139–189 °C was lower than 5.0 Pa·s, showing a minimum viscosity of 2.0 Pa·s. BMG significantly increased the toughness of the BZ/EP/DDS/BMG system while barely decreasing its heat resistance. The impact strength of the BZ/EP/BMG resin increased by 71% when 20% BMG was added. Furthermore, theBZ/EP/DDS/BMG resin demonstrated excellent bonding performance, with lap shear strength and peel strength at room temperature reaching 30.6 MPa, and 37.2 N/cm, respectively. Therefore, the prepared BZ/EP/DDS/BMG resin is suitable as a matrix for BZ structural adhesives and composite surface films.
- 16 February 2022
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 37 (4) , 740-754
Toughening of benzoxazine structural adhesives and surface films
In this paper, acrylic triblock copolymer (BMG) was used to toughen the benzoxazine/epoxy (BZ/EP) resin system and prepare a BZ/EP/DDS/BMG resin. BZ/EP/DDS/BMG resin curing characteristics, viscosity-temperature characteristics, heat resistance, toughness, morphology, and bonding performance were studied. The results show that the curing agent 4,4-diamino diphenyl sulfone (DDS) can lower the curing temperature of the BZ/EP/DDS system, making it suitable for co-curing of benzoxazine prepreg. The BMG did not affect the curing temperature of the BZ/EP resin. When 15 phr BMG was added, the viscosity of the BZ/EP/BMG resin at 139–189 °C was lower than 5.0 Pa·s, showing a minimum viscosity of 2.0 Pa·s. BMG significantly increased the toughness of the BZ/EP/DDS/BMG system while barely decreasing its heat resistance. The impact strength of the BZ/EP/BMG resin increased by 71% when 20% BMG was added. Furthermore, theBZ/EP/DDS/BMG resin demonstrated excellent bonding performance, with lap shear strength and peel strength at room temperature reaching 30.6 MPa, and 37.2 N/cm, respectively. Therefore, the prepared BZ/EP/DDS/BMG resin is suitable as a matrix for BZ structural adhesives and composite surface films.
- Open Access
Surface Treatment of Composites with Bismaleimide Resin-Based Wet Peel Ply for Enhanced Adhesive Bonding Performance
Surface treatment is typically required to improve the bonding performance of carbon-fiber-reinforced composites. Herein, a wet peel ply was prepared using bismaleimide (BMI) resins as a matrix resin. The temperature–heating rate extrapolation method and rheological method were employed to study the reaction characteristics and viscosity-temperature characteristics of the matrix in the BMI wet peel ply. The curing temperatures of the BMI wet peel ply and the BMI prepreg were the same (200 °C), making this wet peel ply suitable for co-curing with the BMI prepreg. After treatment with the wet peel ply, the bonding strength of the BMI composite joint showed a mean shear strength of 35.5 MPa, which was 1.72% higher than that of the sanded composite and 17.5% higher than that of the composite treated with the dry peel ply. In addition, the BMI composite treated with the BMI wet peel ply exhibited good bonding stability with a coefficient of variation of 3.9. After damp-heat aging for 1440 h, the retention rate of shear strength at room-temperature was 82.3%. The relatively loosely woven carrier in the BMI wet peel ply increased the surface roughness of the composite, thus improving the bonding strength.
Open AccessSurface Treatment of Composites with Bismaleimide Resin-Based Wet Peel Ply for Enhanced Adhesive Bonding Performance
Surface treatment is typically required to improve the bonding performance of carbon-fiber-reinforced composites. Herein, a wet peel ply was prepared using bismaleimide (BMI) resins as a matrix resin. The temperature–heating rate extrapolation method and rheological method were employed to study the reaction characteristics and viscosity-temperature characteristics of the matrix in the BMI wet peel ply. The curing temperatures of the BMI wet peel ply and the BMI prepreg were the same (200 °C), making this wet peel ply suitable for co-curing with the BMI prepreg. After treatment with the wet peel ply, the bonding strength of the BMI composite joint showed a mean shear strength of 35.5 MPa, which was 1.72% higher than that of the sanded composite and 17.5% higher than that of the composite treated with the dry peel ply. In addition, the BMI composite treated with the BMI wet peel ply exhibited good bonding stability with a coefficient of variation of 3.9. After damp-heat aging for 1440 h, the retention rate of shear strength at room-temperature was 82.3%. The relatively loosely woven carrier in the BMI wet peel ply increased the surface roughness of the composite, thus improving the bonding strength.